169 resultados para neutron powder diffraction


Relevância:

40.00% 40.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Titanium alloys have several advantages over ferrous and non-ferrous metallic materials, such as high strengthto-weight ratio and excellent corrosion resistance. A blended elemental titanium powder metallurgy process has been developed to offer low cost commercial products. The process employs hydride-dehydride (HDH) powders as raw material. In this work, results of the Ti-35Nb alloy sintering are presented. This alloy due to its lower modulus of elasticity and high biocompatibility is a promising candidate for aerospace and medical use. Samples were produced by mixing of initial metallic powders followed by uniaxial and cold isostatic pressing with subsequent densification by isochronal sintering between 900 up to 1600 °C, in vacuum. Sintering behavior was studied by means of microscopy and density. Sintered samples were characterized for phase composition, microstructure and microhardness by X-ray diffraction, scanning electron microscopy and Vickers indentation, respectively. Samples sintered at high temperatures display a fine plate-like alpha structure and intergranular beta. A few remaining pores are still found and density above 90% for specimens sintered in temperatures over 1500 °C is reached.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Nickel ferrite powders with a nominal NiFe2O4 composition were synthesized by combustion reaction using urea as fuel. The powder was obtained using a vitreous silica basin heated directly on a hot plate at 480 degrees C until self-ignition occurred. After combustion, the powder was calcined at 700 degrees C for 2 h. The formation of the spinel phase and the distribution of cations in the tetrahedral and octahedral sites of the crystal structure were investigated by the Rietveld method, using synchrotron X-ray diffraction data and Mossbauer spectroscopy. The material presented a crystallite size of 120 nm and magnetic properties. The resulting stoichiometry after the Rietveld refinement was (Fe-0.989(2) Ni-0.011(2)) [Fe-1.012(2) Ni-0.989(2)] O-4.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Nanocrystalline ZrO2-12 mol % CeO2 powders were synthesized using a polymeric precursor method based on the Pechini process. X-ray diffraction (XRD) patterns showed that the method was effective to synthesize tetragonal zirconia single-phase. The mean crystallite size attained ranges from 6 to 15 nm. The BET surface areas were relatively high reaching 97 m(2)/g. Studies by nitrogen adsorption/desorption on powders, dilatometry of the compacts, and transmission electron microscopy (TEM) of the powders, were also developed to verify the particles agglomeration state. Both citric acid : ethylene glycol ratio and calcination temperature affected the powder morphology, which influenced the sinterability and microstructure of the sintered material, as showed by scanning electron microscopy (SEM). (C) 2001 Kluwer Academic Publishers.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Reactive ZrxTi1-xO4 (x=0.65, 0.50 and 0.35) powder was prepared by the polymeric precursor method. Studies by X-ray diffraction (XRD), nitrogen adsorption/desorption, and thermogravimetric analysis (TG) showed that powders with high crystallinity (>90%) and high surface areas (>40 m(2)/g) are obtained after calcination at 700 degrees C for 3 h. Infrared spectroscopy and XRD results showed that these titanates nucleate from the amorphous phase with no intermediate phases, at low temperature (450 degrees C).

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The SrWO4 (SWO) powders were synthesized by the polymeric precursor method and annealed at different temperatures. The SWO structure was obtained by X-ray diffraction and the corresponding photoluminescence (PL) spectra was measured. The PL results reveal that the structural order-disorder degree in the SWO lattice influences in the PL emission intensity. Only the structurally order-disordered samples present broad and intense PL band in the visible range. To understand the origin of this phenomenon, we performed quantum-mechanical calculations with crystalline and order-disordered SWO periodic models. Their electronic structures were analyzed in terms of band structure. The appearance of localized levels in the band gap of the order-disordered structure was evidenced and is a favorable condition for the intense PL to occur.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Disordered and crystalline Mn-doped BaTiO3 (BTO:Mn) powders were synthesized by the polymeric precursor method. After heat treatment, the nature of visible photoluminescence (PL) at room temperature in amorphous BTO:Mn was discussed, considering results of experimental and theoretical studies. X-ray diffraction (XRD), PL, and UV-vis were used to characterize this material. Rietveld refinement of the BTO:Mn from XRD data was used to built two models, which represent the crystalline BTO:Mn (BTO:Mn,) and disordered BTO:Mn (BTO:Mn-d) structures. Theses models were analyzed by the periodic ab initio quantum mechanical calculations using the CRYSTAL98 package within the framework of density functional theory at the B3LYP level. The experimental and theoretical results indicated that PL is related with the degree of disorder in the BTO:Mn powders and also suggests the presence of localized states in the disordered structure. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The effect of the properties of starting boron powders on the superconducting properties of MgB2 has been studied. The 92% and 96% pure powders produce lower surface reactivity and larger particle size than the 99% boron powder, as can be seen from Brunauer - Emmett - Teller (BET) and scanning electron microscopy (SEM) results, indicating that the low purity powders cannot be used to archive the same superconducting properties as those of samples made from pure 99% boron powder. However, the purity of 92% and 96% boron powders can be improved by using a simple chemical process, leading to enhanced magnetic critical current densities J(c). From x-ray diffraction (XRD) measurement, oxide impurity has been observed, which might be originated from the B2O3 phase in the boron powders. In order to get high performance MgB2, it is obviously important to control the phase composition and microstructure of amorphous boron starting powders and solid reaction conditions.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Ultra-fine NaNbO3 powder was prepared by the use of polymeric precursors. X-ray diffraction (XRD) results showed that this niobate nucleates from the amorphous precursor, with no intermediate phases, at low temperature (500°C). Studies by XRD and nitrogen adsorption/desorption showed that powders with high crystallinity ( ≈ 100%) and high surface areas (>20 m2/g) are obtained after calcination at 700°C for 5 h. Compacts of calcined powders showed high sinterability reaching 98% of theoretical density when sintered at 1190°C for 3 h.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Non-linear electrical properties of SnO2-based ceramics were investigated as a function of powder agglomeration condition and as a function of dopant addition. All doped powders presented a single phase, cassiterite, as evidenced by X-ray diffraction analysis. The effect of milling was quite evident, with non-milled powder showing higher agglomerated particle size than milled powder. Cr addition seemed to increase the non-linear coefficient. Cu and Mn rendered dense ceramics, but α values for systems with Mn were higher than for systems with Cu.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A quantitative phase analysis was made of LixCoO2 powders obtained by two distinct chemical methodologies at different temperatures (from 400 to 700°C). A phase analysis was made using Rietveld refinements based on X-ray diffraction data, considering the Li xCoO2 powders as a multiphase system that simultaneously contained two main phases with distinct, layered and spinel-type structures. The results showed the coexistence of both structures in LixCoO 2 obtained at low temperature (400 and 500°C), although only the layered structure was detected at higher temperatures (600 and 700°C), regardless of the chemical powder process employed. The electrochemical performance, evaluated mainly by the cycling reversibility of Li xCoO2 in the form of cathode insertion electrodes, revealed that there is a close correlation between structural features and the electrochemical response, with one of the redox processes (3.3 v/3.9 v) associated only with the presence of the spinel-type structure. © 2003 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Titanium and its alloys provide high strength-to-weight ratios, good fatigue strength and increased corrosion resistance compared with others materials. Its acceptance in aerospace has been limited by costs considerations such as high cost of raw material, high buy-to-fly ratios and expensive machining operations. Significant cost reductions can be obtained by vacuum sintering and powder metallurgy (P/M) techniques by producing near net shapes and consequently minimizing material waste and machining time. The Ti 35Nb alloy exhibit a low modulus of elasticity. Stemming from the unique combination of high strength, low modulus of elasticity and low density, this alloy is intrinsically more resistant to shock and explosion damages than most other engineering materials. Samples were produced by mixing of initial metallic powders followed by uniaxial and cold isostatic pressing with subsequent densification by sintering between 900 and 1600 °C, in vacuum. Sintering behavior was studied by means of dilatometry. Sintered samples were characterized for phase composition, microstructure and microhardness by X-ray diffraction, scanning electron microscopy and Vickers indentation, respectively. Density was measured by Archimedes method. Copyright © 2004 Society of Automotive Engineers, Inc.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Titanium alloys of Ti-Si-B system were manufactured by blended elemental powder method using Ti, Si and B powders as starting materials. It was found that uniaxial and isostatic pressing followed by hot pressing at around 1000°C, for 20 minutes, provided good densification of such alloys. The physicochemical studies were performed by means of scanning electron microscopy, X-ray diffraction, atomic force microscopy and microindentation/wear tests. The investigations revealed a multiphase microstructure formed mainly by α-titanium, Ti6Si2B, Ti5Si3, TiB and Ti3Si phases. The phase transformations after pressureless sintering at 1200°C was also studied by X-ray diffraction for the Ti-18Si-6B composition. As stated in some other researches, these intermetallics in the α-titanium matrix provide high wear resistance and hardness, with the best wear rate of 0.2 mm3/N.m and the highest hardness of around 1300 HV. © (2012) Trans Tech Publications, Switzerland.