246 resultados para PZT ceramics


Relevância:

20.00% 20.00%

Publicador:

Resumo:

The physical properties of self-polarized PbZr1-xTixO3 thin films with no preferential orientation in a range of compositions 0.46 <= x <= 0.50 were investigated. Structural analysis revealed the coexistence of monoclinic-tetragonal and monoclinic-rhombohedral phases at compositions 0.46 <= x <= 0.49, where the monoclinic phase was in the majority and both the tetragonal and the rhombohedral phases in the minority. The dielectric permittivity (epsilon'= 447) reached its maximum at around composition x = 0.48. Asymmetries in the macroscopic and local hysteresis loops confirmed the existence of the self-polarization effect in the studied films.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this work we present a Raman study of PbZr1-xTi xO3 ceramics with composition values close to the morphotropic phase boundary region. The analysis of the Raman spectra leads to the determination of the monoclinic phase extension at different temperatures in a very good agreement with those determined by diffraction techniques. Therefore the obtained results show that Raman spectroscopy is a powerful and suitable technique to study structural phase transitions in PbZr 1-xTixO3. © 2002 Taylor & Francis.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The Pb1-xLaxTiO3 sintered ferroelectric ceramics with x equal to 0, 0.10, 0.15, 0.20, and 0.30 were studied by X-ray photoelectron spectroscopy (XPS). The binding energy of the Ti 2p lines is consistent with only one chemical state, Ti4+. on the other hand, in the case of Pb 4f and 0 Is XPS spectra, apart from the main peaks attributed to the lattice ions, minor peaks related to the surface states were also observed. The presence of Pb-0 state on the surface of all samples was due to the reduction of lead ions caused by the preferential removal of the oxygen ions after sputtering. The non observation of Ti3+ ions confirms that the mechanism of charge compensation that should occurs owing to the substitution of Ph2+ by La3+ is due to the preferential formation of Pb site vacancies, and not to a reduction from Ti4+ to Ti3+ states. Within the limits of the present experiment, there is no evidence of the existence of non-equivalent Pb, Ti, and La sites as the Pb1-xLaxTiO3 ceramic changes from a normal to a relaxor ferroelectric state. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Precursor glass and glass-ceramics with molar composition 2Na2O·1CaO·3SiO2 are studied by infrared, conventional, and microprobe Raman techniques. The Gaussian deconvoluted Raman spectrum of the glass presents bands at 625 and 660 cm-1, attributed to bending vibrations of Si-O-Si bonds, and at 860, 920, 975, and 1030 cm-1, attributed to symmetric stretching vibrations of SiO4 tetrahedra with 4, 3, 2, and 1 nonbridging oxygens, respectively. The Raman microprobe spectrum of a highly crystallized sample presents two narrow and intense bands at about 590 and 980 cm-1, associated with vibrations of SiO4 tetrahedra with two nonbridging oxygens, in agreement with the predicted chain-like structure of crystalline metasilicates. Scanning electron microscopy shows that the crystals distributed in partially crystallized samples have a spherical shape, built up by radially oriented needle-like single crystals. The Raman microprobe spectra of these spherulites show that they still contain residual amorphous material. A comparison of Raman and infrared spectra of amorphous and highly crystallized samples is presented.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Cientifico e Tecnológico (CNPq)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

With the currently strict environmental law in present days, researchers and industries are seeking to reduce the amount of cutting fluid used in machining. Minimum quantity lubrication is a potential alternative to reduce environmental impacts and overall process costs. This technique can substantially reduce cutting fluids in grinding, as well as provide better performance in relation to conventional cutting fluid application (abundant fluid flow). The present work aims to test the viability of minimum quantity lubrication (with and without water) in grinding of advanced ceramics, when compared to conventional method (abundant fluid flow). Measured output variables were grinding power, surface roughness, roundness errors and wheel wear, as well as scanning electron micrographs. The results show that minimum quantity lubrication with water (1:1) was superior to conventional lubrication-cooling in terms of surface quality, also reducing wheel wear, when compared to the other methods tested.