280 resultados para Pressureless sintering


Relevância:

10.00% 10.00%

Publicador:

Resumo:

Electrical conductivity and thermoelectric power measurements carried out in a heamatite ceramic showed a strong anisotropy in directions normal and parallel to the uniaxial pressing direction. This behaviour is similar to that verified in alpha-Fe2O3 single crystal. The results suggest that the extended structural defects, generated during sintering, disturb the magnetic order on the (001) planes of alpha-Fe2O3 and limit the mobility of n type carriers.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The Pechini method as well as the simultaneous addition of seeds particles and dopant solutions of BaTiO3 (BT) and PbTiO3 (PT) were used to prepare the perovskite phase 0.88 PZN-0.07 BT-0.05 PT. To study the influence of seed particle frequency on the synthesis of the PZN ceramic, two ranges of seed particle size were used: the range from 30 to 100 nm, termed small seed particles (frequency of 10(15) particles/cm(3)); and the range from 100 to 900 nm, termed large seed particles (frequency of 10(13) particles/cm(3)). The crystalline nuclei size influenced the calcining process, the sintering process and the microstructure. Samples prepared with lower seed frequency displayed more amount of pyroclore phase, need higher temperatures for sintering and showed a more heterogeneous microstructure with poor dielectric properties. (C) 2000 Elsevier B.V. Ltd and Techna S.r.l. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The 9.5/65/35 PLZT was prepared from the polymeric precursors (the Pechini and partial oxalate process) and by sintering in two stages in an oxygen atmosphere. After thermal treatment at 400 degreesC, the powders were calcinated and sintered at 1200 degreesC with slow heating and cooling rates. The second stage of sintering consisted of hot pressing at the same temperature in oxygen atmosphere. After calcination of PLZT powders obtained by both methods, as well as after sintering of PLZT obtained by Pechini process, the paraelectric cubic phase was formed. After sintering of PLZT obtained by partial oxalate procedure, small tetragonality of crystal structure was observed. After hot pressing PLZT was pseudocubic. SEM microstructural analyses were carried out of the sintering and hot pressed samples and indicated the small grain size less than 2 mum. (C) 2001 Elsevier B.V. B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

To obtain SnO2 films to be used for surface protection of fluoride glasses, a non-aqueous sol-gel route for the preparation was developed. An ethanolic SnO2 colloidal suspension was prepared by thermohydrolysis of SnCl4 solution at 70 degreesC. By using this procedure, redispersable powders with nanometer sized particles were obtained. Films were obtained by dip coating on glass and mica substrates. The structures of the ethanolic precursor suspension and films were compared to those of similar samples prepared by the classical aqueous sol-gel route. Comparative analyses performed by photon correlation spectroscopy demonstrated that the powders obtained by freeze-drying are fully redispersable either in aqueous or in alcoholic solutions at pH greater than or equal to 8. As prepared sols and redispersed colloidal suspensions have hydrodynamic radius distribution (2-14 nm) with an average size close to 7 nm. The variations in film structures with firing temperature were investigated by small-angle X-ray scattering and X-ray reflectometry. The experimental results show that the films have a two level porous structure composed of agglomerates of primary colloidal particles. The sintering of the primary particles leads to the densification of agglomerates and to the formation of inter-agglomerate spatially correlated pores. The volume fraction of intra-agglomerate pores is reduced from approximate to 50% to approximate to 30% by the precipitation of precursor salts partially hydrolyzed in ethanolic solution. (C) 2001 Elsevier B.V. B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Barium titanate ceramics were prepared through mechanochemical synthesis starting from fresh prepared barium oxide and titanium oxide in rutile form. Mixture of oxides was milled in zirconia oxide jar in the planetary ball-mill during 30, 60, 120 and 240 min. Extended time of milling directed to formation of higher amount of barium titanate perovskite phase. Barium titanate with good crystallinity was formed after 240 min. Sintering without pre-calcinations step was performed at 1330 degrees C for 2 hours with heating rate of 10 degrees C/min. The XRD, DSC, IR and TEM analyses were performed. Electric and ferroelectric properties were studied. Very well defined hysteresis loop was obtained.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Recently, mechanochemical synthesis was widely used in preparation of perovskite type of materials, such as BaTiO3, PbTiO3, PZT, etc. In this work, the possibility of mechanochemical synthesis of CaTiO3 from different precursors, such as CaCO3 or CaO and TiO2 was investigated. Intensive milling of mixture of CaO and TiO2, under optimal milling conditions, resulted in synthesis of single phase CaTiO3. It was also found that intensive milling of powder mixture containing CaCO3 and TiO2 only activate the powders for the sintering process; hence the CaTiO3 could be obtained at lower temperatures of sintering. To complete reaction of CaTiO3 formation during milling it is necessary to reduce CO2 partial pressure, i.e. it is necessary to change the atmosphere inside the vials during milling. In this work, an explanation for difference in milling behavior of different precursors was proposed and discussed. (c) 2006 Elsevier Ltd. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Barium titanate (BT) thick films were prepared from mechanically activated powders based on BaCO(3) and TiO(2). After homogenization and milling in a high-energy vibro mill, the powders were calcined at 700 degreesC for 2 h by slow heating and cooling rates. A thick film paste was prepared by mixing BT fine powders with small amount of low temperature sintering aid and organic binder. The thick films were screen-printed on alumina substrates electroded with Ag-Pd. The BT films were sintered at 850 degreesC for 1 h. The thickness was 25-75 mum depending of number of layers. The microstructure of thick films and the compatibility between BT layers and substrate were investigated by SEM Results of dielectric property measurements are also reported. (C) 2002 Elsevier B.V. Ltd and Techna S.r.l. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A 9.5/65/35 PLZT ceramic with a Pb-0.905 La-0.095 (Zr-0.65 Ti-0.35)(0.976) O-3 + 35 w% PbO formula was prepared using the Pechini method for powder preparation and two-step sintering in an oxygen atmosphere. Thr first step consisted of sintering at 1200 degrees C for 4 h with slow heating and cooling rates. The second step consisted of hot pressing at 1200 degrees C for 3 h, with slow heating and cooling rates and pressing pressures of 20 MPa (initial pressure) and 40 MPa (at sintering temperature). Investigations were made of the powder phase formation and powder morphology, i.e. The structure of sintered and hot-pressed PLZT ceramics. SEM microstructural analyses were carried out on the sintering and hot-pressing processes. (C) 2000 Elsevier B.V. Ltd and Techna S.r.l. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A study was made on the effect of the addition of BaO (0.025-0.05 mol%) and Bi2O3 (0.025-0.05 mol%) to the TiO2.Ta2O5.MnO2 material. The samples were characterized by X-ray diffraction, and current-voltage measurements were accomplished for determination of the nonlinear coefficient. An analysis was made to evaluate the microstructural characteristics of the materials. The most appropriate sintering conditions for the materials were analyzed with the purpose of obtaining the best nonlinear coefficient associated with the smallest breakdown electric field. After sintering at 1400 degreesC for 2 h, a low-voltage (30 V cm(-1)) varistor was obtained, which, however, presented a low nonlinear coefficient (6). It was found that the sintering conditions must be controlled in order to improve the electrical properties of these materials. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Samples of sintered AISI 316L stainless steel were plasma nitrided in a mixture of H-2-20% N-2, for 3 or 4 h. The treatment temperature was selected in 400-550 degreesC interval, in steps of 50 degreesC. X-ray diffraction (glancing angle geometry-GAXRD), conversion electron Mossbauer spectroscopy (CEMS), optical microscopy and Vickers microhardness were used as analytical techniques. For T greater than or equal to 500 degreesC and t = 4 h, a 40-mum layer is formed. The GAXRD results showed a transformation of the austenite gamma phase to the martensite in the sinterization process and showed as well, that the gamma' (Fe4N) phase is the predominant nitride besides small amounts of epsilon-Fe2N, gamma(N) CrN, Cr2O3 and the fcc nitrogen supersatured solid phase gamma(N). The CrN phase seems to decrease with temperature while the gamma(N) phase fraction is almost less than or equal to10%, independently on the temperature. The CEMS results indicated that while the gamma(N) fraction decreases with temperature of plasma nitriding, the gamma' fraction increases proportionally. (C) 2003 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Acicular monodispersed Fe1-xREx (RE= Nd, Sm,Eu,Tb;x=0, 0.05, 0.10) metallic nanoparticles (60 +/- 5 nm in length and axial ratio similar to6) obtained by reduction of alumina-coated goethite nanoparticles-containing rare earth (RE) under hydrogen flow are reported. Alumina and maghemite thin layers on particle surface were used to protect the goethite particles against sintering and oxidation, respectively. Al and RE additions were obtained by successive heterocoagulation reactions. Aluminum sulfate (10 at.% based on Fe) was dissolved in water and the pH adjusted to 12.5 with NaOH solution. Goethite particles were suspended in this solution and CO2 gas was blown into the slurry to neutralize it to a pH 8.5 or less. Particles were purified and dehydrated to effect transformation to alumina-coated hematite nanoparticles, which were re-suspended in aqueous solution in which RE sulfate (0-0.15 at.% based on Fe) has been dissolved, and the pH increased by ammonia aqueous solution addition. Resulted alumina-coated RE-doped hematite nanoparticles were reduced to metal at 450 degreesC/12 h under hydrogen flow and passivated with nitrogen-containing ethanol vapor at room temperature. Acicular monodispersed metallic nanoparticle systems were obtained and the presence of Al and RE were confirmed by induced-coupled plasma spectrometry analysis. X-ray diffraction, Mossbauer spectroscopy, and magnetization data are in agreement with the nanosized alpha-Fe core in a bcc structure, having a spinel structure, gammaFe(2)O(3), with thickness similar to1.5 run on particle surface. Main magnetic parameters showed saturation magnetization decreases and significant increasing in the coercive field with the RE composition increases. Magnetic properties of these particles, similar to40% smaller than those commercially available, suggest a decrease in the bit-size for high-density magnetic or magneto-optics recording media application. (C) 2004 Published by Elsevier B.V.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This work presents the preparation of SrBi2Nb2O9 (SBN) directly by the combustion synthesis. Strontium nitrate, niobium ammonium oxalate (NH4H2[NbO-(C2O4)(3)].3H(2)O) and bismuth oxide were used as oxidant reactants and urea as fuel. The influence of the fuel was evaluated by the addition of different fuel amounts (50%, 100%, 200% and 300%), 100% being the stoichiometric proportion. The XRD patterns showed that the SBN perovskite crystallized as the majority phase. The as-synthesized stoichiometric powder presented a specific surface area of around 13 m(2)/g and a mean grain size of around 16 nm. Dilatometric measurements showed that the maximum sintering rate occurs at 1275degreesC. The determination of the ferroparaelectric transition showed a Curie temperature (T-c) of 429degreesC. (C) 2002 Elsevier B.V. B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Various properties of particles can be altered by coating them with a layer of different chemical composition. Yttrium iron garnet (YIG) particles has been coated with silica for control of their sintering, corrosion resistance, and stabilization of magnetic properties. This silica cover was obtained by hydrolysis of tetraethylorthosilicate (TEOS) in 2-propanol. This material was characterized by transmission (TEM) electron microscopy, (XEDS) X-ray energy-dispersive spectrometry, (XPS) X-ray photoemission spectroscopy and (VSM) vibrating sample magnetometry. YIG was heterocoagulated by silica as indicated by TEM micrographies. XPS measurements indicated that only binding energy for silicon and oxygen was found on the silica shell, which confirms that the YIG was covered. The values of the saturation magnetization differ from the heterocoagulated system to well-crystallized YIG.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This paper reports on a study of the: effect of replacing CoO by MnO2 on the sintering and electrical propel-ties of the 98.95% SnO2 + (1 - x)% CoO + x% MnO2 + 0.05% Ta2O5 system. All the samples were compacted into pellets and sintered at 1300 degrees C for 1 h, when they reached densities of about 98% of the theoretical density. An X-ray diffraction (XRD) analysis showed no other detectable phases other than SnO2. Current-voltage characterization indicated varistor behavior in the systems. The non-linear coefficient (alpha) and breakdown electric field (Eb) increased as the amount of MnO2 was increased. The results are explained in terms of an electric barrier modification, due to the presence of adsorbed negative oxygen species at the grain boundary inter face. (C) 2000 Elsevier B.V. B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The X-ray reflectivity technique was applied in the study of tin oxide films deposited by sol-gel dip-coating on borosilicate glasses. The influence of the withdrawal speed and temperature of thermal treatment on the film structure was analyzed. We have compared the thermal evolution of the density and the shrinkage of the films with these properties measured for the monolithic xerogel by helium picnometry and thermomechanical analysis. In agreement with the Landau-Levich model, the layer thickness increases by increasing the withdrawal speed. Nevertheless, it decreases with the increase of the thermal treatment temperature, due to the densification process. The values of apparent density are smaller than the skeletal density, which shows that the films are porous. The comparison between the film and the monolith indicates that shrinkage during firing is anisotropic, occurring essentially perpendicular to the coating surface.