262 resultados para IPS Empress ceramic


Relevância:

90.00% 90.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Pós-graduação em Reabilitação Oral - FOAR

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Pós-graduação em Odontologia Restauradora - ICT

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Pós-graduação em Ciências Odontológicas - FOAR

Relevância:

90.00% 90.00%

Publicador:

Resumo:

The aim of this study was to evaluate the surface roughness of 5 indirect restorative materials treated with hydrofluoric acid to 10%, with aluminum oxide jet and a combination of both. The specimens was prepared with 10 mm in diameter and 2 mm thickness, divided into fi ve groups: (1) Ceromer (CeseadII-Kuraray), (2) Leucite crystals ceramics (IPS EmpressIIIvoclarforcasket), (3) glass ceramic with fluorapatite (IPS D. Sign-Ivoclar), (4) lithium disilicate ceramic (IPS Empress II-Ivoclar restorations), (5) ceramics (Cergogold-Degussa). For all groups were performed the controls, and the surfaces with the 3 types of treatment. For testing roughness used the rugosimeter Taylor/Hobson-Precision, model form tracerSV-C525 high sensitivity. After confi rmation of variance analysis with a signifi cance level of 1% (p < 0.01), there was equality between the average roughness of materials from groups 1, 3 and 5, and the group 2 was different from the others. It was also found that the ceramics of the group 5 behaved similar to group 4. However the lowest average roughness was observed in group 2 ceramic. In the evaluation between the types of treatment, the aluminum oxide jet and associations and blasting with hydrofl uoric acid were similar, and different isolated hydrofl uoric acid, and 3 types of treatment signifi cantly higher than the control group. All treatments promoted superfi cial alterations in all tested materials.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The purpose of this study was to evaluate in vitro the shear bond strenght to bovine dentin, during 24h and 30 days with the following variables: resin cements Enforce and Panavia F; aesthetics restorative materials Art Glass, IPS Empress 2 and Targis, with surface treatment with microetching with aluminium oxide, fluoridric acid and silane. Two hundred eighty eight sound bovine teeth from 3 years old animals constituted the samples after inclusion on polyester resin box. lnstron model 430 Universal Testing Machine, a crosshead speed 0,5 mm/min and load cells of 500 Kg, was used for shear bond strenght testing (MPa). The results were statistically analysed by ANOVA The best result was obtained with /PS Empress 2, microetched with aluminium oxide, fluoridric acid and silane, cemented with Panavia F and stored in distilled water, 3f'C during 30 days

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Statement of problem. Different combinations of Co-Cr alloys bonded to ceramic have been used in dentistry; however, the bond strength of ceramic to metal can vary because of different compositions of these alloys.Purpose. The purpose of this study was to evaluate the shear bond strength of a dental ceramic to 5 commercially available Co-Cr alloys.Material and methods. Five Co-Cr alloys (IPS d.SIGN 20, IPS d.SIGN 30, Remanium 2000, Heranium P, and Wirobond C) were tested and compared to a control group of an Au-Pd alloy (Olympia). Specimen disks, 5 mm high and 4 mm in diameter, were fabricated with the lost-wax technique. Sixty specimens were prepared using opaque and dentin ceramics (VITA Omega 900), veneered, 4 mm high and 4 mm in diameter, over the metal specimens (n = 10). The shear bond strength test was performed in a universal testing machine with a crosshead speed of 0.5 mm/min. After shear bond testing, fracture surfaces were evaluated in a stereomicroscope under x25 magnification. Ultimate shear bond strength (MPa) data were analyzed with 1-way ANOVA and the Tukey HSD test (alpha = .05).Results. The mean (SID) bond strengths (MPa) were: 61.4 (7.8) for Olympia; 94.0 (18.9) for IPS 20; 96.8 (10.2) for I PS 30; 75.1 (12.4) for Remanium; 71.2 (14.3) for Heranium P; and 63.2 (10.9) for Wirobond C. Mean bond strengths for IPS 20 and IPS 30 were not significantly different, but were significantly (P<.001) higher than mean bond strengths for the other 4 alloys, which were not significantly different from each other.Conclusions. Bond strength of a dental ceramic to a Co-Cr alloy is dependent on the alloy composition.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Purpose: Existing composite restorations on teeth are often remade prior to the cementation of fixed dental prostheses. The aim of this study was to evaluate the effect of static and cyclic loading on ceramic laminate veneers adhered to aged resin composite restorations.Materials and Methods: Eighty sound maxillary incisors were collected and randomly divided into four groups: group 1: control group, no restorations; group 2: two Class III restorations; group 3: two Class IV restorations; group 4: complete composite substrate. Standard composite restorations were made using a microhybrid resin composite (Anterior Shine). Restored teeth were subjected to thermocycling (6000 cycles). Window preparations were made on the labial surface of the teeth for ceramic laminate fabrication (Empress II). Teeth were conditioned using an etch-and-rinse system. Existing composite restorations representing the aged composites were silica coated (CoJet) and silanized (ESPE-Sil). Ceramic laminates were cemented using a bis-GMA-based cement (Variolink Veneer). The specimens were randomly divided into two groups and were subjected to either static (groups 1a, 2a, 3a, 4a) or cyclic loading (groups 1b, 2b, 3b, 4b). Failure type and location after loading were classified. Data were analyzed using one-way ANOVA and Tukey's test.Results: Significantly higher fracture strength was obtained in group 4 (330 +/- 81 N) compared to the controls in group 1 (179 +/- 120 N) (one-way ANOVA, p < 0.05). Group lb survived a lower mean number of cyclic loads (672,820 cycles) than teeth of groups 2b to 4b (846x10(3) to 873x10(3) cycles). Failure type evaluation after the fracture test showed predominantly adhesive failures between dentin and cement, but after cyclic loading, more cohesive fractures in the ceramic were seen.Conclusion: Ceramic laminate veneers bonded to conditioned aged composite restorations provided favorable results. Surface conditioning of existing restorations may eliminate the necessity of removing aged composite restorations.