122 resultados para Mechanical properties


Relevância:

100.00% 100.00%

Publicador:

Resumo:

© 2015 Elsevier Ltd. All rights reserved. Most researches on graphene/polymer composites are focusing on improving the mechanical and electrical properties of polymers at low graphene content instead of paying attention to constructing graphene's macroscopic structures. In current study the homo-telechelic functionalized polyethylene glycols (FPEGs) were tailored with π-orbital-rich groups (namely phenyl, pyrene and di-pyrene) via esterification reactions, which enhanced the interaction between polyethylene glycol (PEG) molecules and chemical reduced graphene oxide (RGO) sheets. The π-π stacking interactions between graphene sheets and π-orbital-rich groups endowed the composite films with enhanced tensile strength and tunable electrical conductivity. The formation of graphene network structure mediated by the FPEGs fillers via π-π stacking non-covalent interactions should account for the experimental results. The experimental investigations were also complemented with theoretical calculation using a density functional theory. Atomic force microscope (AFM), scanning electron microscope (SEM), X-ray diffraction (XRD), nuclear magnetic resonance (NMR), thermal gravimetric analysis (TGA), UV-vis and fluorescence spectroscopy were used to monitor the step-wise preparation of graphene composite films.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Titanium alloys are widely used in various engineering design application due to its superior material properties. The traditional manufacturing of titanium products is always difficult, time consuming, high material wastage and manufacturing costs. Selective laser melting (SLM), an additive manufacturing technology has widely gained attention due to its capability to produce near net shape components with less production time. In this technical paper,microstructure,chemical composition,tensile properties and hardness are studied for the wrought and additive manufactured SLM cylindrical bar. Microstructure,mechanical properties and hardness were studied in both the longitudinal and transverse directions of the bar to study the effect of orientation. It was found that additive manufactured bar have higher yield strength, ultimate tensile strength and hardness than the wrought bar. For both conventional and SLM test samples, the yield strength, ultimate tensile strength and hardness was found to be high in the transverse direction. The difference in the properties can be attributed to the difference in microstructure as a result of processing conditions. The tensile fracture area was quantified by careful examination of the fracture surfaces in the scanning electron microscope.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This paper focuses on the influence of processing temperature and inclusion of micron-sized B4C, TiB2 and ZrSiO4 on the mechanical performance of aluminium matrix composites fabricated through stir casting. The ceramic/aluminium composite could withstand greater external loads, due to interfacial ceramic/aluminium bonding effect on the movement of grain and twin boundaries. Based on experimental results, the tensile strength and hardness of ceramic reinforced composite are significantly increased. The maximum improvement is achieved through adding ZrSiO4 and TiB2, which has led to 52% and 125% increase in tensile strength and hardness, respectively. To predict the effect of incorporating ceramic reinforcements on the mechanical properties of composites, experimental data of mechanical tests are used to create 3 models named Levenberg-Marquardt Algorithm (LMA) neural networks. The results show that the LMA- neural networks models have a high level of accuracy in the prediction of mechanical properties for ceramic reinforced-aluminium matrix composites.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Polypropylene (PP) and polystyrene (PS) blends were prepared by melt processing in a haake at 180 °C. PP/PS blends are immiscible and the blend morphologies were characterized by scanning electron microscopy. The viscoelastic properties were characterized using dynamic mechanical analysis (DMA) with reference to blend ratio. The blend morphologies such as matrix droplet and phase inverted morphologies were observed. The storage modulus of the blends increased with increase in PS content and the value was maximum for neat PS. DMA showed changes in the polystyrene glass transition temperatures (Tg) over the entire composition range. There was a sharp increase in the Tg of PS with increasing PP content in the blend and a 12 °C elevation in Tg was observed. The increase in Tg was explained by proposing a new model based on the physical interaction between the blend components. It is assumed that the different effects by the PP phase resulted in the formation of constrained PS chains leading to high Tg values. The addition of PP-g-MAH has a positive effect on the morphology, increases the storage modulus, and decreases the Tg till 80/20 blends. However, for PP/PS blends with higher concentrations of PS, the PP-g-MAH has little effect or adverse effect on the morphology, and storage modulus, but decreases the Tg.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this study, a series of Ti-xNb-yMo (x = 5-40 wt.% in 5 wt.% increments; and y = 3, 5, 10 wt%) alloys were fabricated by powder metallurgy and studied with respect to their microstructures, compressive mechanical properties and hardness. Increases in Nb and Mo content led to decreases in compressive and yield strengths, elastic modulus and hardness of the sintered alloys. Among the studied alloys, Ti-10Nb-3Mo alloy exhibited the optimum combination of strength and ductility. Alloys with a lower amount of Nb (≤ 25 wt.%) and Mo (≤ 5 wt.%) developed Widmanstätten structure, while further increase in Nb and Mo additions led to the microstructure predominantly consisting of β phase with varying regions of α + β phase. The effects of sintering temperature on elastic modulus and hardness were also investigated for Ti-xNb-3Mo alloys.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The mechanical behavior under uniaxial tension of Al-Mg alloy 5182 pre-deformed in conventional rolling (CR), asymmetric rolling-continuous (ASRC), and asymmetric rolling-reversed (ASRR) was investigated and modeled with a rate dependent crystal plasticity finite element method and VPSC (Visco-Plastic Self Consistent) model. M-K theory combined with Yld2000 model by Barlat et al. (Int. J. Plasticity 2003, 19, 1297) was used to predict the strain-based and stress-based formability for AA 5182 material. It was concluded that the new ASRR process has very compatible formability with improved strength compared to CR process. These merits can be directly applied for clam-shell resistant design in rigid-packaging industry.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Effects of neodymium (Nd) on the microstructures, mechanical properties, in vitro corrosion behavior, and cytotoxicity of as-cast Mg- 1Mn-2Zn-xNd alloys (x = 0.5, 1.0, 1.5, mass%) have been investigated to assess whether Nd is an effective element to increase the strength and corrosion resistance of Mg alloys, and to evaluate whether those alloys are suitable for biomedical applications. The microstructures were examined by X-ray diffraction analysis and optical microscopy. The mechanical properties were determined from uniaxial tensile and compressive tests. The corrosion behavior was studied using electrochemical measurement and cytotoxicity was evaluated using osteoblast-like SaOS2 cell. The results indicate that all the cast Mg-1Mn-2Zn-xNd alloys are composed of both alpha phase of magnesium (Mg) and a compound of Mg7Zn3, and their grain sizes decrease with Nd content. Nd is not an effective element to improve the strength and corrosion resistance of cast Mg-Mn-Zn alloys. Increase of Nd content from 0.5 to 1.5 does not significantly change biocompatibility of alloys. The cast alloys exhibit much better corrosion resistance than pure Mg and good biocompatibility.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In order to improve the miscibility and mechanical properties of poly(l-lactic acid) (PLLA) and poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV) bio-alloy, small amount of transesterification catalyst, zinc acetate was added in the melt blending process. We show that the PLLA-PHBV copolymer generated during the melt blending significantly improves the miscibility and therefore enhances the mechanical properties of the product. Dynamic mechanical analysis (DMA), scanning electron microscopy (SEM), and tensile tests were performed to study the miscibility and mechanical properties of the blends. Fourier transform infrared spectroscopy (FTIR) and gel permeation chromatography (GPC) were used to reveal the molecular structural, and molecular weight changes of PLLA and PHBV after melt mixing with zinc acetate. SEM and FTIR results have clearly shown that the PLLA-PHBV copolymer generated from transesterification reaction acted as a compatibilizer and therefore resulted in an improved interfacial miscibility and ductility of PLLA/PHBV blend. In our mechanistic study, a competition between the PLLA/PHBV transesterification reaction and the thermal decomposition of PHBV was identified for the first time. On the basis of these observations, a new mechanism of transesterification reaction was proposed.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The development behaviors of ultrafine grains (UFGs) due to continuous dynamic recrystallization (cDRX) were investigated in hot compression of a Mg-4Y-2Nd-0.2Zn-0.5Zr alloy pretreated in solution and subsequently peak-aging. In the aging sample containing statically precipitated particles (SPPs), the occurrence of cDRX starts to take place at medium to high strains, and finally a stable size of UFGs are fully developed in a whole volume. In the as-solution sample with no SPPs, by contrast, the size of UFGs evolved increases rapidly at lower strains, slowly at medium strains and then finally shows a bimodal distribution in high strain. In the latter, smaller grains accompanying with an incomplete formation of UFGs are developed by any effect of dynamically precipitated particles (DPPs). The microtexture evolved is effectively randomized in the regions of UFGs, leading to the formation of a weaker texture. The tensile elongation of the aging sample, with SPPs and fully developed UFGs, was around 17.4%. This was much higher than that of the as-solution one, with no SPPs and incompletely developed UFGs, that was 11.8%, which might result from the more randomized texture due to fully developed UFGs.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this work, a high-manganese Fe-23Mn-1.5Al-0.3C Twinning-Induced Plasticity (TWIP) steel was subjected to plastic shear deformation using Equal-Channel Angular Pressing (ECAP) at 300 °C following route BC and additional annealing. The microstructure evolution during both deformation by ECAP and subsequent annealing was investigated and correlated with the mechanical properties. The successive grain refinement during ECAP was promoted by two parallel mechanisms, namely dislocation driven grain fragmentation and twin fragmentation, and accounted for the ultra-high strength. In addition, due to the relatively low volume fraction of deformation twins after ECAP at 300 °C, further contribution of deformation twinning during room temperature deformation allowed additional work-hardening capacity and elongation. During subsequent recovery annealing the ultra-fine grains and deformation twins were thermally stable, which supported retainment of the high yield strength along with regained uniform elongation. For the first time, the texture evolution during ECAP and during the following heat treatment was analyzed. After 1, 2, and 4 ECAP passes a transition texture with the characteristic texture components of both high- and low-SFE materials developed. During the following heat treatment the texture evolution proceeded similar to that observed in the same material after cold rolling. Retaining of the ECAP texture components due to oriented nucleation at grain boundaries and triple junctions as well as annealing twinning accounted for the formation of a weak, retained ECAP texture after recrystallization.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Microstructure evolution, mechanical properties, formability, and texture development were determined for AA6111 samples processed by asymmetric rolling (ASR) with different roll friction, velocity, or diameters, conventional rolling (CR), and equal-channel-angular pressing (ECAP). Highly elongated or sheared grain structures were developed during ASR/CR and ECAP, respectively. ASR led to improved r-values and formability compared with CR primarily as a result of the development of moderate shear-texture components analogous to those developed during ECAP of billet material. ASR based on different roll diameters gave the best combination of strength, ductility, and formability.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Poly(methyl methacrylate)/poly(styrene-co-acrylonitrile) (PMMA/SAN) blends, with varying concentrations, were prepared by melt-mixing technique. The miscibility is ensured by fixing the acrylonitrile (AN) content of styrene acrylonitrile (SAN) as 25% by weight. The blends were transparent as well. The Fourier transform infrared spectroscopic (FTIR) studies did not reveal any specific interactions, supporting the well accepted 'copolymer repulsion effect' as the driving mechanism for miscibility. Addition of SAN increased the stability of PMMA towards ultraviolet (UV) radiations and thermal degradation. Incorporation of even 0.05% by weight of multi-walled carbon nanotubes (MWCNTs) significantly improved the UV absorbance and thermal stability. Moreover, the composites exhibited good strength and modulus. However, at higher concentrations of MWCNTs (0.5 and 1% by weight) the thermo-mechanical properties experienced deterioration, mainly due to the agglomeration of MWCNTs. It was observed that composites with 0.05% by weight of finely dispersed and well distributed MWCNTs provided excellent protection in most extreme climatic conditions. Thus, PMMA/SAN/MWCNTs composites can act as excellent light screens and may be useful, as cost-effective UV absorbers, in the outdoor applications.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Ti-Zr alloys have recently started to receive a considerable amount of attention as promising materials for dental applications. This work compares mechanical properties of a new Ti-15Zr alloy to those of commercially pure titanium Grade4 in two surface conditions - machined and modified by sand-blasting and etching (SLA). As a result of significantly smaller grain size in the initial condition (1-2µm), the strength of Ti-15Zr alloy was found to be 10-15% higher than that of Grade4 titanium without reduction in the tensile elongation or compromising the fracture toughness. The fatigue endurance limit of the alloy was increased by around 30% (560MPa vs. 435MPa and 500MPa vs. 380MPa for machined and SLA-treated surfaces, respectively). Additional implant fatigue tests showed enhanced fatigue performance of Ti-15Zr over Ti-Grade4.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The acoustic and mechanical properties of silk membranes of different thicknesses were tested to determine their suitability as a repair material for tympanic membrane perforations. Membranes of different thickness (10-100μm) were tested to determine their frequency response and their resistance to pressure loads in a simulated ear canal model. Their mechanical rigidity to pressure loads was confirmed by tensile testing. These membranes were tested alongside animal cartilage, currently the strongest available myringoplasty graft as well as paper, which is commonly used for simpler procedures. Silk membranes showed resonant frequencies within the human hearing range and a higher vibrational amplitude than cartilage, suggesting that silk may offer good acoustic energy transfer characteristics. Silk membranes were also highly resistant to simulated pressure changes in the middle ear, suggesting they can resist retraction, a common cause of graft failure resulting from chronic negative pressures in the middle ear. Part of this strength can be explained by the substantially higher modulus of silk films compared with cartilage. This allows for the production of films that are much thinner than cartilage, with superior acoustic properties, but that still provide the same level of mechanical support as thicker cartilage. Together, these in vitro results suggest that silk membranes may provide good hearing outcomes while offering similar levels of mechanical support to the reconstructed middle ear.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Our previous studies have demonstrated that Mg-Zr-Sr alloys can be anticipated as excellent biodegradable implant materials for load-bearing applications. In general, rare earth elements (REEs) are widely used in magnesium (Mg) alloys with the aim of enhancing the mechanical properties of Mg-based alloys. In this study, the REE holmium (Ho) was added to an Mg-1Zr-2Sr alloy at different concentrations of Mg1Zr2SrxHo alloys (x = 0, 1, 3, 5 wt. %) and the microstructure, mechanical properties, degradation behaviour and biocompatibility of the alloys were systematically investigated. The results indicate that the addition of Ho to Mg1Zr2Sr led to the formation of the intermetallic phases MgHo3, Mg2Ho and Mg17Sr2 which resulted in enhanced mechanical strength and decreased degradation rates of the Mg-Zr-Sr-Ho alloys. Furthermore, Ho addition (≤5 wt. %) to Mg-Zr-Sr alloys led to enhancement of cell adhesion and proliferation of osteoblast cells on the Mg-Zr-Sr-Ho alloys. The in vitro biodegradation and the biocompatibility of the Mg-Zr-Sr-Ho alloys were both influenced by the Ho concentration in the Mg alloys; Mg1Zr2Sr3Ho exhibited lower degradation rates than Mg1Zr2Sr and displayed the best biocompatibility compared with the other alloys.