145 resultados para Compressão nervosa
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior
Resumo:
Nearly 3 x 1011 m3 of medium and light oils will remain in reservoirs worldwide after conventional recovery methods have been exhausted and much of this volume would be recovered by Enhanced Oil Recovery (EOR) methods. The in-situ combustion (ISC) is an EOR method in which an oxygen-containing gas is injected into a reservoir where it reacts with the crude oil to create a high-temperature combustion front that is propagated through the reservoir. The High Pressure Air Injection (HPAI) method is a particular denomination of the air injection process applied in light oil reservoirs, for which the combustion reactions are dominant between 150 and 300°C and the generation of flue gas is the main factor to the oil displacement. A simulation model of a homogeneous reservoir was built to study, which was initially undergone to primary production, for 3 years, next by a waterflooding process for 21 more years. At this point, with the mature condition established into the reservoir, three variations of this model were selected, according to the recovery factors (RF) reached, for study the in-situ combustion (HPAI) technique. Next to this, a sensitivity analysis on the RF of characteristic operational parameters of the method was carried out: air injection rate per well, oxygen concentration into the injected gas, patterns of air injection and wells perforations configuration. This analysis, for 10 more years of production time, was performed with assistance of the central composite design. The reservoir behavior and the impacts of chemical reactions parameters and of reservoir particularities on the RF were also evaluated. An economic analysis and a study to maximize the RF of the process were also carried out. The simulation runs were performed in the simulator of thermal processes in reservoirs STARS (Steam, Thermal, and Advanced Processes Reservoir Simulator) from CMG (Computer Modelling Group). The results showed the incremental RF were small and the net present value (NPV) is affected by high initial investments to compress the air. It was noticed that the adoption of high oxygen concentration into the injected gas and of the five spot pattern tends to improve the RF, and the wells perforations configuration has more influence with the increase of the oil thickness. Simulated cases relating to the reservoir particularities showed that smaller residual oil saturations to gas lead to greater RF and the presence of heterogeneities results in important variations on the RF and on the production curves
Resumo:
Although there are a wide variety of additives that act in fresh state, to adjust the properties of cement, there is also a search by additions that improve the tenacity of the cement in the hardened state. This, in turn, can often be increased by inserting fibers, which act on the deflection of microcracks. This study aimed to use a microfiber glass wool (silica-based) as an additive reinforcing the cement matrix, improving the rupture tenacity, in order to prevent the propagation of microcracks in the cement sheath commonly found in oil wells submitted to high temperatures. The fibers were added at different concentrations, 2 to 5% (BWOC) and varied average sizes, grinding for 90 s, 180 s, 300 s, 600 s. The cement slurries were made with a density of 1,90 g/ cm3 (15,6 lb/gal), using Portland cement CPP- Special Class as the hydraulic binder and 40% silica flour. The characterization of the fiber was made by scanning electron microscopy (SEM), particle size by sieving, X-ray fluorescence (XRF), X-ray diffraction (XRD) and thermogravimetry (TG / DTG). Were performed technological tests set by the API (American Petroleum Institute) by rheology, stability, free water, compressive strength, as well as testing rupture energy, elastic modulus and permeability. The characterization results showed good thermal stability of the microfiber glass wool for application in oil wells submitted to steam injection and, also, that from the particle size data, it was possible to suggest that microfibers milled up to 300 s, are ideal to act as reinforcement to the cement slurries. The rheological parameters, there was committal of plastic viscosity when larger lengths were inserted of microfiber (F90). The values obtained by free water and stability were presented according to API. The mechanical properties, the incorporation of microfiber to the cement slurries gave better rupture tenacity, as compared to reference cement slurries. The values of compressive strength, elastic modulus and permeability have been maintained with respect to the reference cement slurries. Thus, cement slurries reinforced with microfiber glass wool can ensure good application for cementing oil wells submitted to steam injection, which requires control of microcracks, due to the thermal gradients
Resumo:
Cementing operation is one of the most important stages in the oil well drilling processes and has main function to form hydraulic seal between the various permeable zones traversed by the well. However, several problems may occur with the cement sheath, either during primary cementing or during the well production period. Cements low resistance can cause fissures in the cement sheath and compromise the mechanical integrity of the annular, resulting in contamination of groundwater and producing zones. Several researches show that biomass ash, in particular, those generated by the sugarcane industry have pozzolanic activity and can be added in the composition of the cementing slurries in diverse applications, providing improvements in mechanical properties, revenue and cement durability. Due to the importance of a low cost additive that increases the mechanical properties in a well cementing operations, this study aimed to potentiate the use of sugarcane bagasse ash as pozzolanic material, evaluate the mechanisms of action of this one on cement pastes properties and apply this material in systems slurries aimed to cementing a well with 800 m depth and geothermal gradient of 1.7 °F/100 ft, as much primary cementing operations as squeeze. To do this, the ash beneficiation methods were realized through the processes of grinding, sifting and reburning (calcination) and then characterization by X-ray fluorescence, XRD, TG / DTG, specific surface area, particle size distribution by laser diffraction and mass specific. Moreover, the ash pozzolanic activity added to the cement at concentrations of 0%, 20% and 40% BWOC was evaluated by pozzolanic activity index with lime and with Portland cement. The evaluation of the pozzolanic activity by XRD, TG / DTG and compressive strength confirmed the ash reactivity and indicated that the addition of 20% in the composition of cement slurries produces improvement 34% in the mechanical properties of the slurry cured. Cement slurries properties evaluated by rheological measurements, fluid loss, free fluid, slurry sedimentation, thickening time and sonic strength (UCA) were satisfactory and showed the viability of using the sugarcane ash in cement slurries composition for well cementing
Resumo:
The preparation of cement slurries for offshore well cementing involves mixing all solid components to be added to the mixing water on the platform. The aim of this work was to study the formulation of pre-prepared dry mixtures, or grouts, for offshore oilwell cementing. The addition of mineral fillers in the strength of lightweight grouts applied for depths down to 400 m under water depths of 500 m was investigated. Lightweight materials and fine aggregates were selected. For the choice of starting materials, a study of the pozzolanic activity of low-cost fillers such as porcelain tile residue, microsilica and diatomaceous earth was carried out by X-ray diffraction and mechanical strength tests. Hardened grouts containing porcelain tile residue and microsilica depicted high strength at early ages. Based on such preliminary investigation, a study of the mechanical strength of grouts with density 1.74 g/cm3 (14.5 lb/gal) cured initially at 27 °C was performed using cement, microsilica, porcelain tile residue and an anti-foaming agent. The results showed that the mixture containing 7% of porcelain tile residue and 7% of microsilica was the one with the highest compressive strength after curing for 24 hours. This composition was chosen to be studied and adapted for offshore conditions based on testes performed at 4 °C. The grout containing cement, 7% of porcelain tile residue, 7% of active silica and admixtures (CaCl2), anti-foaming and dispersant resulted satisfactory rheology and mechanical strength after curing for 24 hours of curing
Resumo:
The relationship between lipid peroxidation, antioxidant defense and diabetic osteopenia remains unclear. This study evaluated the relationship between lipid peroxidation index, antioxidant defense parameter and bone metabolism in a premenopausal diabetic model by measurements such as thiobarbituric acid-reactive substances concentration (TBARS) and reduced glutathione (GSH) content in brain homogenates, histomorphometric analysis, biomechanical testing and bone mineral density (BMD). Female Wistar rats with regular estrous cycle were divided into two groups: Group 1: control rats (n = 15) and Group 2: diabetic rats (n = 15). Diabetes mellitus was induced by alloxan and confirmed by glycemia 250 mg/dL. The experimental period understood 1 and 5 after days induction and 45, 75 and 120 days after the installation of diabetes mellitus.The lipid peroxidation index, measured by TBARS concentration, showed a significant increase (p<0.05) in diabetic animals in comparison to animals control. However, the antioxidant parameter, measured by GSH content, was significantly decrease (p<0.05) in diabetic animals. Histomorphometric analysis showed a significant increase (p<0.05) in femoral trabecular separation together with a significant decrease (p<0.05) in trabecular thickness and reduced trabecular bone volume in diabetic rats. Moreover, biomechanical testing and BMD values were significant decrease (p<0.05) in diabetic group. Thus, our results demonstrated that increased lipid peroxidation and altered antioxidant defense could be related to the development of oxidative stress and diabetic osteopenia in premenopausal rats
Resumo:
This works aims at investigating the effects of adding waste from RCBP-polyester button manufacturing to Portland cement concrete, particularly regarding its consistency and mechanic strength. The RCBP used came from a button factory located in Parnamirim, RN, Brazil. The waste was added to the concrete on different ratios: 5 %, 10 %, 15 % and 20 % of the total cement mass. A sample of concrete without the RCBP was used as reference, 1:1,33:2,45:0,50. For the mechanic strength test four samples were tested with different ages (3, 7 and 28 days old) and mixtures. Furthermore, a Slump Test was also conducted in order to verify the concrete s consistency. A tendency to a reduction in the compression resistance was noticed for all samples. For the samples with 5 % and 10 %, there was also an increase in the traction resistance during inflexion, regarding the reference concrete. In the microstructural analysis, the RBCP was observed to show an irregular and porous surface, thus explaining the consistency decrease
Resumo:
Soil improved with the addition of cement have been utilized as an alternative to the construction of various types of geotechnical works, almost always present economic and environmental advantages. This paper presents a study on the usage of cement in the improvement of mechanical properties of sandy soils, characteristic of the region of Natal, collected from its dunes. This research was made in order to analyze the influence of cement content, voids, and also including water immersion and confining pressure. Samples molded from cement-soil mixtures were tested for unconfined compression tests and triaxial tests. The samples had the percentage of cement mixed in 2.5%, 5% and 10% by weight. The cement agent used was the Portland Cement of High Early strength(CPV-ARI), which promoted agility to the experimental procedure for presenting a rapid gain in strenght. The void ratio used ranged from 0.7 (more compact), 0,9 and 1,1(softer). The soil under study can be considered as pure sand. In general, it can be stated that the larger the amount of cement added to the sand studied is, the greater ultimate strength will be. Likewise, as more compact the soil is, the less void ratio and more resistant it will be present. The confining pressure tends to increase the resistance of the specimens. The cementing adopted grades showed that the use of different criteria for failure did not significantly alter the stress-strain parameters for the sand studied. The angle of friction values were found within the typical range of medium and compact sands. Cementing acted in the sand providing an intercepted cohesion which increased enhancing the potential cementation. In triaxial compression tests, the sand with void ratio is equal to 0.7 and showed the expected behavior for a compact sand while the stress-strain behavior of the same sand with the void ratio of 0.9 tended to be expected for the soft sand as well
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior
Resumo:
With the increase in cement consumption, it has quickly become one of the inputs most consumed by mankind over the last century. This has caused an increase in CO2 emissions, as cement production releases large quantities of this gas into the atmosphere. Adding this fact to the growing consciousness of environmental preservation, it has led to a search for alternatives to cement to complement its derivatives, in the form of waste materials like the ashes. This research aimed to analyze the properties of mortars in fresh and hardened state with partial replacement of Portland cement by residual algaroba wood ash (CRLA) potteries produced by the state of Rio Grande do Norte. The CRLA was collected and sieved, where part of it was ground and characterized in comparison with that just sifted, being characterized according to its chemical composition, grain size, fineness, density, bulk density and index of pozzolanic activity. It was found that the wood ash does not act as pozzolan, and grinding it has not changed its characteristics compared to those just sifted, not justifying its use. Two traces were adopted for this research: 1:3 (cement: fine sand) and 1:2:8 (cement: hydrated lime: medium sand); both in volume, using as materials the CRLA just sifted, CP II F-32 Portland cement, CH-I hydrated lime, river sand and water from the local utility. For each trace were adopted six percentages of partial replacement of cement for wood ash: 0% (control) 5%, 7%, 10%, 12% and 15%. In the fresh state, the mortars were tested towards their consistency index and mass density. In the hardened state, they were tested towards their tensile strength in bending, compressive strength and tensile adhesion strength, and its mass density in the hardened state. The mortar was also analyzed by scanning electron microscopy and X-ray diffraction. Furthermore, it was classified according to NBR 13281 (2005). The results showed that up to a content of 5% substitution and for both traces, the residual algaroba wood ash can replace Portland cement without compromising the mortars microstructure and its fresh and hardened state
Resumo:
Concrete is the second most consumed product in the world and the incorporation of the Sugar Bagasse Ash (SBA) into this material can provide solutions for the utilization of by-products from other industries, thus reducing the environmental impact. The general aim of this dissertation focuses on analyzing the mechanical behavior of concrete with addition of SBA from three different species of sugar cane, through tests of consistency, compressive strength, porosity, absorption, voids and Scanning Electron Microscopy (SEM). Were prepared 13 specimens for each specific pattern and level of incorporation of SBA (10%, 20% and 30%) of the three varieties collected, totaling 130 samples of concrete. The trait was employed 1:2:3 (cement: sand: aggregates) in relation to the cement mass with a water / cement ratio of 0.532 and 1% additive Tec 400 Mult also based on the weight of cement. According to the results obtained in this study, it was concluded that the variety of cane sugar, used in the production of the CBC, influenced the mechanical behavior of the resulting concrete. All concrete with addition of SBA, reported a reduction of at least 10% in the properties related to permeability and an increase in the compressive strength of at least 16% compared to standard concrete at 28 days
Resumo:
From the 70`s, with the publication of the Manifesto for Environment UN Conference, held in Stockholm, in Sweden (1972), defend and improve the environment became part of our daily lives. Thus, several studies have emerged in several segments in order to reuse the waste. Some examples of waste incorporated in portland cement concrete are: rice husk ash, bagasse ash of cane sugar, powder-stone, microsilica, tire rubber, among others. This research used the residue of the mining industry Scheelite, to evaluate the incorporation of the residue composition of Portland cement concrete, replacing the natural sand. The percentage of residue were incorporated from 0% to 100%, with a variation of 10%, 11 being produced concrete mix in the ratio 1:2:3:0.60, by mass. We evaluated the following characteristics of concrete: slump test, compressive strength, tensile strength by diametral compression, water absorption, porosity and density, based on the ABNT, through tests performed in the Laboratory of Civil Construction, UFRN. The trace with the addition of 60% scheelite residue was obtained which better performance. Therefore, the use of the waste from the production of Scheelite is feasible due to the durability parameters (water absorption and porosity), sustainability, and the good results of the resistance of the concrete
Resumo:
O desenvolvimento das grandes cidades tem gerado um dos maiores desafios ambientais enfrentados na atualidade, que é a gestão eficaz de resíduos sólidos. A grande variedade e quantidade dos resíduos produzidos diariamente, tem tornado a destinação ecologicamente correta e sustentável destes materiais cada vez mais difícil. Dentre os vários resíduos produzidos diariamente destacam-se os lodos oriundos de estações de tratamento de esgotos, denominados de lodos de esgoto, cuja destinação final segura tem sido discutida mundialmente em diversos estudos, tendo em vista que a tendência de geração deste tipo de resíduo tende a crescer com o aumento do saneamento das cidades. Uma forma amplamente difundida nos países desenvolvidos para destinação dos lodos de esgoto é a incineração destes materiais para posterior envio das cinzas geradas neste processo a aterros sanitários. Porém, tem-se estudado formas alternativas de disposição, destacando-se a utilização destas cinzas como adição mineral em concretos e argamassas de cimento Portland. Sabe-se que o desempenho de resíduos de incineração como adição mineral em matrizes cimentícias, depende em grande parte da capacidade de atuação destes materiais como elementos pozolânicos ou como fileres, podendo estas características serem influenciadas pela temperatura de queima ao qual estes resíduos foram submetidos. Neste sentido, verificou-se com esta pesquisa a influência da temperatura empregada na queima dos lodos sépticos no índice de atividade pozolânica (IAP) das cinzas geradas como resíduo deste processo, aqui denominadas de cinzas de lodo séptico (CLS), sendo em seguida, avaliadas as implicações técnicas e microestruturais da utilização deste resíduo em teores de 10%, 20% e 30% como adição mineral em concretos de cimento Portland. Os resultados obtidos demonstraram não haver alterações significativas no IAP das CLS em decorrência da temperatura utilizada durante o processo de queima dos lodos de esgoto. Além disso, verificou-se que embora a utilização das CLS tenham provocado diminuição da trabalhabilidade dos concretos para todos os teores de incorporação, estas melhoraram a resistência mecânica à compressão, o índice de vazios, a absorção de água e o comportamento microestrutural dos concretos contendo 10% e 20% de resíduo
Resumo:
The use of sewage sludge as a raw material falls within the waste recycling key in the current process model environmental sustainability .Waste recycling has been consolidated as a sustainable environmentally sound technical solution, and. Despite showing very variable composition and characteristics, sewage sludge, can be considered as a residue with a high recycling potential in the building sector. In this paper the feasibility of using sewage sludge ash was studied in addition to Portland cement mortar in 1:3 mass considered the standard dash. This gray additions were studied in proportions of 5%, 10 %, 15 %, 20 %, 25% and 30% by mass of cement. The methodology was focused on the characterization of materials by physical, chemical , mechanical , environmental and morphological followed by the production of mortar tests ,and finalized by the characterization tests of mortar in the fresh state, through the consistency index, content of entrained air, bulk density and water retention, and in the hardened state by bulk density, water absorption by capillarity capillarity coefficient, compressive strength, tensile strength in bending ,tensile bond strength and microstructural analysis for percentages of 0 to 20%. After comparing with the standard mortar mortars with addition of ash, it is concluded that the ash of sewage sludge did not impair the integrity and properties of mortars with addition, including increasing resistance to compression and tension, being 20% more indicated percentage. Thus, it becomes feasible the addition of sewage sludge ash in Portland cement mortar for the trait studied
Resumo:
Usually masonry structures has low tension strength, hence the design to flexural efforts can results in high reinforcement ratio, specification of high unit and prism strength, structural members with larger section dimensions and modification in structural arrangement to be possible to use masonry members. The main objective of this study is to evaluate the stiffness, the efforts distribution and the effect of horizontal elements (girders) and vertical elements (counterforts) distribution on the behavior of masonry blocks retaining walls. For this purpose, numerical modeling was performed on typical retaining wall arrangements by varying the amount and placement of horizontal and vertical elements, beyond includes elements simulating the reactions of the soil supporting the foundation of the wall. The numerical modeling also include the macro modeling strategy in which the units, mortar and grout are discretized by a standard volume that represents the masonry elastic behavior. Also, numerical model results were compared with those ones of simplified models usually adopted in bending design of masonry elements. The results show horizontal displacements, principal and shear stresses distribution, and bending moments diagrams. From the analysis it was concluded that quantity and manner of distribution of the girders are both important factors to the panel flexural behavior, the inclusion of the foundation changed significantly the behavior of the wall, especially the horizontal displacements, and has been proposed a new way of considering the flanges section of the counterforts