59 resultados para Dimensional stability
Resumo:
The aim of this study was to evaluate the dimensional stability and detail reproduction of two silicones used for facial prosthesis, under the influence of chemical disinfection and storage time. Twenty-eight test specimens were obtained, half made of Silastic MDX 4-4210 silicone, and the other half of Silastic 732 RTV silicone. The test specimens were divided into 4 groups: Silastic 732 RTV and Silastic MDX 4-4210, with disinfection 3 times a week with Efferdent and without disinfection. Dimensional change was analyzed using an electronic comparison microscope and detail reproduction was observed under a stereo microscope, immediately and 2 months after the test specimens were made. Once the results were obtained, an analisis of variance (ANOVA) was applied, followed by the Tukey's Test with 1% confidence. The storage time factor had a statistical influence on dimensional stability: Silastic MDX 4-4210 had less contraction than Silastic 732 RTV. Chemical disinfection did not significantly alter the dimensional stability of the materials used. Regarding detail reproduction, no alteration of values was observed in any of the materials analyzed, regardless of storage period or disinfection.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Pós-graduação em Odontologia - FOA
Resumo:
Pós-graduação em Odontologia - FOA
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Nowadays, bamboo is being studied because of their strength properties according with their specific mass and speed of growth, which makes it an important alternative as a new resource that will help reduce pressure on forests and helpping them favoring the minimization of uncontrolled deforestation in many regions of Brazil. This study aimed, in general, to analyze physical and mechanical properties of the material with the divulgation of its potential for industrial application. To do so, in this research were determined in relation to the physical properties, moisture content, dimensional stability and the apparent densities and the mechanics and basic, just a tension parallel to grain, in order to observe the interference of various kinds of treatments (chemical, thermal and natural) on the strength and modulus of elasticity in this request. The species used was the Guadua angustifolia, a species native of Brazil. All tests were performed at Universidade Estadual Paulista - Campus Experimental Itapeva in the laboratory of Materials Properties. The methodology used for testing of moisture, density and tension parallel to grain were based on NBR 7190/1997 for the wood, and dimensional stability tests were based on much the same as in COPANT 462/1972 (South American) . The preservative treatments conducted followed the recommendation of each manufacturer. The values obtained in tests of physical properties were satisfactory especially with respect to density and dimensional stability analyzed by the coefficient of anisotropy, showed that, compared to wood, excellent quality for the shrinkage test, obtaining a coefficient of 1.2. With respect to parallel tensile tests to fibre results showed, in most cases, that test specimens with the presence of us have lower values of resistance and modulus of elasticity when compared with those without us. In the treatment of thermal-treatment there was an apparent treatment there was an apparent increase in...
Resumo:
Objective:This study investigated the efficacy of different techniques for the union of fragments of a denture before repair and on the accuracy of the reposition.Materials and methods:For this study, 20 maxillary dentures made with Lucitone 550 heat-cured resin were used. Points were determined with a scanner on the cusp of the teeth, as a measurement of the segments. After digitisation, each model was exported to the AUTOCAD R 14 program and two-dimensional measurements of the distances between the marked points were made. After the initial analysis, the dentures were fractured into two segments using an impact test machine. For the repair, maxillary dentures were divided into two groups; in the first, the repair was carried out using Kerr's sticky wax and in the second group, Super Bonder was used to join the fragments, with subsequent inclusion of DENTSPLY((R)) Repair Material resin. After the repair, the points of the maxillary dentures were measured again. The numerical values obtained were tabulated to compare the measurements before fracture and after the repair. For statistical analysis, analysis of variance was employed, using a single factor and double factor, followed by the Tukey test with a reliability of 95%.Results:The results demonstrated a statistically significant difference between the materials used to join the dentures for repair, where the dentures were joined with sticky wax presented a larger variation in the distances between the points.Conclusion:The variation in distances between the points is influenced by the agent of repair.
Resumo:
Denture fractures are common in daily practice, causing inconvenience to the patient and to the dentists. Denture repairs should have adequate strength, dimensional stability and color match, and should be easily and quickly performed as well as relatively inexpensive. Objective: The aim of this study was to evaluate the flexural strength of acrylic resin repairs processed by different methods: warm water-bath, microwave energy, and chemical polymerization. Material and methods: Sixty rectangular specimens (31x10x2.5 mm) were made with warm water-bath acrylic resin (Lucitone 550) and grouped (15 specimens per group) according to the resin type used to make repair procedure: 1) specimens of warm water-bath resin (Lucitone 550) without repair (control group); 2) specimens of warm water-bath resin repaired with warm water-bath; 3) specimens of warm water-bath resin repaired with microwave resin (Acron MC); 4) specimens of warm water-bath resin repaired with autopolymerized acrylic resin (Simplex). Flexural strength was measured with the three-point bending in a universal testing machine (MTS 810 Material Test System) with load cell of 100 kgf under constant speed of 5 mm/min. Data were analyzed statistically by Kruskal-Wallis test (p<0.05). Results: The control group showed the best result (156.04 +/- 1.82 MPa). Significant differences were found among repaired specimens and the results were decreasing as follows: group 3 (43.02 +/- 2.25 MPa), group 2 (36.21 +/- 1.20 MPa) and group 4 (6.74 +/- 0.85 MPa). Conclusion: All repaired specimens demonstrated lower flexural strength than the control group. Repairs with autopolymerized acrylic resin showed the lowest flexural strength.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
We have developed a biodegradable composite scaffold for bone tissue engineering applications with a pore size and interconnecting macroporosity similar to those of human trabecular bone. The scaffold is fabricated by a process of particle leaching and phase inversion from poly(lactide-co-glycolide) (PLGA) and two calcium phosphate (CaP) phases both of which are resorbable by osteoclasts; the first a particulate within the polymer structure and the second a thin ubiquitous coating. The 3-5 mu m thick osteoconductive surface CaP abrogates the putative foreign body giant cell response to the underlying polymer, while the internal CaP phase provides dimensional stability in an otherwise highly compliant structure. The scaffold may be used as a biomaterial alone, as a carrier for cells or a three-phase drug delivery device. Due to the highly interconnected macroporosity ranging from 81% to 91%, with macropores of 0.8 similar to 1.8 mm, and an ability to wick up blood, the scaffold acts as both a clot-retention device and an osteoconductive support for host bone growth. As a cell delivery vehicle, the scaffold can be first seeded with human mesenchymal cells which can then contribute to bone formation in orthotopic implantation sites, as we show in immune-compromised animal hosts. We have also employed this scaffold in both lithomorph and particulate forms in human patients to maintain alveolar bone height following tooth extraction, and augment alveolar bone height through standard sinus lift approaches. We provide a clinical case report of both of these applications; and we show that the scaffold served to regenerate sufficient bone tissue in the wound site to provide a sound foundation for dental implant placement. At the time of writing, such implants have been in occlusal function for periods of up to 3 years in sites regenerated through the use of the scaffold.
Resumo:
Aim: To evaluate the physicochemical and mechanical properties of Portland cement-based experimental sealers (ES) with different radiopacifying agents (zirconium oxide and niobium oxide micro- and nanoparticles) in comparison with the following conventional sealers: AH Plus, MTA Fillapex and Sealapex. Methodology: The materials were tested for setting time, compressive strength, flow, film thickness, radiopacity, solubility, dimensional stability and formaldehyde release. Data were subjected to anova and Tukey tests (P < 0.05). Results: MTA Fillapex had the shortest setting time and lowest compressive strength values (P < 0.05) compared with the other materials. The ES had flow values similar to the conventional materials, but higher film thickness (P < 0.05) and lower radiopacity (P < 0.05). Similarly to AH Plus, the ES were associated with dimensional expansion (P > 0.05) and lower solubility when compared with MTA Fillapex and Sealapex (P < 0.05). None of the endodontic sealers evaluated released formaldehyde after mixing. Conclusion: With the exception of radiopacity, the Portland cement-based experimental endodontic sealers presented physicochemical properties according to the specifications no 57 ANSI/ADA (ADA Professional Product Review, 2008) and ISO 6876 (Dentistry - Root Canal Sealing Materials, 2012, British Standards Institution, London, UK). The sealers had setting times and flow ability that was adequate for clinical use, satisfactory compressive strength and low solubility. Additional studies should be carried out with the purpose of decreasing the film thickness and to determine the ideal ratio of radiopacifying agents in Portland cement-based root canal sealers. © 2013 International Endodontic Journal.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)