44 resultados para Styrene
em Cochin University of Science
Resumo:
Natural rubber, styrene-butadiene rubber, and polybutadiene rubber were used to replace part of the butadieneacrylonitrile rubber in a 70/30 butadiene-acrylonitrile rubber/ poly(vinyl chloride) blend. Such replacement up to 15% of the total weight of the blend improved the mechanical properties, while decreasing the cost of the blend. Styrenebutadiene rubber could replace butadiene-acrylonitrile rubber up to 30% of the total weight of the blend without deterioration in the mechanical properties.
Resumo:
A carbon black filled 50/50 natural rubber (NR)/styrene-butadiene rubber (SBR) blend is vulcanized using several conventional curing systems designed by varying the amounts of sulphur and accelerator. The cure characteristics and the properties of the vulcanizates are compared. The quantity and quality of crosslinks in each case are evaluated by chemical probes to correlate them with the properties.
Resumo:
Waste latex products are converted to a processabto material by a novel economical process developed in our laboratory , It contains rubber hydrocarbon of very high quality and Is lightly cross -linked. Styrene-butadlene rubber is mixed with latex reclaim In different proportions . The mechanical properties are found to be improved up to 60 percent replacement of styrene-butadlene rubber by latex reclaim . The curing of styrene-butadiene rubber Is found to be accelerated by the addition of latex reclaim. The processablllty study shows that the blends can be processed similar to SBRINR blends.
Resumo:
Gum and filled compounds of styrene-butadiene rubber are extruded through a laboratory extruder by varying the feeding rase at different temperatures and screw speed (rpm). The extruded compounds are vulcanized up4o their optimum cure times and the mechanical properties of the vulcanizates are determined. From the properties data obtained it Is concluded that there is a specific feeding rate wit in the starved fed region, which results In maximum Improved mechanical properties . The enhancement In properties is found to be due to better thermal and shear homogeneity.
Resumo:
Blends of styrene butadiene rubber (SBR) with maleic anhydride grafted whole tire reclaim (MA-g-WTR) have been prepared and the cure and mechanical properties have been studied with respect to the reclaim content. The grafting was carried out in the presence of dicumylperoxide (DCP) in a Brabender Plasticorder at 150'C. The presence of anhydride group on the WTR was confirmed by infrared spectrometry (IR) study. The properties were compared with those of the blends containing unmodified WTR. Though the cure time was marginally higher, the mechanical properties of the blends containing grafted WTR were better than that of the unmodified blends.
Resumo:
The rheological characteristics of short Nylon-6 fiber-reinforced Styrene Butadiene rubber (SBR) in the presence of epoxy resin-based bonding agent were studied with respect to the effect of shear rate, fiber concentration , and temperature on shear viscosity and die swell using a capillary rheonzeter. All the composites containing bonding agent showed a pseudoplastic nature, which decreased with increasing temperature. Shear viscosity was increased in the presence of fibers. The temperature sensitivity of the SBR matrices was reduced on introduction of fibers. The temperature sensitivity of the melts was found to be lower at higher shear rates. Die swell was reduced in the presence of fibers. Relative viscosity of the composites increased with shear rate. In the presence of epoxy resin bonding agent the temperature sensitivity of the mixes increased. Die swell was larger in the presence of bonding agent.
Resumo:
The rheological characteristics of short Nylon-6 fiber reinforced styrene butadiene rubber (SBR) were studied using a capillary rheometer. The study was done with respect to the effect of shear rate, fiber concentration, and temperature on shear viscosity and die swell. All the melts showed pseudoplastic nature, which decreased with increasing temperature. Shear viscosity increased in the presence of fibers. Introduction of fiber reduces the temperature sensitivity of the rubber matrix. A reduction in die swell was found in presence of fibers.
Resumo:
The thermal properties of short Nylon-6 fiber-reinforced Styrene butadiene rubber (SBR) composites were studied by Thermogravimetric Analysis (TGA). The effect of epoxy-based bonding agent on thermal degradation of the gum and the composites was also studied. The thermal stability of the SBR was enhanced in the presence of Nylon-6 fibers and the stability of the composites increased in the presence of bonding agent. The epoxy resin did not significantly change the thermal stability of SBR gum vulcanizate. Results of kinetic studies showed that the degradation of SBR and the short nylon fiber-reinforced composites with and without bonding agents followed first-order kinetics.
Resumo:
The cure characteristics and mechanical properties of short nylon fiber- styrene /whole tyre reclaim (SBR/WTR) composites with and without an interfacial bonding agent based on 4,4 diphenyl methane diisocyanate and polyethylene glycol (MDI/PEG) have been studied. An 80:40 blend of SBR/ WTR reinforced with 20 phr of short nylon fiber has been selected and the MDI/ PEG ratio has been changed from 0.67:1 to 2:1. The minimum and maximum torques increased with isocyanate concentration. The scorch time and cure time showed an initial reduction. The cure rate showed an initial improvement. Tensile strength, tear strength and abrasion resistance increased with MDI/PEG ratio, these values were higher in longitudinal direction. Resilience and compression set increased with isocyanate concentration.
Resumo:
Cure characteristics and mechanical properties of styrene butadiene rubber reclaimed rubber blends were studied. The blends showed improved processability, as indicated by the minimum torque values. Cure characteristics like minimum torque, (maximum-minimum) torque, cure time and cure rate decreased in the presence of reclaimed rubber. Tensile strength, tear strength, elongation at break were higher for blends. Resilience decreased with reclaim content. Compression set and abrasion loss were higher in the blends.
Resumo:
We describe the synthesis of diblock and triblock copolymers by sequential atom transfer radical polymerization of styrene and acetoxymethylstyrene. Contrary to the usual block copolymerization involving isolation of the macroinitiator, a convenient one-pot procedure is developed. This is possible because of the preferential polymerization of acetoxymethylstyrene, even in the presence of residual styrene, as inferred from characterization of the intermediate polystyrenes and the block copolymers by size exclusion chromatography, 1H NMR, Fourier transform infrared spectroscopy, differential scanning calorimetry, and GPEC techniques. The latent acetoxy functionalities in these block copolymers are shown to be easily unmasked to OOH and OBr functionalities, with the potential for block ionomers and dense graft architectures.
Resumo:
Vibrational overtone spectra of styrene (liquid) and polystyrene (solid), studied by the laser-induced thermal lens (for ΔV=6) and the conventional near infrared absorption (for ΔV=3–5) techniques, are reported. For polystyrene, the overtone energy-bond length correlation predicts that the aryl CH bonds are ∼0.0005 Å longer than that in benzene, while no such conclusions could be drawn on styrene. Thesp 3 CH overtones in polystyrene are observed on the low energy side of the aryl CH overtones.
Resumo:
Novel thermo-reversible zinc sulphonated ionomers based on styrene butadiene rubber (SBR), and high styrene rubber (HSH) were synthesized by sulphonation followed by neutralization with zinc. The sulphonate content of the ionomer was estimated by using x-ray fluorescence spectroscopy. Presence of sulphonate groups has been confirmed by FTIR and FTNMR spectra. The TGA results show improvement in the thermo~oxidative stability of the modified rubber. Both DSC and DMTA studies show that the incorporation of the ionic groups affect the glass rubber transition of the base polymer. lntroduction ol ionic functionality in to the base material improved the physical properties. Retention of the improved physical properties of the novel ionomers even after three repeated cycles of mixing and molding may be considered as the evidence for the reprocessability of the ionomer. Effect of particulate fillers (HAF black, silica and zinc stearate) on the properties of the zinc sulphonated styrene butadiene rubber ionomer has been evaluated. Incorporation of tillers results in improvement in mechanical properties. Zinc stearate plays the dual role of reinforcement and plasticization. The evaluation of dielectric properties of zinc sulphonated styrene butadiene rubber iorpmers at microwave frequencies reveal that the materials show conductivity at semiconductor level. The real and imaginary parts of the complex permittivity increases with increase in ionic functionality. Use of the 38.5 ZnS-SBR ionomer as a compatibiliser for obtaining the technologically compatible blends from the immiscible SBR/NBR system has been discussed.
Resumo:
Catalysis is an essential technology in manufacturing industries. The investigation based on supported vanadia catalysts and it’s sulfated analogues. Vanadia is a transition metal oxide and is used in oxidation reactions in chemical industry. It is more active and selective catalysts on suitable supports. The work deals with preparation of vanadia incorporated tin oxide and zirconia systems by wet impregnation. Physico-chemical characterization using instrumental techniques like BET etc. The surface acidic properties were determined by the ammonia TPD studies, Perylene absorption studies and Cumene conversion reaction. The catalytic activities of the prepared systems are tested by Friedel-Crafts benzylation of arenes and Bechmann rearrangement of Cyclohexanol oxime. Here the rector reactions are relatively rare. So to test the application of the catalyst systems for the selective oxidation of cyclohexanol to cyclohexanone and finally evaluate the catalytic activity of the systems for the vapour phase oxidative dehydrogenation of Ethylbenzene, which leads to the formation of Industrially important compound ‘styrene’ is another objective of this work