Resumo:

Nanoindentation was performed in selected grain orientations close to [. 112-0] and [. 101-0] in magnesium alloy Mg-3Al-1Zn. The atomic force microscopy (AFM) and electron backscatter diffraction (EBSD) were used to examine the nanoindentation imprint. Two critical events, yielding and pop-in were observed in the depth-load curves. Slip trace analysis suggests that basal slip is responsible for yielding. The following pop-in events at higher loads are associated with the appearance {. 101-2} twins on the surface. The critical resolved shear stress (CRSS) was estimated to be in the range of 220-400. MPa for the initiation of basal slip.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Nanoporous titania nanoparticles (NTNs) were synthesized and used as an additive at a low concentration of 0.1-1 wt % in the fabrication of poly(ethersulfone) (PES) ultrafiltration membranes via non-solvent-induced phase separation. The structure and properties of nanoparticles were characterized using nitrogen sorption, X-ray diffraction, scanning electron microscopy, and transmission electron microscopy. The NTNs have a size distribution with a particle size of mainly <100 nm and have a Brunauer, Emmett, and Teller surface area of ∼100 m2 g-1. The modified membranes were fabricated and investigated in terms of their pure water flux, solute rejection, and fouling resistance. The water permeability and molecular weight cutoffs (MWCOs) of membranes were determined under constant-pressure filtration in dead-end mode at 100 kPa. The membrane fouling resistance was characterized under constant flux operation using bovine serum albumin as a model foulant. The membranes were characterized in terms of morphology, porosity, pore size distribution, energy-dispersive X-ray spectroscopy, contact angle goniometry, surface free energy, and viscosity of the dope solution. Overall, the modified membrane showed increased wettability and reduced surface free energy and pore size. The modified UF membrane with 0.5 wt % NTN loading exhibited improved fouling resistance (fouling rate of 0.58 kPa/min compared to a rate of 0.70 kPa/min for the control membrane) with ∼80% water flux recovery. The same membrane showed an ∼20% increase in water flux, an improvement in MWCO, and a narrower pore size distribution.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The normalised polarity E and Kamlet-Taft parameters of recently described solvate ionic liquids, composed of lithium bis(trifluoromethyl)sulfonimide (LiTFSI) in tri- () or tetraglyme () have been determined and compared to the parent glyme ( and ). We show that these solvate ionic liquids have a high polarity (, (E) = 1.03; , (E) = 1.03) and display very high electron pair accepting characteristics (, α = 1.32; , α = 1.35). Molecular dynamics simulations suggest that the chelated lithium cation is responsible for this observation. The relatively small hydrogen bond acceptor (β) values for these systems (, β = 0.41; , β = 0.37) are thought to be due primarily to the TFSI anion, which is supplemented slightly by the glyme oxygen atom. In addition, these solvate ionic liquids are found to have a high polarisability (, π* = 0.94; , π* = 0.90).