Resumo:

This paper details the synthesis, characterisation and physical analyses of a series of hydrogen bonded urethane supramolecular polymer systems that are created by a facile one-step synthesis from inexpensive and commercially available starting materials. We report the synthesis and characterisation of a series of low molecular weight bisurethanes (<650 a.m.u.) that exhibit physical properties in the bulk that are characteristic of polyurethane materials possessing far higher molecular weight. The physical characteristics of these low molecular weight bisurethanes were investigated by using temperature-dependent rheological analysis and viscometry and the nature in which these compounds assembled was assessed using IR and NMR spectroscopies. These studies reveal that these simple bisurethanes self-assemble via hydrogen bonding interactions.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The present paper details the synthesis, characterization, and preliminary physical analyses of a series of polyisobutylene derivatives featuring urethane and urea end-groups that enable supramolecular network formation to occur via hydrogen bonding. These polymers are readily accessible from relatively inexpensive and commercially available starting materials using a simple two-step synthetic approach. In the bulk, these supramolecular networks were found to possess thermoreversible and elastomeric characteristics as determined by temperature-dependent rheological analysis. These thermoreversible and elastomeric properties make these supramolecular materials potentially very useful in applications such as adhesives and healable surface coatings.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A series of six low molecular weight elastomers with hydrogen bonding end-groups have been designed, synthesised and studied. The poly(urethane) based elastomers all contained essentially the same hard block content (ca. 11%) and differ only in the nature of their end-groups. Solution state 1H NMR spectroscopic analysis of model compounds featuring the end-groups demonstrate that they all exhibit very low binding constants, in the range 1.4 to 45.0 M-1 in CDCl3, yet the corresponding elastomers each possess a markedly different nanoscale morphology and rheology in the bulk. We are able to correlate small variations of the binding constant of the end-groups with dramatic changes in the bulk properties of the elastomers. These results provide an important insight into the way in which weak non-covalent interactions can be utilized to afford a range of self-assembled polyurethane based materials that feature different morphologies.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The electrospinning of urethane based low molecular weight polymers differing only in the nature of the hydrogen bonding end-groups has been investigated. For the end-groups with the lowest binding constants at maximum solubility only droplets, are produced at the electrode; in contrast, increasing the binding constant of the end-group results in electrospun fibres being produced. The properties of the fibres produced are subject to changes in solvent, concentration and temperature. Typical diameters for these fibres were found to be some 10 s of μm, rather than the sub-micron dimensions often produced in electrospinning systems. Such diameters are related to the high initial concentrations required; this also may influence the rate of solvent removal and preferential surface solidification which feature in these examples. A simple theoretical model is used to relate the association constant to the molecular weight required for fibre formation; significantly lower levels of association are required for higher molecular weight macromonomers compared to smaller molecular systems.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Characterization of neural and hemodynamic biomarkers of epileptic activity that can be measured using noninvasive techniques is fundamental to the accurate identification of the epileptogenic zone (EZ) in the clinical setting. Recently, oscillations at gamma-band frequencies and above (N30 Hz) have been suggested to provide valuable localizing information of the EZ and track cortical activation associated with epileptogenic processes. Although a tight coupling between gamma-band activity and hemodynamic-based signals has been consistently demonstrated in non-pathological conditions, very little is known about whether such a relationship is maintained in epilepsy and the laminar etiology of these signals. Confirmation of this relationship may elucidate the underpinnings of perfusion-based signals in epilepsy and the potential value of localizing the EZ using hemodynamic correlates of pathological rhythms. Here, we use concurrent multi-depth electrophysiology and 2- dimensional optical imaging spectroscopy to examine the coupling between multi-band neural activity and cerebral blood volume (CBV) during recurrent acute focal neocortical seizures in the urethane-anesthetized rat. We show a powerful correlation between gamma-band power (25–90 Hz) and CBV across cortical laminae, in particular layer 5, and a close association between gamma measures and multi-unit activity (MUA). Our findings provide insights into the laminar electrophysiological basis of perfusion-based imaging signals in the epileptic state and may have implications for further research using non-invasive multi-modal techniques to localize epileptogenic tissue

Relevância:

10.00% 10.00%

Publicador:

Resumo:

High explosives are highly sensitive to accidental detonation by impact, fire, shrapnel and small arms fire. This sensitivity can be reduced by storing the energetic material within a rubbery polymer matrix and are known as plastic bonded explosives (PBX). The current procedure used to manufacture PBX involves mixing the energetic material with a hydroxy-functionalised aliphatic polymer. Upon the addition of an isocyanate crosslinker an immediate polymerisation occurs and thus the rapidly curing mixture must be used to fill the missile or shells, referred to as ‘stores’. This process can lead to poor distribution of the crosslinker resulting in the formation of an inhomogeneously crosslinked matrix and the formation of voids. One solution to this problem involves containing the crosslinker within polyurethane microcapsules that are uniformly dispersed in the explosive-polymer mixture. Upon the application of a stimulus the crosslinker can be released from the microcapsules and the formation of a uniformly crosslinked PBX achieved. Herein is reported the design and synthesis of polyurethane microcapsules that release isocyanate crosslinkers when desired using a thermal stimulus. This has been achieved by exploiting the thermally-reversible nature of oxime-urethane and Diels-Alder adducts that have been incorporated into the shell wall of the microcapsules. An alternative approach to controlling the polymerisation of PBX materials has also been achieved using thermally-reversible blocked isocyanates that regenerate the isocyanate crosslinker when exposed to heat.