Resumo:
The composition of petroleum may change from well to well and its resulting characteristics influence significantly the refine products. Therefore, it is important to characterize the oil in order to know its properties and send it adequately for processing. Since petroleum is a multicomponent mixture, the use of synthetic mixtures that are representative of oil fractions provides a better understand of the real mixture behavior. One way for characterization is usually obtained through correlation of physico-chemical properties of easy measurement, such as density, specific gravity, viscosity, and refractive index. In this work new measurements were obtained for density, specific gravity, viscosity, and refractive index of the following binary mixtures: n-heptane + hexadecane, cyclohexane + hexadecane, and benzene + hexadecane. These measurements were accomplished at low pressure and temperatures in the range 288.15 K to 310.95 K. These data were applied in the development of a new method of oil characterization. Furthermore, a series of measurements of density at high pressure and temperature of the binary mixture cyclohexane + n-hexadecane were performed. The ranges of pressure and temperature were 6.895 to 62.053 MPa and 318.15 to 413.15 K, respectively. Based on these experimental data of compressed liquid mixtures, a thermodynamic modeling was proposed using the Peng-Robinson equation of state (EOS). The EOS was modified with scaling of volume and a relatively reduced number of parameters were employed. The results were satisfactory demonstrating accuracy not only for density data, but also for isobaric thermal expansion and isothermal compressibility coefficients. This thesis aims to contribute in a scientific manner to the technological problem of refining heavy fractions of oil. This problem was treated in two steps, i.e., characterization and search of the processes that can produce streams with economical interest, such as solvent extraction at high pressure and temperature. In order to determine phase equilibrium data in these conditions, conceptual projects of two new experimental apparatus were developed. These devices consist of cells of variable volume together with a analytical static device. Therefore, this thesis contributed with the subject of characterization of hydrocarbons mixtures and with development of equilibrium cells operating at high pressure and temperature. These contributions are focused on the technological problem of refining heavy oil fractions
Resumo:
The trioxsalen (Tri) is a low-dose drug used in the treatment of psoriasis and other skin diseases. The aim of the study was applying the thermal analysis and complementary techniques for characterization, evaluation of the trioxsalen stability and components of manipulated pharmaceutical formulations. The thermal behavior of the Tri by TG/DTG-DTA in dynamic atmosphere of synthetic air and nitrogen showed the same profile with a melting peak followed by a volatilization-related event. From the curves TG / DTG is observed a single stage of mass loss. By heating the drug in the stove at temperatures of 80, 240 and 260 °C, it had no change in chemical structure through the techniques of XRD, HPLC, MIR, OM and SEM. From the non-isothermal and isothermal TG kinetic studies was possible to calculate the activation energy and reaction order for the Tri. The drug showed good thermal stability. Studies on drug-excipient compatibility showed interaction of trissoralen with sodium lauryl sulfate 1:1. There was no interaction with aerosol, pregelatinized starch, sodium starch glycolate, cellulose, croscarmellose sodium, magnesium stearate, lactose and mannitol.The characterization of three trioxsalen formulations at concentrations of 2.5, 5, 7.5, 10, 12.5 and 15 mg was performed by DSC, TG / DTG, XRD, NIR and MIR. The PCA classification method based on spectral data from the NIR and MIR of trissoralen formulations allows successful differentiation into three groups. The formulation 3 was the one that best showed analytical profile with the following composition of aerosil excipients, pre-gelatinized starch and cellulose. The activation energy of the volatilization process of the drug was determined in binary mixtures and formulation 3 through fitting and isoconversional methods. The binary mixture with sodium starch glycolate and lactose showed differences in kinetic parameters compared to the drug isolated. The thermoanalytical techniques (DSC and TG / DTG) were shown to be promising methodologies for quantifying trioxsalen obtained by the linearity, selectivity, no use solvents, without sample preparation, speed and practicality.
Resumo:
The present work is to study the characteristics and technological properties of soil-cement bricks made from binary and ternary mixtures of Portland cement, sand, water, with or without addition of gravel from the drilling of oil wells, which could be used by industry, aiming to improve its performance and reduce cost by using the residue and, consequently, increasing its useful life. The soil-cement bricks are one of the alternatives to masonry construction. These elements, after a short curing period, provide compressive strength similar to that of solid bricks and ceramic blocks, and the higher the resistance the higher the amount of cement used. We used the soil from the city of São José do Mipibu / RN, the banks of the River Baldun, cement CPIIZ-32 and residue of drill cuttings from oil wells drilling onshore wells in the town of Mossley, RN, provided Petrobras. To determine the optimum mix, we studied the inclusion of different residues (100%, 80%, 70%, 60% and 50%) where 15 bodies were made of the test piece. The assessment was made of bricks made from simple compression tests, mass loss by immersion and water absorption. The experimental results proved the efficiency and high utilization of the waste from the drilling of oil wells, making the brick-cement-soil residue with a higher strength and lower water absorption. The best result in terms of mechanical strength and water absorption for the ternary mixture was 10% soil, 14% cement and 80% residue. In terms of binary mixtures, we obtained the best result for the mix-cement residue, which was 14% cement incorporated in the residue
Resumo:
Among the options for plastics modification more convenient, both from a technical-scientific and economic, is the development of polymer blends by processing in the molten state. This work was divide into two stages, with the aim to study the phase morphology of binary blend PMMA / PET blend and this compatibilized by the addition of the poly(methyl methacrylate-co-glycidyl methacrylate-co-ethyl acrylate) copolymer (MMA-GMA-EA). In the first stage is analyzed the morphology of the blend at a preliminary stage where we used the bottle-grade PET in a Haake torque rheometer and the effect of compatibilizer in this blend was evaluated. In the second stage the blend was processed using the recycled PET in a single screw extruder and subsequently injection molding in the shape of specimens for mechanical tests. In both stages we used a transmission electron microscopy (TEM) to observe the morphologies of the samples and an image analyzer to characterize them. In the second stage, as well as analysis by TEM, tensile test, scanning electron microscopy (SEM) and atomic force microscopy (AFM) was performed to correlate the morphology with the mechanical properties. The samples used in morphological analyzes were sliced by cryo-ultramicrotomy technique for the analysis by TEM and the analysis by SEM and AFM, we used the flat face of the block after cut cryogenic. It was found that the size of the dispersed phase decreased with the addition of MMA-GMA-EA in blends prepared in a Haake. In the tensile test, the values of maximum tensile strength and modulus of elasticity is maintained in a range between the value of pure PMMA the pure PET, while the elongation at break was influenced by the composition by weight of the PMMA mixture. The coupling agent corroborated the results presented in the blend PMMA / PETrec / MMA-GMA-EA (80/15/5 %w/w), obtained by TEM, AFM and SEM. It was concluded that the techniques used had a good morphologic correlation, and can be confirmed for final analysis of the morphological characteristics of the blends PMMA / PET
Resumo:
The development of new materials to fill the demand of technological advances is a challenge for many researchers around the world. Strategies such as making blends and composites are promising alternatives to produce materials with different properties from those found in conventional polymers. The objective of this study is to evaluate the effect of adding the copolymer poly(ethylene methyl acrylate) (EMA) and cotton linter fibers (LB) on the properties of recycled poly(ethylene terephthalate) (PETrec) by the development of PETrec/EMA blend and PETrec/EMA/LB blend composite. In order to improve the properties of these materials were added as compatibilizers: Ethylene - methyl acrylate - glycidyl methacrylate terpolymer (EMA-GMA) and maleic anhydride grafted polyethylene (PE-g-MA). The samples were produced using a single screw extruder and then injection molded. The obtained materials were characterized by thermogravimetry (TG), melt flow index (MFI) mensurements, torque rheometry, pycnometry to determinate the density, tensile testing and scanning electron microscopy (SEM). The rheological results showed that the addition of the EMA copolymer increased the viscosity of the blend and LB reduces the viscosity of the blend composite. SEM analysis of the binary blend showed poor interfacial adhesion between the PETrec matrix and the EMA dispersed phase, as well as the blend composite of PETrec/EMA/LB also observed low adhesion with the LB fiber. The tensile tests showed that the increase of EMA percentage decreased the tensile strength and the Young s modulus, also lower EMA percentage samples had increased the elongation at break. The blend composite showed an increase in the tensile strength and in the Young`s modulus, and a decrease in the elongation at break. The blend formulations with lower EMA percentages showed better mechanical properties that agree with the particle size analysis which showed that these formulations presented a smaller diameter of the dispersed phase. The blend composite mechanical tests showed that this material is stronger and stiffer than the blend PETrec/EMA, whose properties have been reduced due to the presence of EMA rubbery phase. The use of EMA-GMA was effective in reducing the particle size of the EMA dispersed phase in the PETrec/EMA blend and PE-g-MA showed evidences of reaction with LB and physical mixture with the EMA
Resumo:
According to the global framework regarding new cases of tuberculosis, Brazil appears at the 18th place. Thus, the Ministry of Health has defined this disease as a priority in the governmental policies. As a consequence, studies concerning treatment and prevention have increased. Fixed-dose combination formulations (FDC) are recognized as beneficial and are recommended by WHO, but they present instability and loss on rifampicin bioavailability. The main purpose of this work was to carry out a pre-formulation study with the schedule 1 tuberculosis treatment drugs: rifampicin, isoniazid, pyrazinamide and ethambutol and pharmaceutical excipients (lactose, cellulose, magnesium stearate and talc), in order to develop an FDC product (150 mg of rifampicin + 75 mg of isoniazid + 400 mg of pyrazinamide + 250 mg of ethambutol). The studies consisted of the determination of particle size and distribution (Ferret s diameter) and shape through optical microscopy, as well as rheological and technological properties (bulk and tapped densities, Hausner Factor, Carr s Index, repose angle and flux rate) and interactions among drugs and drug excipient through thermal analysis (DSC, DTA, TG and your derivate). The results showed that, except isoniazid, the other drugs presented poor rheological properties, determined by the physical characteristics of the particles: small size and rod like particles shape for rifampicin; rectangular shape for pyrazinamide and ethambutol, beyond its low density. The 4 drug mixture also not presented flowability, particularly that one containing drug quantity indicated for the formulation of FDC products. In this mixture, isoniazid, that has the best flowability, was added in a lower concentration. The addition of microcrystalline cellulose, magnesium stearate and talc to the drug mixtures improved flowability properties. In DSC analysis probable interactions among drugs were found, supporting the hypothesis of ethambutol and pyrazinamide catalysis of the rifampicin-isoniazid reaction resulting in 3- formylrifamycin isonicotinyl hydrazone (HYD) as a degradation product. In the mixtures containing lactose Supertab® DSC curves evidenced incompatibility among drugs and excipient. In the DSC curves of mixtures containing cellulose MC101®, magnesium stearate and talc, no alterations were observed comparing to the drug profiles. The TG/DTG of the binary and ternary mixtures curves showed different thermogravimetrics profiles relating that observed to the drug isolated, with the thermal decomposition early supporting the evidences of incompatibilities showed in the DSC and DTA curves
Resumo:
This dissertation aims to assess the representativeness of the manual chilled mirror analyzer (model II Chanscope 13-1200-CN-2) used for the determination of condensed hydrocarbons of natural gas compared to the indirect methods, based on thermodynamic models equation of state. Additionally, it has been implemented in this study a model for calculating the dew point of natural gas. The proposed model is a modification of the equation of state of Peng-Robinson admits that the groups contribution as a strategy to calculate the binary interaction parameters kij (T) temperature dependence. Experimental data of the work of Brown et al. (2007) were used to compare the responses of the dew point of natural gas with thermodynamic models contained in the UniSim process simulator and the methodology implemented in this study. Then two natural gas compositions were studied, the first being a standard gas mixture gravimetrically synthesized and, second, a mixture of processed natural gas. These experimental data were also compared with the results presented by UniSim process simulator and the thermodynamic model implemented. However, data from the manual analysis results indicated significant differences in temperature, these differences were attributed to the formation of dew point of water, as we observed the appearance of moisture on the mirror surface cooling equipment
Resumo:
The synthesis of MFI-type zeolite membranes was carried by the process in situ or hydrothermal crystallization. We studied the homogenization time of the room temperature and gel filtration just before the crystallization step performed out in an oven, thus obtaining a more uniform zeolite film. The powder synthesized zeolite (structure type MFI, Silicalite) was characterized by several complementary techniques such as Xray diffraction (XRD), scanning electron microscopy (SEM), thermal analysis, temperature programmed desorption (TPD), Fourier Transform infrared spectroscopy (FTIR) and textural analysis by nitrogen adsorption (specific surface area). For the purpose of evaluating the quality of the layer supported on the ceramic support, N2 permeation tests were carried starting from room temperature to 600 °C, where values were observed values more appropriate permeation from 200 °C. With the data obtained, it was made into a graph of temperature versus permeation function, the curve of surface diffusion was found. For scanning electron microscopy, we observed the formation of homogeneous crystals and the zeolite film showed no fissures or cracks, indicating that the process of synthesis and subsequent treatments not damaged the zeolite layer on the support. Carried permeation studies were found values ranging from 3.64x10-6 to 3.78x10-6, 4.71x10-6 to 5.02x10-6, to pressures 20 and 25 psi, respectively. And the mixture xylenes/N2 values were between 5.39x10-6 to 5.67x10-6 and 8.13x10-6 to 8.36x10-6, also for pressures of 20 and 25 psi. The values found for the separation factor were 15.22 at 400 °C in the first experiment and 1.64 for the second experiment at a temperature of 150 °C. It is concluded that the Silicalite membrane was successfully synthesized and that it is effective in the separation of binary mixtures of xylenes
Resumo:
Surfactants are versatile organic compounds that have, in a single molecule, double chemical affinity. The surfactant molecule is composed by a hy drophobic tail group, a hydrocarbon chain (linear, branched, or mixed), and by a hydrophilic head group, which contains polar groups that makes it able to be applied in the organophilization process of natural clays. Microemulsions are microheterogeneous b lends composed by: a surfactant, an oily phase (non - polar solvent), an aqueous phase, and, sometimes, a co - surfactant (short - chain alcohol). They are systems with thermodynamic stability, transparent, and have high solubility power. Vermiculite is a clay m ineral with an expandable crystalline structure that has high cation exchange capacity. In this work vermiculite was used to obtain organoclays. The ionic surfactants dodecyl ammonium chlori de (DDAC) and cetyltrimethylammonium bromide (C 16 TAB) were used in the organophilization process. They were used as surfactant aqueous solutions and, for DDAC, as a microemulsion system. The organoclays were used to promote the separation of binary mixtures of xylene isomers (ortho - and meta - xylene). Dif ferent analytical techniques were used to characterize microemulsion systems and also the nanoclays. It was produced a water - rich microemulsion system with 0.92 nm droplet average diameter. The vermiculite used in this work has a cationic exchange capacity of 172 meq/100g and magnesium as main cation (24.25%). The basal spacing of natural vermiculite and organo - vermiculites were obtained by X - ray Diffraction technique. The basal spacing was 1.48nm for natural vermiculite, 4.01nm for CTAB - vermiculite (CTAB 4 ) , and 3.03nm for DDAC - vermiculite (DDAC M1A), that proves the intercalation process. Separation tests were carried out in glass columns using three binary mixtures of xylene (ortho - xylene and meta - xylene). The results showed that the organovermiculite pre sented an enhanced chemical affinity by the mixture of hydrocarbons, when compared with the natural vermiculite, and also its preference by ortho - xylene. A factorial experimental design 2 2 with triplicate at the central point was used to optimize the xylen e separation process. The experimental design revealed that the initial concentration of isomers in the mixture and the mass of organovermiculite were the significant factors for an improved separation of isomers. In the experiments carried out using a bin ary mixture of ortho - xylene and meta - xylene (2:1), after its percolating through the organovermiculite bed (DDAC M1), it was observed the preference of the organoclay by the ortho - xylene isomer, which was retained in greater quantity than the meta - xylene o ne. At the end of the treatment, it was obtained a final concentration in meta - xylene of 47.52%.
Resumo:
The present work is to study the characteristics and technological properties of soil-cement bricks made from binary and ternary mixtures of Portland cement, sand, water, with or without addition of gravel from the drilling of oil wells, which could be used by industry, aiming to improve its performance and reduce cost by using the residue and, consequently, increasing its useful life. The soil-cement bricks are one of the alternatives to masonry construction. These elements, after a short curing period, provide compressive strength similar to that of solid bricks and ceramic blocks, and the higher the resistance the higher the amount of cement used. We used the soil from the city of São José do Mipibu / RN, the banks of the River Baldun, cement CPIIZ-32 and residue of drill cuttings from oil wells drilling onshore wells in the town of Mossley, RN, provided Petrobras. To determine the optimum mix, we studied the inclusion of different residues (100%, 80%, 70%, 60% and 50%) where 15 bodies were made of the test piece. The assessment was made of bricks made from simple compression tests, mass loss by immersion and water absorption. The experimental results proved the efficiency and high utilization of the waste from the drilling of oil wells, making the brick-cement-soil residue with a higher strength and lower water absorption. The best result in terms of mechanical strength and water absorption for the ternary mixture was 10% soil, 14% cement and 80% residue. In terms of binary mixtures, we obtained the best result for the mix-cement residue, which was 14% cement incorporated in the residue
Resumo:
Among the options for plastics modification more convenient, both from a technical-scientific and economic, is the development of polymer blends by processing in the molten state. This work was divide into two stages, with the aim to study the phase morphology of binary blend PMMA / PET blend and this compatibilized by the addition of the poly(methyl methacrylate-co-glycidyl methacrylate-co-ethyl acrylate) copolymer (MMA-GMA-EA). In the first stage is analyzed the morphology of the blend at a preliminary stage where we used the bottle-grade PET in a Haake torque rheometer and the effect of compatibilizer in this blend was evaluated. In the second stage the blend was processed using the recycled PET in a single screw extruder and subsequently injection molding in the shape of specimens for mechanical tests. In both stages we used a transmission electron microscopy (TEM) to observe the morphologies of the samples and an image analyzer to characterize them. In the second stage, as well as analysis by TEM, tensile test, scanning electron microscopy (SEM) and atomic force microscopy (AFM) was performed to correlate the morphology with the mechanical properties. The samples used in morphological analyzes were sliced by cryo-ultramicrotomy technique for the analysis by TEM and the analysis by SEM and AFM, we used the flat face of the block after cut cryogenic. It was found that the size of the dispersed phase decreased with the addition of MMA-GMA-EA in blends prepared in a Haake. In the tensile test, the values of maximum tensile strength and modulus of elasticity is maintained in a range between the value of pure PMMA the pure PET, while the elongation at break was influenced by the composition by weight of the PMMA mixture. The coupling agent corroborated the results presented in the blend PMMA / PETrec / MMA-GMA-EA (80/15/5 %w/w), obtained by TEM, AFM and SEM. It was concluded that the techniques used had a good morphologic correlation, and can be confirmed for final analysis of the morphological characteristics of the blends PMMA / PET
Resumo:
The development of new materials to fill the demand of technological advances is a challenge for many researchers around the world. Strategies such as making blends and composites are promising alternatives to produce materials with different properties from those found in conventional polymers. The objective of this study is to evaluate the effect of adding the copolymer poly(ethylene methyl acrylate) (EMA) and cotton linter fibers (LB) on the properties of recycled poly(ethylene terephthalate) (PETrec) by the development of PETrec/EMA blend and PETrec/EMA/LB blend composite. In order to improve the properties of these materials were added as compatibilizers: Ethylene - methyl acrylate - glycidyl methacrylate terpolymer (EMA-GMA) and maleic anhydride grafted polyethylene (PE-g-MA). The samples were produced using a single screw extruder and then injection molded. The obtained materials were characterized by thermogravimetry (TG), melt flow index (MFI) mensurements, torque rheometry, pycnometry to determinate the density, tensile testing and scanning electron microscopy (SEM). The rheological results showed that the addition of the EMA copolymer increased the viscosity of the blend and LB reduces the viscosity of the blend composite. SEM analysis of the binary blend showed poor interfacial adhesion between the PETrec matrix and the EMA dispersed phase, as well as the blend composite of PETrec/EMA/LB also observed low adhesion with the LB fiber. The tensile tests showed that the increase of EMA percentage decreased the tensile strength and the Young s modulus, also lower EMA percentage samples had increased the elongation at break. The blend composite showed an increase in the tensile strength and in the Young`s modulus, and a decrease in the elongation at break. The blend formulations with lower EMA percentages showed better mechanical properties that agree with the particle size analysis which showed that these formulations presented a smaller diameter of the dispersed phase. The blend composite mechanical tests showed that this material is stronger and stiffer than the blend PETrec/EMA, whose properties have been reduced due to the presence of EMA rubbery phase. The use of EMA-GMA was effective in reducing the particle size of the EMA dispersed phase in the PETrec/EMA blend and PE-g-MA showed evidences of reaction with LB and physical mixture with the EMA