This work makes use of the Pechini process for synthesis of the solutions and the dip-coating process for the addition of zirconium oxide films pure and doped cerium metal substrates. The metals with ceramic substrates were subjected to severe conditions of salinity. The x-ray fluorescence of the substrate showed a great diversity of chemical elements. The x-ray diffraction of the samples showed the phase of iron substrate because the thickness of nano-thin film. Tests using an LPR probe showed that the film presents with zirconia corrosion independent of film thickness. The substrates of ZrO2-doped ceria showed low chemical attack of the salt in films with less than 15 dives. The results imply that ultrathin films are shown in protecting metallic substrates

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In this work a biodegradable composite using the carnauba straw s powder as reinforcement on chitosan matrix polymeric were manufactured. Firstly, were carried out the chemistry characterization of the carnauba straw s powder before and after treatments with NaOH and hexane. Goering and Van Soest method (1970), flotation test, moisture absorption, FTIR, TG/DTG, DSC and SEM have also being carried out. Composites were developed with variations in granulometry and in powder concentrations. They were characterized by TG/DTG, SEM and mechanicals properties. The results of chemical composition showed that the carnauba straw s powder is composed of 41% of cellulose; 28,9% of hemicellulose and 14% of lignin.The flotation test have indicated that the chemical treatment with NaOH decreased the powder s hidrophilicity.The thermal analysis showed increased of thermal stability of material after treatments. The results of FTIR and SEM revealed the removal of soluble materials from the powder (hemicelluloses and lignin), the material became rougher and clean. The composites obtained showed that the mechanicals properties of the composites were decreased in respect at chitosan films, and the composites with the powder at 150 Mesh showed less variation in the modulus values. The speed test of 10 mm/min showed the better reproducibility of the results and is in agreement to the standard ASTM D638. The SEM analysis of fracture showed the low adhesion between the fiber/matrix. The increase of volume of powder in the composite caused a decrease in values of stress and strain for the samples with untreated powder and treated with hexane. The composite with 50% of the powder s treated in NaOH didn t have significant variation in the values of stress and strain as compared with the composites with 10% of the powder, showing that the increase in the volume of fiber didn t affect the stress and strain of the composite. Thereby, it is concluded that the manufacture of polymeric composites of chitosan using carnauba straw s powder can be done, without need for pre-treatment of reinforcement, become the couple of carnauba straw s powder-chitosan a good alternative for biodegradable composites

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The synthesis of MFI-type zeolite membranes was carried by the process in situ or hydrothermal crystallization. We studied the homogenization time of the room temperature and gel filtration just before the crystallization step performed out in an oven, thus obtaining a more uniform zeolite film. The powder synthesized zeolite (structure type MFI, Silicalite) was characterized by several complementary techniques such as Xray diffraction (XRD), scanning electron microscopy (SEM), thermal analysis, temperature programmed desorption (TPD), Fourier Transform infrared spectroscopy (FTIR) and textural analysis by nitrogen adsorption (specific surface area). For the purpose of evaluating the quality of the layer supported on the ceramic support, N2 permeation tests were carried starting from room temperature to 600 °C, where values were observed values more appropriate permeation from 200 °C. With the data obtained, it was made into a graph of temperature versus permeation function, the curve of surface diffusion was found. For scanning electron microscopy, we observed the formation of homogeneous crystals and the zeolite film showed no fissures or cracks, indicating that the process of synthesis and subsequent treatments not damaged the zeolite layer on the support. Carried permeation studies were found values ranging from 3.64x10-6 to 3.78x10-6, 4.71x10-6 to 5.02x10-6, to pressures 20 and 25 psi, respectively. And the mixture xylenes/N2 values were between 5.39x10-6 to 5.67x10-6 and 8.13x10-6 to 8.36x10-6, also for pressures of 20 and 25 psi. The values found for the separation factor were 15.22 at 400 °C in the first experiment and 1.64 for the second experiment at a temperature of 150 °C. It is concluded that the Silicalite membrane was successfully synthesized and that it is effective in the separation of binary mixtures of xylenes

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Corrosion usually occurs in pipelines, so that it is necessary to develop new surface treatments to control it. Surfactants have played an outstanding role in this field due to its capacity of adsorbing on metal surfaces, resulting in interfaces with structures that protect the metal at low surfactant concentrations. The appearance of new surfactants is a contribution to the area, as they increase the possibility of corrosion control at specific conditions that a particular oil field presents. The aim of this work is to synthesize the surfactants sodium 12 hydroxyocadecenoate (SAR), sodium 9,10-epoxy-12 hydroxyocadecanoate (SEAR), and sodium 9,10:12,13-diepoxy-octadecanoate (SEAL) and apply them as corrosion inhibitors, studying their action in environments with different salinities and at different temperatures. The conditions used in this work were chosen in order to reproduce oil field reality. The study of the micellization of these surfactants in the liquid-gas interface was carried out using surface tensiometry. It was observed that cmc increased as salt concentration was increased, and temperature and pH were decreased, while cmc decreased with the addition of two epoxy groups in the molecule. Using the values of cmc and the Gibbs equation, the values of Gibbs free energy of adsorption, area per adsorbed molecule, and surface excess were calculated. The surface excess increases as salt concentration and temperature decreases, increasing as pH is increased. The area per adsorbed molecule and the free energy of adsorption decrease with salt concentration, temperature, and pH increase. SAXS results showed that the addition of epoxy group in surfactant structure results in a decrease in the repulsion between the micelles, favoring the formation of more oblong micellar structures, ensuring a better efficiency of metal coverage. The increase in salt and surfactant concentrations provides an increase in micellar diameter. It was shown that the increase in temperature does not influence micellar structure, indicating thermal stability that is advantageous for use as corrosion inhibitor. The results of inhibition efficiency for the surfactants SEAR and SEAL were considered the best ones. Above cmc, adsorption occurred by the migration of micelles from the bulk of the solution to the metal surface, while at concentrations below cmc film formation must be due to the adsorption of semi-micellar and monomeric structures, certainly due to the presence of the epoxy group, which allows side interactions of the molecule with the metal surface. The metal resistance to corrosion presented values of 90% of efficiency. The application of Langmuir and Frumkin isotherms showed that the later gives a better description of adsorption because the model takes into account side interactions from the adsorbing molecules. Wettability results showed that micelle formation on the solid surface occurs at concentrations in the magnitude of 10-3 M, which isthe value found in the cmc study. This value also justifies the maximum efficiencies obtained for the measurements of corrosion resistance at this concentration. The values of contact angle as a function of time suggest that adsorption increases with time, due to the formation of micellar structures on metal surface

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In this paper, the technique of differential pulse voltammetry (DPV) has been studied for monitoring the concentration of oxalic acid (OA) during their electrochemical oxidation (EO) in acidic medium using platinum anode supported on titanium (Ti / Pt). The DPV was standardized and optimized using a glassy carbon electrode modified with cysteine. The modification with cysteine was developed electrochemically, forming a polymeric film on the surface of the glassy carbon electrode. The formation of the polymer film was confirmed by analysis of scanning electron microscope and atomic force microscope, confirming the modification of the electrode. The electrochemical degradation was developed using different current densities 10, 20 30 and 40 mA cm -2 electrode with Ti / Pt observing the degradation of oxalic acid, and monitored using the method of KMnO4 titration. However, the analyzes with DPV showed the same behavior elimination of oxalic acid titration. Compared with the titration method classical observed and DPV could be a good fit, confidence limits of detection and confirming the applicability of the technique electroanalytical for monitoring the degradation of oxalic acid

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A new self-sustainable film was prepared through the sol-gel modified method, previously employed in our research group; sodium alginate was used as the polymer matrix, along with plasticizer glycerol, doped with titanium dioxide (TiO2) and tungsten trioxide (WO3). By varying WO3 concentration (0,8, 1,6, 2,4 and 3,2 μmol) and keeping TiO2 concentration constant (059 mmol), it was possible to study the contribution of these oxides on the obtained films morphological and electrical properties. Self-sustainable films have analyzed by Fourier Transform Infrared Spectroscopy (FTIR), X-Ray Diffraction (XDR), Scanning Electron Microscope (SEM), Energy Dispersive X-ray Spectroscopy (EDS) and Electrochemical Impedance Spectroscopy (EIS). By the IR specters, it was possible identify the TiO2, and posteriorly WO3, addition has provided dislocation of alginate characteristics bands to smaller vibrations frequencies indicating an electrostatic interaction between the oxides and the polymer matrix. Diffractograms show predominance of the amorphous phase in the films. SEM, along with EDX, analysis revealed self-sustainable films showed surface with no cracks and relative dispersion of the oxides throughout the polymer matrix. From Impedance analysis, it was observe increasing WO3 concentration to 2,4 μmol provided a reduction of films resistive properties and consequent improvement of conductive properties

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The circadian behavior associated with the 24 hours light-dark (LD) cycle (T24) is due to a circadian clock , which in mammals is located in the hypothalamic suprachiasmatic nucleus (SCN). Under experimental conditions in which rats are espoused to a symmetric LD 22h cycle (T22) the two SCN regions, ventrolateral (vl) and dorsomedial (dm), can be functionally isolated, suggesting that each region regulates distinct physiological and behavioral components. The vl region regulates the locomotor activity and slow wave sleep (SWS) rhythms, while the dm region assures the body temperature and paradoxical sleep (PS) rhythms regulation. This research aimed to deepen the knowledge on the functional properties of circadian rhythmicity, specifically about the internal desynchronization process, and its consequences to locomotor activity and body temperature rhythms as well as to the sleep-wake cycle pattern in rats. We applied infrared motion sensors, implanted body temperature sensors and a telemetry system to record electrocorticogram (ECoG) and electromyogram (EMG) in two rat groups. The control group under 24h period LD cycle (T24: 12hL-12hD) to the baseline record and the experimental group under 22h period LD cycle (T22: 11hL- 11hD), in which is known to occur the uncoupling process of the circadian locomotor activity rhythm where the animals show two distinct locomotor activity rhythms: one synchronized to the external LD cycle, and another expressed in free running course, with period greater than 24h. As a result of 22h cycles, characteristic locomotor activity moment appear, that are coincidence moments (T22C) and non coincidence moments (T22NC) which were the main focus or our study. Our results show an increase in locomotor activity, especially in coincidence moments, and the inversion of locomotor activity, body temperature, and sleep-wake cycle patterns in non coincidence moments. We can also observe the increase in SWS and decrease in PS, both in coincidence and non coincidence moments. Probably the increases in locomotor activity as a way to promote the coupling between circadian oscillators generate an increased homeostatic pressure and thus increase SWS, promoting the decreasing in PS

Relevância:

10.00% 10.00%

Publicador:

Resumo:

O presente trabalho tem como objetivo investigar as características de filmes de SnO2 depositados em substrato de vidro borosilicato por um processo de silk-screen modificado para obtenção de espessura fina compatível com a aplicação em células solares policristalinas de baixo custo. O filme de SnO2 é um dos mais apropriados para obtenção de vidro TCO (transparent conductive oxide) para uso em células solares devido a sua baixa resistividade elétrica e alta transmitância, sendo quimicamente inerte, mecanicamente duro e tem resistência a altas temperaturas, o que facilita então a calcinação das amostras entre 500º C a 550º C. Os filmes foram obtidos a partir de uma solução precursora básica, preparada pela dissolução de SnCl2.2H2O em Etanol (99,5 %). Foi realizado um planejamento fatorial 2(3-1) para analisar a influência dos parâmetros concentração da solução precursora (CETN), temperatura de calcinação (TC) e taxa de aquecimento (tX) na calcinação, sendo a concentração CETN o parâmetro que apresentou maior efeito sobre os parâmetros de respostas investigados: espessura do filme (ω), resistividade de superfície (ρ) e a transmitância relativa (θ). Foi possível obter com a metodologia utilizada, filmes com espessuras da ordem de 1 Nm com resistividade de superfície de 10 / e transmitância relativa entre 70 e 80 %.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

We report a theoretical investigation of thermal hysteresis in magnetic nanoelements. Thermal hysteresis originates in the existence of meta-stable states in temperature intervals which may be tuned by small values of the external magnetic field, and are controlled by the systems geometric dimensions as well as the composition. Two systems have been investigated. The first system is a trilayer consisting of one antiferromagnetic MnF2 film, exchange coupled with two Fe lms. At low temperatures the ferromagnetic layers are oriented in opposite directions. By heating in the presence of an external magnetic field, the Zeeman energy induces a gradual orientation of the ferromagnets with the external field and the nucleation of spin- op-like states in the antiferromagnetic layer, leading eventually, in temperatures close to the Neel temperature, to full alignment of the ferromagnetic films and the formation of frustrated exchange bonds in the center of the antiferromagnetic layer. By cooling down to low temperatures, the system follows a different sequence of states, due to the anisotropy barriers of both materials. The width of the thermal hysteresis loop depends on the thicknesses of the FM and AFM layers as well as on the strength of the external field. The second system consists in Fe and Permalloy ferromagnetic nanoelements exchange coupled to a NiO uncompensated substrate. In this case the thermal hysteresis originates in the modifications of the intrinsic magnetic

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior

Relevância:

10.00% 10.00%

Publicador:

Resumo:

We report a theoretical investigation of the magnetic phases and hysteresis of exchange biased ferromagnetic (F) nanoelements for three di erent systems: exchange biased nanoparticles, exchange biased narrow ferromagnetic stripes and exchange biased thin ferromagnetic lms. In all cases the focus is on the new e ects produced by suitable patterns of the exchange energy coupling the ferromagnetic nanoelement with a large anisotropy antiferromagnetic (AF) substrate. We investigate the hysteresis of iron and permalloy nanoparticles with a square basis, with lateral dimensions between 45 nm and 120 nm and thickness between 12 nm and 21 nm. Interface bias is aimed at producing large domains in thin lms. Our results show that, contrary to intuition, the interface exchange coupling may generate vortex states along the hysteresis loop. Also, the threshold value of the interface eld strength for vortex nucleation is smaller for iron nanoelements. We investigate the nucleation and depinning of an array of domain walls pinned at interface defects of a vicinal stripe/AF bilayer. The interface exchange eld displays a periodic pattern corresponding to the topology of the AF vicinal substrate. The vicinal AF substrate consists of a sequence of terraces, each with spins from one AF subalattice, alternating one another. As a result the interface eld of neighboring terraces point in opposite direction, leading to the nucleation of a sequence of domain walls in the ferromagnetic stripe. We investigated iron an permalloy micrometric stripes, with width ranging from 100 nm and 300 nm and thickness of 5 nm. We focused in domain wall sequences with same chirality and alternate chirality. We have found that for 100nm terraces the same chiraility sequence is more stable, requiring a larger value of the external eld for depinning. The third system consists of an iron lm with a thickness of 5 nm, exchange coupled to an AF substrate with a periodic distribution of islands where the AF spins have the opposite direction of the spins in the background. This corresponds to a two-sublattice noncompensated AF plane (such as the surface of a (100) FeF2 lm), with monolayer-height islands containing spins of one sublattice on a surface containing spins of the opposite sublattice. The interface eld acting in the ferromagnetic spins over the islands points in the opposite direction of that in the spins over the background. This a model system for the investigation of interface roughness e ects. We have studied the coercicivity an exchange bias hysteresis shift as a function of the distance between the islands and the degree of interface roughness. We have found a relevant reduction of coercivity for nearly compensated interfaces. Also the e ective hysteresis shift is not proportional to the liquid moment of the AF plane. We also developed an analytical model which reproduces qualitatively the results of numerical simulations

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Pyrometamorphism results from conditions of high temperatures and very low pressures provoked by the intrusion of hypabyssal basic bodies into sedimentary or metassedimentary hosting rocks. The onshore portion of the Potiguar Basin in NE Brazil offers examples of this type of metamorphism nearby the contacts of Paleogene to Neogene plugs, sills and dikes of diabases and basalts crosscutting sandstones, siltstones and shales of the Açu Formation (Albian-Cenomanian). The thermal effects over these rocks are reflected on textures and minerals assemblages that characterize the sanidinite facies of metamorphism, often with partial melting of the feldspathic and mica-rich matrix. The liquid formed is potassic and peraluminous, with variably colored rhyolitic glass (colorless, yellow, brown) comprising microcrystals of tridymite, sanidine and clinoenstatite, besides residual detrital clasts of quartz and rarely zircon, staurolite and garnet. Lenses of shale intercalated within the sandstones display crystallites of Fe-cordierite (sekaninaite), mullite, sanidine, armalcolite (Fe-Ti oxide) and brown spinel. The rocks formed due to the thermal effect of the intrusions are called buchites for which two types are herein described: a light one derived from feldspathic sandstone and siltstone protoliths; and a dark one derived from black shale protoliths. Textures indicating partial melting and minerals such as sanidine, mullite, tridymite and armalcolite strongly demonstrate that during the intrusion of the basic bodies the temperature reached 1,000-1,150°C, and was followed by quenching. Cooling of the interstitial melts has as consequences the closure of pores and decrease of the permeability of the protolith, which varies from about 17-11% in the unaffected rocks to zero in the thermally modified types. Although observed only at contacts and over small distances, the number of basic intrusions hosted within the Potiguar Basin in both onshore and offshore portions leaves opened the possibility of important implications of the thermal effects over the hydrocarbon exploration in this area as well in other Cretaceous and Paleozoic basins in Brazil