7 resultados para styrene-butadiene rubber

em CentAUR: Central Archive University of Reading - UK


Relevância:

20.00% 20.00%

Publicador:

Resumo:

A cylinder forming poly(styrene-b-butadiene-b-styrene) triblock copolymer melt is cyclically processed through a capillary at a high shear rate in the Cambridge Multipass Rheometer (MPR). In situ X-ray diffraction experiments enable observation of the effect of the shear on the block copolymer (BCP) nanophase orientation, both during and after processing. Temporal resolution of the X-ray exposures is increased, whilst retaining intensity, by exploiting the cyclical nature of the shear and the material's response to it; short exposures from many cycles, individually having few counts, are added together to produce well resolved X-ray patterns. Orientation of the cylinders reduces during processing, then increases during pauses between processing. The loss of orientation is attributed to the high shear rate deforming the melt faster than the structure can respond, whilst it is believed that melt relaxation, linked to the compressibility of the material, produces much lower shear rates after mechanical processing has ceased, which induces strong orientation of the nanostructure.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A series of multicarboxylic acid appended imidazolium ionic liquids ( McaILs) with chloride [ Cl](-) or bromide [ Br](-) as anions have been synthesized and characterized. Deprotonation of these ionic acids gives the corresponding zwitterions. Re-protonation of the zwitterions with strong Bronsted acids gives a series of new ionic acid-adducts, many of which remained as room-temperature ionic liquids. A new catalytic system, McaIL/PdCl2 for the selective catalytic oxidation of styrene to acetophenone with hydrogen peroxide as an oxidant has been attempted. In the presence of McaILs, it is found that the quantity of palladium chloride PdCl2 used can be greatly reduced while the activity ( TOF) and selectivity towards acetophenone are enhanced sharply. It is also shown that the catalytic properties of this system could be finely tuned through the molecular design of the McaILs. The best TOF value obtained so far is 146 h(-1) with 100% conversion of styrene at 93% selectivity to acetophenone. In addition, the catalytic activity has been maintained for at least ten catalytic cycles.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Two styrene-isoprene-styrene block copolymers Vector 4111 and 4113, exhibiting cylindrical (18 wt % PS) and spherical (16 wt % PS) morphology, respectively, have been examined under uniaxial elongation up to 200% strain. On the basis of stress-strain data, mechanical properties are compared for isotropic and oriented polystyrene domains. The structure at various stages of deformation has been determined from SAXS patterns in three planes and two principal deformation directions with respect to orientation. Samples showed a very high degree of hexagonal packing, resulting in an X-ray pattern taken parallel to the cylinder alignment approaching single crystal ordering. Cylinders were aligned with the closest packed planes parallel to film surface. Particular attention has been paid to a lattice deformation process occurring during the first stretching and relaxation cycle. For a copolymer with oriented cylindrical morphology the deformation was affine up to 120% strain. The microdomain spacing was calculated parallel and perpendicular to the stretching direction. The cylindrical microstructure orientation, quantified by Hermans' orientation factor reduced during elongation of oriented polymer, while the elongation of isotropic sample caused an increase of orientation. Deformation of all studied morphologies was reversible.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We studied how the integration of seen and felt tactile stimulation modulates somatosensory processing, and investigated whether visuotactile integration depends on temporal contiguity of stimulation, and its coherence with a pre-existing body representation. During training, participants viewed a rubber hand or a rubber object that was tapped either synchronously with stimulation of their own hand, or in an uncorrelated fashion. In a subsequent test phase, somatosensory event-related potentials (ERPs) were recorded to tactile stimulation of the left or right hand, to assess how tactile processing was affected by previous visuotactile experience during training. An enhanced somatosensory N140 component was elicited after synchronous, compared with uncorrelated, visuotactile training, irrespective of whether participants viewed a rubber hand or rubber object. This early effect of visuotactile integration on somatosensory processing is interpreted as a candidate electrophysiological correlate of the rubber hand illusion that is determined by temporal contiguity, but not by pre-existing body representations. ERPmodulations were observed beyond 200msec post-stimulus, suggesting an attentional bias induced by visuotactile training. These late modulations were absent when the stimulation of a rubber hand and the participant’s own hand was uncorrelated during training, suggesting that pre-existing body representations may affect later stages of tactile processing.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Addition of the dithioethers (−)-DIOSR2 (R=Me, iPr) (2,3-O-isopropylidene-1,4-dimethyl (and diisopropyl) thioether-L-threitol) to a dichloromethane solution of [Rh(COD)2]ClO4 (COD=1,5-cyclooctadiene) yielded the mononuclear complexes [Rh(COD)(DIOSR2)]ClO4. X-ray diffraction methods showed that the [Rh(COD)(DIOSiPr2)]ClO4 complex had an square-planar coordination geometry at the rhodium atom with the iPr groups in anti position. Cyclooctadiene complexes react with carbon monoxide to form dinuclear tetracarbonylated complexes [(CO)2Rh(μ-DIOSR2)2(CO)2](ClO4)2. [Rh(COD)(DIOSR2)]ClO4 are active catalyst precursors in styrene hydroformylation at 30 atm and 65°C which give conversions of up to 99% with a regioselectivity in 2-phenylpropanal as high as 74%. In all cases enantioselectivities are low.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Addition of 1,4-dithiols to dichloromethane solutions of [PtCl2(P-P)] (P-P = (PPh3)2, Ph2P(CH2)3PPh2, Phd2P(CH2)4PPh2; 1,4-dithiols = HS(CH2)4SH, (−)DIOSH2 (2,3-O-isopropylidene-1,4-dithiol-l-threitol), BINASH2 (1,1′-dinaphthalene-2,2′-dithiol)) in the presence of NEt3 yielded the mononuclear complexes [Pt(1,4-dithiolato)(P-P)]. Related palladium(II) complexes [Pd(dithiolato)(P-P)] (P-P=Ph2P(CH2)3PPh2, Ph2P(CH2)4PPh2; dithiolato = −S(CH2)4S−, (−)-DIOS) were prepared by the same method. The structure of [Pt((−)DIOS)(PPh3)2] and [Pd(S(CH2)4S)(Ph2P(CH2)3PPh2)] complexes was determined by X-ray diffraction methods. Pt—dithiolato—SnC12 systems are active in the hydroformylation of styrene. At 100 atm and 125°C [Pt(dithiolate)(P-P)]/SnCl2 (Pt:Sn = 20) systems provided aldehyde conversion up to 80%.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Molecular orientation parameters have been measured for the non-crystalline component of crosslinked natural rubber samples deformed in uniaxial tension as a function of the extension ratio and of temperature. The orientation parapeters 〈P2(cosα)〉 and 〈P4(cosα)〉 were obtained by an analysis of the anisotropy of the wide-angle X-ray scattering functions. For the measurements made at high temperatures the level of crystallinity detected was negligible and the orientation-strain behaviour could be compared directly with the predictions of molecular models of rubber elasticity. The molecular orientation behaviour with strain was found to be at variance with the estimates of the affine model particularly at low and moderate strains. Extension of the crosslinked rubber at room temperature led to strain-crystallization and measurements of both the molecular orientation of the non-crystalline chains and the degree of crystallinity during extension and relaxation enabled the role of the crystallites in the deformation process to be considered in detail. The intrinsic birefringence of the non-crystalline component was estimated, through the use of the 〈P2(cosα)〉 values obtained from X-ray scattering measurements, to be 0.20±0.02.