Resumo:
ABSTRACT: Nylon tire cord (1680/2) was dipped in different adhesives based on resorcinol formaldehyde resin and latex (RFL) and was bonded to natural rubber-based compounds. The resin-rubber ratio in the RFL adhesive was optimized. The variation of pull-through load was studied by varying the drying and curing temperature of the dipped nylon tire cord. RFL adhesive based on vinylpyridine latex was found to have better rubber-to-nylon tire cord bonding, compared with the one based on natural rubber latex. Addition of a formaldehyde donor into the RFL adhesive/rubber compound improves adhesion.
Resumo:
Blends of styrene butadiene rubber (SBR) with maleic anhydride grafted whole tire reclaim (MA-g-WTR) have been prepared and the cure and mechanical properties have been studied with respect to the reclaim content. The grafting was carried out in the presence of dicumylperoxide (DCP) in a Brabender Plasticorder at 150'C. The presence of anhydride group on the WTR was confirmed by infrared spectrometry (IR) study. The properties were compared with those of the blends containing unmodified WTR. Though the cure time was marginally higher, the mechanical properties of the blends containing grafted WTR were better than that of the unmodified blends.
Resumo:
Chloroprene rubber was blended with whole tire reclaimed rubber (WTR) in presence of different levels of a coupling agent Si69 [bis- (3-(triethoxysilyl)propy1)tetrasuIfide] and the cure characteristics and mechanical properties were studied. The rate and state of cure were also affected by the coupling agent. While the cure time was increased, the cure rate and scorch time were decreased with increasing silane content. Tensile strength, tear strength, and abrasion resistance were improved in the presence of coupling agent. Compression set and resilience were adversely affected in presence of silane-coupling agent.Aging studies showed that the blends containing the coupling agent were inferior to the unmodified blends.
Resumo:
The primary objective of this investigation has been to develop more efficient and low cost adhesives for bonding various elastomer combinations particularly NR to NR, NR/PB to NR/PB, CR to CR,NR to CR and NR to NBR.A significant achievement of the investigation was the development of solventless and environment friendly solid adhesives for NR to NR and NR/PB to NR/PB particularly for precured retreading. Conventionally used adhesives in this area are mostly NR based adhesive strips in the presence of a dough. The study has shown that an ultra accelerator could be added to the dough just before applying it on the tire which can significantly bring down the retreading time resulting in prolonged tire service and lower energy consumption. Further latex reclaim has been used for the preparation of the solid strip which can reduce the cost considerably.Another significant finding was that by making proper selection of the RF resin, the efficiency and shelflife of the RFL adhesive used for nylon and rayon tire cord dipping can be improved. In the conventionally used RFL adhesive, the resin once prepared has to be added to the latex within 30 minutes and the RFL has to be used after 4 hours maturation time maximum shelf life of the RFL dip solution being 72 hours. In this study a formaldehyde deficient resin was used and hence more flexibility was available for mixing with latex and maturing. It also has a much longer shelf life. In the method suggested in this study, formaldehyde donors were added only in the rubber compound to make up the formaldehyde deficiency in the RFL. The results of this investigation show that the pull through load by employing this method and the conventional method are comparable. This study has also shown that the amount of RF resin with RFL adhesive can be partially replaced by other modifying agents for cost reduction.Cashew nut shell liquid (CNSL) resin can be employed for improving the bonding of dipped nylon and rayon cord with NR.Since CNSL resin cannot be added in the dip solution since it is not soluble in water, it was added in the rubber compound. The amount of wood rosin in the rubber compound can be reduced by using CNSL resin.Another interesting result of the investigation was the use of CR based adhesive modified with chlorinated natural rubber for CR to CR bonding. Addition of chlorinated natural rubber was found to improve sea water resistance of CR based adhesive. In the bonding of a polar rubber like nitrile rubber or polychloroprene rubber to a non polar rubber like natural rubber, an adhesive based on polychloroprene rubber was found to be effective.
Resumo:
The research work has been in the area of compounding and characterization of rubbers for use in under water electro acoustic transducers. The study also covers specific material system such as encapsulation materials, baffle material, seal material, etc. Life prediction techniques of under water rubbers in general have been established with reference to more than one functional property. Ranges of passive materials, besides the active sensing material go into the construction of underwater electro acoustic transducers. Reliability of the transducer is critically dependent on these passive materials. Rubbers are a major class of passive materials. The present work concentrates on these materials. Conventional rubbers are inadequate to meet many of the stringent function specific requirements. There exists a large gap of information in the rubber technology of underwater rubbers, particularly relating to underwater electro acoustic transducers. This study is towards filling up the gaps of information in this crucial area. Water intake into rubber is considered as the single most important issue for the long-term performance of rubbers, especially Neoprene. In this study, the cause and effects of a range of parameters affecting the water absorption by diffusion and permeation have been investigated.
Resumo:
The present work is to impart radiopacity in various natural polymers like chitosan, natural rubber and derivatives of chitosan and to characterize it. This thesis collated the radiopaque properties of these radiopaque polymers and various technological applications in the medical field. The applications of radiopaque polymers leads to an exploitation of radiopaque properties like X-ray visibility, optical density, effective atomic number, attenuation coefficient of biopolymers like chitosan, chitosan formate, chitosan acetate, carboxy methyl chitosan and natural rubber. The radiopaqe properties of these materials highly depend upon the size, shape, amount of radiopacifier and crystallinity of the radiopaque material. Radiopaque chitosan microspheres were prepared by cross linking with glutaraldehyde followed by the encapsulation of barium sulpahte. The effect of different emulsion systems on the morphology of chitosan microspheres were studied. The study concentrates radiopaque natural rubber for shielding applications. It reveals that to improve the particle size, morphology and crystalline phase of the zinc oxide particles, a novel method for the preparation of zinc oxide is adopted. A detailed radiopacity study was done in natural rubber containing 100phr precipitated zinc oxide prepared from different zinc salts. One of the significant findings of this investigation is that NR vulcanizates containing precipitated zinc oxide (from zinc acetate) shows higher attenuation coefficient. These interesting findings reveal the applications of these natural radiopaque systems in various fields like surgical tools, medical tubings, catheters, radiation shielding,etc.
Resumo:
In this article, we report the preparation of conducting natural rubber (NR) with polyaniline (Pani). NR was made into a conductive material by the compounding of NR with Pani in powder form. NR latex was made into a conductive material by the in situ polymerization of aniline in the presence of NR latex. Different compositions of Pani- NR semi-interpenetrating networks were prepared, and the dielectric properties of all of the samples were determined in microwave frequencies. The cavity perturbation techpique was used for this study. A HP8510 vector network analyzer with a rectangular cavity resonator was used for this study. S bands 2-4 GHz in frequency were used. Thermal studies were also carried out with thermogravimetric analysis and differential scanning calorimetry.
Resumo:
In this article, we report the preparation of conducting natural rubber (NR) with polyaniline (Pani). NR was made into a conductive material by the compounding of NR with Pani in powder form. NR latex was made into a conductive material by the in situ polymerization of aniline in the presence of NR latex. Different compositions of Pani- NR semi-interpenetrating networks were prepared, and the dielectric properties of all of the samples were determined in microwave frequencies. The cavity perturbation techpique was used for this study. A HP8510 vector network analyzer with a rectangular cavity resonator was used for this study. S bands 2-4 GHz in frequency were used. Thermal studies were also carried out with thermogravimetric analysis and differential scanning calorimetry.
Resumo:
Prevulcanized natural rubber latex was prepared by the heating of the latex compound at 55°C for different periods of time (2, 4, 6, 8, and 10 h). The changes in the colloidal stability and physical properties were evaluated during the course of prevulcanization. The prevulcanized latex compounds were stored for 300 days, and the properties were monitored at different storage intervals (0, 20, 40, 60, 120, 180, 240, and 300 days). During prevulcanization, the mechanical stability time increased, and the viscosity remained almost constant. The tensile strength increased during storage for a period of 20 days. The degree of crosslinking, modulus, elongation at break, and chloroform number were varied with the time of storage.
Resumo:
A novel method of blending natural rubber with polyvinylchloride in the latex stage was developed, Dioctyl phthalate (DOP) and Amine terminated natural rubber (ATNR) were used as plasticisers, for improving the mechanical properties of these blends. Properties of the latex stage blends were compared with those of dry blends. Latex stage blends showed superior mechanical properties compared to the blends prepared in the dry state. The ageing resistance, oil resistance and processability were found to be improved by latex stage blending.
Resumo:
Natural rubber/isora fibre composites were cured at various temperatures. The solvent swelling characteristics of natural rubber composites containing both untreated and alkali treated fibres were investigated in aromatic and aliphatic solvents like toluene, and n-hexane. The diffusion experiments were conducted by the sorption gravimetric method. The restrictions on elastomer swelling exerted by isora fibre as well as the anisotropy of swelling of the composite have been confirmed by this study. Composite cured at 100°C shows the lowest percentage swelling. The uptake of aromatic solvent is higher than that of aliphatic solvent for the composites cured at all temperatures. The effect of fibre loading on the swelling behaviour of the composite was also investigated in oils like petrol, diesel, lubricating oil etc. The % swelling index and swelling coefficient of the composite were found to decrease with increase in fibre loading. This is due to the increased hindrance exerted by the fibres at higher fibre loadings and also due to the good fibre-rubber interactions. Maximum uptake of solvent was observed with petrol followed by diesel and then lubricating oil. The presence of bonding agent in the composites restrict the swelling considerably due to the strong interfacial adhesion. At a fixed fibre loading, the alkali treated fibre composite showed lower percentage swelling compared to the untreated one.
Resumo:
A series of short-isora-fiber-reinforced natural rubber composites were prepared by the incorporation of fibers of different lengths (6, 10, and 14 mm) at 15 phr loading and at different concentrations (10, 20, 30, and 40 phr) with a 10 mm fiber length. Mixes were also prepared with 10 mm long fibers treated with a 5% NaOH solution. The vulcanization parameters, processability, and stress-strain properties of these composites were analyzed. Properties such as tensile strength, tear strength, and tensile modulus were found to be at maximum for composites containing longitudinally oriented fibers 10 mm in length. Mixes containing fiber loadings of 30 phr with bonding agent (resorcinol-formaldehyde [RF] resin) showed mechanical properties superior to all other composites. Scanning electron microscopy (SEM) studies were carried out to investigate the fiber surface morphology, fiber pullout, and fiber-rubber interface. SEM studies showed that the bonding between the fiber and rubber was improved with treated fibers and with the use of bonding agent.
Resumo:
Polymers exhibit low electron density and they are radiolucent. Polymers can be made radiopaque by different techniques. We report a method for the preparation of radiopaque material from natural rubber (NR). NR in its latex form was iodinated. Iodinated natural rubber (INR) was characterized by using UV, thermo gravimetric analysis (TGA), and X-ray images. INR was compounded at high and low temperatures and its physical properties were measured. The low temperature cured samples show good radiopacity and conductivity. The optical density of low temperature cured samples was measured.
Resumo:
The mechanism of devulcanization of sulfur-vulcanized natural rubber with aromatic disulfides and aliphatic amines has been studied using 23-dimethyl-2-butene (C5H1,) as a low-molecular weight model compound. First C6H12 was vulcanized with a mixture of sulfur, zinc stearate and N-cyclohexyl-2-benzothiazylsulfenamide (CBS) as accelerator at 140 °C, resulting in a mixture of addition products (C(,H 1 i-S,-C5H 1 i ). The compounds were isolated and identified by High Performance Liquid Chromatography (HPLC) with respect to their various sulfur ranks. In it second stage, the vulcanized products were devulcanized using the agents mentioned above at 200 °C. The kinetics and chemistry of the breakdown of the sulfur-hridges were monitored. Both devulcanization agents decompose sulfidic vulcanization products with sulfur ranks equal or higher than 3 quite effectively and with comparable speed. Di phenyldisulfide as devulcanization agent gives rise to a high amount of mono- and disulfidic compounds formed during the devulcanization, hexadecylamine, as devulcanization agent, prevents these lower sulfur ranks from being formed.
Resumo:
It is observed that reclamation of natural rubber latex based rubber using 2,2'-dibenzamidodiphenvldisulphide as reclaiming agent is an optional methodology for recycling of waste latex rubber (WLR). For progressive replacement of virgin natural rubber by the reclaim, two alternatives curing system were investigated: adjustment or reduction of the curing system with increasing reclaim content, to compensate for the extra amount of curatives brought along by the reclaim. For fixed curing system, as if the reclaim were equivalent to virgin NR. The cure behavior, final crosslink density and distribution, mechanical properties, and dynamic viscoelastic properties of the blends with reclaimed WLR are measured and compared with the virgin compound. The morphology of the blends, sulfur migration, and final distribution are analyzed.The mechanical and dynamic viscoelastic properties deteriorate for both curing systems, but to a lesser extent for fixed curing system compared to adjusted curing system. With the fixed cure system, many properties like tensile strength and compression set do still deteriorate, but tan 6 and Mrrr„/Murxr, representative for the rolling resistance of tires are improved. On the other hand, with the adjusted cure system both mechanical and dynamic properties still deteriorate.