Resumo:

Due to properties such as excellent biocompatibility, high resistance to corrosion and low specific weight, titanium has been considered a material of great interest for Dentistry. It has been widely used in implants and orthognathic surgeries. Recently, titanium has been seen as a feasible alternative for the fabrication of removable partial denture frameworks, either in pure titanium (99.75%) or in titanium alloy forms (Ti-6Al-4V; Ti-6A1-7Nb). Based on a review of the literature, this work studied the use of titanium for the fabrication of removable partial denture frameworks, focusing on its advantages and disadvantages as well as its characteristics. It was concluded that the use of titanium is a convenient option for partially edentulous arches rehabilitation with quite satisfactory and promising clinical results. However, the need for highly-equipped laboratories increases the cost, preventing its large scale use.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Due to properties such as excellent biocompatibility, high resistance to corrosion and low specific weight, titanium has been considered a material of great interest for Dentistry. It has been widely used in implants and orthognathic surgeries. Recently, titanium has been seen as a feasible alternative for the fabrication of removable partial denture frameworks, either in pure titanium (99.75%) or in titanium alloy forms (Ti-6Al-4V; Ti-6A1-7Nb). Based on a review of the literature, this work studied the use of titanium for the fabrication of removable partial denture frameworks, focusing on its advantages and disadvantages as well as its characteristics. It was concluded that the use of titanium is a convenient option for partially edentulous arches rehabilitation with quite satisfactory and promising clinical results. However, the need for highly-equipped laboratories increases the cost, preventing its large scale use.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

NASCIMENTO,R.M. et al.Interface microstructure of alumina mechanically metallized with Ti brazed to Fe–Ni–Co using different fillers. Materials Science and Engineering A, v.466, n.1/2, p. 195-200, 2007.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Since the 1980s, different devices based on superelastic alloys have been developed to fulfill orthodontic applications. Particularly in the last decades several researches have been carried out to evaluate the mechanical behavior of Ni-Ti alloys, including their tensile, torsion and fatigue properties. However, studies regarding the dependence of elastic properties on residence time of Ni-Ti wires in the oral cavity are scarce. Such approach is essential since metallic alloys are submitted to mechanical stresses during orthodontic treatment as well as pH and temperature fluctuations. The goal of the present contribution is to provide elastic stress-strain results to guide the orthodontic choice between martensitic thermal activated and austenitic superelastic Ni-Ti alloys. From the point of view of an orthodontist, the selection of appropriate materials and the correct maintenance of the orthodontic apparatus are essential needs during clinical treatment. The present work evaluated the elastic behavior of Ni-Ti alloy wires with diameters varying from 0.014 to 0.020 inches, submitted to hysteresis tensile tests with 8% strain. Tensile tests were performed after periods of use of 1, 2 and 3 months in the oral cavity of patients submitted to orthodontic treatment. The results from the hysteresis tests allowed to exam the strain range covered by isostress lines upon loading and unloading, as well as the residual strain after unloading for both superelastic and thermal activated Ni-Ti wires. Superelastic Ni-Ti wires exhibited higher load isostress values compared to thermal activated wires. It was found that such differences in the load isostress values can increase with increasing residence time.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A frequently encountered difficulty in oral prosthetics is associated with the loss of metallic alloys during the melting stage of the production of metal-ceramic replacement systems. Remelting such materials could impar their use in oral rehabilitation due to loss in esthetics, as well as in the chemical, physical, electrochemical and mechanical properties. Nowadays, the Ni-Cr-Mo-Ti alloy is widely used in metal-ceramic systems. Manufacturers state that this material can be remelted without significant alterations in its behavior, however little has been established as to the changes in the performance of this alloy after successive remelting, which is common practice in oral prosthetics. Therefore, the objective of this study was to evaluate possible changes in the esthetics and associated properties of metalceramic samples consisting of Ni-Cr-Mo-Ti and dental porcelain. Three to five remelting steps were carried out. The results revealed that Ni-Cr-Mo-Ti can be safely used even after three remelting steps. Further remelting significantly affect the characteristics of the alloys and should not be recommended for the manufacture of metal-ceramic systems

Relevância:

30.00% 30.00%

Publicador:

Resumo:

NASCIMENTO,R.M. et al.Interface microstructure of alumina mechanically metallized with Ti brazed to Fe–Ni–Co using different fillers. Materials Science and Engineering A, v.466, n.1/2, p. 195-200, 2007.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Since the 1980s, different devices based on superelastic alloys have been developed to fulfill orthodontic applications. Particularly in the last decades several researches have been carried out to evaluate the mechanical behavior of Ni-Ti alloys, including their tensile, torsion and fatigue properties. However, studies regarding the dependence of elastic properties on residence time of Ni-Ti wires in the oral cavity are scarce. Such approach is essential since metallic alloys are submitted to mechanical stresses during orthodontic treatment as well as pH and temperature fluctuations. The goal of the present contribution is to provide elastic stress-strain results to guide the orthodontic choice between martensitic thermal activated and austenitic superelastic Ni-Ti alloys. From the point of view of an orthodontist, the selection of appropriate materials and the correct maintenance of the orthodontic apparatus are essential needs during clinical treatment. The present work evaluated the elastic behavior of Ni-Ti alloy wires with diameters varying from 0.014 to 0.020 inches, submitted to hysteresis tensile tests with 8% strain. Tensile tests were performed after periods of use of 1, 2 and 3 months in the oral cavity of patients submitted to orthodontic treatment. The results from the hysteresis tests allowed to exam the strain range covered by isostress lines upon loading and unloading, as well as the residual strain after unloading for both superelastic and thermal activated Ni-Ti wires. Superelastic Ni-Ti wires exhibited higher load isostress values compared to thermal activated wires. It was found that such differences in the load isostress values can increase with increasing residence time.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A frequently encountered difficulty in oral prosthetics is associated with the loss of metallic alloys during the melting stage of the production of metal-ceramic replacement systems. Remelting such materials could impar their use in oral rehabilitation due to loss in esthetics, as well as in the chemical, physical, electrochemical and mechanical properties. Nowadays, the Ni-Cr-Mo-Ti alloy is widely used in metal-ceramic systems. Manufacturers state that this material can be remelted without significant alterations in its behavior, however little has been established as to the changes in the performance of this alloy after successive remelting, which is common practice in oral prosthetics. Therefore, the objective of this study was to evaluate possible changes in the esthetics and associated properties of metalceramic samples consisting of Ni-Cr-Mo-Ti and dental porcelain. Three to five remelting steps were carried out. The results revealed that Ni-Cr-Mo-Ti can be safely used even after three remelting steps. Further remelting significantly affect the characteristics of the alloys and should not be recommended for the manufacture of metal-ceramic systems