The present work examines the microstructure and texture evolution in a Ni-30wt.%Fe austenitic model alloy deformed in torsion at 1000 °C, with a particular emphasis on the orientation dependence of the substructure characteristics within the deformed original grains. Texture of these grains was principally consistent with that expected for simple shear and comprised the main A, B and C components. The deformation substructure within the main texture component grains was characterised by "organised" arrays of parallel microbands with systematically alternating misorientations, locally accompanied by micro-shear bands within the C grains. With increasing strain, the mean subgrain size gradually decreased and the mean misorientation angle concurrently increased towards the saturation. The stored deformation energy within the main texture component grains was principally consistent with the respective Taylor factor values. The microband boundaries corresponded to the expected single slip {111} plane for the A oriented grains while these boundaries for the C oriented grains represented a variety of planes even for a single grain.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Single pass warm rolling and compression experiments were carried out from ambient to 800°C for ultra-low carbon (ULC) steel with ∼100 ppm carbon and interstitial free (IF) steels, both with two levels of silicon. Subsequently, annealing was done in order to recrystallize the deformed specimens. The main purpose of this study was to understand the effects of rolling temperature and silicon on stress responses and textures. This study comprises two main themes: flow stress and strain rate sensitivity during compression and shear banding and textures in warm rolled specimens. The effects of deformation temperature on in-grain shear bands were different between ULC-Si and IF-Si steels. As in previous work with more conventional steels, in-grain shear bands in the IF grade had low sensitivity to rolling temperature, while those in the ULC grade depended significantly on the deformation temperature. However, the temperature profile of shear banding in the ULC grade was approximately 150°C higher than in previous work. Deformation and recrystallisation textures for both IF and ULC grades depended on their rolling temperatures. The variation of both grain size and texture after annealing can be explained by the rise and fall of in-grain shear banding activity which is related to the strain rate sensitivity.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Instabilities of plastic flow in the form of localised shear bands were experimentally observed to result from equal-channel angular pressing (ECAP) of magnesium alloy AZ31. The appearance of shear bands and their spacing were dependent on velocity of the pressing and applied back-pressure. A generic gradient plasticity theory involving second-order strain gradient terms in a constitutive model was applied to the case of AZ31 deformed by ECAP. Linear stability analysis was applied to the set of equations describing the deformation behaviour in the process zone idealised as a planar shear zone. A full analytical solution providing a dispersion relation between the rate of growth of a perturbation and the wave number was obtained. It was shown that the pattern of incipient localised shear bands exhibits a spectrum of characteristic lengths corresponding to admissible wave numbers. The interval of the spectrum of wave numbers of viable, i.e. growing, perturbations predicted by linear stability analysis was shown to be in good agreement with the experimentally observed spectrum. The effect of back-pressure applied during ECAP was also considered. The predicted displacement of the shear band spectrum towards lower wave numbers, shown to be a result of the decreased shear strain rate in the shear zone, was consistent with the experimentally observed increase of the band spacing with increased back-pressure. A good predictive capability of the general modelling frame used in conjunction with linear stability analysis was thus demonstrated in the instance of the particular alloy system and the specific processing conditions considered.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Of considerable importance to the generation of ultrafine microstructures is the development of high misorientations. The present work examines the effect of the crystallographic rotation field in simple shear upon the evolution of misorientation during plastic working. A series of Taylor simulations are presented and it is shown that the rotation field is such that small differences in orientation in the region of the main torsion texture components are considerably increased with the application of shear strain. This did not occur in simulations of rolling. The torsion simulations compare favourably with the nature of the misorientations evident in hot worked 1050 Al and Ti-IF steel. It is concluded that shear deformation, by its nature, facilitates the generation of higher misorientations.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We investigate all algebraically special, not conformally flat, shear-free, isentropic (p(w), w + p ≠ 0), perfect fluid solutions of Einstein's field equations. We show, using the GHP formalism, that if the repeated principle null direction of the Weyl tensor is coplanar with the fluid's 4-velocity and vorticity vector (assumed nonzero), then the fluid's expansion must vanish.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The giant lantern shark, Etmopterus baxteri, is taken as bycatch of commercial fisheries that operate in deepwater off southeastern Australia. Bands on the second dorsal spine were used to obtain age estimates. The number of bands on the external surface of the spine and within the inner dentine layer increased with animal length. Most spines had more bands on the external surface, and the rate of band formation was significantly different between the external surface and the inner dentine layer. Females had a maximum of 57 external bands and 26 internal bands, while males had up to 48 external bands and 22 internal bands. Age estimates from external bands suggest maturity (A 50) at 20 years for males and 30 years for females. Internal band age estimates suggest maturity at 10.5 years for males and 11.5 years for females. Although there is a large discrepancy between these two preliminary (i.e., unvalidated) age estimates, they both suggest that E. baxteri is a long-lived and late maturing species that is likely to be susceptible to over fishing.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Bands on the external surface of the second dorsal-fin spine proved to be a novel method of estimating the age and growth of Centroselachus crepidater. Bands that followed the shape of the spine base were enhanced with an alizarin red derivative. Internal bands in spine cross sections were also examined. The number of both external and internal bands increased with animal size, although most spines had more external than internal bands. External bands were more reliable and were assumed to be annuli. The rate of band formation differed after five bands had been formed, and internal bands ceased forming after 30 years. Females to 54 years old and males to 34 years old were examined. Maturity occurred over a wide age range, with estimates of 20 years for females and 9 years for males. The youngest pregnant female was 27 years old. The Francis reparameterized von Bertalanffy growth model found similar growth for males and females, and the von Bertalanffy equations were Lt = 96.12(1 – e(–0.072(t+6.13))) for females and Lt = 73.22(1 – e(–0.141(t+2.99))) for males.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An investigation into the production of ultrafine (1 µm) equiaxed ferrite (UFF) grains in low-carbon steel was made using laboratory rolling, compression dilatometry, and hot torsion techniques. It was found that the hot rolling of thin strip, with a combination of high shear strain and high undercooling, provided the conditions most suitable for the formation of this type of microstructure. Although high strains could be applied in compression and torsion experiments, large volume fractions of UFF were not observed in those samples, possibly due to the lower level of undercooling achieved. It is thought that ferrite refinement was due to a strain-induced transformation process, and that ferrite grains nucleated on parallel and linear deformation bands that traversed austenite grains. These bands formed during the deformation process, and the undercooling provided by the contact between the strip and the work rolls was sufficient to drive the transformation to homogeneous UFF grains.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Interaction of Lamb waves with structural damage can lead to wave mode conversion. In this study, the shear horizontal (SH) wave, from the mode conversion of the fundamental symmetric Lamb wave (S0), was used for quantitative identification of delamination in composite beams, based on advanced signal processing using an inverse approach. SH wave propagation under various delamination conditions in CF/EP beams made of orthotropic plain woven fabrics was simulated, and signal characteristics were extracted in terms of the concept of digital damage fingerprints (DDF). With the aid of an artificial neural algorithm, the relation between the DDF of delamination-scattered SH mode and damage parameters was calibrated, whereby the occurrence, location and size of delamination in the composite beams were assessed. The approach was experimentally validated, and the results demonstrate the effectiveness of SH mode for quantitative damage evaluation of composite structures.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We show that shear-free perfect fluids obeying an equation of state p = (γ − 1)μ are non-rotating or non-expanding under the assumption that the spatial divergence of the magnetic part of the Weyl tensor is zero.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Efficient and accurate finite elements are crucial for finite element analysis to provide adequate prediction of the structural behavior. A large amount of laminated plate elements have been developed for finite element analysis of laminated composite plates based on the various lamination theories. A recent and complete review of the laminated finite elements based on the higher-order shear deformation theories, including the global higher-order theories, zig-zag theories and the global-local higher-order theories is presented in this paper. Finally some points on the development of the laminated plate elements are summarized.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Background

Polyethyleneterephthalate (PET) and polytetrafluoroethylene (PTFE) are polymers successfully used as large diameter arterial grafts for peripheral vascular surgery. However, these prosthetic grafts are rarely used for coronary bypass surgery because of their low patency rates. Endothelialisation of the lumenal surface of these materials may improve their patency. This study aimed to compare the endothelialisation of PET, PTFE and pericardium by examining their seeding efficiency over time and the effect of various shear stresses on retention of endothelial cells.

Methods


Ovine endothelial cells at 4 × 105 cells/cm2 were seeded onto PET, PTFE and pericardium, and cultured for 1–168 hours. Cell coverage was determined via en face immunocytochemistry and cell retention was quantified after being subjected to shear stresses ranging from 0.018 to 0.037 N/m2 for 15, 30 and 60 minutes.

Results

Endothelial cells adhered to all of the materials one hour post-seeding. PET exhibited better cell retention rate, ranging from 66.9 ± 5.6% at 0.018 N/m2 for 15 min to 44.7 ± 1.9% at 0.037 N/m2 for 60 minutes, when compared to PTFE and pericardium (p < 0.0001, three-way ANOVA).

Conclusion

PET shows superior retention of endothelial cells during shear stress compare to PTFE and pericardium.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

RF MEMS plays an important role in microwave switching. The high performance of RF MEMS shunt such as high bandwidth, low insertion loss, and high isolation have made these switches well suitable for high performing microwave and millimeter wave circuits. This paper presents a RF MEMS shunt capacitive switch for Ka and V band application. This paper investigates the effect of various geometrical parameters on RF characteristics of the switch. The simulation results are presented and discussed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We investigate shear-free perfect fluid solutions of the Einstein field equations where the fluid pressure satisfies a barotropic equation of state and the spatial divergence of the magnetic part of the Weyl tensor is zero. We prove, with the exception of certain quite restricted special cases within the class of solutions in which there exists a Killing vector aligned with the vorticity and for which the magnitude of the vorticity ω is not a function of the matter density μ alone, that such a fluid is either non-rotating or non-expanding. In the restricted cases the equation of state must satisfy an over-determined differential system.