9 resultados para PEG 6000
em Cochin University of Science
Resumo:
Marine fungus BTMFW032, isolated from seawater and identified as Aspergillus awamori, was observed to produce an extracellular lipase, which could reduce 92% fat and oil content in the effluent laden with oil. In this study, medium for lipase production under submerged fermentation was optimized statistically employing response surface method toward maximal enzyme production. Medium with soyabean meal- 0.77% (w/v); (NH4)2SO4-0.1 M; KH2PO4-0.05 M; rice bran oil-2% (v/v); CaCl2-0.05 M; PEG 6000-0.05% (w/v); NaCl-1% (w/v); inoculum-1% (v/v); pH 3.0; incubation temperature 35 8C and incubation period-five days were identified as optimal conditions for maximal lipase production. The time course experiment under optimized condition, after statistical modeling, indicated that enzyme production commenced after 36 hours of incubation and reached a maximum after 96 hours (495.0 U/ml), whereas maximal specific activity of enzyme was recorded at 108 hours (1164.63 U/mg protein). After optimization an overall 4.6- fold increase in lipase production was achieved. Partial purification by (NH4)2SO4 precipitation and ion exchange chromatography resulted in 33.7% final yield. The lipase was noted to have a molecular mass of 90 kDa and optimal activity at pH 7 and 40 8C. Results indicated the scope for potential application of this marine fungal lipase in bioremediation.
Resumo:
The mechanical properties of filled natural rubber latex vulcanizates were found to be improved by the addition of polyethylene glycols of different molecular weight and glycerol. There is a slight reduction in the optimum cure times of the compounds containing PEG/Glycerol. The morphology study shows that the filler distribution is more uniform in the compounds containing PEG/Glycerol.
Resumo:
The effect of diphenylmethane diisocyanate (MDI) -polyethyleneglycol (PEG) resin on the cure characteristics and mechanical properties of nitrile rubber/whole tyre eclaim-short nylon fiber composite-was studied. At a constant loading of 5 phr, the resin composition was varied. The minimum torque .,id (maximum - minimum) torque increased with isocyanate concentration. Scorch time and cure time showed a reduction on introduction of bonding agent. Properties like tensile strength, tear strength, and abrasion resistance increased with increase in MDI/PEG ratio, and these properties are higher in the longitudinal direction of fiber orientation. Compression set increased with isocyanate concentration and the resilience remain unchanged.
Resumo:
The cure characteristics and mechanical properties of short nylon fiber- styrene /whole tyre reclaim (SBR/WTR) composites with and without an interfacial bonding agent based on 4,4 diphenyl methane diisocyanate and polyethylene glycol (MDI/PEG) have been studied. An 80:40 blend of SBR/ WTR reinforced with 20 phr of short nylon fiber has been selected and the MDI/ PEG ratio has been changed from 0.67:1 to 2:1. The minimum and maximum torques increased with isocyanate concentration. The scorch time and cure time showed an initial reduction. The cure rate showed an initial improvement. Tensile strength, tear strength and abrasion resistance increased with MDI/PEG ratio, these values were higher in longitudinal direction. Resilience and compression set increased with isocyanate concentration.
Resumo:
Low-protein content natural rubber latex was produced by using a nonionic surfactant-polyethylene glycol (PEG). Extractable protein content of natural rubber latex was found to decrease with PEG treatment and reduction increased with increase in the molecular weight of PEG. The low-protein latex samples were characterized by tensile testing, Fourier transform infrared and thermogravimetric analysis. The results have shown 35% reduction in the extractable protein content, without any compromise on the mechanical properties of the latex; however, thermal stability of low-protein latex was found to be reduced marginally with PEG treatment.
Resumo:
The thesis deals with the development of short nylon fiber-reclaimed rubber/elastomer composites. Three rubbers viz, natural rubber, acrylonitrile butadiene rubber and styrene butadiene rubber were selected and were partially replaced with reclaimed rubber. The blend ratio was optimized with respect to cure characteristics and mechanical properties. Reclaimed rubber replaced 40 parts of NR and SBR and 20 parts of NBR without much affecting the properties. These blends were then reinforced with short nylon fibers. The mechanical properties of the composites were studied in detail. In all the cases the tensile strength, tear strength and the abrasion resistance increased with increase in fiber content. In the case of NRlreclaimed rubber blends, the tensile strength-fiberloading relationship was non-linear where as in the case of NBRlreclaimed rubber blends and SBRlreclaimed rubber blends the tensile strength-fiber loading relationship was linear. All the composites showed anisotropy in mechanical properties. The effect of bonding system on the composite properties was also studied with respect to cure characteristics and mechanical properties. For this, a 20 phr fiber loaded reclaimed rubber/elastomer composites were selected and the effect of MDI/PEG resin system was studied. The resin used was 5 phr and the resin ratios used were 0.67: I, 1:1, 1.5:1 and 2:1. The bonding system improved the tensile strength, tear strength and abrasion resistance. The best results are with SBRlreclaimed rubber-short nylon fiber composites. The optimized resin ratio was 1:1 MDI/PEG for all the composites.
Resumo:
S. album L. is the source of highly priced and fragrant heartwood which on steam distillation yields on an average 57 per cent oil of high perfumery value. Global demand for sandalwood is about 5000-6000 tons/year and that of oil is 100 tons/year. Heartwood of sandal is estimated to fetch up to Rs. 3.7 million/ton and wood oil Rs.70,000-100,000/ kg in the international market. Sandal heartwood prices have increased from Rs. 365/ton in 1900 to Rs. 6.5 lakhs/ton in 1999-2000 and to Rs. 37 lakhs/ton in 2007. Substantial decline in sandalwood production has occurred from 3176 tons/year during 1960-‘ 65 to 1500 tons/year in 1997-98, and to 500 tons/year in 2007.Depletion of sandal resources is attributed to several factors, both natural and anthropogenic. Low seed setting, poor seed germination, seedling mortality, lack of haustorial connection with host plant roots, recurrent annual fires in natural sandal forests, lopping of trees for fodder, excessive grazing, hacking, encroachments, seedling diseases and spread of sandal spike disease are the major problems facing sandal. While these factors hinder sandal regeneration in forest areas, the situation is accelerated by human activities of chronic overexploitation and illicit felling.Deterioration of natural sandal populations due to illicit felling, encroachments and diseases has an adverse effect on genetic diversity of the species. The loss of genetic diversity has aggravated during recent years due to extensive logging, changing landuse patterns and poor natural regeneration. The consequent genetic erosion is of serious concern affecting tree improvement programme in sandal. Conservation as well as mass propagation are the two strategies to be given due importance. To initiate any conservation programme, precise knowledge of the factors influencing regeneration and survival of the species is essential. Hence, the present study was undertaken with the objective of investigating the autotrophic and parasitic phase of sandal seedlings growth, the effects of shade on morphology, chlorophyll concentration and chlorophyll fluorescence of sandal seedlings, genetic diversity in sandal seed stands using ISSR markers, and the diversity of fungal isolates causing sandal seedling wilt using RAPD markers. All these factors directly influence regeneration and survival of sandal seedlings in natural forests and plantations.
Resumo:
This thesis entitled Physicochemical and molecular characterization of bacteriophages ΦSP-1and ΦSP-3, specific for pathogenic Salmonella and evaluation of their potential as biocontrol agent . Salmonella were screened using standard methodologies from various environmental samples including chicken caecum. Salmonella strains, which were previously isolated and stocked in the lab, were also included in this study as host, for screening Salmonella specific lytic phages. The Salmonella strain in this study designated as S49 which helped in phage propagation by acting as host bacteria was identified as Salmonella enterica subsp. enterica by 16S rRNA gene analysis and serotyping . A total of three Salmonella specific phage named as ΦSP-1, ΦSP-2 and ΦSP-3 were isolated from chicken intestine samples via an enrichment protocol employing the double agar overlay method. ΦSP-1 and ΦSP-3 showing consistent lytic nature were selected for further study and were purified by repeated plating after picking of single isolated plaques from the lawns of Salmonella S49 plates. Both the phages produced small, clear plaques indicating their lytic nature. ΦSP-1 and ΦSP-3 were concentrated employing PEG-NaCl precipitation method before further characterization. The focus of present study was to isolate, characterize and verify the efficacy of lytic bacteriophages against the robust pathogen Salmonella, capable of surviving under various hostile conditions. Two phages, ΦSP-1 and ΦSP-3, belonging to two families, Podovoridae and Siphoviridae were isolated.
Resumo:
Unsaturated polyester resins (UPRs) are extensively used by the fiber-reinforced plastic (FRPs) industry. These resins have the disadvantages of brittleness and poor resistance to crack propagation. In this study, UPRs were chemically modified by reactive blending with polyurethane prepolymers having terminal isocyanate groups. Hybrid networks were formed by copolymerisation of unsaturated polyesters with styrene and simultaneous reaction between terminal hydroxyl groups of unsaturated polyester and isocyanate groups of polyurethane prepolymer. The prepolymers were based on toluene diisocyanate (TDI) and each of hydroxy-terminated natural rubber (HTNR), hydroxy- terminated polybutadiene (HTPB), polyethylene glycol (PEG), and castor oil. Properties like tensile strength, toughness, impact resistance, and elongation-at-break of the modified UPRs show considerable improvement by this modification. The thermal stability of the copolymer is also marginally better