Resumo:
Dielectric resonator ceramics with composition formula Ba[(D3+0.3 Bi0.2)Nb0.5]O3,where D3+=Y,Pr,Sm,Gd,Dy and Er,were prepared by the conventional ceramic preparation route
Resumo:
Microwave ceramic dielectric resonators (DRs) based on RETiNbO6 (RE = Ce, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Y, and Yb) have been prepared using the conventional solid -state ceramic route. The DR samples are characterized using XRD and SEM methods. The microwave dielectric properties are measured using resonant methods and a net work analyzer . The ceramics based on Ce, Pr, Nd, and Sin have dielectric constants in the range 32-54 and positive coefficient of thermal variation of resonant frequency (r,). The ceramics based on Gd, Tb, Dy, Y. and Yb have dielectric constants in the range 19-22 and negative Tf
Resumo:
Microwave dielectric ceramics based on RETiTaO6 (RE = La, Cc, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Y, Er, Yb, Al, and In) were prepared using a conventional solid-state ceramic route. The structure and microstructure of the samples were analyzed using x-ray diffraction and scanning electron microscopy techniques. The sintered samples were characterized in the microwave frequency region. The ceramics based on Ce, Pr, Nd, Sm, Eu, Gd, Tb, and Dy, which crystallize in orthorhombic aeschynite structure, had a relatively high dielectric constant and positive T f while those based on Ho, Er, and Yb, with orthorhombic euxenite structure, had a low dielectric constant and negative Tf. The RETiTaO6 ceramics had a high-quality factor. The dielectric constant and unit cell volume of the ceramics increased with an increase in ionic radius of the rare-earth ions, but density decreased with it. The value of Tf increased with an increase in RE ionic radii, and a change in the sign of Tf occurred when the ionic radius was between 0.90 and 0.92 A. The results indicated that the boundary of the aeschynite to euxenite morphotropic phase change lay between DyTiTaO6 and HoTiTaO6. Low-loss ceramics like ErTiTaO6 (Er = 20.6, Qxf = 85,500), EuTiTaO6 (Er = 41.3, Qxf = 59,500), and YTiTaO6 (Er = 22.1, Q„xf = 51,400) are potential candidates for dielectric resonator applications
Resumo:
Microwave dielectric resonators (DRs) based on Ba(B1,2Nbi/2)03 [B' = La, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Y, Yb, and In] complex perovskites have been prepared by conventional solid state ceramic route. The dielectric properties (relative permittivity, Er; quality factor, Q; and resonant frequency, rr) of the ceramics have been measured in the frequency range 4-6 GHz using resonance methods. The resonators have relatively high dielectric constant in the range 36-45, high quality factor and small temperature variation of resonant frequency. The dielectric properties are found to depend on the tolerance factor (t), ionic radius (r), and lattice parameter (ap)
Resumo:
The method of preparation of ZnS phosphors doped with praseodymium and copper is given. The electroluminescence (EL) spectrum of ZnS:Pr,Cl has two broad bands at 470 and 570 nm. ZnS:Cu,Pr,Cl gives white emission with spectral peaks at 470, 520, 570 and 640 nm. The EL spectra of both types of phosphor exhibit a conspicuous colour shift as the frequency of the excitation voltage is varied. Detailed investigations show that the relative intensities of spectral peaks are strongly dependent on the frequency of the excitation voltage. The colour shift is explained on the basis of the Schon-Klasens model.
Resumo:
Polarized Raman spectral changes with respect to temperature were investigated for Pr(BrO3)3·9H2O single crystals. FTIR spectra of hydrated and deuterated analogues were also recorded and analysed. Temperature dependent Raman spectral variation have been explained with the help of the thermograms recorded for the crystal. Factor group analysis could propose the appearance ofBrO3 ions at sites corresponding to C3v (4) and D3h (2). Analysis of the vibrational bands at room temperature confirms a distorted C3v symmetry for the BrO3 ion in the crystal. From the vibrations of water molecules, hydrogen bonds of varying strengths have also been identified in the crystal. The appearance υ1 mode of BrO3− anion at lower wavenumber region is attributed to the attachment of hydrogen atoms to the BrO3− anion. At high temperatures, structural rearrangement is taking place for bothH2Omolecule and BrO3 ions leading to the loss ofwater molecules and structural reorientation of bromate ions causing phase transition of the crystal at the temperature of 447 K.