81 resultados para Esmalte dentário, dureza


Relevância:

10.00% 10.00%

Publicador:

Resumo:

The hardness test is thoroughly used in research and evaluation of materials for quality control. However, this test results are subject to uncertainties caused by the process operator in the moment of the mensuration impression diagonals make by the indenter in the sample. With this mind, an automated equipment of hardness mensuration was developed. The hardness value was obtained starting from the mensuration of plastic deformation suffered by the material to a well-known load. The material deformation was calculated through the mensuration of the difference between the progress and retreat of a diamond indenter on the used sample. It was not necessary, therefore, the manual mensuration of the diagonals, decreasing the mistake source caused by the operator. Tension graphs of versus deformation could be analyzed from data obtained by the accomplished analysis, as well as you became possible a complete observation of the whole process. Following, the hardness results calculated by the experimental apparatus were compared with the results calculated by a commercial microhardness machine with the intention of testing its efficiency. All things considered, it became possible the materials hardness mensuration through an automated method, which minimized the mistakes caused by the operator and increased the analysis reliability

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Present work proposed to map and features the wear mechanisms of structural polymers of engineering derived of the sliding contact with a metallic cylindrical spindle submitted to eccentricity due to fluctuations in it is mass and geometric centers. For this it was projected and makes an experimental apparatus from balancing machine where the cylindrical counterbody was supported in two bearings and the polymeric coupon was situated in a holder with freedom of displacement along counterbody. Thus, the experimental tests were standardized using two position of the two bearings (Fixed or Free) and seven different positions along the counterbody, that permit print different conditions to the stiffness from system. Others parameters as applied normal load, sliding velocity and distance were fixed. In this investigation it was used as coupon two structural polymers of wide quotidian use, PTFE (polytetrafluroethylene) and PEEK (poly-ether-ether-ketone) and the AISI 4140 alloy steel as counterbody. Polymeric materials were characterized by thermal analysis (thermogravimetric, differential scanning calorimetry and dynamic-mechanical), hardness and rays-X diffractometry. While the metallic material was submitted at hardness, mechanical resistance tests and metallographic analysis. During the tribological tests were recorded the heating response with thermometers, yonder overall velocity vibration (VGV) and the acceleration using accelerometers. After tests the wear surface of the coupons were analyzed using a Scanning Electronic Microscopy (SEM) to morphological analysis and spectroscopy EDS to microanalysis. Moreover the roughness of the counterbody was characterized before and after the tribological tests. It was observed that the tribological response of the polymers were different in function of their distinct molecular structure. It were identified the predominant wear mechanisms in each polymer. The VGV of the PTFE was smaller than PEEK, in the condition of minimum stiffness, in function of the higher loss coefficient of that polymer. Wear rate of the PTFE was more of a magnitude order higher than PEEK. With the results was possible developed a correlation between the wear rate and parameter (E/ρ)1/2 (Young modulus, E, density, ρ), proportional at longitudinal elastic wave velocity in the material.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Low cost seals are made of NBR, Nitrile Butadiene Rubber, a family of unsaturated copolymers that is higher resistant to oils the more content of nitrile have in its composition, although lower its flexibility. In Petroleum Engineering, NBR seal wear can cause fluid leakage and environmental damages, promoting an increasing demand for academic knowledge about polymeric materials candidate to seals submitted to sliding contacts to metal surfaces. This investigation aimed to evaluate tribological responses of a commercial NBR, hardness 73 ± 5 Sh A, polytetrafluoroethylene (PTFE), hardness 60 ± 4 HRE and PTFE with graphite, 68 ± 6 HRE. The testings were performed on a sliding tribometer conceived to explore the tribological performance of stationary polymer plane coupons submitted to rotational cylinder contact surface of steel AISI 52100, 20 ± 1 HRC Hardness, under dry and lubricated (oil SAE 15W40) conditions. After screening testings, the normal load, relative velocity and sliding distance were 3.15 N, 0.8 m/s and 3.2 km, respectively. The temperatures were collected over distances of 3.0±0.5 mm and 750±50 mm far from the contact to evaluate the heating in this referential zone due to contact sliding friction by two thermocouples K type. The polymers were characterized through Thermogravimetric Analysis (TGA), Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA). The wear mechanisms of the polymer surfaces were analyzed by Scanning Electron Microscopy (SEM) and EDS (Energy-Dispersive X-ray Spectroscopy). NBR referred to the higher values of heating, suggesting higher sliding friction. PTFE and PTFE with graphite showed lower heating, attributed to the delamination mechanism

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In recent years there has been a significant growth in technologies that modify implant surfaces, reducing healing time and allowing their successful use in areas with low bone density. One of the most widely used techniques is plasma nitration, applied with excellent results in titanium and its alloys, with greater frequency in the manufacture of hip, ankle and shoulder implants. However, its use in dental implants is very limited due to high process temperatures (between 700 C o and 800 C o ), resulting in distortions in these geometrically complex and highly precise components. The aim of the present study is to assess osseointegration and mechanical strength of grade II nitrided titanium samples, through configuration of hollow cathode discharge. Moreover, new formulations are proposed to determine the optimum structural topology of the dental implant under study, in order to perfect its shape, make it efficient, competitive and with high definition. In the nitriding process, the samples were treated at a temperature of 450 C o and pressure of 150 Pa , during 1 hour of treatment. This condition was selected because it obtains the best wettability results in previous studies, where different pressure, temperature and time conditions were systematized. The samples were characterized by X-ray diffraction, scanning electron microscope, roughness, microhardness and wettability. Biomechanical fatigue tests were then conducted. Finally, a formulation using the three dimensional structural topology optimization method was proposed, in conjunction with an hadaptive refinement process. The results showed that plasma nitriding, using the hollow cathode discharge technique, caused changes in the surface texture of test specimens, increases surface roughness, wettability and microhardness when compared to the untreated sample. In the biomechanical fatigue test, the treated implant showed no flaws, after five million cycles, at a maximum fatigue load of 84.46 N. The results of the topological optimization process showed well-defined optimized layouts of the dental implant, with a clear distribution of material and a defined edge

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The competitiveness of the trade generated by the higher availability of products with lower quality and cost promoted a new reality of industrial production with small clearances. Track deviations at the production are not discarded, uncertainties can statistically occur. The world consumer and the Brazilian one are supported by the consumer protection code, in lawsuits against the products poor quality. An automobile is composed of various systems and thousands of constituent parts, increasing the likelihood of failure. The dynamic and security systems are critical in relation to the consequences of possible failures. The investigation of the failure gives us the possibility of learning and contributing to various improvements. Our main purpose in this work is to develop a systematic, specific methodology by investigating the root cause of the flaw occurred on an axle end of the front suspension of an automobile, and to perform comparative data analyses between the fractured part and the project information. Our research was based on a flaw generated in an automotive suspension system involved in a mechanical judicial cause, resulting in property and personal damages. In the investigations concerning the analysis of mechanical flaws, knowledge on materials engineering plays a crucial role in the process, since it enables applying techniques for characterizing materials, relating the technical attributes required from a respective part with its structure of manufacturing material, thus providing a greater scientific contribution to the work. The specific methodology developed follows its own flowchart. In the early phase, the data in the records and information on the involved ones were collected. The following laboratory analyses were performed: macrography of the fracture, micrography with SEM (Scanning Electron Microscope) of the initial and final fracture, phase analysis with optical microscopy, Brinell hardness and Vickers microhardness analyses, quantitative and qualitative chemical analysis, by using X-ray fluorescence and optical spectroscopy for carbon analysis, qualitative study on the state of tension was done. Field data were also collected. In the analyses data of the values resulting from the fractured stock parts and the design values were compared. After the investigation, one concluded that: the developed methodology systematized the investigation and enabled crossing data, thus minimizing diagnostic error probability, the morphology of the fracture indicates failure by the fatigue mechanism in a geometrically propitious location, a tension hub, the part was subjected to low tensions by the sectional area of the final fracture, the manufacturing material of the fractured part has low ductility, the component fractured in an earlier moment than the one recommended by the manufacturer, the percentages of C, Si, Mn and Cr of the fractured part present values which differ from the design ones, the hardness value of the superior limit of the fractured part is higher than that of the design, and there is no manufacturing uniformity between stock and fractured part. The work will contribute to optimizing the guidance of the actions in a mechanical engineering judicial expertise

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The use of composite materials and alternative is being increased every day, as it becomes more widespread awareness that the use of renewable and not harmful to the environment is part of a new environmentally friendly model. Since its waste (primarily fiberglass) can not be easily recycled by the difficulty that still exists in this process, since they have two phases mixed, a polymeric matrix thermoset difficult to recycle because it is infusible and phase of fiber reinforcements. Thermoset matrix composites like Polyester + fiberglass pose a threat due to excessive discharge. Aiming to minimize this problem, aimed to reuse the composite Polyester + fiber glass, through the wastes obtained by the grinding of knifes and balls. These residues were incorporated into the new composite Polyester/Fiberglass for hot compression mold and compared tribological to composites with filler CaCO3, generally used as filler, targeting a partial replacement of CaCO3 by such waste. The composites were characterized by thermal analysis (TGA, DSC and DMA), by the surface integrity (roughness determination, contact angle and surface energy), mechanical properties (hardness) and tribological tests (wear and coefficient of dynamic friction) in order to evaluate the effect of loads and characterize these materials for applications that can take, in the tribological point of view since waste Polyester + fiberglass has great potential for replacement of CaCO3

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Wear mechanisms and thermal history of two non-conforming sliding surfaces was investigated in laboratory. A micro-abrasion testing setup was used but the traditional rotative sphere method was substituted by a cylindrical surface of revolution which included seven sharp angles varying between 15o to 180o. The micro-abrasion tests lead to the investigation on the polyurethane response at different contact pressures. For these turned counterfaces with and without heat treatment. Normal load and sliding speeds were changed. The sliding distance was fixed at 5 km in each test. The room and contact temperatures were measured during the tests. The polyurethane was characterized using tensile testing, hardness Shore A measurement, Thermogravimetric Analysis (TGA), Differential Scanning Calorimetry (DSC) and Thermomechanical Analyze (TMA). The Vickers micro-hardness of the steel was measured before and after the heat treatment and the metallographic characterization was also carried out. Worn surface of polyurethane was analysed using Scanning Electron Microscope (SEM) and EDS (Electron Diffraction Scanning) microanalyses. Single pass scratch testing in polyurethane using indenters with different contact angles was also carried out. The scar morphology of the wear, the wear mechanism and the thermal response were analyzed in order to correlate the conditions imposed by the pressure-velocity pair to the materials in contact. Eight different wear mechanisms were identified on the polyurethane surface. It was found correlation between the temperature variation and the wear scar morphology.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Composites based on PEEK + PTFE + CARBON FIBER + Graphite (G_CFRP) has increased application in the top industries, as Aerospace, Aeronautical, Petroleum, Biomedical, Mechanical and Electronics Engineering challenges. A commercially available G_CFRP was warmed up to three different levels of thermal energy to identify the main damage mechanisms and some evidences for their intrinsic transitions. An experimental test rig for systematize a heat flux was developed in this dissertation, based on the Joule Effect. It was built using an isothermal container, an internal heat source and a real-time measurement system for test a sample by time. A standard conical-cylindrical tip was inserted into a soldering iron, commercially available and identified by three different levels of nominal electrical power, 40W (manufacturer A), 40W (manufacturer B), 100W and 150W, selected after screening tests: these power levels for the heat source, after one hour of heating and one hour of cooling in situ, carried out three different zones of degradation in the composite surface. The bench was instrumented with twelve thermocouples, a wattmeter and a video camera. The twelve specimens tested suffered different degradation mechanisms, analyzed by DSC (Differential Scanning Calorimetry) and TG (Thermogravimetry) techniques, Scanning Electron Microscopy (SEM) and Energy-Dispersive X-Rays (EDX) Analysis. Before and after each testing, it was measured the hardness of the sample by HRM (Hardness Rockwell M). Excellent correlations (R2=1) were obtained in the plots of the evaporated area after one hour of heating and one hour of cooling in situ versus (1) the respective power of heat source and (2) the central temperature of the sample. However, as resulting of the differential degradation of G_CFRP and their anisotropy, confirmed by their variable thermal properties, viscoelastic and plastic properties, there were both linear and non-linear behaviour between the temperature field and Rockwell M hardness measured in the radial and circumferential directions of the samples. Some morphological features of the damaged zones are presented and discussed, as, for example, the crazing and skeletonization mechanism of G_CFRP

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The technique of ion nitriding, despite being fully consolidated in the industry, has great limitations when applied to the treatment of small parts. This is because effects that occur due to non-uniformity of the electric field, generate localized heating in parts, damaging the uniformity of nitrided layer. In addition, because the samples are treated static parts thereof are untreated. To expand the use of plasma nitriding, this work presents the development, assembly and testing of a prototype plasma reactor with rotatory cathodic cage [patent pending], able to meet these needs, giving the material a uniform treatment and opening doors to industrial scale production. The samples tested with hexagonal nuts are 6.0 mm in diameter, made of stainless steel AISI 304 nitrided at a pressure of 1 mbar in an atmosphere of 20% H2 + 80% N2 for 1 h. After treatment, testing visual inspection, optical microscopy and microhardness were carried out to check the effectiveness of the process for uniformity and hardness of the parts. All samples exhibited uniform color, and matte brownish, unlike the untreated samples, silver color and gloss. The hardness of the surface (top and sides) was 65% and even higher than the original hardness. The nitrided layer showed great uniformity in microstructure and thickness. It is concluded, therefore, that the unit was effective constructed for the purposes for which it was designed

Relevância:

10.00% 10.00%

Publicador:

Resumo:

O gradiente térmico da superfície para o interior do sólido depende da taxa de colisões das partículas e da condutividade térmica do material utilizado. Quando um sólido é imerso em plasma, a transferência de energia ocorre por radiação e colisões das partículas sobre a superfície do material. Dependendo da taxa de colisões das particulas e da condutividade térmica do sólido existirão gradientes térmicos da superfície para o interior das amostras, ocorrendo picos térmicos na superficie, ou seja, o aquecimento pontual nas regiões de colisões. A fim de estudar esse efeito, amostras de aço rápido AISI M35 cujos valores de dureza são fortemente sensíveis à temperatura de revenimento, foram utilizadas como micro sensores térmicos. Amostras foram temperadas em forno resistivo e, em seguida, parte das mesmas foram revenidas em forno resistivo e a outra parte em plasma. A partir do gráfico da dureza (Hv) em função da temperatura (T) das amostras revenidas em forno resistivo foi possível obter uma função Hv(T) para determinação indireta do perfil térmico das amostras tratadas em plasma. As amostras foram revenidas em plasma utilizando temperatura de referência igual a 550 oC. Em seguida foi obtido o perfil de dureza dessas amostras ao longo da seção transversal e, subsequentemente, o perfil de temperatura. Verificou-se que amostras tratadas em plasma, ao contrário daquelas tratadas em forno resistivo, apresentaram gradiente de temperatura da superfície para o núcleo. Além disso, verificou-se que as amostras tratadas em configuração planar apresentaram gradientes térmicos inferiores àquelas tratadas em configuração cátodo oco, variando de 20 a 120 °C, respectivamente

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Thermal insulation is used to protect the heated or cooled surfaces by the low thermal conductivity materials. The rigid ricin polyurethane foams (PURM) are used for thermal insulation and depend on the type and concentration of blowing agent. Obtaining PURM occurs by the use of polyol, silicone, catalyst and blowing agent are pre -mixed, reacting with the isocyanate. The glass is reusable, returnable and recyclable heat insulating material, whose time of heat dissipation determines the degree of relaxation of its structure; and viscosity determines the conditions for fusion, operating temperatures, annealing, etc. The production of PURM composites with waste glass powder (PV) represents economical and renewable actions of manufacturing of thermal insulating materials. Based on these aspects, the study aimed to produce and characterize the PURM composites with PV, whose the mass percentages were 5, 10, 20, 30, 40 and 50 wt%. PURM was obtained commercially, while the PV was recycled from the tailings of the stoning process of a glassmaking; when the refining process was applied to obtain micrometer particles. The PURM + PV composites were studied taking into account the standard sample of pure PURM and the influence of the percentage of PV in this PURM matrix. The results of the chemical, physical and morphological characterization were discussed taking into account the difference in the microstructural morphology of the PURM+PV composites and the pure PURM, as well the results of the physicochemical, mechanical e thermophysical tests by values obtained of density, hardness, compressive strength, specific heat, thermal conductivity and diffusivity. In general, the structure of pure PURM showed large, elongated and regular pores, while PURM+PV composites showed irregular, small and rounded pores with shapeless cells. This may have contributed to reducing their mechanical strength, especially for PURM - PV50. The hardness and density were found to have a proportional relationship with the PV content on PURM matrix. The specific heat, thermal diffusivity and thermal conductivity showed proportional relationship to each other. So, this has been realized that the increasing the PV content on PURM matrix resulted in the rise of diffusivity and thermal conductivity and the decrease of the specific heat. However, the values obtained by the PURM composites were similar the values of pure PURM, mainly the PURM-PV5 and PURM-PV10. Therefore, these composites can be applied like thermal insulator; furthermore, their use could reduce the production costs and to preserve the environment

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In machining of internal threads, dedicated tools, known as taps, are needed for each profile type, diameter, and low cutting speed values are used when compared to main machining processes. This restriction in the cutting speed is associated with the difficulty of synchronizing the tool s rotation speed and feed velocity in the process. This fact restricts the flexibility and makes machining lead times longer when manufacturing of components with threads is required. An alternative to the constraints imposed by the tap is the thread milling with helical interpolation technique. The technique is the fusion of two movements: rotation and helical interpolation. The tools may have different configurations: a single edge or multiple edges (axial, radial or both). However, thread milling with helical interpolation technique is relatively new and there are limited studies on the subject, a fact which promotes challenges to its wide application in the manufacturing shop floor. The objective of this research is determine the performance of different types of tools in the thread milling with helical interpolation technique using hardened steel workpieces. In this sense, four tool configurations were used for threading milling in AISI 4340 quenched and tempered steel (40 HRC). The results showed that climb cut promoted a greater number of machined threads, regardless of tool configuration. The upcut milling causes chippings in cutting edge, while the climb cutting promotes abrasive wear. Another important point is that increase in hole diameter by tool diameter ratio increases tool lifetime

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The detention and infiltration ponds of urban drainage system has function to protect the population from undesirable effects of floods. In general these ponds are not completly used and it potential is wasted. As it are disseminated at different places at cities it can reduce costs with water transport and permit water preservation of best quality. Some it utilities includes use in green areas irrigation, industrial among than cooling towers and boiler, soil compaction, cleaning urban road, pisciculture and fire fighting system. The quality these water is influenced by anauthorized sewage in the drainage system. This study was performed in six detention and infiltration ponds at drainage system of Natal, which aim was to verify the non-portable use these ponds on urban environment. As indirect aim would to incentive the water utilization these ponds as a water source to another uses in urban environment. These ponds represents the characteristics of detention and infiltration of Natal city and consequently of Brazil. As the water quality, the ponds presents following characteristics: three has apparently good quality, other showed intermediate condition and two had water polluted. Were performed twenty sample in each ponds and the following parameters assessed: pH, temperature, dissolved oxygen, turbidity, electrical conductivity, coliform thermotolerant, ammonia, organic nitrogen, TKN, nitrate, total phosphorus and alkalinity, bicarbonate, chloride, total hardness, calcium and magnesium hardness, total solids, TSS, TDS, COD and SAR°. To utilization on pisciculture we recommend use in ponds which presents the best quality. Only one pond presented higher pollutants and it not being appropriated for use in cooling tower. The content of solids suspension restricted the water use in all ponds in boilers. As water use in soil compaction, cleaning urban road and fire fighting system the water from these ponds are not appropriated. However, the recommended limits from literature are to domestic sewage, due to this, the parameters are restrictive to diminish the sanitary risk that could be offered with it utilization. The infiltration velocity of water these assessed ponds restrict a moderato use, however the effects are potentiated only in soil less sandy, which not occur in Natal. It is recommend the unrestricted irrigation utilization in ponds with best quality of water, and a restricted irrigation to ponds with worst quality of water. As load of pollutants, it is recommended a complementary treatment in those ponds whit higher load to diminish sanitary risks. In only one pond was found one helminth eggs and due to the convention formula of results, it was found for all ponds less than 1 helminth/liter eggs.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The hospitalization is an event that can attack any person, independent of gender, race, social and economical condition. Last year, the prevalence of hospitalization was 8.1 for 100 inhabitants and the average time of hospitalization was 8.5 days for each patient one in Natal city. Therefore, an important point is whether the attention to the patients during the permanence in these health establishments incorporates the health integral model suggested by the principles proposed by the National Health System in Brazil (SUS), with actions of promotion and protection by different kinds of professionals, beside those called convalescence. Then, the aim of this study was to evaluate the patient s oral health conditions hosted in public hospitals of the Natal city, looking for to establish its relationship with several risk factors by two dimensions: the characteristics of the hospitalization and the patient s general and economical conditions. We accomplished a cross-sectional study with 205 patients distributed among the hospitals Onofre Lopes, Giselda Trigueiro and Monsenhor Walfredo Gurgel, looking for to know the socio-demographic characteristics, the food habits and of oral hygiene and the conditions of oral health, through the Visible Plaque Index and Gingival Bleeding Index. We observed that the conditions of the patient s oral health interned at public hospitals of reference of the municipal district of Natal is bad, existing accumulation of dental plaque and, consequently, a great number of patients with gingival bleeding. However, the time of hospitalization and its reason, the type of medicine used in this time and the toothbrush frequency were not configured as risk factors for this oral health condition

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Periodontal infections consist of a group of inflammatory conditions caused by microorganisms that colonize the tooth surface through the formation of dental biofilm. Chronic infections such as periodontitis have been associated to the development and progression of atherosclerosis. AIM: Detect cultivatable and non-cultivatable periodontopathogenic bacteria in atheromatous plaques; search for factors associated to the presence of these bacteria in the atheromatous plaques and characterize the presence of cultivatable and non-cultivatable bacteria in these plaques. METHODOLOGY: A cross-sectional study was performed with a sample of 30 patients diagnosed with atherosclerosis in the carotid, coronary or femoral arteries and surgically treated with angioplasty and stent implant, bypass or endarterectomy. The plaques were collected during surgery and analyzed using the PCR molecular technique for the presence of the DNA of the cultivatable bacteria Aggregatibacter actinomycetemcomitans, Porphyromonas gingivalis and Treponema denticola and of the non-cultivatable Synergistes phylotypes. The patients were examined in the infirmary, after the surgery, where they also responded to a questionnaire aimed at determining factors associated to the presence of periodontopathogenic bacteria in the atheromatous plaques. RESULTS: All patients with tooth (66,7%) possessed disease periodontal, being 95% severe and 65% widespread. No periodontopathogenic bacteria were found in the atheromatous plaques. However, four samples (13.3%) were positive for the presence of bacteria. Of these, three participants were dentate, being two carriers of widespread severe chronic periodontite and one of located severe chronic periodontitis. None of them told the accomplishment of procedures associated to possible bacteremia episodes, as treatment endodontic, extraction the last six months or some procedure surgical dental. CONCLUSION: The periodontopathogenic bacteria studied were not found in the atheromatous plaques, making it impossible to establish the prevalence of these pathogens or the factors associated to their presence in plaques, the detection of positive samples for bacteria suggests that other periodontal and non-periodontal pathogens be studied in an attempt at discovering the association or not between periodontal disease and/or others infections and atherosclerosis, from the presence of these bacteria in atheromas