174 resultados para METHACRYLATE
Resumo:
Using the sol-gel process, organic-inorganic hybrid coatings were synthesized by incorporation of different concentrations of functionalized carbon nanotubes, to improve their mechanical strength and thermal resistance without changing its passivation character. The siloxane-PMMA hybrids were prepared by radical polymerization of methyl methacrylate (MMA) with 3-methacryloxipropiltrimethoxisilane (MPTS) using the thermal initiator benzoyl peroxide (BPO), followed by acid catalyzed hydrolysis and condensation of tetraethoxysilane (TEOS). The analysis of pristine and functionalized carbon nanotubes was carried out using Scanning Electron Microscopy, X-ray Photoelectron Spectroscopy and Raman Spectroscopy. Structural analysis of hybrids was performed by Nuclear Magnetic Resonance, Atomic Force Microscopy and Raman Spectroscopy. For analysis of mechanical strength and thermal stability were performed mechanical compression tests and thermogravimetric analysis, respectively. Electrochemical Impedance Spectroscopy was used to evaluate the corrosion resistance in saline environment. The results showed an effective functionalization of carbon nanotubes with carboxyl groups and conservation of its structure. The hybrids showed high siloxane network connectivity and roughness of approximately 0.3 nm. The incorporation of carbon nanotubes in the hybrid matrix did not change significantly their thermal stability. Samples containing carbon nanotubes exhibit good corrosion resistance (on the order of MΩ in saline environment), but the lack of complete dispersion of carbon nanotubes in the hybrid, resulted in a loss of mechanical and corrosion resistance compared to hybrid matrix.
Resumo:
Objectives: This study aimed to assess dimensional changes in acrylic resin base and artificial teeth position after water storage and thermocycling using computer graphics measurements. Methods: Twenty-four waxed replicas were obtained from a previous upper complete denture. For linear measurements, points in cusps tips of left central incisor and second premolars and molars were marked in one of the prostheses with graphite and transferred to the others using an acrylic resin guide. The prostheses were scanned after waxing, polymerization and treatments and the images were exported to “AutoCad 2002 Today®” software for measurements. Results: There was no statistically significant difference in changes of each segment for each group and between the phases evaluated after polymerization and thermocycling. In groups I and III, the values after polymerization are higher than those after treatment, which suggests shrinkage while the prostheses in group II have expanded. Conclusion: The three groups exhibited artificial teeth movement after tests in comparison to the polymerized prosthesis. The prostheses submitted to water storage in kiln at 36ºC during seven days showed different behavior than the other groups.
Resumo:
The purpose of this study was to evaluate the impact of different disinfection solutions on flexural resistance of chemically-activated acrylic resin. Test pieces were made of clear acrylic resin using a rectangular mold and employing two techniques: wet polymerization under pressure (n = 20) and dry polymerization under pressure (n = 20). Test pieces were subdivided into four equal groups: distilled water (control), sodium bicarbonate, 1% sodium hypochlorite and effervescent ats. The 30-day cycling technique consisted of immersing the test pieces in 100 ml of solution for 10 min three times a day and placing them in closed containers containing artificial saliva at 37°C. Subsequently, the flexural resistance of samples was tested. Data were analyzed using two-way analysis of variance (ANOVA) with forces serving as the dependent variables and the polymerization technique and cleaning agents as independent variables. Post hoc multiple comparisons were performed using Tukey’s test. There was no statistically significant difference in the flexural strength between the two polymerization techniques. The greatest flexural strength was observed for the effervescent tablets group followed by the control and 1% sodium hypochlorite groups which were statistically similar. Thus, the sodium bicarbonate solution caused the lowest flexural resistance of the test pieces.
Resumo:
Processo FAPESP: 2012/24545-3
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Clinical performance of composite resins depends largely on their mechanical properties,and those are influenced by several factors,such as the light-curing mode. The purpose of this study was to evaluate the influence of different light sources on degree of conversion(DC), Knoop hardness(KHN) and plasticization(P) of a composite resin. Disc-shaped specimens (5 x 2 mm) of Esthet-X(Dentsply) methacrylate-based microhybrid composite were light-cured using quartz-tungsten-halogen (QTH) Optilight Plus(Gnatus) or light-emitting diode(LED) Ultraled(Dabi Atlante) curing units at 400 and 340 mW/cm2 of irradiance, respectively. After 24 h, absorption spectra of composite were obtained using Nexus 670(Nicolet)FT-IR spectrometer in order to calculate the DC.The KHN was measured in the HMV-2000(Shimadzu) microhardness tester under 50 g loads for 15 s, and P was evaluated by percentage reductio of hardness after 24 h of alcohol storage. Data were subjected to t-Student test(alpha=0.05).QTH device showed lower P and higher KHN$ than LED (p<0.05), and no difference between the light-curing units was found for DC (p>0.05). The halogen-curing unit with higher irradiance promoted higher KHN and lower softening in alcohol than LED.
Resumo:
Pós-graduação em Química - IBILCE
Resumo:
Purpose: Ti-Ta alloys have high potential for dental application due to a good balance between high strength and low modulus. Absence of primary anchoring may occur when dental implants are installed immediately after tooth extraction. Tranexamic acid (TEA) is used to reduce fibrin degradation and can prevent early blood clot breakdown. The aim of this study was to evaluate the biocompatibility of Ti-30Ta implants associated or not with tranexamic acid and installed with compromised primary stability. Methods and materials: Fabricated were 20 implants of titanium ASTM F67 (Grade 4) and 20 implants of Ti-30Ta alloy with dimensions of 2.1 mm × 2.8 mm Ø. They were divided (n = 10) into Group I (Ti machined), Group II (Ti machined/tranexamic acid), Group III (Ti-30Ta alloy) and Group IV (Ti-30Ta/tranexamic acid) and were implanted in tibia (defects with 2.5 mm × 3.2 mm Ø) of 40 male rats (250 g). The surgical sites were rinsed with 5% tranexamic acid solution in Groups II and IV. The animals were euthanized at 45 days postoperative. The pieces were processed in methyl methacrylate (Stevenel's blue/Alizarin red). The percentage of peri-implant tissue repair was analyzed via images obtained by an optical microscope coupled to a digital camera using Leica software and Adobe Photoshop QWin. Data were analyzed statistically with a significance level of 5%. Results: Histomorphometric results showed 97.16% of bone-implant contact for group IV, 89.78% of bone contact for group III, 70.89% for group II and 61.59% of bone contact for group I. The statistical analyses demonstrated significant differences (P < 0.05) among group I and other groups. Conclusion: The results suggest that (a) Ti-30Ta promoted an increase of bone healing and apposition around implant; (b) tranexamic acid favored the stabilization of blood clot and bone formation.
Resumo:
Pós-graduação em Química - IQ