Resumo:

An economical solution for cementing oil wells is the use of pre-prepared dry mixtures containing cement and additives. The mixtures may be formulated, prepared and transported to the well where is added water to be pumped.Using this method, becomes dispensable to prepare the cement mixes containing additives in the cementing operation, reducing the possibility of error. In this way, the aim of this work is to study formulations of cement slurries containing solid additives for primary cementing of oil wells onshore for typical depths of 400, 800 and 1,200 meters. The formulations are comprised of Special Class Portland cement, mineral additions and solids chemical additives.The formulated mixtures have density of 1.67 g / cm ³ (14.0 lb / gal). Their optimization were made through the analysis of the rheological parameters, fluid loss results, free water, thickening time, stability test and mechanical properties.The results showed that mixtures are in conformity the specifications for cementing oil wells onshore studied depths

Relevância:

100.00% 100.00%

Publicador:

Resumo:

An economical solution for cementing oil wells is the use of pre-prepared dry mixtures containing cement and additives. The mixtures may be formulated, prepared and transported to the well where is added water to be pumped.Using this method, becomes dispensable to prepare the cement mixes containing additives in the cementing operation, reducing the possibility of error. In this way, the aim of this work is to study formulations of cement slurries containing solid additives for primary cementing of oil wells onshore for typical depths of 400, 800 and 1,200 meters. The formulations are comprised of Special Class Portland cement, mineral additions and solids chemical additives.The formulated mixtures have density of 1.67 g / cm ³ (14.0 lb / gal). Their optimization were made through the analysis of the rheological parameters, fluid loss results, free water, thickening time, stability test and mechanical properties.The results showed that mixtures are in conformity the specifications for cementing oil wells onshore studied depths

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The preparation of cement slurries for offshore well cementing involves mixing all solid components to be added to the mixing water on the platform. The aim of this work was to study the formulation of pre-prepared dry mixtures, or grouts, for offshore oilwell cementing. The addition of mineral fillers in the strength of lightweight grouts applied for depths down to 400 m under water depths of 500 m was investigated. Lightweight materials and fine aggregates were selected. For the choice of starting materials, a study of the pozzolanic activity of low-cost fillers such as porcelain tile residue, microsilica and diatomaceous earth was carried out by X-ray diffraction and mechanical strength tests. Hardened grouts containing porcelain tile residue and microsilica depicted high strength at early ages. Based on such preliminary investigation, a study of the mechanical strength of grouts with density 1.74 g/cm3 (14.5 lb/gal) cured initially at 27 °C was performed using cement, microsilica, porcelain tile residue and an anti-foaming agent. The results showed that the mixture containing 7% of porcelain tile residue and 7% of microsilica was the one with the highest compressive strength after curing for 24 hours. This composition was chosen to be studied and adapted for offshore conditions based on testes performed at 4 °C. The grout containing cement, 7% of porcelain tile residue, 7% of active silica and admixtures (CaCl2), anti-foaming and dispersant resulted satisfactory rheology and mechanical strength after curing for 24 hours of curing

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The preparation of cement slurries for offshore well cementing involves mixing all solid components to be added to the mixing water on the platform. The aim of this work was to study the formulation of pre-prepared dry mixtures, or grouts, for offshore oilwell cementing. The addition of mineral fillers in the strength of lightweight grouts applied for depths down to 400 m under water depths of 500 m was investigated. Lightweight materials and fine aggregates were selected. For the choice of starting materials, a study of the pozzolanic activity of low-cost fillers such as porcelain tile residue, microsilica and diatomaceous earth was carried out by X-ray diffraction and mechanical strength tests. Hardened grouts containing porcelain tile residue and microsilica depicted high strength at early ages. Based on such preliminary investigation, a study of the mechanical strength of grouts with density 1.74 g/cm3 (14.5 lb/gal) cured initially at 27 °C was performed using cement, microsilica, porcelain tile residue and an anti-foaming agent. The results showed that the mixture containing 7% of porcelain tile residue and 7% of microsilica was the one with the highest compressive strength after curing for 24 hours. This composition was chosen to be studied and adapted for offshore conditions based on testes performed at 4 °C. The grout containing cement, 7% of porcelain tile residue, 7% of active silica and admixtures (CaCl2), anti-foaming and dispersant resulted satisfactory rheology and mechanical strength after curing for 24 hours of curing

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This work targetet the caprine ice cream production added with probiotic bacteria Bifidobacterium animalis subsp. lactis. It is divided into two parts. In the first one, four caprine ice cream formulations were evaluated, in which it was used hydrogenated fat (F1 and F3) or fat substitute (F2 and F4) in two different flavors (F1 and F2, passion fruit, F3 and F4, guava). Statistical differences (p<0.05) were detected for their physical-chemical properties, mainly for total solids and fat, but no differences were observed for melting test results. When it went to sensory acceptance, all four ice cream formulations reached high acceptance indexes, mostly formulation F4, which was selected for further studies. In the second part, F4 formulation was prepared with the addition of probiotic bacteria Bifidobacterium animalis subsp. lactis. The growth kinetics was studied and it was observed that the cellular concentration peak was reached after four fermentation hours (10.14 log UFC/g). This time was selected for pre-fermentation procedure and posterior addition at ice cream syrup. In this part of the study, two experimental groups were evaluated: group G1, in which the probiotic addition occurred before the maturation step and group G2, which included a pre-fermentation step and probiotic addition after ice cream maturation. The physical-chemical properties of these two ice cream groups were similar, except for pH, which was higher for group G2 (p<0.05). G1 samples had superior melting rate (3.566 mL/min) and both groups presented microbiological and sanitary results in accordance to current Brazilian legislation. Also, G1 and G2 were considered sensory accepted due to their acceptance indexes higher than 70%. G1 and G2 sensory profiles were similar (p>0.05), and both ice cream samples exhibited high creaminess (6.76 to 6.91) and mouth melting sensation (6.53 to 6.67) scores, while low sandiness scores (0.85 to 0.86) were observed, positive characteristics for this kind of food product. During the first 24 hours after ice cream production, the population of B. animalis subsp. lactis decreased, reaching 7.15 e 6.92 log CFU/g for G1 and G2, respectively. Probiotic bacteria counts fluctuated in ice cream samples during the first 108 days at frozen storage, especially for G2 group. Decreased probiotic viability was observed for G1 samples during the first 35 days of frozen storage, mild variation between 35 and 63 days and stabilized counts were observed after this time. After 21 days at frozen storage, ice cream samples of G1 and G2 groups reached 1.2 x 109 and 1.3 x 109 CFU/portion, respectively. After 108 days under these storage conditions, the survival rate of B. animalis subsp. lactis was 94.26% and 81.10% for G1 and G2 samples, respectively. After simulation of gastroenteric conditions, G2 group reached 9.72 x 105 CFU/portion. Considering the current requirements of Brazilian legislation, which stipulates that functional foods must have minimum probiotic count between 108 and 109 CFU/portion and detectable probiotic bacteria after being submitted to gastroenteric conditions, it is concluded that the ice cream with the addition of Bifidobacterium animalis subsp. lactis made as shown in this work, can be considered as a dairy functional food

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The generation of industrial wastes has been increased more and more in recent decades, motivating studies about a correct sustainable allocation and that also represents advantages for their generators. In this context, are included two companies of cleaning products niche, located in São José do Mipibu/RN, that produces industrial sludge at a sewage treatment plant, and that is the main approach of this research. Given this, it was studied the incorporation potentiality of this sludge as a mineral addition in cement matrix for concrete production due it high capacity of wastes immobilization inside this material, which are subsequently used in the company for making precast articles. Were added different sludge concentrations (5, 10, 15 and 20%) in a common trait (1: 2: 3), and evaluated their techniques and microstructural implications via workability test in fresh state and compressive strength, full porosity and scanning electron microscopy (SEM) in the hardened state. The results demonstrated the feasibility of the process both from a technical and environmental view as economical. All concretes produced with residue showed an increase of workability given the nature of the waste that had surfactants substances capable of adsorbing tiny particles of air into the batter. However, for all concentrations were obtained lower compressive resistances than standard concrete, with a reduction of 39% for samples with 20% of sludge. This are attributed mainly to an increase of porosity in the transition zone of these material, resulting from increased formation of ettringite at the detriment to the formation of other compounds, but which still allows the use of these for the manufacture of concrete articles with non-structural nature, such as precast floor. In addition, the water absorption and void ratio increased slightly for all samples, except the concrete with 20% of waste that has a reduction for the last parameter. Given this context, the recommended maximum level is 20%, constituting a significant proportion and able to allocate sustainably all waste generated in the industry.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

To study the teaching/learning process about the Nursing procedures carried out in the laboratory, and learn both the sapiens and the demens dimensions of such process, is the main purpose of this study. The objectives are to: identify the major laboratory contributions to the teaching/learning process from the point of view of undergraduate students and the feelings they express; describe the difficulties they have identified; and analyze the relevance of the laboratory to this process. As part of the inquiry procedure, four core group meetings were held with 26 undergraduate students who had completed the course on Semiology and Semiotics in Nursing, which is the course where the Nursing laboratory is most needed as a learning space. The analysis, based on a qualitative approach, had as fundamental theoretical support studies made by Friedlander and Hayashida, who deal with learning/teaching in the Nursing laboratory, and by authors who favor humanization in teaching such as, among others, Freire, Maturana, Morin, Assmann. Results point toward the relevance of the Nursing laboratory as a facilitator for the learning/teaching process. In their speech the students repeatedly state that the development of procedures in simulated situations enable them to become more self-assured and technically prepared for caring. In addition, they emphasize that feelings such as fear, lack of confidence, anxiety, anguish and panic become diminished at the time of their clinic experience when they have had previous learning in the laboratory. They have also acknowledged that some difficulties of structural nature have become obstacles to a high-quality learning development. In summary, in spite of the difficulties that have been pointed out by the students concerning the use of the Nursing laboratory in the learning/teaching process, they also recognize that this is the locus par excellence where they can develop their skills and appease their anxieties

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Grautes are dry mixes with hydraulic characteristics widely used in construction. This material comprises cement, mineral additives and dosed in accordance with the desired properties. The use of grautes in cementing oil wells potentially increases the precision in the composition of the mixture, since it is requires only the addition of the mixing water before its pumping. Such benefit may be availed in cementing wells since the formulations grautes meet the temperature and pressure characteristics typical of wells. The objective of this study is to evaluate the effect of adding different percentages of industrial minerals properties of light grautes for onshore oil wells. For the formulation of the employees were grautes light industrial minerals and waste minerals abundant in the Northeast, in addiction to Portland cement and chemical additives Special class. Grautes were formulated with densities between 1.55 g/cm3 (13.0 lb/gal) and 1.68 g/cm3 (14 lb/gal). Tests results showed that grautes with higher density in the range studied meet the specifications for cementation of shallow wells onshore. The compositions lighter can also be adjusted for applying the material in the cementation of oil wells

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Grautes are dry mixes with hydraulic characteristics widely used in construction. This material comprises cement, mineral additives and dosed in accordance with the desired properties. The use of grautes in cementing oil wells potentially increases the precision in the composition of the mixture, since it is requires only the addition of the mixing water before its pumping. Such benefit may be availed in cementing wells since the formulations grautes meet the temperature and pressure characteristics typical of wells. The objective of this study is to evaluate the effect of adding different percentages of industrial minerals properties of light grautes for onshore oil wells. For the formulation of the employees were grautes light industrial minerals and waste minerals abundant in the Northeast, in addiction to Portland cement and chemical additives Special class. Grautes were formulated with densities between 1.55 g/cm3 (13.0 lb/gal) and 1.68 g/cm3 (14 lb/gal). Tests results showed that grautes with higher density in the range studied meet the specifications for cementation of shallow wells onshore. The compositions lighter can also be adjusted for applying the material in the cementation of oil wells

Relevância:

50.00% 50.00%

Publicador:

Resumo:

Oil wells subjected to cyclic steam injection present important challenges for the development of well cementing systems, mainly due to tensile stresses caused by thermal gradients during its useful life. Cement sheath failures in wells using conventional high compressive strength systems lead to the use of cement systems that are more flexible and/or ductile, with emphasis on Portland cement systems with latex addition. Recent research efforts have presented geopolymeric systems as alternatives. These cementing systems are based on alkaline activation of amorphous aluminosilicates such as metakaolin or fly ash and display advantageous properties such as high compressive strength, fast setting and thermal stability. Basic geopolymeric formulations can be found in the literature, which meet basic oil industry specifications such as rheology, compressive strength and thickening time. In this work, new geopolymeric formulations were developed, based on metakaolin, potassium silicate, potassium hydroxide, silica fume and mineral fiber, using the state of the art in chemical composition, mixture modeling and additivation to optimize the most relevant properties for oil well cementing. Starting from molar ratios considered ideal in the literature (SiO2/Al2O3 = 3.8 e K2O/Al2O3 = 1.0), a study of dry mixtures was performed,based on the compressive packing model, resulting in an optimal volume of 6% for the added solid material. This material (silica fume and mineral fiber) works both as an additional silica source (in the case of silica fume) and as mechanical reinforcement, especially in the case of mineral fiber, which incremented the tensile strength. The first triaxial mechanical study of this class of materials was performed. For comparison, a mechanical study of conventional latex-based cementing systems was also carried out. Regardless of differences in the failure mode (brittle for geopolymers, ductile for latex-based systems), the superior uniaxial compressive strength (37 MPa for the geopolymeric slurry P5 versus 18 MPa for the conventional slurry P2), similar triaxial behavior (friction angle 21° for P5 and P2) and lower stifness (in the elastic region 5.1 GPa for P5 versus 6.8 GPa for P2) of the geopolymeric systems allowed them to withstand a similar amount of mechanical energy (155 kJ/m3 for P5 versus 208 kJ/m3 for P2), noting that geopolymers work in the elastic regime, without the microcracking present in the case of latex-based systems. Therefore, the geopolymers studied on this work must be designed for application in the elastic region to avoid brittle failure. Finally, the tensile strength of geopolymers is originally poor (1.3 MPa for the geopolymeric slurry P3) due to its brittle structure. However, after additivation with mineral fiber, the tensile strength became equivalent to that of latex-based systems (2.3 MPa for P5 and 2.1 MPa for P2). The technical viability of conventional and proposed formulations was evaluated for the whole well life, including stresses due to cyclic steam injection. This analysis was performed using finite element-based simulation software. It was verified that conventional slurries are viable up to 204ºF (400ºC) and geopolymeric slurries are viable above 500ºF (260ºC)

Relevância:

50.00% 50.00%

Publicador:

Resumo:

Lightweight oilwell cement slurries have been recently studied as a mean to improve zonal isolation and sheath-porous formation adherence. Foamed slurries consisting of Portland cement and air-entraining admixtures have become an interesting option for this application. The loss in hydrostatic pressure as a consequence of cement hydration results in the expansion of the air bubbles entrapped in the cement matrix, thus improving the sheath-porous formation contact. Consequently, slurries are able to better retain their water to complete the hydration process. The main objective of the present study was to evaluate the effect of the addition of an air-entraining admixture on the density, stability and permeability of composite slurries containing Portland cement and diatomite as light mineral load. Successful formulations are potential cementing materials for low fracture gradient oilwells. The experimental procedures used for slurry preparation and characterization were based on the American Petroleum Institute and ABNT guidelines Slurries containing a pre-established concentration of the air-entraining admixture and different contents of diatomite were prepared aiming at final densities of 13 to 15 lb/gal. The results revealed that the reduction of 15 to 25% of the density of the slurries did not significantly affect their strength. The addition of both diatomite and the air-entraining admixture increased the viscosity of the slurry providing better air-bubble retention in the volume of the slurry. Stable slurries depicted bottom to top density variation of less than 1.0 lb/gal and length reduction of the stability sample of 5.86 mm. Finally, permeability coefficient values between 0.617 and 0.406 mD were obtained. Therefore, lightweight oilwell cement slurries depicting a satisfactory set of physicochemical and mechanical properties can be formulated using a combination of diatomite and air-entraining admixtures for low fracture gradient oilwells

Relevância:

50.00% 50.00%

Publicador:

Resumo:

Oil wells subjected to cyclic steam injection present important challenges for the development of well cementing systems, mainly due to tensile stresses caused by thermal gradients during its useful life. Cement sheath failures in wells using conventional high compressive strength systems lead to the use of cement systems that are more flexible and/or ductile, with emphasis on Portland cement systems with latex addition. Recent research efforts have presented geopolymeric systems as alternatives. These cementing systems are based on alkaline activation of amorphous aluminosilicates such as metakaolin or fly ash and display advantageous properties such as high compressive strength, fast setting and thermal stability. Basic geopolymeric formulations can be found in the literature, which meet basic oil industry specifications such as rheology, compressive strength and thickening time. In this work, new geopolymeric formulations were developed, based on metakaolin, potassium silicate, potassium hydroxide, silica fume and mineral fiber, using the state of the art in chemical composition, mixture modeling and additivation to optimize the most relevant properties for oil well cementing. Starting from molar ratios considered ideal in the literature (SiO2/Al2O3 = 3.8 e K2O/Al2O3 = 1.0), a study of dry mixtures was performed,based on the compressive packing model, resulting in an optimal volume of 6% for the added solid material. This material (silica fume and mineral fiber) works both as an additional silica source (in the case of silica fume) and as mechanical reinforcement, especially in the case of mineral fiber, which incremented the tensile strength. The first triaxial mechanical study of this class of materials was performed. For comparison, a mechanical study of conventional latex-based cementing systems was also carried out. Regardless of differences in the failure mode (brittle for geopolymers, ductile for latex-based systems), the superior uniaxial compressive strength (37 MPa for the geopolymeric slurry P5 versus 18 MPa for the conventional slurry P2), similar triaxial behavior (friction angle 21° for P5 and P2) and lower stifness (in the elastic region 5.1 GPa for P5 versus 6.8 GPa for P2) of the geopolymeric systems allowed them to withstand a similar amount of mechanical energy (155 kJ/m3 for P5 versus 208 kJ/m3 for P2), noting that geopolymers work in the elastic regime, without the microcracking present in the case of latex-based systems. Therefore, the geopolymers studied on this work must be designed for application in the elastic region to avoid brittle failure. Finally, the tensile strength of geopolymers is originally poor (1.3 MPa for the geopolymeric slurry P3) due to its brittle structure. However, after additivation with mineral fiber, the tensile strength became equivalent to that of latex-based systems (2.3 MPa for P5 and 2.1 MPa for P2). The technical viability of conventional and proposed formulations was evaluated for the whole well life, including stresses due to cyclic steam injection. This analysis was performed using finite element-based simulation software. It was verified that conventional slurries are viable up to 204ºF (400ºC) and geopolymeric slurries are viable above 500ºF (260ºC)

Relevância:

50.00% 50.00%

Publicador:

Resumo:

Lightweight oilwell cement slurries have been recently studied as a mean to improve zonal isolation and sheath-porous formation adherence. Foamed slurries consisting of Portland cement and air-entraining admixtures have become an interesting option for this application. The loss in hydrostatic pressure as a consequence of cement hydration results in the expansion of the air bubbles entrapped in the cement matrix, thus improving the sheath-porous formation contact. Consequently, slurries are able to better retain their water to complete the hydration process. The main objective of the present study was to evaluate the effect of the addition of an air-entraining admixture on the density, stability and permeability of composite slurries containing Portland cement and diatomite as light mineral load. Successful formulations are potential cementing materials for low fracture gradient oilwells. The experimental procedures used for slurry preparation and characterization were based on the American Petroleum Institute and ABNT guidelines Slurries containing a pre-established concentration of the air-entraining admixture and different contents of diatomite were prepared aiming at final densities of 13 to 15 lb/gal. The results revealed that the reduction of 15 to 25% of the density of the slurries did not significantly affect their strength. The addition of both diatomite and the air-entraining admixture increased the viscosity of the slurry providing better air-bubble retention in the volume of the slurry. Stable slurries depicted bottom to top density variation of less than 1.0 lb/gal and length reduction of the stability sample of 5.86 mm. Finally, permeability coefficient values between 0.617 and 0.406 mD were obtained. Therefore, lightweight oilwell cement slurries depicting a satisfactory set of physicochemical and mechanical properties can be formulated using a combination of diatomite and air-entraining admixtures for low fracture gradient oilwells

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The drilling of wells for petroleum extraction generates rocks and soils fragments, among other residues. These fragments are denominated petroleum drilling gravel or simply petroleum drilling residue. On the sites of onshore exploration are formed big deposits of drilling gravel, an expensive final destination material. This work aims at evaluating the addition of drilling residue to a lateritic soil, as composite material, for construction of compacted fills for earth work projects. Soil and residue were evaluated by X-ray diffraction (XRD) and X-ray fluorescence (XRF) and by laboratory tests traditionally used in soil mechanics, as particle-size analysis of soils, determination of liquid and plasticity indexes and compaction test. After soil and residue characterization, soil-residue mixtures were studied, using dosages of 2,5%, 5%, 10%, and 15% of residue in relation to the dry soil mass. These mixtures were submitted to compaction test, CBR, direct shear test and consolidation test. The test results were compared to the current legislation of DNIT for compacted fill construction. The results showed that the mixtures presented the minimal necessary parameters, allowing, from the point of view of geotechnical analysis, the use of these mixtures for construction of compacted fills

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Oil well cementing materials consist of slurries of Special class Portland cement dispersed in water. Admixtures can be used to provide the necessary fluidity, so the material can be efficiently pumped down as well as penetrate porous rocks with controlled filter loss. Construction admixtures can be used to modify the properties of oil well cements provided they can withstand and hold their properties at the higher than ambient temperatures usually encountered in oil fields. In civil construction, superplasticizer play the role of dispersants that reduce the facto r of water cement improve mechanical properties and fluidity of the cement, whereas anti-segregation agents improve the workability of the slurry. In the present study, oil well cement slurries were produced adding both a dispersant and an anti-segregation agent conventionally used in Portland CPII-Z-32 RS cement aiming at materials for primary cementing and squeeze operations. Three basic aspects were evaluated: fluidity, filter loss and the synergetic effect of the admixtures at two temperatures, i.e., 27°C and 56°C, following API RP 10B practical recommendations. The slurries were prepared using admixture concentrations varying from 2.60 Kgf/m3 (0.02 gallft3) to 5.82 Kgf/m3 (0.045 galJft3) BWOC. The density of the slurries was set to 1.89 g/cm3 (15.8 Ib/gal). 0.30 to 0.60% BWOC of a CMC-based anti-segregation agent was added to the cement to control the filter loss. The results showed that the addition of anti-segregation at concentrations above 0.55% by weight of cement resulted in the increased viscosity of the folders in temperatures evaluated. The increasing the temperature of the tests led to a reduction in the performance of anti-segregation. At concentrations of 5.20 kgf/m3 (0,040 gallft3) and 5.82 Kgf/m3 (0,045 gal/ft 3) observed a better performance of the properties evaluated in the proposed system. At low temperature was observed instability in the readings of rheology for all concentrations of anti-segregation. Contents that increasing the concentration of anti¬-segregation is limited concentrations greater than 0.55 % BWOC of the CMC in temperature analyzed. The use of the system with CMC promoted a good performance against the properties evaluated. The principal function of anti¬-segregation was optimized with increasing concentration of superplasticizer, at temperatures above the 2rC. The study of the behaviour of systemic additives, resulting in slurries of cement, which can be optimized face studies of other intrinsic properties in oil fields