391 resultados para Thin Films. Magnetron Sputtering and Optical Emission Spectroscopy
Resumo:
The effect of tungsten (W6+) ion substituting on dielectric and ferroelectric behavior in SrBi2(Ta0.5Nb0.5)(2)O-9 (SBTN) thin films prepared by polymeric precursor method was investigated at room temperature. The addition of W6+ ion in the SBTN lattice was evaluated by X-ray diffraction (XRD), microstructural and dielectrical properties. An increase in the grain size is evident when tungsten is introduced in the SBTN lattice. Substitution of tungsten until 10% on B site leads to introduce space charge polarization into the system, resulting in an appreciable decrease in both dielectric constant and tangent loss. The morphology of the thin films investigated by atomic force microscopy leads to an increase in the grain size after tungsten addition. Fatigue resistance was noted with increase in tungsten addition. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
In this work, we report on the synthesis of SrMoO4 powders by co-precipitation method and processed in a microwave-hydrothermal at 413 K for 5 h. These powders were analyzed by X-ray diffraction (XRD), Fourier transform Raman (FT-Raman), ultraviolet-visible (UV-vis) absorption spectroscopy and photoluminescence (PL). XRD analyses revealed that the SrMoO4 powders are free of secondary phases and crystallize in a tetragonal structure. FT-Raman investigations showed the presence of Raman-active vibration modes correspondent for this molybdate. UV-vis technique was employed to determine the optical band gap of this material. SrMoO4 powders exhibit an intense PL emission at room temperature with maximum peak at 540 nm (green region) when excited by 488 nm wavelength of an argon ion laser. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
In this work, GdAlO3:RE3+ (RE = Eu or Tb) was successfully prepared by the Pechini method at lower temperatures when compared to others methods as solid-state synthesis and sol-gel process. In accordance to the XRD data, the fully crystalline single-phase GdAlO3 could be obtained at 900 degrees C. The differential thermal analysis (DTA) shows a crystallization peak at 850 degrees C. The samples are composed by monocrystalline particles (50-120 nm) exhibiting the formation of aggregates among them, which indicates the beginning of the sinterization process. This feature indicates a strong tendency to the formation of aggregates, which is a suitable ability for the close-packing of particles, and hence a potential application in X-ray intensifying screens. Luminescence measurements indicate Gd3+ -> RE3+ energy transfer. The Eu3+ emission spectra exhibit all the characteristics D-5(0) -> F-7(j) transitions and the observed profile suggests that RE3+ ions occupy at least one site without center of symmetry. For terbium-doped samples, the D-5(3) -> F-7(j) (blue emission) and D-5(4) -> F-7(j) (green emission) transitions were observed and the ratio between them may depend on the Tb3+ content due to cross-relaxation processes. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
LiNbO3 thin films were grown on (0001) sapphire substrates by a chemical route, using the polymeric precursor method. The overall process consists of preparing a coating solution from the Pechini process, based on metallic citrate polymerization, the precursor films, deposited by dip coating, are then heat treated to eliminate the organic material and to synthesize the phase. In this work, we studied the influence of the heat treatment on the structural and optical properties of single-layered films. Two routes were also investigated to increase the film thickness: increasing the viscosity of the coating solution and/or increasing the number of successively deposited layers. The x-ray diffraction theta -2 theta scans revealed the c-axis orientation of the single- and multilayered films and showed that efficient crystallization can be obtained at temperatures as low as 400 degreesC, the phi-scan diffraction evidenced the epitaxial growth with two in-plane variants, A microstructural study revealed that the films were crack free, homogeneous, and relatively dense. Finally, the investigation of the optical properties (optical transmittance and refractive index) confirmed the good quality of the films. These results indicate that the polymeric precursor method is a promising process to develop lithium niobate waveguides.
Resumo:
Ferroelectric SrBi2Ta2O9 thin films on Pt/Ti/SiO2/Si were successfully synthesized by the modified polymeric precursor method. The films were deposited by spin coating and crystallized by rapid thermal annealing in a halogen lamp furnace, followed by postannealing at temperatures ranging from 700 degreesC to 800 degreesC in an oxygen atmosphere. Microstructural and phase evaluations were followed by x-ray diffraction and atomic force microscopy. The films displayed spherical grain structures with a superficial roughness of approximately 3-6 nm. The dielectric constant values were 121 and 248 for films treated at 700 degreesC and 800 degreesC, respectively. The P-E curve showed a voltage shift toward the positive side, which was attributed to crystallization under the halogen illumination. The remanent polarization (2P(r)) and coercive field (E-c) were 7.1 muC/cm(2) and 113 kV/cm, and 18.8 muC/cm(2) and 93 kV/cm for the films treated at 700 degreesC and 800 degreesC, respectively. (C) 2001 American Institute of Physics.
Resumo:
Polycrystalline Pb-0.Sr-60(0).40TiO3 thin films with the tetragonal perovskite structure were grown on platinum-coated silicon substrates by a chemical method. Raman results reveal that A1 (1 TO) symmetry modes, also known as soft modes, persist above the phase transition 14 temperature. This is due to the high structural distortion caused by the substitution effect of Sr2+ for Pb2+ ions. In contrast, the E(1TO) symmetry mode vanishes at 498 K, characterizing the ferroelectric-paraelectric transition phase. However, the Raman spectra, as a function of temperature, reveal that the ferroelectric-paraelectric phase transition may be correlated with a diffuse phase transition. The experimental data obtained from measurements of the dielectric constant as a function of temperature and frequencies showed a classical behavior of ferroelectric phase transition in Pb-0.Sr-60(0).40TiO3 thin films, rather than a relaxor ferroelectric phase transition. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Organic-inorganic hybrids were prepared using ureapropyltriethoxysilane, methacryloxypropyltrimethoxysilane and acrylic acid modified zirconium(IV) n-propoxide precursors and were characterized by small angle X-ray scattering, X-ray diffraction and photoluminescence spectroscopy. The results indicate an effective interaction between the zirconium-based nanoparticles and the siliceous nanodomains that induces changes in the hybrids' emission features. Planar waveguides were obtained by spin-coating of the prepared sols on sodalime and silica substrates. Refractive index, thickness, number of propagating modes, and attenuation coefficient were measured at 543.5, 632.8 and 1550 nm by the prism coupling technique. The synergism between the two hybrid precursors resulted in monomode planar waveguides with low losses in the infrared ( from 0.6-1.1 dB cm(-1)) which also support a number of propagating modes in the visible ( losses from 0.4-1.5 dB cm(-1)). Channel waveguides were also obtained by UV photopatterning using amplitude or phase masks and propagating modes were observed at 1550 nm.
Resumo:
Ferroelectric CaBi4Ti4O15 (CBTi144) thin films were deposited on Pt/Ti/SiO2/Si substrates by the polymeric precursor method. The films present a single phase of layered-structured perovskite with polar axis orientation after annealing at 700 degrees C for 2 h in static air and oxygen atmosphere. The a/b-axis orientation of the ferroelectric film is considered to be associated with the preferred orientation of the Pt bottom electrode. It is noted that the films annealed in static air showed good polarization fatigue characteristics at least up to 10(10) bipolar pulse cycles and excellent retention properties up to 10(4) s. on the other hand, oxygen atmosphere seems to be crucial in the decrease of both, fatigue and retention characteristics of the capacitors. Independently of the applied electric field, the retained switchable polarization approached a nearly steady-state value after a retention time of 10 s. (C) 2006 Elsevier B.V. All rights reserved.
Resumo:
Electrically detected magnetic resonance (EDMR) and electron paramagnetic resonance (EPR) were used to investigate emeraldine base polyaniline films. The magnetic susceptibility presented a Curie (localized spins)-Pauli (delocalized spins) transition at 240 K, when we also observed a transition in the dependence of the g factor with temperature (T). Peak-to-peak linewidth decreases with increasing temperature, reflecting that motional narrowing limits the hyperfine and dipolar broadening in this polymer. EDMR spectra could only be observed above 250 K in accordance to EPR results. Surface and bulk transport could be separated and their analysis reflected the effect of magnetic interaction with oxygen. (c) 2007 American Institute of Physics.
Resumo:
SnO2 thin films were obtained by the sol-gel method starting from inorganic precursor solutions. In this work, we compare the structure of undoped and Sb-doped SnO2 films prepared by dip-coating. The films were deposited on quartz substrates and then fired at different temperatures ranging from 383 up to 1173 K. The density and the thickness of the films were determined by X-ray reflectivity (XRR) and their porous nanostructure was characterized by grazing-incidence small angle X-ray scattering (GISAXS). XRR results corresponding to undoped and Sb-doped samples indicate a monotonous decrease in film thickness when they are fired at increasing temperatures. At same time, the apparent density of undoped samples exhibits a progressive increase while for Sb-doped films it remains invariant up to 973 K and then increases for T = 1173 K. Anisotropic GISAXS patterns of both films, Sb-doped and undoped, fired above 573 K indicate the presence of elongated pores with their major axis perpendicular to the film surface. For all firing temperatures the nanopores in doped samples are larger than in undoped ones. This suggests that Sb-doping favours the pore growth hindering the film densification. At the highest firing temperature (1173 K) this effect is reversed.
Resumo:
Intense photoluminescence in highly disordered strontium titanate amorphous thin films prepared by the polymeric precursor method was observed at room temperature (300 K). The luminescence spectra of SrTiO3 amorphous thin films at room temperature revealed an intense single-emission band in the visible region. X-ray absorption near edge structure was used to probe the local atomic structure of SrTiO3 amorphous and crystalline thin films. Photoluminescence intensity in the 535 nm range was found to be correlated with the presence of non-bridging oxygen defects. A discussion is presented of the nature of this photoluminescence, which may be related to the disordered structure in SrTiO3 amorphous thin films. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
The authors investigated the influence of defects on the piezoelectric and dielectric properties of Bi4Ti3O12 (BIT), SrBi4Ti4O15 (SBTi) and CaBi4Ti4O15 (CBTi144) thin films by x-ray photoemission spectroscopy measurements. In the SBTi film, Sr which is a nonpolarizable ion restricting the movement of Ti4+ ions and thus leads to a low piezoresponse. Meanwhile, the oxygen environment is quite different in the BIT and CBTi144 films exhibiting excellent piezoelectric properties. The piezoelectric coefficient and the dielectric behavior were larger for a-b axis oriented than for c axis-oriented films due to the defects created during the films crystallization. (c) 2007 American Institute of Physics.
Resumo:
Ferroelectric Pb1-xCaxTiO3 (x = 0.24) thin films were formed on a Pt/Ti/SiO2/Si substrate by the polymeric precursor method using the dip-coating technique for their deposition. Characterization of the films bq X-ray diffraction showed a perovskite single phase with a tetragonal structure after annealing at 700 degreesC. Atomic force microscopy (AFM) analyses showed that the film had a smooth and crack-free surface with low surface roughness. In addition, the PCT thin film had a granular structure with an 80 nm grain size. The thickness of the films observed by the scanning electron microscopy (SEM) is 550 nm and there is a good adhesion between the film and substrate. For the electrical measurements metal-ferroelectric-metal of the type capacitors were obtained, where the thin films showed good dielectric and ferroelectric properties. The dielectric constant and dissipation factor at 1 kHz and measured at room temperature were found to be 457 and 0.03. respectively. The remanent polarization and coercive field for the: deposited films were P-r = 17 muC/cm(2) and E-c = 75 kV/cm, respectively. Moreover. The 550-nm-thick film showed a current density in the order of 10(-8) A/cm(2) at the applied voltage of 2 V. The high values of the thin film's dielectric properties are attributed to its excellent microstructural quality and the chemical homogeneity obtained by the polymeric precursor method. (C) 2001 Elsevier science Ltd. All rights reserved.