417 resultados para Polymeric precursor method and perovskite
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
In this work, a SiO2 spherical were prepared by the Stober Method and then recovered with a single layer of Eu2O3 oxide (SiO2@Eu2O3) obtained by the Polymeric Precursor Method. The SiO2@Eu2O3 powder was heated treated at 100, 300, 400, 500 and 800 A degrees C. The samples were characterized by the Scanning Electonic Microscopy (SEM), Thermal Analysis (TGA/DTA), and the luminescent properties of the SiO2@Eu2O3 powders were studied by their emission and excitation spectra as well as by the lifetime measurements of the Eu3+ D-5(0) -> aEuro parts per thousand F-7(2) transition. The SEM analysis shows that the silica prepared by the Stober Method is spherical with a particle size of 460 nm. The emission spectra of the SiO2@Eu2O3 powders presented the Eu3+ characteristics bands related to the D-5(0) -> aEuro parts per thousand F-7(J) (J = 0, 1, 2, 3, 4) transitions at 577, 591, 616, 649 and 695 nm, respectively. The band related to the D-5(0) -> aEuro parts per thousand F-7(2) transition is the most intense in the spectra, and its intensity decreases with the temperature enhancement. The decay curves of the SiO2@Eu2O3 samples presented monoexponential features, and the obtained lifetime values were higher than the Eu2O3 oxide. It was possible to conclude that the D-5(0) -> aEuro parts per thousand F-7(2) hypersensitive transition is strongly dependent on the Eu3+ surrounding.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Europium(III) Concentration Effect on the Spectroscopic and Photoluminescent Properties of BaMoO4:Eu
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
The aim of this work is to investigate the structural properties of the (Pb1-xErx)TiO3 (PET) powders, with x varying from 0.01 to 0.08, prepared by the polymeric precursor method. Combined X-ray diffraction, Raman spectroscopy and ab initio calculation reveal a diffuse phase-transition of a tetragonal to a cubic phase. The crystalline models built allowed to calculate electronic properties and to analyze the behavior of the doping element in the structure of the material, which are consistent with the experimental results that indicate the beginning of phase-transition from tetragonal to cubic. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
We investigated the dielectric properties of pure and lanthanum modified bismuth titanate thin films obtained by the polymeric precursor method. X-ray diffraction of the film annealed at 300 degrees C for 2h indicates a disordered structure. Lanthanum addition increases gradually the dielectric permittivity of films, keeping unchanged their loss tangent. From C-V curve we can see no hysteresis behavior indicating the absence of domain structure. The decrease in the conductivity for the heavily doped Bi4Ti3O12 (BIT) must be associated to the unidentified crystal defects. For comparison, dielectric properties of crystalline BIT film were also investigated. (C) 2007 Published by Elsevier B.V.
Resumo:
Complex cluster [TiO5 center dot V-O(z)] and [SrO11 center dot V-O(z)] (where V-O(z)=V-O(X), V-O(center dot), V-O(center dot center dot)) vacancies were identified in disordered SrTiO3 powders prepared by the polymeric precursor method, based on experimental measurements by x-ray absorption near edge structure spectroscopy. The paramagnetic complex states of [TiO5 center dot V-O(center dot)] and [SrO11 center dot V-O(center dot)] with unpaired electrons were confirmed by electron paramagnetic resonance spectroscopy. The disordered powders showed strong photoluminescence at room temperature. Structural defects of disordered powders, in terms of band diagram, density of states, and electronic charges, were interpreted using high-level quantum mechanical calculations in the density functional framework. The four periodic models used here were consistent with the experimental data and explained the presence of photoluminescence. (C) 2008 American Institute of Physics.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Intense photoluminescence in highly disordered (amorphous) BaTiO3, PbTiO3, and SrTiO3 prepared by the polymeric precursor method was observed at room temperature. The emission band maxima from the three materials are in the visible region and depend on the exciting wavelength. The origin of the photoluminescence was not exactly identified. However, the line shape indicates that confinement effects are not probable. The experimental results indicate that it could be related to the disordered perovskite structure. © 2000 American Institute of Physics.
Resumo:
In this study the preparation of 9.5/65/35 PLZT ceramic powders were investigated. The powders with the formula Pb0.905La0.095(Zr0.65 Ti0.35)0.976O3 + 3.5 w% PbO were prepared using Pechini process and partial oxalate method. The powder phase formation, powder morphology, and green density of PLZT were shown.
Resumo:
Lead zirconate titanate (PZT) solutions were prepared using a polymeric precursor method, Zr n-propoxide and Ti i-propoxide were used as starting materials with ethylene glycol and water as solvents. The PZT solution was spin-coated on Pt/Ti/SiO2/Si substrates, baked on a hot plate, and finally heat-treated in a tube furnace between 400 and 800°C. The surface morphology and grain size of the films were characterized by atomic force microscopy (AFM), using a tapping mode with amplitude modulation. The films, thermal annealed at temperatures higher than 500°C, exhibited a dense microstructure, without noticeable cracks or voids. Electrical properties were investigated as a function of composition and annealing temperature.
Resumo:
This paper discusses the preparation and characterization of Zn 0.95Mn0.05O phase obtained by the polymeric precursor method for DMS applications. The as-obtained powders were calcined between 500 to 800°C and characterized by XRD, SEM and BET. The XRD analysis of the powder showed a crystalline material containing second phase. The crystallite sizes ranged from 20 to 51 nm. The micrographs showed that the powders consisted of soft and homogeneous agglomerations. The nitrogen adsorption/desorption curves of the Zn0.95Mn0.05O phases were type II curves, which is characteristic of mesoporous materials.
Resumo:
Ba(Zr0.75Ti0.25)O3 (BZT-75/25) powders were synthesized by the polymeric precursor method. Samples were structurally characterized by X-ray diffraction (XRD), Rietveld refinement, X-ray absorption near-edge structure (XANES) and extended X-ray absorption fine structure (EXAFS) techniques. Their electronic structures were evaluated by first-principle quantum mechanical calculations based on density functional theory at the B3LYP level. Their optical properties were investigated by ultraviolet-visible (UV-Vis) spectroscopy and photoluminescence (PL) measurements at room temperature. XRD patterns and Rietveld refinement data indicate that the samples have a cubic structure. XANES spectra confirm the presence of pyramidal [TiO5] clusters and octahedral [TiO6] clusters in the disordered BZT-75/25 powders. EXAFS spectra indicate distortion of Ti-O and Ti-O-Ti bonds the first and second coordination shells, respectively. UV-Vis absorption spectra confirm the presence of different optical bandgap values and the band structure indicates an indirect bandgap for this material. The density of states demonstrates that intermediate energy levels occur between the valence band (VB) and the conduction band (CB). These electronic levels are due to the predominance of 4d orbitals of Zr atoms in relation to 3d orbitals of Ti atoms in the CB, while the VB is dominated by 2p orbitals related to O atoms. There was good correlation between the experimental and theoretical optical bandgap values. When excited at 482 nm at room temperature, BZT-75/25 powder treated at 500 C for 2 h exhibited broad and intense PL emission with a maximum at 578 nm in the yellow region. © 2013 Elsevier Ltd. All rights reserved.