Relevância:

100.00% 100.00%

Publicador:

Resumo:

Natural rubber, styrene-butadiene rubber, and polybutadiene rubber were used to replace part of the butadieneacrylonitrile rubber in a 70/30 butadiene-acrylonitrile rubber/ poly(vinyl chloride) blend. Such replacement up to 15% of the total weight of the blend improved the mechanical properties, while decreasing the cost of the blend. Styrenebutadiene rubber could replace butadiene-acrylonitrile rubber up to 30% of the total weight of the blend without deterioration in the mechanical properties.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Sensitisation of natural rubber latex by addition of a small quantity of an anionic surfactant prior to the addition of a coacervant results in quick coagulation. The natural rubber prepared by the novel coagulation method shows improved raw rubber characteristics, better cure characteristics in gum and carbon black filled compounds and improved mechanical properties as compared to the conventionally coagulated natural rubber. Compounds based on dried masterbatches prepared by the incorporation of fluffy carbon black in different forms of soap sensitised natural rubber latices such as fresh latex, preserved field latex, centrifuged latex and a blend of preserved field latex and skim latex show improved cure characteristics and vucanizate properties as compared to an equivalent conventional dry rubber-fluffy carbon black based compound. The latex masterbatch based vulcanizates show higher level of crosslinking and better dispersion of filler. Vulcanizates based on fresh natural rubber latex- dual filler masterbatches containing a blend of carbon black and silica prepared by the modified coagulation process shows very good mechanical and dynamic properties that could be correlated to a low rolling resistance. The carbon black/silica/nanoclay tri-filler - fresh natural rubber latex masterbatch based vulcanizates show improved mechanical properties as the proportion of nanoclay increased up to 5 phr. The fresh natural rubber latex based carbon black-silica masterbatch/ polybutadiene blend vulcanizates show superior mechanical and dynamic properties as compared to the equivalent compound vulcanizates prepared from the dry natural rubber-filler (conventional dry mix)/polybutadiene blends

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Zinc butyl xanthate [Zn(bxt)2] was prepared in the laboratory . The effect of this xanthate with zinc diethyl dithiocarbamate (ZDC) on the vulcanization of natural rubber ( NR), polybutadiene rubber (BR), and NR/BR blend has been studied at different temperatures. The amounts of Zn (bxt)2 and ZDC in the compounds were optimized by varying the amount of ZDC from 0 . 75 to 1.5 phr and Zn (bxt)2 from 0 . 75 to 1 .5 phr. The cure characteristics were also studied . HAF filled NR, BR, and NR / BR blend compounds were cured at different temperatures from 60 to 150 C. The sheets were molded and properties such as tensile strength, tear strength, crosslink density and elongation at break, compression set, abrasion resistance, etc. were evaluated. The results show that the mechanical properties of 80NR/20BR blends are closer to that of NR vulcanizates, properties of 60NR/40BR blends are closer to BR vulcanizates, while the 70NR/30BR blends show an intermediate property.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Polymer-solvent interaction parameters for the blends of natural rubber (NR) with styrene-butadiene rubber (SBR) and polybutadiene rubber ( BR) are calculated using the Flory-Rehner equation by equating the network density of the vulcanizates in two solvents.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Blends of natural rubber (NR) with styrene-butadiene rubber (SBR), polybutadiene rubber (BR), ethylene-propylene terpolymer (EPDM) and acrylonitrile-butadiene rubber (NBR) were vulcanised using an efficient vulcanisation (EV) system and a semi-EV system. Compatible blends show a definite pattern of curing whereas the incompatible blends show no such pattern.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A carbon black filled 50/50 Natural Rubber (NR)/Polybutadiene Rubber (BR) blend is vulcanized using several conventional systems designed by varying the amounts of sulphur and accelerator . The cure characteristics and the vulcanizate properties are compared. The quality and quantity of crosslinks in each case are deciphered by chemical probes to correlate them with the vulcanizate properties.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The primary aim of this work has been to prepare efficient and cost effective polymer bound antioxidants by direct’ attachment of conventional antioxidants to a modified polymer. Due to the importance and easy availability of natural rubber in Kerala, it is proposed to make use of low molecular weight natural rubber as the polymer substrate for binding the antioxidant in most cases. The molecular weight of such low molecular weight natural rubber can be easily manipulated by varying the time of mastication, UV—irradiation etc. Further, the bound antioxidant may also get vulcanized during the vulcanization of the elastomer to which it is added, making the antioxidant non—volatile and non extractable. Several methods are proposed to be investigated for attaching the antioxidant to the low molecular weight natural rubber such as modified Friedel-Craft's alkylation reaction, binding during UV—irradiation, binding during aggressive mastication etc. The efficiency of such rubber bound antioxidants is proposed to be compared with that of conventional antioxidants in terms of volatility, extractability in solvents, ageing resistance etc. Naturally occuring antioxidants such as cardanol, are also proposed to be modified by binding them to low molecular weight natural rubber. The study is undertaken with the intention of generating a class of bound antioxidants which can be used in elastomers for aggressive and long term application.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

There are a large number of commercial examples and property advantages of immiscible elastomer blends.73 Blends of natural rubber (NR) and polybutadiene (BR) have shown various advantages including heat stability, improved elasticity and abrasion resistance. Ethylene-propylene-diene-rubber (EPDM) blended with styrene-butadiene rubber (SBR) has shown improvements in ozone and chemical resistance with better compression set properties. Blends of EPDM and nitrile rubber (NBR) have been cited as a compromise for obtaining moderate oil and ozone resistance with improved low temperature properties. Neoprene (CR)/BR blends offer improved low temperature properties and abrasion resistance with better processing characteristics etc. However, in many of the commercial two-phase elastomer blends, segregation of the crosslinking agents, carbon black or antioxidants preferentially into one phase can result in failure to attain optimum properties. Soluble and insoluble compounding ingredients are found to be preferentially concentrated in one phase. The balance of optimum curing of both phases therefore presents a difficult problem. It has been the aim of this study to improve the performance of commercially important elastomer blends such as natural rubber (NR)/styrene-butadiene rubber (SBR) and natural rubber/polybutadiene rubber (BR) by industrially viable procedures

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Microcellular (MC) soles based on polybutadiene (BR) and low-density polyethylene (LDPE) blends for low-temperature applications were developed. A part of BR in BR-LDPE blend was replaced by natural rubber (NR) for property improvement. The BR-NR-LDPE blend-based MC sole shows good technical properties. Sulphur curing and DCP curing were tried in BR-LDPE and NR-BR-LDPE blends. Study shows that sulphur-cured MC sheets possess better technical properties than DCPcured MC sheets. 90/10 BR-LDPE and 60/30/10 BR-NR-LDPE blend combinations are found to be suitable for low-temperature applications.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The research work has been in the area of compounding and characterization of rubbers for use in under water electro acoustic transducers. The study also covers specific material system such as encapsulation materials, baffle material, seal material, etc. Life prediction techniques of under water rubbers in general have been established with reference to more than one functional property. Ranges of passive materials, besides the active sensing material go into the construction of underwater electro acoustic transducers. Reliability of the transducer is critically dependent on these passive materials. Rubbers are a major class of passive materials. The present work concentrates on these materials. Conventional rubbers are inadequate to meet many of the stringent function specific requirements. There exists a large gap of information in the rubber technology of underwater rubbers, particularly relating to underwater electro acoustic transducers. This study is towards filling up the gaps of information in this crucial area. Water intake into rubber is considered as the single most important issue for the long-term performance of rubbers, especially Neoprene. In this study, the cause and effects of a range of parameters affecting the water absorption by diffusion and permeation have been investigated.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The present work is to impart radiopacity in various natural polymers like chitosan, natural rubber and derivatives of chitosan and to characterize it. This thesis collated the radiopaque properties of these radiopaque polymers and various technological applications in the medical field. The applications of radiopaque polymers leads to an exploitation of radiopaque properties like X-ray visibility, optical density, effective atomic number, attenuation coefficient of biopolymers like chitosan, chitosan formate, chitosan acetate, carboxy methyl chitosan and natural rubber. The radiopaqe properties of these materials highly depend upon the size, shape, amount of radiopacifier and crystallinity of the radiopaque material. Radiopaque chitosan microspheres were prepared by cross linking with glutaraldehyde followed by the encapsulation of barium sulpahte. The effect of different emulsion systems on the morphology of chitosan microspheres were studied. The study concentrates radiopaque natural rubber for shielding applications. It reveals that to improve the particle size, morphology and crystalline phase of the zinc oxide particles, a novel method for the preparation of zinc oxide is adopted. A detailed radiopacity study was done in natural rubber containing 100phr precipitated zinc oxide prepared from different zinc salts. One of the significant findings of this investigation is that NR vulcanizates containing precipitated zinc oxide (from zinc acetate) shows higher attenuation coefficient. These interesting findings reveal the applications of these natural radiopaque systems in various fields like surgical tools, medical tubings, catheters, radiation shielding,etc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this article, we report the preparation of conducting natural rubber (NR) with polyaniline (Pani). NR was made into a conductive material by the compounding of NR with Pani in powder form. NR latex was made into a conductive material by the in situ polymerization of aniline in the presence of NR latex. Different compositions of Pani- NR semi-interpenetrating networks were prepared, and the dielectric properties of all of the samples were determined in microwave frequencies. The cavity perturbation techpique was used for this study. A HP8510 vector network analyzer with a rectangular cavity resonator was used for this study. S bands 2-4 GHz in frequency were used. Thermal studies were also carried out with thermogravimetric analysis and differential scanning calorimetry.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this article, we report the preparation of conducting natural rubber (NR) with polyaniline (Pani). NR was made into a conductive material by the compounding of NR with Pani in powder form. NR latex was made into a conductive material by the in situ polymerization of aniline in the presence of NR latex. Different compositions of Pani- NR semi-interpenetrating networks were prepared, and the dielectric properties of all of the samples were determined in microwave frequencies. The cavity perturbation techpique was used for this study. A HP8510 vector network analyzer with a rectangular cavity resonator was used for this study. S bands 2-4 GHz in frequency were used. Thermal studies were also carried out with thermogravimetric analysis and differential scanning calorimetry.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Prevulcanized natural rubber latex was prepared by the heating of the latex compound at 55°C for different periods of time (2, 4, 6, 8, and 10 h). The changes in the colloidal stability and physical properties were evaluated during the course of prevulcanization. The prevulcanized latex compounds were stored for 300 days, and the properties were monitored at different storage intervals (0, 20, 40, 60, 120, 180, 240, and 300 days). During prevulcanization, the mechanical stability time increased, and the viscosity remained almost constant. The tensile strength increased during storage for a period of 20 days. The degree of crosslinking, modulus, elongation at break, and chloroform number were varied with the time of storage.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A novel method of blending natural rubber with polyvinylchloride in the latex stage was developed, Dioctyl phthalate (DOP) and Amine terminated natural rubber (ATNR) were used as plasticisers, for improving the mechanical properties of these blends. Properties of the latex stage blends were compared with those of dry blends. Latex stage blends showed superior mechanical properties compared to the blends prepared in the dry state. The ageing resistance, oil resistance and processability were found to be improved by latex stage blending.