Resumo:

The present thesis focuses on characterisation of microstructure and the resulting mechanical and tribological properties of CVD and PVD coatings used in metal cutting applications. These thin and hard coatings are designed to improve the tribological performance of cutting tools which in metal cutting operations may result in improved cutting performance, lower energy consumption, lower production costs and lower impact on the environment.  In order to increase the understanding of the tribological behaviour of the coating systems a number of friction and wear tests have been performed and evaluated by post-test microscopy and surface analysis. Much of the work has focused on coating cohesive and adhesive strength, surface fatigue resistance, abrasive wear resistance and friction and wear behaviour under sliding contact and metal cutting conditions. The results show that the CVD deposition of accurate crystallographic phases, e.g. α-Al2O3 rather than κ-Al2O3, textures and multilayer structures can increase the wear resistance of Al2O3. However, the characteristics of the interfaces, e.g. topography as well as interfacial porosity, have a strong impact on coating adhesion and consequently on the resulting properties.  Through the deposition of well designed bonding and template layer structures the above problems may be eliminated. Also, the presence of macro-particles in PVD coatings may have a significant impact on the interfacial adhesive strength, increasing the tendency to coating spalling and lowering the surface fatigue resistance, as well as increasing the friction in sliding contacts. Finally, the CVD-Al2O3 coating topography influences the contact conditions in sliding as well as in metal cutting. In summary, the work illuminates the importance of understanding the relationships between deposition process parameters, composition and microstructure, resulting properties and tribological performance of CVD and PVD coatings and how this knowledge can be used to develop the coating materials of tomorrow.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this study, gaseous emissions and particles are measured during start-up and stop periods for an over-fed boiler and an under-fed boiler. Both gaseous and particulate matter emissions are continuously measured in the laboratory. The measurement of gaseous emissions includes oxygen (O2), carbon dioxide (CO2), carbon monoxide (CO), nitrogen oxide and (NO). The emissions rates are calculated from measured emissions concentrations and flue gas flow. The behaviours of the boilers during start-up and stop periods are analysed and the emissions are characterised in terms of CO, NO, TOC and particles (PM2.5 mass and number). The duration of the characterised periods vary between two boilers due to the difference in type of ignition and combustion control. The under-fed boiler B produces higher emissions during start-up periods than the over-fed boiler A. More hydrocarbon and particles are emitted by the under-fed boiler during stop periods. Accumulated mass of CO and TOC during start-up and stop periods contribute a major portion of the total mass emitted during whole operation. However, accumulated mass of NO and PM during start-up and stop periods are not significant as the duration of emission peak is relatively short.