3 resultados para biochars, lithium-sulfur batteries, microporous structure, bamboo carbon–sulfur composites
em Universidade Federal do Rio Grande do Norte(UFRN)
Resumo:
Seeking a greater appreciation of cheese whey was developed to process the hydrogenation of lactose for the production of lactitol, a polyol with high added value, using the catalyst Ni / activated carbon (15% and 20% nickel), the nitride Mo2N, the bimetallic carbide Ni-Mo/ activated carbon and carbide Mo2C. After synthesis, the prepared catalysts were analyzed by MEV, XRD, laser granulometry and B.E.T. The reactor used in catalytic hydrogenation of lactose was the type of bed mud with a pressure (68 atm), temperature (120 oC) and stirring speed (500 rpm) remained constant during the experiments. The system operated in batch mode for the solid and liquid and semi-continuous to gas. Besides the nature of the catalyst, we studied the influence of pH of reaction medium for Mo2C carbide as well as evaluating the character of the protein inhibitor and chloride ions on the activity of catalysts Ni (20%)/Activated Carbon and bimetallic carbide Ni-Mo/Activated Carbon. The decrease in protein levels was performed by coagulation with chitosan and adsorption of chloride ions was performed by ion exchange resins. In the process of protein adsorption and chloride ions, the maximum percentage extracted was about 74% and 79% respectively. The micrographs of the powders of Mo2C and Mo2N presented in the form of homogeneous clusters, whereas for the catalysts supported on activated carbon, microporous structure proved impregnated with small particles indicating the presence of metal. The results showed high conversion of lactose to lactitol 90% for the catalyst Ni (20%)/Activated Carbon at pH 6 and 46% for the carbide Mo2C pH 8 (after addition of NH4OH) using the commercial lactose. Monitoring the evolution of the constituents present in the reaction medium was made by liquid chromatography. A kinetic model of heterogeneous Langmuir Hinshelwood type was developed which showed that the estimated constants based catalysts promoted carbide and nitride with a certain speed the adsorption, desorption and production of lactitol
Resumo:
Structural changes in waste for zeolites synthesis are subject of many studies carried out in the synthesis of molecular sieves. These materials are named molecular sieves because they have well defined pore sizes and they have the capacity of select molecules by its size. In this work, it was studied the synthesis processes of two types of molecular sieves: pillared acid clays using as starting material one natural montmorillonite clay and the synthesis of zeolites from a silico-aluminous residue. This residue is a byproduct of the extraction of lithium -spodumene. The preparation of pillared acid clays was performed in two steps: 1° acid treatment of clay samples (time and temperature studies) and 2°pilarization of them with Al13 (Keggin ion). The temperature and acid concentration affect the removal of cations in the structure and porosity of the material obtained. The analysis of X-ray diffraction (XRD) and infrared spectroscopy (IR), showed that increasing the severity of the acid treatment compromises the structural material. Also the pore size distribution is approximately uniform. Despite presenting a structural disorganization, the samples were pillared. As evidenced by XRD increasing the basal spacing, specific area and uniform porosity by adsorption of N2. Regarding the microporous molecular sieves were synthesized zeolites A and NaP1 from a silico-aluminous residue, a byproduct of extracting lithium. The temperature and time of agitation during the synthesis were the most important factors for obtaining zeolite A. The aging of the gel and the highest crystallization time promoted the formation of zeolite NaP1 using a Si / Al ratio = 3.2
Resumo:
Structural changes in waste for zeolites synthesis are subject of many studies carried out in the synthesis of molecular sieves. These materials are named molecular sieves because they have well defined pore sizes and they have the capacity of select molecules by its size. In this work, it was studied the synthesis processes of two types of molecular sieves: pillared acid clays using as starting material one natural montmorillonite clay and the synthesis of zeolites from a silico-aluminous residue. This residue is a byproduct of the extraction of lithium -spodumene. The preparation of pillared acid clays was performed in two steps: 1° acid treatment of clay samples (time and temperature studies) and 2°pilarization of them with Al13 (Keggin ion). The temperature and acid concentration affect the removal of cations in the structure and porosity of the material obtained. The analysis of X-ray diffraction (XRD) and infrared spectroscopy (IR), showed that increasing the severity of the acid treatment compromises the structural material. Also the pore size distribution is approximately uniform. Despite presenting a structural disorganization, the samples were pillared. As evidenced by XRD increasing the basal spacing, specific area and uniform porosity by adsorption of N2. Regarding the microporous molecular sieves were synthesized zeolites A and NaP1 from a silico-aluminous residue, a byproduct of extracting lithium. The temperature and time of agitation during the synthesis were the most important factors for obtaining zeolite A. The aging of the gel and the highest crystallization time promoted the formation of zeolite NaP1 using a Si / Al ratio = 3.2