Understanding the magneto-hydrodynamic forces generated due to the external magnetic field and current density distribution within the cell (current in cell linings) is important in the optimization of cell dynamics. It is well documented that these factors play a crucial role in establishing the metal-pad stability of the cell. Conventional cells use the cathode-collector-bar assembly to carry the current through molten aluminium, the cathode and the steel collector-bar to nearest external bus. The electrical conductivity of the steel is so poor relative to the molten aluminium that the outer third of the collector bar carries the maximum load, which in turn increases the horizontal components of the current within the cell. Previous studies have modelled improvement in the cell instability through external magnetic compensation by redistributing current in the cathode busbar. Very little to date has been published on work to improve the current distribution within the cell. In this work, the current distribution in an aluminium electrolysis cell with copper collector-bar was predicted using finite element modelling. A 2D cross-section of a commercial cell was used under steady conditions of electrical fields in anode, electrolyte, molten aluminium and copper cathode-assembly. Different shapes and sizes of the cathode assembly are also considered to optimise the distribution of current throughout the cathode lining. The findings indicated that the copper-bar of similar size to steel could save voltage up to 150 mV. There is a reduction of more than 70% in peak current density value due to the copper inserts. The predicted trends of current distribution show a good agreement with previously published data.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An array of pine-shaped nanostructures of aluminum nitride (AlN) was synthesized through direct reaction between Al vapor and nitrogen gas in direct current (DC) arc discharge plasma without any catalyst or template. The as-prepared nanostructure consists of many pine-needle-shaped leaves with conical shape tips. The structure, morphology, and optical property of the nanostructure have been characterized by X-ray powder diffraction, energy-dispersive X-ray spectroscopy, field emission scanning electron microscopy, transmission electron microscopy, high-resolution transmission electron microscopy, Raman spectroscopy, and photoluminescence. A possible growth mechanism of the pine-shaped nanostructure was discussed. Two factors were found to be essential for branched nanostructure growth, i.e., the reaction time and N2 pressure. The photoluminescence spectrum of the nanostructure of AlN revealed an intense emission band, suggesting that there may be potential applications in electronic and optoelectronic nanodevices.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The aqueous corrosion behavior of low-alloy steel with aluminum contents was examined in a 10 wt% H2SO4 (pH 0.13) solution using electrochemical techniques and surface analyses. The corrosion resistance of the new alloy steel was evaluated in terms of electrochemical parameters, such as passive current density, film, and charge transfer resistances. The results showed that a high Al content in the steel imparted better passivation behavior resulting in a lower corrosion rate. It related to the enrichment of iron carbonate and hydrocarbon by the dissolution of the carbide phase.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Precipitation strenghthening is one of the most important approaches for enhancing the strenght of microalloyed steels. This study has made a significant contribution in understanding the nucleation and growth mechanism of nanoscale interphase precipitates in steel during commercial processes. Atom Probe Tomography revealed the existence of nanoscale clusters with precipitates that then dictate the final strength.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Sensitization of 5xxx series Al alloys involving precipitation of β phase (Mg2Al3) at grain boundaries was studied for different exposure times at 100°C upon AA5083-H131 (UNS A95083). In this work, we reveal that fracture surfaces prepared by liquid gallium embrittlement can yield a quantification of grain boundary β phase with significant statistics on β phase size and spacing. This information is a necessary first step toward development of quantitative damage models to describe inter-granular corrosion (IGC) and stress corrosion (IGSCC).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Traditional researches on metal corrosion under salt solutions deposit conditions are usually carried out by visual, electron microscopic observations and simple electrochemical measurement via a traditional one-piece electrode. These techniques have difficulties in measuring localized corrosion that frequently occur in inhomogeneous media. This paper reports the results from the experiments using specially shaped coupons and a relatively new method of measuring heterogeneous electrochemical processes, namely, the wire beam electrode(WBE). Preliminary results from copper and aluminum corrosion in highly concentrated sodium chloride solutions with and without solid deposits show that the method is useful in simulating and studying corrosion especially localized corrosion in pipelines.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An electrochemically integrated multi-electrode array namely the wire beam electrode (WBE) has been used to characterize the behavior of cerium chloride (CeCl3) and lanthanum chloride (LaCl3) in inhibiting localized corrosion of AA2024-T3 and AA1100. CeCl3 has been found to inhibit AA2024-T3 corrosion in 0.005 M sodium chloride (NaCl) solution by suppressing galvanic corrosion activities and by creating a large number of insignificant anodes. It has also been shown to inhibit localized corrosion of AA1100 in 0.5 M NaCl solution by promoting the random distribution of minor anodes. LaCl3 has been found to inhibit localized corrosion of AA2024-T3 at 1000 ppm, although its efficiency dropped significantly when its concentration decreased to 500 ppm. The addition of CeCl3 and LaCl3 to corrosion testing cells at later stages was unable to effectively suppress existing corrosion anodes.