This paper reports on the corrosion of Mg alloy AZ31 in simulated body fluid (SBF) using static immersion tests and electrochemical impedance spectroscopy. A preliminary study on the effect of flowing SBF on the corrosion behaviour of AZ31 has also been carried out. Low toxicity ionic liquids (ILs) trimethyl(butyl)phosphonium diphenyl phosphate P1444DPP and trihexyl(tetradecyl)-phosphonium bis-2,4,4trimethylpentyl-phosphinate [P66614][ i(C8) 2PO2] have been used to provide corrosion protection for AZ31 in SBF. Time dependent immersion tests indicate that under static conditions, AZ31 suffers severe localised corrosion in SBF, with pits developing predominantly beside the Al-Mn intermetallic phase in the α matrix. At longer immersion times, the corrosion product eventually precipitates and covers the entire specimen surface. When exposed to SBF under flowing conditions with a shear stress of 0·88 Pa, more uniform corrosion was observed. The optical profilometry results and electrochemical impedance spectroscopy analysis suggest that both P
1444DPP and [P66614][i(C8)2PO2] pretreatments can increase the corrosion resistance of AZ31 in SBF, in particular by decreasing the number of deeper pits found on the alloy surface. Cytotoxic test shows that the presence of the ILs P
1444DPP and [P66614][i(C8)2PO2] in cell culture media slightly inhibits the growth of human coronary artery endothelial cells in comparison with the good cell viability around the treated specimen. A pretreatment with IL is used in order to improve the corrosion resistance of this alloy in SBF. © 2012 Institute of Materials, Minerals and Mining.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Scanning white beam X-ray microdiffraction has been used to study the heterogeneous grain deformation in a polycrystalline Mg alloy (MgAZ31). The high spatial resolution achieved on beamline 7.3.3 at the Advanced Light Source provides a unique method to measure the elastic strain and orientation of single grains as a function of applied load. To carry out in-situ measurements a light weight (~0.5kg) tensile stage, capable of providing uniaxial loads of up to 600kg, was designed to collect diffraction data on the loading and unloading cycle. In-situ observation of the deformation process provides insight about the crystallographic deformation mode via twinning and dislocation slip.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

As-cast AZ80 Mg alloy contains α-Mg, partially divorce eutectic of α and γ (Mg 17Al 12), fully divorce eutectic of α and γ, and lamellar eutectic of α and γ phases. During homogenization, second phase (γ-Mg 17Al 12) gets dissolved can change the mechanical properties. Therefore, the aim of the present work is to bring out the kinetics of dissolution of γ phase and evaluate its effect on mechanical properties. Microstructure evolution during homogenization was investigated as a function of time for 0.5 to 100 h and at the temperatures of 400° and 439°C. In as-cast state, this material was found to contain 70% α-Mg and 30% eutectic phase. With increasing homogenization time, dissolution of lamellar eutectic occurs first which is followed by dissolution of fully divorce eutectic and partially divorce eutectic. The dissolution kinetics of γ phase was analyzed based on the decrease in its volume fraction as a function of time. The time exponent for dissolution was found to be 0.38 and the activation energy for the dissolution of γ phase was found to be 84.1 kJ/mol. This dissolution of γ phase leads to decrease in hardness and tensile strength with increase in homogenization time.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Recently, the use of magnesium alloys as metallic implant materials for biodegradable coronary artery stents has been steadily growing in interest. However, AZ31 magnesium alloys present poor corrosion resistance in the body environment. This work reports on the use of a treatment with low-toxicity IL Trimethyl (butyl) phosphonium diphenyl phosphate P1444DPP, which provides corrosion protection for magnesium alloy AZ31 in simulated body fluid (SBF). Before IL treatment, surface was cleaned by HNO3 and H3PO4 acid pickling solution. The effect of ionic liquid treatment on the corrosion performance of magnesium alloys AZ31in simulated body fluid has been investigated by electrochemical tests and the observation of surface morphology. The results show that this IL treatment succeeded in increasing the corrosion resistance of AZ31 when exposed to SBF.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Exploring high performance cathode materials is essential to realize the adoption of Li-ion batteries for application in electric vehicles and hybrid electric vehicles. FeF3, as a typical iron-based fluoride, has been attracting considerable interest due to both the high electromotive force value of 2.7 V and the high theoretical capacity of 237 mA h g_1 (1e_ transfer). In this study, we report a facile lowtemperature solution phase approach for synthesis of uniform iron fluoride nanocrystals on reduced graphene sheets stably suspended in ethanol solution. The resulting hybrid of iron fluoride nanocrystals and graphene sheets showed high specific capacity and high rate performance for iron fluoride type cathode materials. High stable specific capacity of about 210 mA h g_1 at a current density of 0.2 C was achieved, which is much higher than that of LiFePO4 cathode material. Notably, these iron fluoride/ nanocomposite cathode materials demonstrated superior rate capability, with discharge capacities of 176, 145 and 113 mA h g_1 at 1, 2 and 5 C, respectively.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The static recrystallisation behaviour of two magnesium alloys after hot rolling have been examined. The alloys chosen for study were the conventional alloy AZ31, and an alloy containing the rare earth element Gadolinium. The recrystallisation kinetics were lower for the rareearth alloy at low annealing temperatures, but at high annealing temperatures the kinetics were higher for the rare-earth alloy. It is suggested that this change in the comparative recrystallisation kinetics is a result of the improved mobility of the rare-earth solute at higher temperatures. This affects the recrystallisation kinetics through solute partitioning to the grain boundaries. The effect of this segregation on the recrystallisation texture is also discussed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Surface mechanical attrition treatment (SMAT) is a mechanical peening process used to generate ultrafine grain surfaces on a metal. SMAT was carried out on pure magnesium using different attrition media (zirconia [ZiO2], alumina [Al2O3], and steel balls) to observe the effect on microstructure, surface residual stress, surface composition, and corrosion. Surface contamination from SMAT was characterized using glow discharge optical emission spectroscopy (GDOES). The SMAT process produced a refined grain structure on the surface of Mg but resulted in a region of elemental contamination extending ~10 μm into the substrate, regardless of the media used. Consequently, SMAT-treated surfaces showed an increased corrosion rate compared to untreated Mg, primarily through increased cathodic kinetics. This study highlights the issue of contamination resulting from the SMAT process, which is a penalty that accompanies the significant grain refinement of the surface produced by SMAT. This must be considered if attempting to exploit grain refinement for improving corrosion resistance.