54 resultados para GHZ


Relevância:

10.00% 10.00%

Publicador:

Resumo:

Photonic band-gap (PBG) structures are utilized in microwave components as filters to suppress unwanted signals. In this work, rectangular perforations were created in the ground plane of a microstrip line to construct a PBG structure. A gold-coated alumina substrate was utilized to switch or tune the bandstop characteristics of this structure. It was demonstrated that the bandstop characteristics were switched off from - 35 to - 1 dB at 16 GHz. Tuning of the bandstop edge with a shift of 1.5 GHz was also shown

Relevância:

10.00% 10.00%

Publicador:

Resumo:

rectangular low-density, high-permittivity dielectric resona or antenna (DRA) excited by T-shaped microstrip feed offering a 2:1 VSWR bandwidth of -22% at 2.975 GHz is reported. The design methoaology and experimental results of the antenna are discussed. The excellent gain and radiation performance of the proposed antenna project: it as a potential candidate for telecommunication applications

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In this paper, the generation of a multiwavelength laser source from a Brillouin -Erbium fiber laser in the long wavelength band (L-band) region is experimentally demonstrated. The proposed laser system utilizes a Fabrv-Perot cavity formed by fiber-loop mirrors. Twenty-four lines of Brillouin-Stokes with line spacings of 10 GHz are obtained in the L-band region

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A new microwave dielectric resonator Ba(Tb1/2Nb1/2)03 has been prepared and characterized in the microwave frequency region. 1 wt% CeO2 is used as additive to reduce the sintering temperature. The sintered samples were characterized by XRD, SEM and Raman spectroscopic methods. Microwave DR properties such as er, Q factor and temperature-coefficient of resonant frequency (Ti) have been measured using a HP 8510 B Network Analyzer. Cylindrical DRs of Ba(Tb1/2Nbi/2)03 showed high Er (~ 37), high Q (~3,200) and low Tf (~10 ppm /°C) at 4 GHz and hence are useful for practical applications

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Single-phase polycrystalline ceramics in the MO-La2O3-Ti02 (M = Ca, Sr, Ba) system, such as cation-deficient hexagonal perovskites CaLa4Ti4O15, SrLa4Ti4O15, BaLa4Ti4O15, and Ca2La4Ti5O18 and the orthorhombic phases CaLa4Ti5O17 and CaLa8Ti9O31, were prepared through the solid-state ceramic route. The phases and structure of the ceramics were analyzed through x-ray diffraction and scanning electron microscopy. The microwave dielectric properties of the ceramics were studied using a network analyzer. The investigated ceramics show high Er in the range 42 to 54, high quality factors with Q x f in the range 16,222 to 50,215 GHz, and low Tf in the range -25 to +6 ppm3/°C. These high dielectric constant materials with high Q x f up to 50,215 GHz are suitable for applications where narrow bandwidth and extremely low insertion loss is necessary, especially at frequencies around 1.9 GHz

Relevância:

10.00% 10.00%

Publicador:

Resumo:

microwave dielectric properties of ceramics based on Ba(Mgv3Ta(2-2x)t3W,t3Tixt3)O3 is investigated as a function of x. The 15 densification as well as dielectric properties deteriorate with increase in the substitution levels of (Ti 1,3W113)333 + at (Ta213)3.33+ site 16 in Ba(Mg113Ta213)03. The rt is approaching zero between x = 0.1 and 0.15 in Ba(Mg it3Ta(2-2,,.)t3W,it3Ti,Tt3)O3 where quality factor is 17 reasonably good (Qu x f = 80,000-90,000 GHz). The Ba(Mg1,3Ta(2_,013W,13Ti,,13)03 with x = 1.0 has e, = 15.4, rf= -25.1 ppm/ 18 "C, Q„ x f = 35,400 GHz

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The microwave dielectric properties of ZnAl2O4 spinels were investigated and their properties were tailored by adding different mole fractions of Ti02. The samples were synthesized using the mixed oxide rout.e. The phase purity and crystal structure were identified using X-ray diffraction technique. The sintered specimens were characterized in the microwave frequency range (3-13 GHz). The ZnA12O4 ceramics exhibited interesting dielectric properties (dielectric constant (e,.) = 8.5, unloaded quality factor (Q.) = 4590 at 12.27 GHz and temperature coefficient of resonant frequency (Tf) = -79 ppm/°C). Addition of Ti02 into the spinel improved its properties and the Tf approached zero for 0.83ZnAl2O4- 0.17TiO2• This temperature compensated composition has excellent microwave dielectric properties (Cr _ 12.67, Q, = 9950 at 10.075 GHz) which can be exploited for microwave substrate applications

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Microwave dielectric resonators (DRs) based on Ba(B1,2Nbi/2)03 [B' = La, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Y, Yb, and In] complex perovskites have been prepared by conventional solid state ceramic route. The dielectric properties (relative permittivity, Er; quality factor, Q; and resonant frequency, rr) of the ceramics have been measured in the frequency range 4-6 GHz using resonance methods. The resonators have relatively high dielectric constant in the range 36-45, high quality factor and small temperature variation of resonant frequency. The dielectric properties are found to depend on the tolerance factor (t), ionic radius (r), and lattice parameter (ap)

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The effect of glass additives on the densification , phase evolution, microstructure and microwave dielectric properties of Ba(Mg1;3 Ta2i3)03 (BMT) was investigated . Different weight percentages of quenched glass such as B203 , Si02, B203-SiO2, ZnO-B203, 5ZnO-2B2O3, Al203-SiO2, Na20-2B203.10H20, BaO-B203-SiO2, MgO-B203-SiO2, PbO-B203-SiO2 , ZnO-B203-SiO2 and 2MgO-Al203-5SiO2 were added to calcined BMT precursor . The sintering temperature of the glass -added BMT samples were lowered down to 1300 °C compared to solid-state sintering where the temperature was 1650 °C. The formation of high temperature satellite phases such as Ba5Ta4O15 and Ba7Ta6O22 were found to be suppressed by the glass addition . Addition of glass systems such as B203, ZnO-B203, 5ZnO-2B203 and ZnO-B203-SiO2 improved the densification and microwave dielectric properties. Other glasses were found to react with BMT to form low-Q phases which prevented densification . The microwave dielectric properties of undoped BMT with a densification of 93 . 1 % of the theoretical density were Cr = 24 . 8, Tr = 8 ppm/°C and Q„ x f= 80,000 GHz. The BMT doped with 1.0 wt% of B203 has Q„ x f = 124,700GHz, Cr = 24.2, and T f = -1.3 ppm /°C. The unloaded Q factor of 0.2 wt% ZnO-B203-doped BMT was 136,500 GHz while that of 1.0 wt% of 5ZnO-2B203 added ceramic was Q„ x f= 141,800 GHz . The best microwave quality factor was observed for ZnO -B203-SiO2 (ZBS) glass-added ceramics which can act as a perfect liquid-phase medium for the sintering of BMT. The microwave dielectric properties of 0.2wt% ZBS-added BMT dielectric was Q„ x f= 152,800 GHz, F,= 25.5, and Tr = - 1.5 ppm/°C

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Chemically modified novel thermo-reversible zinc sulphonated ionomers based on natural rubber (NR), radiation induced styrene grafted natural rubber (RI-SGNR), and chemically induced styrene grafted natural rubber (CI-SGNR) were synthesized using acetyl sulphate/zinc acetate reagent system. Evidence for the attachment of sulphonate groups has been furnished by FTIR spectra. which was supplanted by FTNMR results. Estimation of the zinc sulphonate group was done using spectroscopic techniques such as XRFS and ICPAES. The TGA results prove improvement in the therrno-oxidative stability of the modified natural rubber. Both DSC and DMTA studies show that the incorporation of the ionic groups affect the thermal transition of the base polymer. Retention of the improved physical properties of the novel ionomers even after three repeated cycles of mastication and molding at 120 degree C may be considered as the evidence for the reprocessabiJity of the ionomer. Effect of both particulate (carbon black. silica & zinc stearate) and fibrous fillers (nylon & glass) on the properties of the radiation induced styrene grafted natural rubber ionomer has been evaluated. Incorporation of HAF carbon black results in maximum improvement in physical properties. Silica reinforces the backbone chain and weakens the ionic associations. Zinc stearate plays the dual role of reinforcement and ptasticization. The nylon and glass filled lonorner compounds show good improvement in the physical properties in comparison with the neat ionomer. Dispersion and adhesion of the fillers in the ionomer matrix has been amply supported by their SEM micrographs. Microwave probing of the electrical behavior of the 26.5 ZnSRISGNR ionomer reveals that the maximum relative complex conductivity and the complex permittivity appear at the frequency of 2.6 GHz. The complex conductivity of the base polymer increases from 1.8x 10.12 S/cm to 3.3xlO·4 S/cm. Influence of fillers on the dielectric constant and conductivity of the new ionic thermoplastic elastomer has been studied. The ionomer I nylon compound shows the highest microwave conductivity. Use of the 26.5 ZnS-RISGNR ionomer as a compatibilizer for obtaining the technologically compatible blends from the immiscible SBR/NBR system has been verified. The heat fugitive ionic cross-linked natural rubber may be, therefore, useful as an alternative to vulcanized rubber and thermoplastic elastomer

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The thesis deals with the preparation and dielectric characterization of Poly aniline and its analogues in ISM band frequency of 2-4 GHz that includes part of the microwave region (300 MHz to 300 GHz) of the electromagnetic spectrum and an initial dielectric study in the high frequency [O.05MHz-13 MHz]. PolyaniIine has been synthesized by an in situ doping reaction under different temperature and in the presence of inorganic dopants such as HCl H2S04, HN03, HCl04 and organic dopants such as camphorsulphonic acid [CSA], toluenesulphonic acid {TSA) and naphthalenesulphonic acid [NSA]. The variation in dielectric properties with change in reaction temperature, dopants and frequency has been studied. The effect of codopants and microemulsions on the dielectric properties has also been studied in the ISM band. The ISM band of frequencies (2-4 GHz) is of great utility in Industrial, Scientific and Medical (ISM) applications. Microwave heating is a very efficient method of heating dielectric materials and is extensively used in industrial as well as household heating applications.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Design of a compact microstrip-fed ultra-wideband antenna suitable for USB dongle and other such space constraint applications is presented. The structure consists of a pentagonal monopole element and a modified ground plane that gives an impedance bandwidth from 2.8 to 12 GHz. Radiation patterns are stable and omni-directional throughout the band with an average gain of 2.84 dBi. The antenna occupies only 11 × 30 mm2 on FR4 substrate with permittivity 4.4.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The design and performance of a stepped slot printed monopole antenna in the ultrawideband is presented in this article. Multiple resonances generated by the stepped slot geometry are matched in the ultrawideband using a modified microstrip feed. The impedance bandwidth (SWR < 2) of the antenna is from 3 to 11 GHz. Radiation patterns are stable and omnidirectional with appreciable gain throughout the band. Performance of the antenna is also analyzed in the time domain, which reveals good pulse handling capabilities. Compact geometry of the antenna allows easy commercial deployment.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

An asymmetric coplanar strip-fed uniplanar antenna for wideband applications is presented. The resulting antenna offers a 2:1 VSWR bandwidth greater than 100% from 1.58 to 5.48 GHz covering the DCS/PCS/IEEE 802.11a/WiMAX bands. The antenna has an overall dimension of 44 × 35 mm2 when printed on a substrate of dielectric constant 4.4 and height 1.6 mm. The design equation is also presented in this article. The antenna exhibits good radiation characteristics and moderate gain in the entire operating band.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A compact, dual band coplanar waveguide fed modified T-shaped uniplanar antenna is presented. The antenna has resonances at 1.77 and 5.54 GHz with a wide band from 1.47–1.97 GHz and from 5.13–6.48 GHz with an impedance bandwidth of 34% and 26%, respectively. Also the antenna has an average gain of 3 dBi in lower band and 3.5 dBi in higher band with an average efficiency of 90%.