153 resultados para rubber to rubber bonding
Resumo:
Tissue engineering has special interest in bone tissue aiming at future medical applications Studies have focused on recombinant human bone morphogenetic protein-2 (rhBMP-2) and natural latex proteins due to the osteogenic properties of rhBMP-2 and the angiogenic characteristic of fraction 1 protein (P-1) extracted from the rubber tree Hevea brasiliensis. Furthermore, heterologous fibrin sealant (FS) has been shown as a promising alternative in regenerative therapies. The aim of this study was to evaluate these substances for the repair of bone defects in rats. A bone defect measuring 3 mm in diameter was created in the proximal metaphysis of the left tibia of 60 rats and was implanted with rhBMP-2 or P-1 in combination with a new heterologous FS derived from snake venom. The animals were divided into six groups: control (unfilled bone defect), rhBMP-2 (defect filled with 5 mu g rhBMP-2), P-1 (defect filled with 5 mu g P-1), FS (defect filled with 8 mu g FS), FS/rhBMP-2 (defect filled with 8 mu g FS and 5 mu g rhBMP-2), FS/P-1 (defect filled with 8 mu g FS and 5 mu g P-1). The animals were sacrificed 2 and 6 weeks after surgery. The newly formed bone projected from the margins of the original bone and exhibited trabecular morphology and a disorganized arrangement of osteocyte lacunae. Immunohistochemical analysis showed intense expression of osteocalcin in all groups. Histometric analysis revealed a significant difference in all groups after 2 weeks (p < 0.05), except for the rhBMP-2 and FS/rhBMP-2 groups (p > 0.05). A statistically significant difference (p < 0.05) was observed in all groups after 6 weeks in relation to the volume of newly formed bone in the surgical area. In conclusion, the new heterologous fibrin sealant was found to be biocompatible and the combination with rhBMP-2 showed the highest osteogenic and osteoconductive capacity for bone healing. These findings suggest a promising application of this combination in the regeneration surgery.
Resumo:
Objectives. To compare three different designs for measuring the bond strength between Y-TZP ceramic and a composite material, before and after ceramic surface treatment, evaluating the influence of the size of the adhesive interface for each design.Methods. 'Macro'tensile, microtensile, 'macro'shear, microshear, 'macro'push-out, and micropush-out tests were carried out. Two Y-TZP surface treatments were evaluated: silanization (sil) and tribochemical silica coating (30 mu m silica-modified Al2O3 particles + silanization) (TBS). Failure mode analysis of tested samples was also performed. Results. Both the surface treatment and the size of the bonded interface significantly affected the results (p = 0.00). Regardless of the type of surface treatment, the microtensile and microshear tests had higher values than their equivalent "macro" tests. However, the push-out test showed the highest values for the "macro" test. The tensile tests showed the greatest variability in results. The tribochemical silica coating method significantly increased bond strength for all tests.Significance. Different test designs can change the outcome for Y-TZP/cement interfaces, in terms of mean values and reliability (variability). The 'micro'tests expressed higher bond strengths than their equivalent 'macro'tests, with the exception of the push-out test (macro > micro). (C) 2015 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)