44 resultados para Aço AISI D6
Resumo:
The technique of ion nitriding, despite being fully consolidated in the industry, has great limitations when applied to the treatment of small parts. This is because effects that occur due to non-uniformity of the electric field, generate localized heating in parts, damaging the uniformity of nitrided layer. In addition, because the samples are treated static parts thereof are untreated. To expand the use of plasma nitriding, this work presents the development, assembly and testing of a prototype plasma reactor with rotatory cathodic cage [patent pending], able to meet these needs, giving the material a uniform treatment and opening doors to industrial scale production. The samples tested with hexagonal nuts are 6.0 mm in diameter, made of stainless steel AISI 304 nitrided at a pressure of 1 mbar in an atmosphere of 20% H2 + 80% N2 for 1 h. After treatment, testing visual inspection, optical microscopy and microhardness were carried out to check the effectiveness of the process for uniformity and hardness of the parts. All samples exhibited uniform color, and matte brownish, unlike the untreated samples, silver color and gloss. The hardness of the surface (top and sides) was 65% and even higher than the original hardness. The nitrided layer showed great uniformity in microstructure and thickness. It is concluded, therefore, that the unit was effective constructed for the purposes for which it was designed
Resumo:
O gradiente térmico da superfície para o interior do sólido depende da taxa de colisões das partículas e da condutividade térmica do material utilizado. Quando um sólido é imerso em plasma, a transferência de energia ocorre por radiação e colisões das partículas sobre a superfície do material. Dependendo da taxa de colisões das particulas e da condutividade térmica do sólido existirão gradientes térmicos da superfície para o interior das amostras, ocorrendo picos térmicos na superficie, ou seja, o aquecimento pontual nas regiões de colisões. A fim de estudar esse efeito, amostras de aço rápido AISI M35 cujos valores de dureza são fortemente sensíveis à temperatura de revenimento, foram utilizadas como micro sensores térmicos. Amostras foram temperadas em forno resistivo e, em seguida, parte das mesmas foram revenidas em forno resistivo e a outra parte em plasma. A partir do gráfico da dureza (Hv) em função da temperatura (T) das amostras revenidas em forno resistivo foi possível obter uma função Hv(T) para determinação indireta do perfil térmico das amostras tratadas em plasma. As amostras foram revenidas em plasma utilizando temperatura de referência igual a 550 oC. Em seguida foi obtido o perfil de dureza dessas amostras ao longo da seção transversal e, subsequentemente, o perfil de temperatura. Verificou-se que amostras tratadas em plasma, ao contrário daquelas tratadas em forno resistivo, apresentaram gradiente de temperatura da superfície para o núcleo. Além disso, verificou-se que as amostras tratadas em configuração planar apresentaram gradientes térmicos inferiores àquelas tratadas em configuração cátodo oco, variando de 20 a 120 °C, respectivamente
Resumo:
In machining of internal threads, dedicated tools, known as taps, are needed for each profile type, diameter, and low cutting speed values are used when compared to main machining processes. This restriction in the cutting speed is associated with the difficulty of synchronizing the tool s rotation speed and feed velocity in the process. This fact restricts the flexibility and makes machining lead times longer when manufacturing of components with threads is required. An alternative to the constraints imposed by the tap is the thread milling with helical interpolation technique. The technique is the fusion of two movements: rotation and helical interpolation. The tools may have different configurations: a single edge or multiple edges (axial, radial or both). However, thread milling with helical interpolation technique is relatively new and there are limited studies on the subject, a fact which promotes challenges to its wide application in the manufacturing shop floor. The objective of this research is determine the performance of different types of tools in the thread milling with helical interpolation technique using hardened steel workpieces. In this sense, four tool configurations were used for threading milling in AISI 4340 quenched and tempered steel (40 HRC). The results showed that climb cut promoted a greater number of machined threads, regardless of tool configuration. The upcut milling causes chippings in cutting edge, while the climb cutting promotes abrasive wear. Another important point is that increase in hole diameter by tool diameter ratio increases tool lifetime
Resumo:
In this work thiosemicarbazones [4-N-cinnamoyl-thiosemicarbazone (CTSC), 4-N-(2'-methoxycinnamoyl)-thiosemicarbazone (MCTSC), and 4-N-(4'-hydroxy-3'-methoxybenzoyl)-thiosemicarbazone (HMBTSC)] were solubilized in an microemulsion system (ME_OCS) which is rich in aqueous phase (O/W system). The system ME_OCS was obtained with saponified coconut oil (OCS) as (surfactant), butanol (cosurfactant), and kerosene as oil phase (Fo), using 40% of C/T (cosurfactant/surfactant), 5% of Fo and 55% of aqueous phase. The microemulsions systems CTSC_ME_OCS, MCTSC_ME_OCS and HMBTSC_ME_OCS effectiveness on a AISI 1020 carbon steel corrosion inhibition process were evaluated in a saline solution (NaCl 0.5%), using a galavostatic method. The tested thiosemicarbazones (TSC) showed highest inhibitors effects (85.7% for CTSC_ME_OCS, 84.0% for MCTSC_ME_OCS, and 83.3% HMBTSC_ME_OCS) at lower concentrations [0.19% of CTSC, 0.07% (MCTSC), and 0.26% (HMBTSC)]. Comparatively, the surfactant OCS (solubilized in H2O) as well as the system ME_OCS showed lower efficacy [71% for OCS (at 0.20 - 0.25% of concentration) and 74% for ME_OCS (at 0.5% of concentration)]. Since the microemulsion systems ME_OCS showed satisfactory interfacial adsorption, the greatest inhibitory effect of those TSC_ME_OCS systems could be correlated to both chemical composition of each tested TSC (which is rich in heteroatoms and aromatic ring) and also the presence of the surfactant OCS
Resumo:
Nowadays, the use of chemicals that satisfactorily meet the needs of different sectors of the chemical industry is linked to the consumption of biodegradable materials. In this context, this work contemplated biotechnological aspects with the objective of developing a more environmentally-friendly corrosion inhibitor. In order to achieve this goal, nanoemulsion-type systems (NE) were obtained by varying the amount of Tween 80 (9 to 85 ppm) a sortitan surfactant named polyoxyethylene (20) monooleate. This NE-system was analyzed using phase diagrams in which the percentage of the oil phase (commercial soybean oil, codenamed as OS) was kept constant. By changing the amount of Tween 80, several polar NE-OS derived systems (O/W-type nanoemulsion) were obtained and characterized through light scattering, conductivity and pH, and further subjected to electrochemical studies. The interfacial behavior of these NE-OS derived systems (codenamed NE-OS1, S2, S3, S4 and S5) as corrosion inhibitors on carbon steel AISI 1020 in saline media (NaCl 3.5%) were evaluated by measurement of Open Circuit Potential (OCP), Polarization Curves (Tafel extrapolation method) and Electrochemical Impedance Spectroscopy (EIS). The analyzed NE-OS1 and NE-OS2 systems were found to be mixed inhibitors with quantitative efficacy (98.6% - 99.7%) for concentrations of Tween 80 ranging between 9 and 85 ppm. According to the EIS technique, maximum corrosion efficiency was observed for some tested NE-OS samples. Additionaly to the electrochemical studies, Analysis of Variance (ANOVA) and Principal Component Analysis (PCA) were used, characterization of the nanoemulsion tested systems and adsorption studies, respectively, which confirmed the results observed in the experimental analyses using diluted NE-OS samples in lower concentrations of Tween 80 (0.5 1.75 ppm)
Resumo:
Corrosion is a natural process that causes progressive deterioration of materials, so, reducing the corrosive effects is a major objective of development of scientific studies. In this work, the efficiency of corrosion inhibition on a AISI 1018 carbon steel of the nanoemulsion system containing the oil of the seeds of Azadirachta indica A. Juss (SNEOAI) was evaluated by the techniques of linear polarization resistance (LPR) and weight loss (CPM), a instrumented cell. For that, hydroalcoholic extract of leaves of A. indica (EAI) was solubilized in a nanoemulsion system (SNEOAI) of which O/W system (rich in aqueous phase). This nanoemulsion system (tested in different concentrations) was obtained with oil from the seeds of this plant species (OAI) (oil phase), dodecylammonium chloride (DDAC) (surfactant), butanol (cosurfactant) and water, using 30 % of C/T (cosurfactant/surfactant), 0.5 % of oil phase and 69.5 % of aqueous phase, and characterized by surface tension, rheology and droplet sizes. This systems SNEOAI and SNEOAI-EAI (nanoemulsion containing hydroalcoholic extract - EAI) showed inhibition efficiencies in corrosive environment in saline (1 %), for the method of LPR with significant value of 70.58 % (300 ppm) to SNEOAI, 74.17 % (100 ppm) and 72.51 % (150 ppm) to SNEOAI-EAI. The best efficiencies inhibitions were observed for the method of CPM with 85.41 % for the SNEOAI (300 ppm) and 83.19 % SNEOAI-EAI (500 ppm). The results show that this formulation could be used commercially for use as a corrosion inhibitor, this research contributed to the biotechnological applicability of Azadirachta indica, considering the large use of this plant species rich in limonoids (tetranortriterpenoids), especially azadirachtin
Resumo:
The thermodynamic performance of a refrigeration system can be improved by reducing the compression work by a particular technique for a specific heat removal rate. This study examines the effect of small concentrations of Al2O3 (50 nm) nanoparticles dispersion in the mineral oil based lubricant on the: viscosity, thermal conductivity, and lubrication characteristics as well as the overall performance (based on the Second Law of Thermodynamics) of the refrigerating system using R134a or R600a as refrigerants. The study looked at the influences of variables: i) refrigerant charge (100, 110, 120 and 130 g), ii) rotational speed of the condenser blower (800 and 1100 RPM) and iii) nanoparticle concentration (0.1 and 0.5 g/l) on the system performance based on the Taguchi method in a matrix of L8 trials with the criterion "small irreversibility is better”. They were carried pulldown and cycling tests according to NBR 12866 and NBR 12869, respectively, to evaluate the operational parameters: on-time ratio, cycles per hour, suction and discharge pressures, oil sump temperature, evaporation and condensation temperatures, energy consumption at the set-point, total energy consumption and compressor power. In order to evaluate the nanolubricant characteristics, accelerated tests were performed in a HFRR bench. In each 60 minutes test with nanolubricants at a certain concentration (0, 0.1 and 0.5 g/l), with three replications, the sphere (diameter 6.00 ± 0.05 mm, Ra 0.05 ± 0.005 um, AISI 52100 steel, E = 210 GPa, HRC 62 ± 4) sliding on a flat plate (cast iron FC200, Ra <0.5 ± 0.005 um) in a reciprocating motion with amplitude of 1 mm, frequency 20 Hz and a normal load of 1,96 N. The friction coefficient signals were recorded by sensors coupled to the HFRR system. There was a trend commented bit in the literature: a nanolubricant viscosity reduction at the low nanoparticles concentrations. It was found the dominant trend in the literature: increased thermal conductivity with increasing nanoparticles mass fraction in the base fluid. Another fact observed is the significant thermal conductivity growth of nanolubricant with increasing temperature. The condenser fan rotational speed is the most influential parameter (46.192%) in the refrigerator performance, followed by R600a charge (38.606%). The Al2O3 nanoparticles concentration in the lubricant plays a minor influence on system performance, with 12.44%. The results of power consumption indicates that the nanoparticles addition in the lubricant (0.1 g/L), together with R600a, the refrigerator consumption is reduced of 22% with respect to R134a and POE lubricant. Only the Al2O3 nanoparticles addition in the lubricant results in a consumption reduction of about 5%.
Resumo:
The thermodynamic performance of a refrigeration system can be improved by reducing the compression work by a particular technique for a specific heat removal rate. This study examines the effect of small concentrations of Al2O3 (50 nm) nanoparticles dispersion in the mineral oil based lubricant on the: viscosity, thermal conductivity, and lubrication characteristics as well as the overall performance (based on the Second Law of Thermodynamics) of the refrigerating system using R134a or R600a as refrigerants. The study looked at the influences of variables: i) refrigerant charge (100, 110, 120 and 130 g), ii) rotational speed of the condenser blower (800 and 1100 RPM) and iii) nanoparticle concentration (0.1 and 0.5 g/l) on the system performance based on the Taguchi method in a matrix of L8 trials with the criterion "small irreversibility is better”. They were carried pulldown and cycling tests according to NBR 12866 and NBR 12869, respectively, to evaluate the operational parameters: on-time ratio, cycles per hour, suction and discharge pressures, oil sump temperature, evaporation and condensation temperatures, energy consumption at the set-point, total energy consumption and compressor power. In order to evaluate the nanolubricant characteristics, accelerated tests were performed in a HFRR bench. In each 60 minutes test with nanolubricants at a certain concentration (0, 0.1 and 0.5 g/l), with three replications, the sphere (diameter 6.00 ± 0.05 mm, Ra 0.05 ± 0.005 um, AISI 52100 steel, E = 210 GPa, HRC 62 ± 4) sliding on a flat plate (cast iron FC200, Ra <0.5 ± 0.005 um) in a reciprocating motion with amplitude of 1 mm, frequency 20 Hz and a normal load of 1,96 N. The friction coefficient signals were recorded by sensors coupled to the HFRR system. There was a trend commented bit in the literature: a nanolubricant viscosity reduction at the low nanoparticles concentrations. It was found the dominant trend in the literature: increased thermal conductivity with increasing nanoparticles mass fraction in the base fluid. Another fact observed is the significant thermal conductivity growth of nanolubricant with increasing temperature. The condenser fan rotational speed is the most influential parameter (46.192%) in the refrigerator performance, followed by R600a charge (38.606%). The Al2O3 nanoparticles concentration in the lubricant plays a minor influence on system performance, with 12.44%. The results of power consumption indicates that the nanoparticles addition in the lubricant (0.1 g/L), together with R600a, the refrigerator consumption is reduced of 22% with respect to R134a and POE lubricant. Only the Al2O3 nanoparticles addition in the lubricant results in a consumption reduction of about 5%.
Resumo:
The micro-deformations caused by cyclic loading origins the variation of the distances between atoms of the crystal lattice producing the irreversible component. In order to study and understand the microstructural behavior of the material this paper investigated the influence suffered by residual stresses in thrust rolling bearing races fabricated in AISI 52100 steel, after tests by cyclic rolling contact in a tribometer at 1m/s under two contact pressures (500 MPa and 1400 MPa) in dry and boundary lubrication conditions. Procedures of tests thermo-acustically isolated were developed for monitoring the contact temperature and sound pressure level signals to establish a comparison between the residual stress measurements, micro-hardness Vickers and micrographic registers searching an indication of wear evolution. The sin²ψ method by X-ray diffraction technique was used to quantify the residual stresses. Three raceway zones were selected for the evaluation of wear and surface morphology after predetermined cycling, comparing with their new condition ("as received"). Micro-hardness and residual stress measurements showed significant changes after the tests and it was possible to observe the relationship between the increase of sound pressure level and the residual stress for dry and lubricated conditions.
Resumo:
The micro-deformations caused by cyclic loading origins the variation of the distances between atoms of the crystal lattice producing the irreversible component. In order to study and understand the microstructural behavior of the material this paper investigated the influence suffered by residual stresses in thrust rolling bearing races fabricated in AISI 52100 steel, after tests by cyclic rolling contact in a tribometer at 1m/s under two contact pressures (500 MPa and 1400 MPa) in dry and boundary lubrication conditions. Procedures of tests thermo-acustically isolated were developed for monitoring the contact temperature and sound pressure level signals to establish a comparison between the residual stress measurements, micro-hardness Vickers and micrographic registers searching an indication of wear evolution. The sin²ψ method by X-ray diffraction technique was used to quantify the residual stresses. Three raceway zones were selected for the evaluation of wear and surface morphology after predetermined cycling, comparing with their new condition ("as received"). Micro-hardness and residual stress measurements showed significant changes after the tests and it was possible to observe the relationship between the increase of sound pressure level and the residual stress for dry and lubricated conditions.
Resumo:
The efficiency of inhibition to corrosion of steel AISI 1018 of surfactant coconut oil saponified (SCO) and heterocyclic type mesoionics (1,3,4-triazólio-2-tiolato) in systems microemulsionados (SCO-ME and SCO-ME-MI) Of type O/A (rich in water emulsion) region with the work of Winsor IV. The systems microemulsionados (SCO-ME and SCO-ME-MI) were evaluated with a corrosion inhibitor for use in saline 10,000 ppm of chloride enriched with carbon dioxide (CO2). The assessment of corrosion inhibitors were evaluated by the techniques of linear polarization resistance (LPR) and loss of weight (MW) in a cell instrumented given the gravity and electrochemical devices. The systems were shooting speed of less than 60 minutes and efficiency of inhibition [SCO-ME (91.25%) and SCO-ME-MI (98.54%)]
Resumo:
In the search for products that act as corrosion inhibitors and do not cause environmental, impact the use of plant extracts as corrosion inhibitors is becoming a promising alternative. In this work the efficiency of polar extracts (ethanol extracts) obtained from the plants Anacardium occidentale Linn (AO) and Phyllantus amarus Schum. & Thonn (PA) as corrosion inhibitors were evaluated in different concentrations. For that AO and PA extracts were solubilized in the microemulsion systems (SME) containing saponified coconut oil as surfactant (SME -OCS and SME-OCS-1) in saline (NaCl 3,5 %) solution, which was also used as electrolyte. Both SME-OCS and SME-OCS-1 were characterized by surface tension and viscosity methods showing a Newtonian fluid behavior. The SME-OCS and SME-OCS-1 systems satisfactorily solubilized the polar extracts AO and PA with measurements carried out by ultraviolet spectroscopy. The measurements of corrosion inhibition efficiencies were performed by the electrochemical linear polarization resistance (LPR) technique as well as weight loss, on the surface of AISI 1020 carbon steel. The maximum corrosion inhibition efficiencies were determined by extrapolation of Tafel plots, showing the following values: 95,6 % for the system SME-OCS-AO, 98,9 % for the system SME-OCS-AO-1 and 93,4 % for the system SME-OCS-PA
Resumo:
Nowadays, in the plastic industry are used mills that accomplish the recycling of residues generated in the production of its components. These mills contain cut sheets that suffer accelerated wear, once they are submitted constantly to the tribologic efforts, decreasing its useful life. To reduce this problem, it s used noble steels or takes place superficial treatments. The ionic nitriding process presents some limitations related to the uniformity of the layer in pieces with complex geometry, committing its application in pieces as knives, head offices, engagements, etc. However, the new technique of nitriding in cathodic cage eliminates some problems, as the restrictions rings, inherent to the conventional ionic nitriding. In present work, was studied the use viabilization of steels less noble, as SAE 1020, SAE 4320 and SAE 4340, nitreded by two different techniques, to substitute the AISI 01 steels, usually used in the cut knifes fabrication, seeking to reduce the costs and at the sane time to increase the useful life of these knifes. The steel most viable was the SAE 4340, nitrided in cathodic cage, because it presented uniformity in thickness and in the hardness of the layer, besides of increased 58% in the average its useful life
Resumo:
Doped lanthanum chromite ( LaCrO3 ) has been the most common material used as interconnect in solid oxide fuel cells for high temperature ( SOFC-HT ) that enabling the stack of SOFCs. The reduction of the operating temperature, to around 800 º C, of solid oxide fuel cells enabled the use of metallic interconnects as an alternative to ceramic LaCrO3, From the practical point of view, to be a strong candidate for interconnect the material must have good physical and mechanical properties such as resistance to oxidizing and reducing environments, easy manufacture and appropriate thermo-mechanical properties. Thus, a study on the physic-mechanical interconnects La0,8Sr0,2Cr0,92Co0,08O3 ceramics for SOFC -AT obtained by the method of combustion , as well as thermo-mechanical properties of metallic interconnects (AISI 444) covered with La0,8Ca0,2CrO3 by deposition technique by spray-pyrolysis fuel cells for intermediate temperature (IT-SOFCs). The La0,8Sr0,2Cr0,92Co0,08O3 was characterized by X -ray diffraction(XRD) , density and porosity , Vickers hardness (HV) , the flexural strength at room temperature and 900 °C and scanning electron microscopy (SEM). The X -ray diffraction confirmed the phase formation and LaCrO3 and CoCr2O4, in order 6 GPa hardness and mechanical strength at room temperature was 62 MPa ceramic Interconnector. The coated metal interconnects La0,8Ca0,2CrO3 passed the identification by XRD after deposition of the film after the oxidation test. The oxidative behavior showed increased resistance to oxidation of the metal substrate covered by La0,8Ca0,2CrO3 In flexural strength of the coated metal substrate, it was noticed only in the increased room temperature. The a SEM analysis proved the formation of Cr2O3 and (Cr,Mn)3O4 layers on metal substrate and confirmed the stability of the ceramic La0,8 Ca0,2CrO3 film after oxidative test