4 resultados para endless rolling
em Universidade Federal do Rio Grande do Norte(UFRN)
Resumo:
The advantages of the use of vegetable fibers on the synthetic fibers, such as glass fibers, in the reinforcements in composites are: low cost, low density, good tenacity, good thermal properties and reduced use of instruments for their treatment or processing. However, problems related to poor performance of some mechanical natural fibers, have hindered its direct use in structural elements. In this sense, the emergence of alternative materials such as hybrids composites, involving natural and synthetic fibers, has been encouraged by seeking to improve the performance of structural composites based only on natural fibers. The differences between the physical, chemical and mechanical properties of these fibers, especially facing the adverse environmental conditions such as the presence of moisture and ultraviolet radiation, is also becoming a concern in the final response of these composites. This piece of research presents a comparative study of the strength and stiffness between two composite, both of ortoftalic polyester matrix, one reinforced with fibers of glass-E (CV) and other hybrid reinforced with natural fibers of curauá and fiberglass-E (CH). All the comparative study is based on the influence of exposure to UV rays and steam heated water in composites, simulating the aging environment. The conditions for the tests are accelerated through the use of the aging chamber. The composites will be evaluated through tests of uniaxial static mechanical traction and bending on three points. The composite of glass fiber and hybrid manufacturing industry are using the rolling manual (hand lay-up) and have been developed in the form of composites. All were designed to meet possible structural applications such as tanks and pipes. The reinforcements used in composites were in the forms of short fiber glass-E quilts (450g/m2 - 5cm) of continuous wires and fuses (whose title was of 0.9 dtex) for the curauá fibers. The results clearly show the influence of aging on the environmental mechanical performance of the composite CV and CH. The issues concerning the final characteristics of the fracture for all types of cargoes studied were also analyzed
Resumo:
In 1998 the first decorticator was developed in the Textile Engineering Laboratory and patented for the purpose of extracting fibres from pineapple leaves, with the financial help from CNPq and BNB. The objective of the present work was to develop an automatic decorticator different from the first one with a semiautomatic system of decortication with automatic feeding of the leaves and collection of the extracted fibres. The system is started through a command system that passes information to two engines, one for starting the beater cylinder and the other for the feeding of the leaves as well as the extraction of the decorticated fibres automatically. This in turn introduces the leaves between a knife and a beater cylinder with twenty blades (the previous one had only 8 blades). These blades are supported by equidistant flanges with a central transmission axis that would help in increasing the number of beatings of the leaves. In the present system the operator has to place the leaves on the rotating endless feeding belt and collect the extracted leaves that are being carried out through another endless belt. The pulp resulted form the extraction is collected in a tray through a collector. The feeding of the leaves as well as the extraction of the fibres is controlled automatically by varying the velocity of the cylinders. The semi-automatic decorticator basically composed of a chassis made out of iron bars (profile L) with 200cm length, 91 cm of height 68 cm of width. The decorticator weighs around 300Kg. It was observed that the increase in the number of blades from 8 to twenty in the beater cylinder reduced the turbulence inside the decorticator, which helped to improve the removal of the fibres without any problems as well as the quality of the fibres. From the studies carried out, from each leaf 2,8 to 4,5% of fibres can be extracted. This gives around 4 to 5 tons of fibres per hectare, which is more than that of cotton production per hectare. This quantity with no doubt could generate jobs to the people not only on the production of the fibres but also on their application in different areas
Resumo:
The micro-deformations caused by cyclic loading origins the variation of the distances between atoms of the crystal lattice producing the irreversible component. In order to study and understand the microstructural behavior of the material this paper investigated the influence suffered by residual stresses in thrust rolling bearing races fabricated in AISI 52100 steel, after tests by cyclic rolling contact in a tribometer at 1m/s under two contact pressures (500 MPa and 1400 MPa) in dry and boundary lubrication conditions. Procedures of tests thermo-acustically isolated were developed for monitoring the contact temperature and sound pressure level signals to establish a comparison between the residual stress measurements, micro-hardness Vickers and micrographic registers searching an indication of wear evolution. The sin²ψ method by X-ray diffraction technique was used to quantify the residual stresses. Three raceway zones were selected for the evaluation of wear and surface morphology after predetermined cycling, comparing with their new condition ("as received"). Micro-hardness and residual stress measurements showed significant changes after the tests and it was possible to observe the relationship between the increase of sound pressure level and the residual stress for dry and lubricated conditions.
Resumo:
The micro-deformations caused by cyclic loading origins the variation of the distances between atoms of the crystal lattice producing the irreversible component. In order to study and understand the microstructural behavior of the material this paper investigated the influence suffered by residual stresses in thrust rolling bearing races fabricated in AISI 52100 steel, after tests by cyclic rolling contact in a tribometer at 1m/s under two contact pressures (500 MPa and 1400 MPa) in dry and boundary lubrication conditions. Procedures of tests thermo-acustically isolated were developed for monitoring the contact temperature and sound pressure level signals to establish a comparison between the residual stress measurements, micro-hardness Vickers and micrographic registers searching an indication of wear evolution. The sin²ψ method by X-ray diffraction technique was used to quantify the residual stresses. Three raceway zones were selected for the evaluation of wear and surface morphology after predetermined cycling, comparing with their new condition ("as received"). Micro-hardness and residual stress measurements showed significant changes after the tests and it was possible to observe the relationship between the increase of sound pressure level and the residual stress for dry and lubricated conditions.