23 resultados para Kinetic of cure


Relevância:

40.00% 40.00%

Publicador:

Resumo:

Cure characteristics and mechanical properties of short nylon fiber reinforced acrylonitrile butadiene rubber-reclaimed rubber composites were studied. Minimum torque, (maximum-minimum) torque and cure rate increased with fiber concentration. Scorch time and cure time decreased by the addition of fibers. Properties like tensile strength, tear strength, elongation at break, abrasion loss and heat build up were studied in both orientations of fibers. Tensile and tear properties were enhanced by the addition of fibers and were higher in the longitudinal direction. Heat build up increased with fiber concentration and were higher in the longitudinal direction. Abrasion resistance was improved in presence of short fibers and was higher in the longitudinal direction. Resilience increased on the introduction of fibers. Compression set was higher for blends.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The cure characteristics and mechanical properties of short nylon fiber- styrene /whole tyre reclaim (SBR/WTR) composites with and without an interfacial bonding agent based on 4,4 diphenyl methane diisocyanate and polyethylene glycol (MDI/PEG) have been studied. An 80:40 blend of SBR/ WTR reinforced with 20 phr of short nylon fiber has been selected and the MDI/ PEG ratio has been changed from 0.67:1 to 2:1. The minimum and maximum torques increased with isocyanate concentration. The scorch time and cure time showed an initial reduction. The cure rate showed an initial improvement. Tensile strength, tear strength and abrasion resistance increased with MDI/PEG ratio, these values were higher in longitudinal direction. Resilience and compression set increased with isocyanate concentration.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Cure characteristics of short polyester fiber-polyurethane composites with respect to different bonding agents (MD resins) based on 4, 4' diphenylmethanediisocyanate (MDI) and various diols like propyleneglycol (PG), polypropyleneglycol (PPG) and glycerol (GL) were studied. Tmax. - Tmin. of composites having MD resin were found to be higher than the composite without MD resin. Minimum torque and Tmax. - Tmin., scorch time and optimum cure time were increased with the increase of MDI equivalence. Optimum ratio of MDI / -of in the resin was found to be within the range of 1-1.5. It was observed from the cure characteristics that for getting better adhesion between short polyester fiber and the polyurethane matrix the best choice of MD resin was one based on MDI and 1:1 equivalent mixture of polypropyleneglycol and glycerol.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Nanoscale silica was synthesized by precipitation method using sodium silicate and dilute hydrochloric acid under controlled conditions. The synthesized silica was characterized by Scanning Electron Microscopy (SEM), Transmission Electron Microscopy (TEM), BET adsorption and X-Ray Diffraction (XRD). The particle size of silica was calculated to be 13 nm from the XRD results and the surface area was found to be 295 m2/g by BET method. The performance of this synthesized nanosilica as a reinforcing filler in natural rubber (NR) compound was investigated. The commercial silica was used as the reference material. Nanosilica was found to be effective reinforcing filler in natural rubber compound. Filler-matrix interaction was better for nanosilica than the commercial silica. The synthesized nanosilica was used in place of conventional silica in HRH (hexamethylene tetramine, resorcinol and silica) bonding system for natural rubber and styrene butadiene rubber / Nylon 6 short fiber composites. The efficiency of HRH bonding system based on nanosilica was better. Nanosilica was also used as reinforcing filler in rubber / Nylon 6 short fiber hybrid composite. The cure, mechanical, ageing, thermal and dynamic mechanical properties of nanosilica / Nylon 6 short fiber / elastomeric hybrid composites were studied in detail. The matrices used were natural rubber (NR), nitrile rubber (NBR), styrene butadiene rubber (SBR) and chloroprene rubber (CR). Fiber loading was varied from 0 to 30 parts per hundred rubber (phr) and silica loading was varied from 0 to 9 phr. Hexa:Resorcinol:Silica (HRH) ratio was maintained as 2:2:1. HRH loading was adjusted to 16% of the fiber loading. Minimum torque, maximum torque and cure time increased with silica loading. Cure rate increased with fiber loading and decreased with silica content. The hybrid composites showed improved mechanical properties in the presence of nanosilica. Tensile strength showed a dip at 10 phr fiber loading in the case of NR and CR while it continuously increased with fiber loading in the case of NBR and SBR. The nanosilica improved the tensile strength, modulus and tear strength better than the conventional silica. Abrasion resistance and hardness were also better for the nanosilica composites. Resilience and compression set were adversely affected. Hybrid composites showed anisotropy in mechanical properties. Retention in ageing improved with fiber loading and was better for nanosilica-filled hybrid composites. The nanosilica also improved the thermal stability of the hybrid composite better than the commercial silica. All the composites underwent two-step thermal degradation. Kinetic studies showed that the degradation of all the elastomeric composites followed a first-order reaction. Dynamic mechanical analysis revealed that storage modulus (E’) and loss modulus (E”) increased with nanosiica content, fiber loading and frequency for all the composites, independent of the matrix. The highest rate of increase was registered for NBR rubber.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The nature of the diperiodatocuprate(III) (DPC) species present in aqueous alkaline medium has been investigated by a kinetic and mechanistic study on the oxidation of iodide by DPC. The reaction kinetics were studied over the 1.0 ´ 10)3±0.1 mol dm)3 alkali range. The reaction order with respect to DPC, as well as iodide, was found to be unity when [DPC] [I)]. In the 1.0 ´ 10)3±1.0 ´ 10)2 mol dm)3 alkali region, the rate decreased with increase in the alkali concentration and a plot of the pseudo-®rst order rate constant, k versus 1/[OH)] was linear. Above 5.0 ´ 10)2 mol dm)3, a plot of k versus [OH)] was also linear with a non-zero intercept. An increase in ionic strength of the reaction mixtures showed no e ect on k at low alkali concentrations, whereas at high concentrations an increase in ionic strength leads to an increase in k. A plot of 1/k versus [periodate] was linear with an intercept in both alkali ranges. Iodine was found to accelerate the reaction at the three di erent alkali concentrations employed. The observed results indicated the following equilibria for DPC.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Composite magnetic materials have the unique advantage of property modification for tailoring devices for various applications. Rubber ferrite composites (RFCs) prepared by incorporating ferrites in rubber matrixes have the advantage of easy mouldability and flexibility. RFCs containing various loadings of nickel zinc ferrite (NZF) (Ni1 xZnxFe2O4) in a natural rubber matrix have been prepared. The cure characteristics and the mechanical properties of these composites were evaluated. The effect of loading on the cure characteristics and tensile properties were also evaluated. It is found that the loading dependence on the cure time and mechanical properties exhibit an identical pattern.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Ultra fine nickel ferrite have been synthesized by the sol-gel method. By heat treating different portions of the prepared powder separately at different temperatures, nano-sized particles of nickel ferrite with varying particle sizes were obtained. These powders were characterised by the X-ray diffraction and then incorporated in the nitrile rubber matrix according to a specific recipe for various loadings. The cure characteristics and the mechanical properties of these rubber ferrite composites (RFCs) were evaluated. The effect of loading and the grain size of the filler on the cure characteristics and tensile properties were also evaluated. It is found that the grain size and porosity of the filler plays a vital role in determining the mechanical properties of the RFCs

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Natural rubber latex, an aqueous colloidal dispersion of polyisoprene is widely used in production of gloves, catherers, rubber bands etc. The natural rubber latex content present in products such as gloves causes allergic problems. Of the different types of allergies reported, latex is known to produce Type I and Type IV allergies. Type I is called immediate hypersensitivity and type IV is called delayed hypersensitivity. It has been reported that some of the proteins present in the latex are mainly responsible for the allergic reactions type I. Significant reduction in the allergic response (type I) of natural rubber latex can be achieved by the reduction in its protein content, however out of the total proteins present in the latex or latex film only a fraction is extractable. The major techniques employed to reduce protein content of latex include leaching, autoclaving, chlorination, use of proteolytic enzymes and use of non ionic surfactants. Sulphur vulcanization of dipped products is responsible for Type IV allergy. N-nitrosamine, a carcinogenic substance is produced as a result of sulphur vulcanization. Radiation vulcanization can be used as an alternative for sulphur vulcanization. The current research deals with techniques to reduce the allergy associated with latex products. To reduce the type I allergy, low protein latex is developed using polyethylene glycol, a non- ionic surfactant. The present study employs radiation vulcanization to eliminate type IV allergy. The effect of different cure systems and fillers on the properties of low protein latex is also investigated as a part of the study.