50 resultados para GC pit
Resumo:
Organotin compounds, largely used as biocides in antifouling paints, are among the most toxic materials introduced into the aquatic environment. Sensitive analytical methods are thus required to characterize their occurrence in environmental and biological matrices. The comparison between two different photometric detectors in terms of analytical performance was carried out for the analysis of organotin compounds. A flame photometric detector (FPD) and a pulsed flame photometric detector (PFPD) were optimized. Their respective sensitivity, linearity range and selectivity were evaluated. Limits of detection obtained for a tributyltin compound (TBT) were 5.0 and 0.9 pg (as Sn) for the FPD and PFPD, respectively, using a 390 nm filter. The PFPD showed higher selectivity, besides reduced gas consumption in the flame, and is very attractive for organotin compound speciation in complex environmental matrices.
Resumo:
Metallographic techniques and digital image processing have been used to investigate heat-treated Ti-6Al-4V pitting corrosion, often used as aircraft components. LM and SEM metallography of 'as received', annealed (heating up to 800 degreesC/30 min and cooling furnace) and aged (heating up to 900 degreesC/30 min, quenching in water, heating up to 540 degreesC/240 min and again water-quenched) microstructures reveal pitting sites at primary and secondary alpha/beta interfaces. Microstructural arrangements influence and corrosive environment association on pit morphology could be demonstrated by digital image analysis and results statistical treatment. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
In this communication we report a proof of concept study of the use of cyclic voltammetry with a polyeugenol-modified glassy carbon (GC) electrode to selectively detect L-cysteine in the presence of both DL-homocysteine and glutathione in perchloric acid. The formation of a polyeugenol-modified gold electrode is also reported for the first time.
Resumo:
The aim of this study was to clinically evaluate fluoride-containing sealants in teeth subjected to minimal enamel reduction (preventive resin restorations). Two hundred fourteen sealants (109 Fluro Shield and 105 Delton Fluor) were applied in 153 teeth of 32 subjects. The sealants were evaluated for superficial irregularities, marginal adaptation, retention, and caries after 6, 12, 18, and 24 months. After 6, 12, and 18 months, the attendance at recall was 100.00%. After 24 months, 93.75% of subjects returned for reevaluation. Although total or partial loss of sealant occurred in a few instances, no occlusal caries was found in any tooth at any recall. No statistically significant differences in the results of the clinical evaluation were found between sealant in the maxillary and mandibular dentitions.
Resumo:
This study evaluated the microleakage of pit and fissure sealants after different surface preparation (invasive technique and laser irradiation) and the use of different materials (fluoride resin-filled sealant, resin-modified glass ionomer cement and adhesive system). Eighty-four pre molars were used in this study, which were divided into seven groups. After the accomplishment of the different treatments, these were submitted to thermocycling process and assess for microleakage by examination under an epifluorescent microscope and scored zero to seven. Two specimens of each group were observed under scanning electron microscope (SEM). The results showed that laser irradiation did not lessen microleakage in pit and fissures when using a filled-resin sealant with fluoride or a resin-modified glass ionomer cement. The use of laser irradiation and adhesive system, followed by a resin-filled sealant with fluoride, showed the lowest microleakage scores in pit and fissures. Comparing this group to the resin-modified glass ionomer cement group, there was statistical significance. The use of a adhesive system decreased microleakage when using a fluoride resin-filled sealant with or without previous laser irradiation; although it was not statistically significant.
Resumo:
The aim of this paper was to apply a multiresidue method using Supercritical Fluid Extraction (SFE) and capillary gas chromatography with electron capture and mass spectrometry detections in the analysis of the levels of pesticide residues in fruits and vegetables. Single laboratory validation of both solid-liquid and supercritical fluid extraction methods was carried out for 32 compounds selected from four pesticide classes (organochlorine, organonitrogen, organophosphorus and pyretroid) in blank and fortified samples of fresh lettuce, potato, apple and tomato. Recoveries for the majority of pesticides from fortified samples at fortification level of 0.04-0.10 mg kg -1 ranged 74-96% for both methods and confirmation of pesticide identity was performed by gas-chromatography-mass spectrometry in a selected-ion monitoring mode. Both methods showed good limits of detection (less 0.01 mg kg-1, depending on the pesticide and matrix) and the SFE method minimized environmental concerns, time, and laboratory work. ©2005 Sociedade Brasileira de Química.
Resumo:
It has been characterized and evaluated the 2024-T351 and 7050-T7451 aluminum alloys pitting corrosion in naturally aerated chloride aqueous solutions containing chromate, molybdate and tungstate. It has been carried out electrochemical and non-electrochemical immersion corrosion tests accompanied by surface metallography analysis using an optical microscopy. Chromate for the two alloys and in molybdate for 7050 has corrosion inhibiting effects, whereas tungstate promotes the pitting corrosion for these alloys. Quantitative surface analysis upon the alloys after immersion has indicated that pits are predominantly conical or quasi-conical and irregular. In general, pits have been wider than deep and the widest have been also the deepest. Despite inhibitor presence, when pits have been nucleated, they grow with the same intensity. © 2005 Elsevier B.V. All rights reserved.
Resumo:
The purpose of this study was to employ photographic evaluation to observe the presence or absence of bubbles in pit and fissure sealants Concise and Prisma Shield, at 7 days, 18 months, 36 months and 11 years after accomplishment of treatment. Methods: A hematoxylin-based staining solution was applied to the occlusal surface at the study periods, which allowed assessment of the sealing material on the surface. All occlusal surfaces were photographed and the photographs corresponding to each period were subjected to photographic evaluation. Results: There was statistically significant difference only at 18 months, with a significantly higher number of specimens with bubbles for the Prisma Shield sealant compared to the Concise, whereas the groups were similar at all other study periods. On the other hand, separate analysis of subsequent periods of the sealants did not reveal any significant difference. Conclusions: According to the results of the present longitudinal investigation, it may be concluded that the sealing materials showed that bubbles came into and went out with time. However, this fact did not interfere with its clinical purpose, provided the remaining material covers the expected region of pits and fissures.
Resumo:
A study on the presence of herbicides, namely simazine, metribuzin, metolachlor, trifluralin, atrazine and two metabolites, deisopropylatrazine (DIA) and deethylatrazine (DEA), was performed in ground and surface waters from Primavera do Leste region, Mato Grosso state (Middle West of Brazil). The analytical procedure was based on solid-phase extraction (SPE) with Sep-Pak C18 disposable cartridges and ethyl acetate for elution solvent. Residue levels were determined by gas chromatography with nitrogen-phosphorus detection. For most of the pesticides average recoveries at different fortification levels were >with relative standard deviation < The recoveries of DIA and trifluralin in water were 25% and 56%, respectively, which were attributed to the incomplete retention of DIA and strong retention on the sorbing material and high volatility of trifluralin. Detection limits ranged from 0.023 to 0.088 μg L-1. This method was applied for the analysis of 5 superficial water samples and 28 groundwater samples, in places used for human consumption without previous treatment, collected in Primavera do Leste, Mato Grosso, Brazil. Results indicated that the highest level of contamination in a water sample was 1.732 μg L-1 for metolachlor, while metribuzin was the most frequently detected herbicide with maximum concentration of 0.351 μg L-1. ©2006 Sociedade Brasileira de Química.
Resumo:
PURPOSE: To investigate the penetration (tags) of adhesive materials into enamel etched with phosphoric acid or treated with a self-etching adhesive, before application of a pit-and-fissure sealant. MATERIALS AND METHODS: The sample comprised six study groups with six specimens each. Before pit-and-fissure sealing with the materials Clinpro SealantTM (Groups I and II), Vitro Seal ALPHA (Groups III and IV) and Fuji II LC (Groups V and VI), the teeth in Groups I, III, and V were etched with 35% phosphoric acid for 30 seconds. Teeth in Groups II, IV, and VI received application of the self-etching adhesive Adper Prompt L-Pop. The treated teeth were sectioned buccolingually, ground to 100-microm thickness, decalcified, and analyzed by conventional light microscopy at 400x magnification. RESULTS: The teeth etched with phosphoric acid exhibited significantly greater penetration than specimens treated with self-etching adhesive. CLINICAL SIGNIFICANCE: When compared with enamel treated with a self-etching adhesive, the penetration (tags) of adhesive materials into enamel was greater when applied on enamel etched with phosphoric acid.
Resumo:
The use of inks containing organic solvents by the offset printing process implies in the release of volatile organic compounds to the work environment. Many of these compounds such as benzene, toluene, ethylbenzene, and the xylene isomers (well known by the acronym BTEX) are extremely toxic. In this study, the BTEX concentrations were determined in two different printing plants that use distinct types of inks: the conventional and the so-called ecological, which is manufactured based on vegetal oil. Concentration ranges were 43-84, 15-3,480, 2-133, 5-459, and 2-236 μg m-3 for benzene, toluene, ethylbenzene, m + p-xylene, and o-xylene, respectively, for the conventional printing plant. At the ecological printing plant, concentration ranges were below limit of detection (
Resumo:
Twenty years of investigations on the use of pit and fissure sealants are presented with emphasis on application techniques, types of materials and long-term follow-up. After two decades of routine provision of pit and fissure sealants, we are able to conclude that placement of bonded resin sealant material is a highly effective approach for prevention of pit and fissure caries, provided the sealant material is correctly applied. © 2009 Nova Science Publishers, Inc.
Resumo:
Objective: To analyze the effects of thermal cycling on the microtensile shear bond strength of a self-etching and a conventional pit and fissure sealants to dental enamel. Material and Method: Twenty-four healthy human molars extracted for orthodontic reasons, were sectioned in the mesio-distal direction and divided into two groups (n=24) according to the sealant to be applied: GI - conventional sealant Climpro (3M/ESPE) and GII - self-etching sealant Enamel Loc (Premier Dental). The sealants were applied on flattened enamel in matrixes 1 mm in diameter, in accordance with the manufacturers' recommendations. The specimens were stored in distilled water at 37°C for 24 hours. After this, half the samples of both groups were submitted to 500 thermal cycles in 30s baths at temperatures between 5 and 55°C. Forty-eight hours after the samples were made, the microtensile shear test was performed in an Instron 4411 test machine, with a stainless steel wire with a cylindrical cross section of 0.2mm in diameter at a constant speed of 0.5mm/s. The bond strength values were submitted to ANOVA for 2 factors and the fracture patterns were examined under an optical microscope at 65X magnification. Results: Thermal cycling did not influence the bond strength of the two sealants. The conventional sealant Climpro presented a statistically higher microtensile shear bond strength (11.72MPa, 11.34MPa with and without cycling, respectively) than the self-etching sealant Enamel Loc (5.92MPa, 5.02MPa with and without cycling, respectively). Fracture pattern analysis showed the occurrence of 100% of adhesive failures for Enamel Loc, while the conventional sealant Climpro presented 95% of adhesive failures and 5% of mixed failures. Conclusion: The conventional sealant presented higher microtensile shear bond strength to dental enamel in comparison with the self-etching sealant. Thermal cycling did not affect the bond strength of the sealants used in this study. © 2011 Nova Science Publishers, Inc.