Resumo:
The processing of ferroelectric BaBi4Ti4O15 (BBT) ceramics from powders prepared by conventional solid state reaction (SSR) and mechanochemical activation (MA) has been investigated. It was shown that MA synthesis reduces the synthesis temperature of BBT powders, leading to smaller particles with reduced anisotropy and consequently to smaller grain size of ceramics. Dielectric properties were investigated in a wide range of temperatures (20-800 degrees C) and frequencies (1.21 kHz to 1 MHz). The relative dielectric permittivity at Curie temperature was higher for solid state obtained ceramics than for the mechanically treated ones. The conductivity of sintered samples was studied, suggesting decreasing of conductivity of BBT-MA in comparison with BBT-SS ceramics. The influence of the grain and the grain boundaries contribution to the dielectric behavior in both ceramics was analyzed through impedance spectroscopy. A well-defined ferroelectric hysteresis loop was obtained for both samples. (C) 2014 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
Resumo:
To evaluate the effect of grinding and airborne-particle abrasion on the biaxial flexural strength (BFS) and phase transformation of a Y-TZP ceramic, and examine whether sintering the veneering porcelain renders the previous heat treatment recommended by the manufacturer unnecessary. Materials and Methods: Lava zirconia specimens (N = 108) were obtained with the following dimensions: 14.0 mm diameter × 1.3 mm thickness (n = 36) and 14.0 mm × 1.6 mm (n = 72). The thicker specimens were ground with diamond burs under irrigation and received (heat-treated groups) or not (non-heat-treated groups) a heat treatment (1000°C for 30 min) prior to the four firing cycles applied to simulate the sintering of the veneering porcelain. All specimens were air abraded as follows (n = 12): 1) 30-μm silica-modified Al2O3 particles (Rocatec Soft); 2) 110-μm silica-modified Al2O3 particles (Rocatec Plus); and 3) 120-μm Al2O3 particles, followed by Rocatec Plus. Three specimens of each group were analyzed by x-ray diffraction (XRD) to assess the monoclinic phase content (%). The BFS test was performed in a mechanical testing machine (Instron 8874). Data (MPa) were analyzed by two-way ANOVA (grinding × airborne-particle abrasion and heat treatment × airborne-particle abrasion) and Tukey's post-hoc test (α = 0.05). The strength reliability was analyzed using the Weibull distribution. Results: Grinding significantly decreased the BFS of the non-heat-treated groups (p < 0.01). Within the ground groups, the previous heat treatment did not influence the BFS (p > 0.05). Air abrasion only influenced the BFS of the ground/heat-treated groups (p < 0.01). For the non-heat-treated groups, the grinding did not decrease the Weibull modulus (m), but it did decrease the characteristic strength (σ0). For Rocatec Soft and 120-μm Al2O3 particles + Rocatec Plus, the heat-treated groups presented lower m and higher σ0 than the ground/non-heat-treated groups. The independent variables did not seem to influence phase transformation. Air-abraded surfaces presented higher monoclinic zirconia content than the as-sintered and ground surfaces, which exhibited similar content. Conclusion: Even under irrigation, grinding compromised the Y-TZP ceramic strength. The sintering of the veneering porcelain rendered the previous heat treatment recommended by the manufacturer unnecessary. Airborneparticle abrasion influenced the strength of heat-treated zirconia.
Resumo:
To evaluate the effect of grinding and airborne-particle abrasion on the biaxial flexural strength (BFS) and phase transformation of a Y-TZP ceramic, and examine whether sintering the veneering porcelain renders the previous heat treatment recommended by the manufacturer unnecessary. Materials and Methods: Lava zirconia specimens (N = 108) were obtained with the following dimensions: 14.0 mm diameter × 1.3 mm thickness (n = 36) and 14.0 mm × 1.6 mm (n = 72). The thicker specimens were ground with diamond burs under irrigation and received (heat-treated groups) or not (non-heat-treated groups) a heat treatment (1000°C for 30 min) prior to the four firing cycles applied to simulate the sintering of the veneering porcelain. All specimens were air abraded as follows (n = 12): 1) 30-μm silica-modified Al2O3 particles (Rocatec Soft); 2) 110-μm silica-modified Al2O3 particles (Rocatec Plus); and 3) 120-μm Al2O3 particles, followed by Rocatec Plus. Three specimens of each group were analyzed by x-ray diffraction (XRD) to assess the monoclinic phase content (%). The BFS test was performed in a mechanical testing machine (Instron 8874). Data (MPa) were analyzed by two-way ANOVA (grinding × airborne-particle abrasion and heat treatment × airborne-particle abrasion) and Tukey's post-hoc test (α = 0.05). The strength reliability was analyzed using the Weibull distribution. Results: Grinding significantly decreased the BFS of the non-heat-treated groups (p < 0.01). Within the ground groups, the previous heat treatment did not influence the BFS (p > 0.05). Air abrasion only influenced the BFS of the ground/heat-treated groups (p < 0.01). For the non-heat-treated groups, the grinding did not decrease the Weibull modulus (m), but it did decrease the characteristic strength (σ0). For Rocatec Soft and 120-μm Al2O3 particles + Rocatec Plus, the heat-treated groups presented lower m and higher σ0 than the ground/non-heat-treated groups. The independent variables did not seem to influence phase transformation. Air-abraded surfaces presented higher monoclinic zirconia content than the as-sintered and ground surfaces, which exhibited similar content. Conclusion: Even under irrigation, grinding compromised the Y-TZP ceramic strength. The sintering of the veneering porcelain rendered the previous heat treatment recommended by the manufacturer unnecessary. Airborneparticle abrasion influenced the strength of heat-treated zirconia.
Resumo:
Statement of problem Because airborne-particle abrasion is an efficient method of improving the bond at the zirconia-cement interface, understanding its effect on the strength of yttria-stabilized tetragonal zirconia polycrystal is important. Purpose The purpose of this study was to evaluate the effect of the particle size used for airborne-particle abrasion on the flexural strength and phase transformation of a commercially available yttria-stabilized tetragonal zirconia polycrystal ceramic. Material and Methods For both flexural strength (20.0 × 4.0 × 1.2 mm) (n=14) and phase transformation (14.0-mm diameter × 1.3-mm thickness) (n=4), the zirconia specimens were made from Lava, and their surfaces were treated in the following ways: as-sintered (control); with 50-μm aluminum oxide (Al2O3) particles; with 120-μm Al2O3 particles; with 250-μm Al2O3 particles; with 30-μm silica-modified Al2O3 particles (Cojet Sand); with 120-μm Al2O3 particles, followed by 110-μm silica-modified Al2O3 particles (Rocatec Plus); and with Rocatec Plus. The phase transformation (%) was assessed by x-ray diffraction analysis. The 3-point flexural strength test was conducted in artificial saliva at 37°C in a mechanical testing machine. The data were analyzed by 1-way ANOVA and the Tukey honestly significant difference post hoc test (α=.05). Results Except for the Cojet Sand group, which exhibited statistically similar flexural strength to that of the as-sintered group and for the group abraded with 250-μm Al2O3 particles, which presented the lowest strength, airborne-particle abrasion with the other particle sizes provided the highest values, with no significant difference among them. The as-sintered specimens presented no monoclinic phase. The groups abraded with smaller particles (30 μm and 50 μm) and those treated with the larger ones (110 μm and/or 120 μm particles and 250 μm) exhibited percentages of monoclinic phase that varied from 4% to 5% and from 8.7% to 10%. Conclusions Except for abrasion with Cojet Sand, depending on the particle size, zirconia exhibited an increase or a decrease in its flexural strength. Airborne-particle abrasion promoted phase transformation (tetragonal to monoclinic), and the percentage of monoclinic phase varied according to the particle size.
Resumo:
The effects of ambient nitrite concentrations on larval development of giant river prawn Macrobrachium rosenbergii were evaluated. The trials were conducted in two phases: phase 1, larvae from stages I through VIII and phase 2, larvae from stage VIII until post-larvae. In both phases larvae were kept in water with nitrite (NO2-N) concentrations of 0, 2, 4, 8 and 16 mg/L. Oxygen consumption was analyzed for larvae in stage II at nitrite concentrations of 0, 4, and 8 mg/L. Survival, weight gain, larval stage index and metamorphosis rate decreased linearly with increasing ambient nitrite concentration. However, there was no significant difference between larvae subjected to 0 and 2 mg/L NO2-N. In phase 1, there was total mortality at 16 mg/L NO2-N, while in phase 2 larval development stopped at stage X in this treatment. The oxygen consumption in stage II increased significantly at NO2-N concentration from 0 to 4 mg/L, but there was no difference between 4 and 8 mg/L NO2-N. In conclusion, increasing ambient nitrite up to 16 mg/L NO2-N delays larval development, reduces larval growth rate and causes mortality, whereas no significant effect occurs for levels below 2 mg/L NO2-N. However, the establishment of a general safe level of nitrite to M rosenbergii hatchery may be difficult due to the great variability in larvae individual sensitivity. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
The effects of intensification on growth, survival, productivity, population structure, and distribution of harvested biomass in individual size classes of Macrobrachium amazonicum in semi-intensive culture were evaluated. Postlarvae (0.01 g) were stocked in 12 ponds at densities of 10, 20, 40, and 80/m(2) (three replicates per treatment) and raised for 5.5 mo. Average individual weight significantly decreased and productivity significantly increased as stocking density increased (P < 0.001), while survival was not affected (P > 0.05). Prawn mean weight at harvest ranged from 3.6 (80/m(2)) to 7.0 g (10/m(2)). Average survival ranged from 65.5% (40/m(2)) to 72.8% (20/m(2)), while productivity ranged from 508 (10/m(2)) to 2051 kg/ha (80/m(2)). Harvested biomass showed a clear bimodal distribution in individual size classes indicating the occurrence of heterogeneous growth, which may affect management and market strategies. Harvested biomass of prawns weighing more than 7 g (the best market size) increases for stocking densities up to 40/m(2) and stabilizes between 40 and 80/m(2). Growth reduction was associated with a decreasing frequency and average weight of green claw 1 and green claw 2 male morphotypes and adult females as density increased. Thus, the distribution of male morphotypes and sexually mature females are affected by density-dependent factors. Results suggest that prawn density plays an important role on M. amazonicum grow-out phase, as has been demonstrated for other species of the genus Macrobrachium. M. amazonicum tolerates grow-out intensification and may be raised in both semi-intensive and intensive systems stocked at very high densities yielding high productivity.
Resumo:
O objetivo deste trabalho foi avaliar dietas contendo diferentes doses (0, 100, 200 e 300 ppm) de probiótico sobre a produção diária de fezes (PDF) e teor de macro e microminerais nas fezes de suínos, nas fases de creche e de crescimento e no período total. A PDF, como porcentagem do peso vivo, somente apresentou diferença estatística (P<0,05) na fase inicial 1. Os teores de macro e microminerais excretados nas fezes não apresentaram diferença (P>0,05) entre tratamentos, a exceção de cálcio e sódio na fase inicial 1 e cálcio, zinco e níquel no período total. A adição de um poliprobiótico às dietas, não afetou a produção de fezes dos suínos nas fases de creche e de crescimento. Entretanto, a presença de microrganismos, adicionados (níveis de 200 e 300 ppm) às dietas reduziu a excreção fecal de cálcio, zinco e níquel.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Sonicated mixtures of dimethyldioctadecylammonium chloride (DODAC), egg phosphatidylcholine (PC), dimyristoyl phosphatidylcholine (DMPC), and dipalmitoyl phosphatidylcholine (DPPC) were used to analyze vesicle effects on the rate of decarboxylation of 6-nitrobenzisoxazol-3-carboxylic acid (Nboc). Electron microscopic images of the vesicles were obtained with trehalose, a know cryoprotector. Phase diagrams and phase transitions temperatures of the vesicle bilayers were determined. Nboc decarboxylation rates increased in the presence of vesicles prepared with both phospholipids and DODAC/phospholipid mixtures. Quantitative analysis of vesicular effects was done using pseudophase models. Phospholipids catalyzed up to 140-fold while the maximum catalysis by DODAC/lipid vesicles reached 800-fold. Acceleration depends on alkyl chain length, fatty acid insaturation of the lipids, and the DODAC/phospholipid molar ratio. Catalysis is not related to the liquid crystalline-gel state of the bilayer and may be related to the relative position of Nboc with respect to the interface.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Titanium alloys normally contain oxygen, nitrogen, or carbon as impurities, and although this concentration is low, these impurities cause changes in the mechanical properties of Ti alloys. Oxygen is a strong alpha-phase stabilizer and its addition causes solid-solution strengthening, shape memory effect, and superelasticity. The most promising alloys are those with Nb, Zr, Ta, and Mo as alloying elements. In this paper, the preparation, processing, and characterization of Ti-Mo alloys (5 and 10 wt%) used as biomaterials are presented, along with the influence of oxygen on their mechanical properties. The addition of oxygen causes an increase in the elasticity modulus of the Ti-5Mo alloy due to an increase in the alpha' phase volume fraction, which possesses a higher modulus than the alpha '' phase. Ti-10Mo possesses a mixture between alpha '' and beta phases, oxygen enters these two structures and causes a dominating effect.
Resumo:
The FePt alloy undergoes the cubic to tetragonal lattice transformation in the ferromagnetic state. We calculated the electronic structure for both cubic and tetragonal structures using the FPLAPW method with APW + lo. Comparing the density of states of the cubic and tetragonal structures, it is expected that the lattice transformation is caused by the band Jahn-Teller effect. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
This paper presents a hybrid way mixing time and frequency domain for transmission lines modelling. The proposed methodology handles steady fundamental signal mixed with fast and slow transients, including impulsive and oscillatory behaviour. A transmission line model is developed based on lumped elements representation and state-space techniques. The proposed methodology represents an easy and practical procedure to model a three-phase transmission line directly in time domain, without the explicit use of inverse transforms. The proposed methodology takes into account the frequency-dependent parameters of the line, considering the soil and skin effects. In order to include this effect in the state matrices, a fitting method is applied. Furthermore the accuracy of proposed the developed model is verified, in frequency domain, by a simple methodology based on line distributed parameters and transfer function related to the input/output signals of the lumped parameters representation. In addition, this article proposes the use of a fast and robust analytic integration procedure to solve the state equations, enabling transient and steady-state simulations. The results are compared with those obtained by the commercial software Microtran (EMTP), taking into account a three-phase transmission line, typical in the Brazilian transmission system.