The knowledge of the mechanical properties of nickel-titanium (NiTi) termoactives of the more accessible of the domestic market is still limited. Given this, the objective of this study was to evaluate and compare through deflection tests in brackets NiTi wires 03 term rectangular gauge 0.014 '' enabled x 0.025 '' and 0.016 '' x 0.022 '' of different brands (MORELLI (R), ORMCO (R) ORTHOSOURCE (R), ORTHOMETRIC (R), EURODONTO (R) and ADITEK (R)). All tests were carried out on universal testing machine EMIC DL 2000 under identical conditions and controlled at a temperature of 36 degrees C +/- 0.5 degrees C. Five measurements (N= 5) were performed for each thickness/wire tag that was deflected up to a limit of 4.0mm at a speed of 1.0mm/min. Each 0.2mm (round trip) of corresponding strength measured deflection for the construction of the graph of force x deflection at Tesc program version 3.04. Each graphic was evaluated according to the following variables: beginning of the Martensitic transformation (cN and mm), maximum strength (cN), the beginning and end of the plateau of deactivation (cN and mm) and length (mm) plateau. The average and standard deviation were calculated for all variables and statistical analysis was made by ANOVA tests 2 criteria and Turkey or Kruskal-Wallis and Dunn, a 5% level of significance. The results showed that the tests of 0.014 '' x0.025 '' ORTHOMETRIC (R) brands and ORMCO (R) showed the best results, as well as the wires of the MORELLI (R) and ORTHOSOURCE (R) to wires 0.016 '' x0.022 ''. In General, the gauge wires 0.014 '' x0.025 '' showed strength levels on the plateau of deactivation to 6 x smaller than 0.016 '' x0.022 '' caliber.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
This paper describes the preparation and complementary characterization of a composite formed from the activation of titanium isopropoxide by phosphoric acid and deionized water (TiP). Techniques such as, X-ray diffraction (XRD), Raman, electronic (UV-vis) and Scanning electron microscopies (SEM) were used for characterization of this new composite formed. In the X-ray diffractogram of TIP was observed four intense peaks. A strong absorption was observed in the region 362-445 nm. The scanning electron microscopy of TiP, shows that the prepared material consists mostly of a cluster of spherical particles with diameters ranging from 2.35 to 2.60 mu m.
Resumo:
Pós-graduação em Biopatologia Bucal - ICT
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Statement of problem. Removable partial dentures are affected by fatigue because of the cyclic mechanism of the masticatory system ansi frequent insertion and removal. Titanium and its alloys have been used in the manufacture of denture frameworks; however, preventive agents with fluorides are thought to attack titanium alloy surfaces.Purpose. This study evaluated, compared, analyzed the corrosion-fatigue life of commercially pure titanium and Ti-6Al-4V alloy in different storage environments.Material and methods. For each metal, 33 dumbbell rods, 2.3 mm in diameter at the central segment, were cast in the Rematitan system. Corrosion-fatigue strength test was carried out through a universal testing machine with a load 30% lon er than the 0.2% offset yield strength and a combined influence of different: environments: in air at room temperature, with synthetic saliva, and with fluoride synthetic saliva. After failure, the number of cycles were recorded, and fracture surfaces were examined with on SEM.Results. ANOVA and Tukey's multiple comparison rest indicated that Ti-6Al-4V alloy achieved 21,269 cycles (SD = 8,355) against 19,157 cycles (SD = 3,624) for the commercially purr Ti. There were no significant differences between either metal in the corrosion-fatigue life for dry specimens, but when the solutions were present, the fatigue life was significantly reduced, probably because of the product-ion of corrosion pits caused by superficial reactions.
Resumo:
The present work aims to study the microstructure and mechanical properties of titanium alloys, widely used in the manufacture of orthopedic implants in order to compare a new manufacturing technology of implants, rapid prototyping in metals with conventional manufacturing processes. Rapid prototyping is being used in many areas of human knowledge to assist in the study and often in the manufacture of components for their own use. Nowadays with the advancement of software and equipment such as computed tomography and magnetic resonance imaging, we can reproduce any part of the human body in three-dimensional images with great perfection and it is used in the reproduction of implants, scaffolds, material aid and preparation in surgery. This work aims to do: A comparison between the microstructure of the alloy in the two manufacturing processes (prototyping and conventional), showing the grain size, the nature, form, quantity, and distribution of various ingredients or certain inclusions and study of mechanical properties of titanium in both cases.
Resumo:
Titanium and its alloys have been used for biomedical applications due their excellent properties such as high corrosion resistance, biocompatibility and mechanical properites. In this study, microstructural and mechanical properties of Ti-30Ta alloy was evaluated during its processing. Ti-30Ta alloy ingots were produced from sheets of commercially pure titanium (99.9%) and tantalum (99.9%). Its melting was realized in arc melting furnace in an argon atmosphere. After homogenizing at 1200ºC, ingots were cold worked by swaging. Samples with 13 mm in diameter were obtained. They were forging at the reduction ratios of 15%. After deformation, microstructure was evaluated by optical microscopy in each condition. Also, Vickers microhardness of samples was measured and phase constitution was evaluated using XRD analysis