We have investigated, by in situ small-angle X-ray scattering (SAXS), the kinetics of formation of zinc oxide colloidal suspensions obtained after refluxing alcoholic solution of zinc acetate and catalysed by lithium hydroxide. The experimental results demonstrate that the suspensions are composed of colloidal spheroidal particles with a multimodal size distribution. The average radius of the main mode, approximately 2 nm, is invariant but the number of these basic particles continuously increases for increasing hydrolysis reaction time. The other two modes correspond to particles with average radii close to 6 and 10 nm, respectively. The larger particles are formed by coagulation of the smaller ones. (C) 1999 Elsevier B.V. B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Mössbauer spectroscopy was used to investigate the early aging stage of iron(III) hydroxide sols prepared by oxidation of Fe(CO)5 in ethanolic solution, followed by vacuum drying at room temperature. One sample was composed of amorphous particles, while two other samples were partially crystallized, either as a result of solvent change or of spontaneous aging. The main results of Mössbauer measurements in the 80-320 K temperature range are: (a) partially crystallized particles exhibit a strong, S-shaped temperature dependence of the quadrupole splitting, in contrast to a weak and linear variation for amorphous particles; (b) the recoilless fraction temperature dependence is affected by vibration of the particles as a whole, with an effective force constant which is smaller for crystallized particles than for amorphous ones. Furthermore, the former exhibit anf-factor discontinuity near 0°C, which is attributed to melting of a surface layer built up during the crystallization process. © 1986.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Pentacarbonyliron was oxidized with H2O2, in organic solvents, to give colloidal sols. The aqueous-ethanolic sol is highly stable and undergoes thermally-reversible coagulation. Its solid phase was found to be a non-crystalline Fe (III) hydroxoacetate which is transformed to α-Fe2O3 when heated to 300°C. Iron-bound acetate groups are assumed to have a major role in the sol stability, by preserving the amorphous solid phase. Dry hydroxoacetate particles were heated under vacuum; scanning electron microscopy revealed that these particles coalesce and grow, as in a sintering process but at low temperatures (100-250°). © 1987.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Transparent SnO2 gels were obtained from SnCl4 aqueous solution. The sol formation from tin oxihydroxy peptization in different concentrations and by electrolyte addition in solution was measured. It was verified that the residual presence of chloride ions compromises the colloidal system stability. The sol-gel transition was investigated as a function of the quantity of solid particles in the aqueous environment and of aging time at 60°C by infrared spectroscopy and rheological measurements. The transition from plastic to pseudoplastic flow observed with the increase in loading suggests that a continuous and three-dimensional network formation is closely related to hydrogen bridges and/or hydrogen clusters, culminating in the gel formation. © 1990.