ABSTRACT: Nylon tire cord (1680/2) was dipped in different adhesives based on resorcinol formaldehyde resin and latex (RFL) and was bonded to natural rubber-based compounds. The resin-rubber ratio in the RFL adhesive was optimized. The variation of pull-through load was studied by varying the drying and curing temperature of the dipped nylon tire cord. RFL adhesive based on vinylpyridine latex was found to have better rubber-to-nylon tire cord bonding, compared with the one based on natural rubber latex. Addition of a formaldehyde donor into the RFL adhesive/rubber compound improves adhesion.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Blends of styrene butadiene rubber (SBR) with maleic anhydride grafted whole tire reclaim (MA-g-WTR) have been prepared and the cure and mechanical properties have been studied with respect to the reclaim content. The grafting was carried out in the presence of dicumylperoxide (DCP) in a Brabender Plasticorder at 150'C. The presence of anhydride group on the WTR was confirmed by infrared spectrometry (IR) study. The properties were compared with those of the blends containing unmodified WTR. Though the cure time was marginally higher, the mechanical properties of the blends containing grafted WTR were better than that of the unmodified blends.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Chloroprene rubber was blended with whole tire reclaimed rubber (WTR) in presence of different levels of a coupling agent Si69 [bis- (3-(triethoxysilyl)propy1)tetrasuIfide] and the cure characteristics and mechanical properties were studied. The rate and state of cure were also affected by the coupling agent. While the cure time was increased, the cure rate and scorch time were decreased with increasing silane content. Tensile strength, tear strength, and abrasion resistance were improved in the presence of coupling agent. Compression set and resilience were adversely affected in presence of silane-coupling agent.Aging studies showed that the blends containing the coupling agent were inferior to the unmodified blends.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The primary objective of this investigation has been to develop more efficient and low cost adhesives for bonding various elastomer combinations particularly NR to NR, NR/PB to NR/PB, CR to CR,NR to CR and NR to NBR.A significant achievement of the investigation was the development of solventless and environment friendly solid adhesives for NR to NR and NR/PB to NR/PB particularly for precured retreading. Conventionally used adhesives in this area are mostly NR based adhesive strips in the presence of a dough. The study has shown that an ultra accelerator could be added to the dough just before applying it on the tire which can significantly bring down the retreading time resulting in prolonged tire service and lower energy consumption. Further latex reclaim has been used for the preparation of the solid strip which can reduce the cost considerably.Another significant finding was that by making proper selection of the RF resin, the efficiency and shelflife of the RFL adhesive used for nylon and rayon tire cord dipping can be improved. In the conventionally used RFL adhesive, the resin once prepared has to be added to the latex within 30 minutes and the RFL has to be used after 4 hours maturation time maximum shelf life of the RFL dip solution being 72 hours. In this study a formaldehyde deficient resin was used and hence more flexibility was available for mixing with latex and maturing. It also has a much longer shelf life. In the method suggested in this study, formaldehyde donors were added only in the rubber compound to make up the formaldehyde deficiency in the RFL. The results of this investigation show that the pull through load by employing this method and the conventional method are comparable. This study has also shown that the amount of RF resin with RFL adhesive can be partially replaced by other modifying agents for cost reduction.Cashew nut shell liquid (CNSL) resin can be employed for improving the bonding of dipped nylon and rayon cord with NR.Since CNSL resin cannot be added in the dip solution since it is not soluble in water, it was added in the rubber compound. The amount of wood rosin in the rubber compound can be reduced by using CNSL resin.Another interesting result of the investigation was the use of CR based adhesive modified with chlorinated natural rubber for CR to CR bonding. Addition of chlorinated natural rubber was found to improve sea water resistance of CR based adhesive. In the bonding of a polar rubber like nitrile rubber or polychloroprene rubber to a non polar rubber like natural rubber, an adhesive based on polychloroprene rubber was found to be effective.