62 resultados para Aluminum-alloys
Resumo:
A 1000-kgf resistive strain-gauge load cell has been developed for quality testing of rocket propellant grain. A 7075-T6 aluminum alloy has been used for the elastic column, in which 8 uniaxial, 120-Ω strain gauges have been bonded and connected to form a full Wheatstone bridge to detect the strain. The chosen geometry makes the transducer insensitive to moments and, also, to the temperature. Experimental tests using a universal testing machine to imposed compression force to the load cell have demonstrated that its behavior is linear, with sensitivity of 2.90 μV/kgf ± 0.34%, and negligible hysteresis. The designed force transducer response to a dynamic test has been comparable to that of a commercial load cell. © 2005 IEEE.
Resumo:
The aluminum alloy 2524 (Al-Cu-Mg) was developed during the 90s mainly to be employed in aircraft fuselage panels, replacing the standard Al 2024. In the present analysis the fatigue crack growth (FCG) behavior of 2524-T3 was investigated, regarding the influence of three parameters: load ratio, pre strain and crack plane orientation of the material. The pre strain of aluminum alloys is usually performed in order to obtain a more homogeneous precipitates distribution, accompanied by an increase in the yield strength. In this work, it was evaluated the resistance of Al 2524-T3 sheet samples to the fatigue crack growth, having L-T and T-L crack orientations. FCG tests were performed under constant amplitude loading at three distinct positive load ratios. The three material conditions were tested: as received(AR), pre strained longitudinally (SL) and transversally (ST) in relation to rolling direction. In order to describe FCG behavior, two-parameter kinetic equations were compared: a Paris-type potential model and a new exponential equation introduced in a previous work conducted by our research group. It was observed that the exponential model, which takes into account the deviations from linearity presented by da/dN versus AK data, describes more adequately the FCG behavior of Al 224-T3 in relation to load ratio, pre strain effects and crack plane orientation. © 2011 Published by Elsevier Ltd.
Resumo:
In this work, the electrochemical behavior of Cu-16(wt.%)Zn-6.5(wt.%)Al alloy containing the β'-phase (martensite) was studied in borate buffer solution (pH 8.4) by means of open-circuit potential (EOC), electrochemical impedance spectroscopy (EIS) and cyclic voltammetry (CV). The alloy EOC was -0.29 V vs. Hg/HgO/OH-, similar to that of pure copper in this medium, indicating that the processes which occur on the alloy surface are mainly governed by copper. EIS response was related to the dielectric and transmission properties of the complex oxide layer. The CVs showed peaks concerning the redox reactions for copper and zinc. These peaks were assigned to the formation and reduction of copper and zinc species. Furthermore, they showed that the copper oxidation was suppressed by the presence of zinc and aluminum in the alloy composition. The copper and zinc oxidation to form complex oxide layers and the reduction of the different metallic oxides generated in the anodic potential scan suggest that a solid state reaction could determine the metallic oxide formation. © 2013 Elsevier Ltd. All rights reserved.
Resumo:
In this paper it is proposed a method to characterize the corrosion reactions of many metals and alloys in acid media and to evaluate the corrosion rate. An alloy of aluminum and zinc was partially dissolved in HCl solution and the medium acidity decrease was monitored at different time intervals by using a pHmeter. Data analysis and physical chemistry treatment permitted associate the pH increase with the alloy mass loss. This proposal promotes learning of terminology and concepts involved as well as contribute to better understand the corrosion phenomena.
Resumo:
Pós-graduação em Ciência e Tecnologia de Materiais - FC
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Pós-graduação em Engenharia Mecânica - FEG
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Pós-graduação em Engenharia Mecânica - FEG