The nickel alloys have a chemical composition with high tenor of alloy elements which are responsible for the material's mechanical and thermal properties, but also are the main causative of problems during the machining, making the process difficult. The objective of this work is the study of the machining by external cylindrical turning of the nickel based alloy Nimonic 80A, seeking the machining optimization of this alloy, seeking the best condition of lubricant fluid use, providing real increases of productivity without the need of investments in new production means. Besides, the results of this work should offer more detailed information regarding the behavior of this alloy in relation to machining by turning. The machining experiences were accomplished in a specimen of the nickel alloy, considering the machining parameters: cutting speed (75 and 90 m/min), cutting depth (0,8 mm) and feed rate (0,15 and 0,18 mm/v). The valuations were accomplished in a CNC lathe and tools with of hard metal inserts. After each stage of the turning the measures of the cutting length were accomplished, of the waste of the tools through a magnifying glass (8x) and the roughness of the specimen evaluated in each phase of the process, with the aid of a portable roughness meter. Through light optical microscopy it was possible to observe the wear of the cutting tools for each appraised condition. The roughness values, Ra and Ry, for the appraised conditions were always superiors to the theoretical values. After analysis of the results it was possible to end that, the best acting for this work strip tested it was obtained for ap=0,8mm: f=0,15mm/rev and VC=75m/min, what resulted in a larger cutting length (1811 m)

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Being the corrosion one of the great problems facing the industry today, specifically the internal corrosion of pipes in chemical and petrochemical industries, hence this work proposes a new type of internal coating in order to avoid fouling and decrease the pressure loss in the flow. For this, we use a composition of vinyl ester resins and manometric loads, which after cleaning and preparation of the internal surface of the tube will be applied through a process of centrifugation, adjusted by a lathe. After curing the resin, a test of roughness will be realized in order to analyze the reduction of friction factor and thus be able to conclude whether there was a significant decrease in pressure drop. With test results in hand, we hope to obtain a coating that meets most of the properties required by the industry and to provide a reduction in operating costs and a visible improvement in the conditions of use of the pipe

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The machining of super alloys resistant to high temperatures such as nickel alloys, inconel 718 specifically, is a very difficult job to obtain improvements in the process, due to the difficulty of machining at high cutting speeds, the use of these alloys in industries showed great developments in recent years, its application in aeronautical industry spread being used in vane turbo, compressor parts, props and set elements. The automotive, chemical, medical and others also took advantage of the great features of inconel 718 and has used the material. The high temperature resistant alloys have high machining difficulty, a fact that is associated with high cutting forces generated during machining which result in high temperatures. High levels of temperatures can cause deterioration of the cutting edge, with subsequent deformation or breakage, wear most common obtained in machining such materials are flank wear the formation of built-up edge for cutting and notch wear. The experimental part of the work consists in machining of nickel-based alloy Inconel 718 heat treated for hardness, using a tool based ceramic silicon nitride Sandvik (Si3N4) in order to compare the best results obtained in the master's thesis of SANTOS (2010) who used a tool ceramics also the basis of silicon nitride which was developed in the doctoral thesis of SOUZA (2005). Assays were performed on a CNC lathe and was noted for each cutting edge results obtained. Tests were made starting from an initial condition of the tool with cutting speed of 200 m/min, feed 0.5 mm and 0.5 mm depth of cut was reduced cutting speed for the subsequent tests with the same conditions of feed and depth of cut. The tool presented wear instant under two 200 m/min and 100 m/min, premature rupture of 50 m/min and finally cut provided with difficulty... (Complete abstract click electronic access below)

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Pós-graduação em Engenharia Mecânica - FEIS

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The aim of this study was to evaluate the internal fit, marginal adaptation, and bond strengths of inlays made of computer-aided design/computer-aided manufacturing feldspathic ceramic and polymer-infiltrated ceramic. Twenty molars were randomly selected and prepared to receive inlays that were milled from both materials. Before cementation, internal fit was achieved using the replica technique by molding the internal surface with addition silicone and measuring the cement thicknesses of the pulpal and axial walls. Marginal adaptation was measured on the occlusal and proximal margins of the replica. The inlays were then cemented using resin cement (Panavia F2.0) and subjected to two million thermomechanical cycles in water (200 N load and 3.8-Hz frequency). The restored teeth were then cut into beams, using a lathe, for microtensile testing. The contact angles, marginal integrity, and surface patterns after etching were also observed. Statistical analysis was performed using two-way repeated measures analysis of variance (p<0.05), the Tukey test for internal fit and marginal adaptation, and the Student t-test for bond strength. The failure types (adhesive or cohesive) were classified on each fractured beam. The results showed that the misfit of the pulpal walls (p=0.0002) and the marginal adaptation (p=0.0001) of the feldspathic ceramic were significantly higher when compared to those of the polymer-infiltrated ceramic, while the bond strength values of the former were higher when compared to those of the latter. The contact angle of the polymer-infiltrated ceramic was also higher. In the present study, the hybrid ceramic presented improved internal and marginal adaptation, but the bond strengths were higher for the feldspathic ceramic.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Pós-graduação em Odontologia Restauradora - ICT

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Machining processes are one of the most important manufacturing processes in the modern world. In these processes, there are many elements which will influence in the final result of the machined part. Among them, the tools are the principal factor of the rising cost, because its global influence on the process. In aeronautical industries, this can be more evidenced due the need to machining several alloys, between them, aluminum alloys. These alloys have to demonstrate a specific surface finishing to be used in aircraft's fuselage. This kind of industry is one of the segments which is still rising in Brazil, and they are looking viable alternatives in the manufacturing processes of materials, due the need to produce more and more parts and equipment, with costs increasingly reduced. The purpose of this project is the development of a ceramic with differentiated properties. The ceramics were developed using a pre-sintering at 1200 °C, with posterior sintering at 1600°C, and subjected to dry turning process on aluminum alloy 6005. The characterizations showed that ceramics presented with toughness on the center of 1700 MPa and on the surface of 1950 MPa, density 98,5 ±0,14. g/cm³. Ceramics were grinded and faceted, according to ISO standard 1832, and subjected to turning tests in a ROMI lathe brand, model GL240M, using cutting speeds of 500, 800 and 1000 m/min with different feed rates. The machining results showed low occurrence of flank wear to all cutting speeds, and better surface finishing average values of Ra = 0,4935 μm and Rt = 8,112 μm. In general, it could be seen that the tool presents important potential to machining 6005 alloy, and that the use of correct parameters can decrease and/or eliminate subsequent processes, providing important reductions in costs related to the machining processes