Resumo:

The indentation slope curve from a spherical indentation on elastic-plastic materials is examined. By comparing it with that of an linear elastic material of the same elastic properties, we found that the start point of plastic yielding for an elastic-plastic material can be easily located from the indentation slope curve. Based on this analysis, a simple but effective method is proposed to measure the plastic yield stress of very small samples from a spherical nano-indentation slope curve.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The stability of austenite in a number of Fe–Mn–Si-based shape memory alloys has been investigated. It was found that a grain boundary precipitate of BCC structure is formed over a wide range of alloy compositions and heat treatment temperatures. This grain boundary phase has been identified as the chi (χ) phase. Although up to 3 vol.% of the grain boundary precipitate was generated by isothermal aging in the range 500–800 °C, it was found not to markedly affect the mechanical properties or the shape memory effect. Nano-indentation indicated that the hardness and strength of the parent and precipitate phase are very similar, as are their compositions.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

 In this study, nano-indentation technique is employed to investigate the initiation of basal slip and extension twin separately in magnesium. The present method prove useful in studying the influence of solid solution and precipitates on these two deformation modes.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The detection and control of the temperature variation at the nano-scale level of thermo-mechanical materials during a compression process have been challenging issues. In this paper, an empirical method is proposed to predict the temperature at the nano-scale level during the solid-state phase transition phenomenon in NiTi shape memory alloys. Isothermal data was used as a reference to determine the temperature change at different loading rates. The temperature of the phase transformed zone underneath the tip increased by _3 to 40 _C as the loading rate increased. The temperature approached a constant with further increase in indentation depth. A few layers of graphene were used to enhance the cooling process at different loading rates. Due to the presence of graphene layers the temperature beneath the tip decreased by a further _3 to 10 _C depending on the loading rate. Compared with highly polished NiTi, deeper indentation depths were also observed during the solidstate phase transition, especially at the rate dependent zones. Larger superelastic deformations confirmed that the latent heat transfer through the deposited graphene layers allowed a larger phase transition volume and, therefore, more stress relaxation and penetration depth.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Using dimensional analysis and the finite element method, the spherical indentation hardness of shape memory alloys (SMAs) is investigated. The scaling relationship between the hardness and the mechanical properties of a SMA, such as the forward transformation stress, the maximum transformation strain magnitude, has been derived. Numerical results demonstrated that the hardness increases with the indentation depth but there is no three-fold relationship between the hardness and the forward transformation stress. Increasing the maximum transformation strain magnitude would reduce the hardness of the material. These research results enhance our understanding of the hardness from the spherical indentation of SMAs.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A novel polyvinylalcohol/silica (PVA/SiO2) nano-composite is prepared with the self-assembly monolayer (SAM) technique. The SiO2 nano-particles are homogenously distributed throughout the PVA matrixes as nano-clusters with an average diameter ranged from 15 to 240 nm depending on the SiO2 contents. Using differential scanning calorimetry (DSC), the non-isothermal crystallisation behaviour and kinetics of the PVA/SiO2 nano-composites are investigated and compared to those of the pure PVA. There are strong dependences of the degree of crystallinity (Xc), peak crystallisation temperature (Tp), half time of crystallisation (t1/2), and Ozawa exponent (m) on the SiO2 content and cooling rate. The crystallisation activation energy (E) calculated with the Kissinger model is markedly lower when a small amount of SiO2 is added, then gradually increases and finally becomes higher than that of the pure PVA when there is more than 10% SiO2 in the composite.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Spherical indentation of superelastic shape memory alloys (SMAs) has been theoretically analyzed. Two characteristic points on the superelastic indentation curve have been discovered. The bifurcation force corresponding to the bifurcation point relies on the forward transformation stress and the return force corresponding to the return point relies on the reverse transformation stress.
Based on these theoretical relationships, an approach to determine the transformation stresses of superelastic SMAs has been proposed. To improve the accuracy of the measurement, a slope method to locate the two characteristic points from the slope curves is further suggested. Additionally, the spherical indentation hardness was also analyzed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Dimensional analysis and the finite element method are applied in this paper to study spherical indentation of superelastic shape memory alloys. The scaling relationships derived from dimensional analysis bridge the indentation response and the mechanical properties of a superelastic shape memory alloy. Several key variables of a superelastic indentation curve are revealed and examined. We prove that the bifurcation force in a superelastic indentation curve only relies on the forward transformation stress and the elastic properties of the initial austenite; and the return force in a superelastic indentation curve only relies on the reverse transformation stress and the elastic properties of the initial austenite. Furthermore, the dimensionless functions to determine the bifurcation force and the return force are proved to be identical. These results not only enhance our understanding of spherical indentation of superelastic shape memory alloys, but also provide the theoretical basis for developing a practicable method to calibrate the mechanical properties of a superelastic material from the spherical indentation test.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The contribution of nano-scale particles observed using Atom Probe Tomography in an increase of yield strength of conventional and advanced HSLA steels was studied. The advanced HSLA steel showed higher yield strength than conventional HSLA steel. There were two types of carbides, which primarily contribute to an increase in yield strength of conventional HSLA steel: (i) coarse TiC with average size of 25±5nm and (ii) fine TiC with average radius of 3±1.2nm. The presence of two types of carbides was found in the microstructure of advanced HSLA steel: (i)
nano-scale Ti0.98Mo0.02C0.6 carbides with average radius of 2.2±0.5nm, and (ii) C19Cr7Mo24 particles with an average radius of 1.5±0.3nm. The contribution of precipitation hardening in the yield strength of advanced HSLA steel due to the nano-scale particles was 174MPa, while this value in the conventional HSLA steel was 128MPa.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In the present study, nano- and macro-scale characterisations on the mechanical properties of bovine cortical bones have been performed by using nanoindentation and conventional compressive tests. Nanoindentation results showed that the elastic modulus for the osteons and the interstitial lamellae in the longitude direction were 24.7 ± 2.5 GPa and 30.1 ± 2.4 GPa. As it’s difficult to distinguish osteons from interstitial lamellae in the transverse direction, the average elastic modulus for cortical bovine bone in the transverse direction was 19.8 ± 1.6 GPa. Significant differences were found in the modulus values between different microstructures of bone tissue and in different testing direction. It was found that the elastic modulus of bone bovine material in nano-level was higher than that in macro-level. The elastic modulus and
ultimate stress of large bone samples were 12.5 ± 1.9 GPa and 195 ± 19 MPa respectively from the compression test.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Spherical indentation test was conducted on as-cast and annealed Zr41.2Ti13.8Cu12.5Ni10Be22.5 bulk metallic glass, and the evolution of the morphology of the deformation zone of indents upon annealing was investigated. The DSC traces of the as-cast and annealed samples show that the enthalpy change at the glass transition, ΔH, decreases with the increasing of annealing temperature, indicating the reduction of the free volume upon annealing. The morphology of the indents implies a reduced shear band activity in the annealed samples. The included angles (2θ) between two families of shear bands emanating from the edge of spherical indent in the as-cast and the annealed samples were measured to be in the range of 88-79°, which decrease with the increasing of annealing temperature, indicating pressure sensitive plasticity in the as-cast and annealed samples. By Mohr–Coulomb criterion, the pressure sensitive index, α, can be obtained on the basis of the measured 2θ. The sensitivity index increases with increasing temperature, implying an increase of 'atomistic friction' due to the reduction of the free volume upon annealing.