Resumo:
The distribution of curing agents and fillers in the constituents of an elastomer blend is an important factor which determines the curing behaviour and vulcanizate properties of the blend. The distribution of curatives and fillers largely depends on the nature of elastomers. The curatives tend to migrate preferentially to the rubber of higher unsaturation and/or higher polarity, and reinforcing fillers tend to get distributed in the low viscosity phase, resulting in inferior mechanical properties of the blends. The thesis suggests several methods for improving mechanical properties of blends like NBR/butyl, NR/butyl, NBR/EPDM and NR/.
Resumo:
Attempts have been made to attain satisfactory network structures in each of the phases of a rubber blend by minimising the cure rate imbalance by employing methods such as grafting of accelerators to the slow curing rubber, chemically bonding the crosslinking agents to the rubber in which it has lower solubility, functionalisation of the slow curing rubber, masterbatching of the curing agents to the slow curing rubber etc. Functionalisation of the slow curing constituents of NR/IIR and NR/EIPDM blends is tried using novel reagents as the first part of this study. However, the crux of the present study is a more direct approach to attaining a covulcanized state in NR/IIR and NR/EPDM blends: Precuring the slow curing rubber (IIR or EPDM) to a low level when it can still blend with NR and then to ck) the final curing after blending with NR. TNM3 precuring is also likely to minimise the viscosity mismatch. Since a low level of resmmal crosslink density is likely to be present lJ1 reclaimed rubbers, blending heat resistant reclaimed rubber such as butyl reclaim with NR may also have the same effect of precuring IIR, and then blending with NR. Hence use of IIR reclaim for developing blends with NR is also proposed to be investigated in this study
Resumo:
The work presented in this thesis is regarding the development and evaluation of new bonding agents for short polyester fiber - polyurethane elastomer composites. The conventional bonding system based on hexamethylenetetramine, resorcinol and hydrated silica was not effective as a bonding agent for the composite, as the water eliminated during the formation of the RF resin hydrolysed the urethane linkages. Four bonding agents based on MDI/'I‘DI and polypropyleneglycol, propyleneglycol and glycerol were prepared and the composite recipe was optimised with respect to the cure characteristics and mechanical properties. The flow properties, stress relaxation pattern and the thermal degradation characteristics of the composites containing different bonding agents were then studied in detail to evaluate the new bonding systems. The optimum loading of resin was 5 phr and the ratio of the -01 to isocyanate was 1:1. The cure characteristics showed that the optimum combination of cure rate and processability was given by the composite with the resin based on polypropyleneglycol/ glycerol/ 4,4’diphenylmethanediisocynate (PPG/GL/MDI). From the rheological studies of the composites with and without bonding agents it was observed that all the composites showed pseudoplastic nature and the activation energy of flow of the composite was not altered by the presence of bonding agents. Mechanical properties such as tensile strength, modulus, tear resistance and abrasion resistance were improved in the presence of bonding agents and the effect was more pronounced in the case of abrasion resistance. The composites based on MDI/GL showed better initial properties while composites with resins based on MDI/PPG showed better aging resistance. Stress relaxation showed a multistage relaxation behaviour for the composite. Within the-strain levels studied, the initial rate of relaxation was higher and the cross over time was lesser for the composite containing bonding agents. The bonding agent based on MDI/PPG/GL was found to be a better choice for improving stress relaxation characteristics with better interfacial bonding. Thennogravimetirc analysis showed that the presence of fiber and bonding agents improved the thennal stability of the polyurethane elastomer marginally and it was maximum in the case of MDI / GL based bonding agents. The kinetics of degradation was not altered by the presence of bonding agents
Resumo:
The Human race of our century is in gluttonous search for novel engineering products which led to a skyrocketed progress in research and fabrication of filled polymers. Recently, a big window has been opened up for speciality polymers especially elastomers with promising properties. Among the many reasons why rubbers are widely used in the process industries, three are considered as important. Firstly, rubbers operate in a variety of environments and possess usable ranges of deformity and durability and can be exploited through suitable and more or less conventional equipment design principles. Secondly, rubber is an eminently suitable construction material for protection against corrosion in the chemical plant and equipment against various corrosive chemicals as, acids and alkalies and if property tailored, can shield ionising radiations as X-rays and gamma rays in medical industry, with minimum maintenance lower down time, negligible corrosion and a preferred choice for aggressive corroding and ionising environment. Thirdly, rubber can readily and hastily, and at a relatively lower cost, be converted into serviceable products, having intricate shapes and dimensions. In a century’s gap, large employment of flexible polymer materials in the different segments of industry has stimulated the development of new materials with special properties, which paved its way to the synthesis of various nanoscale materials. At nano scale, one makes an entry into a world where multidisciplinary sciences meet and utilises the previously unapproached infinitesimal length scale, having dimension which measure upto one billionth of a meter, to create novel properties. The nano fillers augment the elastomers properties in an astonishing fashion due to their multifunctional nature and unprecedented properties have been exhibited by these polymer-nanocomposites just to beat the shortcomings of traditional micro composites. The current research aims to investigate the possibility of using synthesised nano barium sulphate for fabricating elastomer-based nanocomposites and thereby imparting several properties to the rubber. In this thesis, nano materials, their synthesis, structure, properties and applications are studied. The properties of barium sulphate like chemical resistance and radiopacity have been utilized in the present study and is imparted to the elastomers by preparing composites
Resumo:
The Human race of our century is in gluttonous search for novel engineering products which led to a skyrocketed progress in research and fabrication of filled polymers. Recently, a big window has been opened up for speciality polymers especially elastomers with promising properties. Among the many reasons why rubbers are widely used in the process industries, three are considered as important. Firstly, rubbers operate in a variety of environments and possess usable ranges of deformity and durability and can be exploited through suitable and more or less conventional equipment design principles. Secondly, rubber is an eminently suitable construction material for protection against corrosion in the chemical plant and equipment against various corrosive chemicals as, acids and alkalies and if property tailored, can shield ionising radiations as X-rays and gamma rays in medical industry, with minimum maintenance lower down time, negligible corrosion and a preferred choice for aggressive corroding and ionising environment. Thirdly, rubber can readily and hastily, and at a relatively lower cost, be converted into serviceable products, having intricate shapes and dimensions. In a century’s gap, large employment of flexible polymer materials in the different segments of industry has stimulated the development of new materials with special properties, which paved its way to the synthesis of various nanoscale materials. At nano scale, one makes an entry into a world where multidisciplinary sciences meet and utilises the previously unapproached infinitesimal length scale, having dimension which measure upto one billionth of a meter, to create novel properties. The nano fillers augment the elastomers properties in an astonishing fashion due to their multifunctional nature and unprecedented properties have been exhibited by these polymer-nanocomposites just to beat the shortcomings of traditional micro composites. The current research aims to investigate the possibility of using synthesised nano barium sulphate for fabricating elastomer-based nanocomposites and thereby imparting several properties to the rubber. In this thesis, nano materials, their synthesis, structure, properties and applications are studied. The properties of barium sulphate like chemical resistance and radiopacity have been utilized in the present study and is imparted to the elastomers by preparing composites.
Resumo:
This thesis aims to develop new toughened systems for epoxy resin via physical and chemical modifications. Initially the synthesis of DGEBA was carried out and the properties compared with that of the commercial sample. Subsequently the modifier resins to be employed were synthesized. The synthesized resin were characterized by spectroscopic method (FTIR and H NMR), epoxide equivalent and gel permeation chromatography. Chemical modification involves the incorporation of thermoset resins such a phenolics, epoxy novolacs, cardanol epoxides and unsaturated polyester into the epoxy resin by reactive belnding. The mechanical and thermal properties of the blends were studied. In the physical modification route, elastomers, maleated elastomers and functional elastomers were dispersed as micro-sized rubber phase into the continuous epoxy phase by a solution blending technique as against the conventional mechanical blending technique. The effect of matrix toughening on the properties of glass reinforced composites and the effect of fillers on the properties of commercial epoxy resin were also investigated. The blends were characterized by thermo gravimetric analysis, differential scanning calorimetry, dynamic mechanical analysis, scanning electron microscopy and mechanical property measurements. Among the thermoset blends, substantial toughening was observed in the case of epoxy phenolic novolacs especially epoxy para cresol novolac (ECN). In the case of elastomer blending , the toughest blends were obtained in the case of maleic anhydride grafted NBR. Among functional elastomers the best results were obtained with CTBN. Studies on filled and glass reinforced composites employing modified epoxy as matrix revealed an overall improvement in mechanical properties
Resumo:
Natural rubber/isora fibre composites were cured at various temperatures. The solvent swelling characteristics of natural rubber composites containing both untreated and alkali treated fibres were investigated in aromatic and aliphatic solvents like toluene, and n-hexane. The diffusion experiments were conducted by the sorption gravimetric method. The restrictions on elastomer swelling exerted by isora fibre as well as the anisotropy of swelling of the composite have been confirmed by this study. Composite cured at 100°C shows the lowest percentage swelling. The uptake of aromatic solvent is higher than that of aliphatic solvent for the composites cured at all temperatures. The effect of fibre loading on the swelling behaviour of the composite was also investigated in oils like petrol, diesel, lubricating oil etc. The % swelling index and swelling coefficient of the composite were found to decrease with increase in fibre loading. This is due to the increased hindrance exerted by the fibres at higher fibre loadings and also due to the good fibre-rubber interactions. Maximum uptake of solvent was observed with petrol followed by diesel and then lubricating oil. The presence of bonding agent in the composites restrict the swelling considerably due to the strong interfacial adhesion. At a fixed fibre loading, the alkali treated fibre composite showed lower percentage swelling compared to the untreated one.
Resumo:
This 'study' deals with a preliminary study of automatic beam steering properly in conducting polyaniline . Polyaniline in its undoped and doped .state was prepared from aniline by the chemical oxidative polymerization method. Dielectric properties of the samples were studied at S-band microwave frequencies using cavity perturbation technique. It is found that undoped po/vanihne is having greater dielectric loss and conductivity contpared with the doped samples. The beam steering property is studied using a perspex rod antenna and HP 85/OC vector network analyzer. The shift in the radiated beam is studied for different do voltages. The results show that polyaniline is a good nutterial far beam steering applications.
Resumo:
New oligomer-bound antioxidants have been prepared by condensation reaction. The efficiency and permanence of these oligomer- bound paraphenylene diamines as antioxidants has been compared with conventional amine type antioxidants in NR, SBR, IIR and NBR and in elastomer blends like NR/BR and NR/SBR. The oligomer-bound antioxidants are found to impart improved ozone, flex resistance and mechanical properties to the vulcanizates of NR, SBR, IIR and NBR and to blends of NR/BR and NR/ SBR in comparison with those containing conventional antioxidants.
Characterization of Short Nylon-6 Fiber/Acrylonitrile Butadiene Rubber Composite by Thermogravimetry
Resumo:
The thermal degradation of short nylon-6 fiber reinforced acrylonitrile butadiene rubber (NBR) composites with and without epoxy-based bonding agent has been studied by thermogravimetric analysis (TGA). It was found that the onset of degradation shifted from 330.5 to 336.1°C in the presence of short nylon fiber, the optimum fiber loading being 20 phr. The maximum rate of degradation of the composites was lower than that of the unfilled rubber compound, and it decreased with increase in fiber concentration. The presence of epoxy resin-based bonding agent in the virgin elastomer and the composites improved the thermal stability. Results of kinetic studies showed that the degradation of NBR and the short nylon fiber reinforced composites followed first-order kinetics.
Resumo:
The present study deals with the short isora fibre reinforced natural rubber composites. In recent years there has been a tremendous advancement in the field of science and technology of short fibre reinforced polymer composites. The low density, high strength, high stiffness to weight ratio, excellent durability and design flexibility are the primary reasons for their use in many diversified fields such as air crafts, automobiles, marine industry etc. Compared to the various natural and synthetic fibres used as reinforcement for elastomer composites isora fibre is superior in many aspects. `Isora' is a natural lignocellulosic fibre which is easily available in South India especially in Kerala. The fibre is separated from the bark of the Helicteres isora plant by retting process. This fibre has excellent mechanical properties and is easily amenable to physical and chemical modifications. The study shows that composites with poor interfacial bonding tend to dissipate more energy than that with to interfacial bonding. The mechanical loss also can be related to interfacial bonding. The effect of chemical treatment of isora fibre on damping was also studied. Both in the low and high temperature region which indicates that this composite posseses low damping and hence good interfacial bonding characteristics. Hence these composites are better candidates for high damping applications. Composites with longitudinally oriented fibres showed high storage modulus than transversely oriented ones due to the effective stress transfer between fibre and matrix.
Resumo:
A new approach, the multipole theory (MT) method, is presented for the computation of cutoff wavenumbers of waveguides partially filled with dielectric. The MT formulation of the eigenvalue problem of an inhomogeneous waveguide is derived. Representative computational examples, including dielectric-rod-loaded rectangular and double-ridged waveguides, are given to validate the theory, and to demonstrate the degree of its efficiency
Direction Dependent Transmission Characteristics of Dye Mixture Doped Polymer Optical Fibre Preforms
Resumo:
The direction dependant wavelength selective transmission mechanism in poly (methyl methacrylate)(PMMA) rods doped with C 540 dye and C 540:Rh.B dye mixture as a combination has been investigated. When a polished slice of pure C 540 doped polymer rod was used side by side with a C540:Rh B doped rod with acceptor concentration [A] = 7x10-4 m/l , we could notice more than 100% change in the transmitted intensity along opposite directions at the C 540, Rh B emission and the excitation wavelengths . A blue high bright LED emitting at a peak wavelength 465nm was used as the excitation source.
Direction Dependent Transmission Characteristics of Dye Mixture Doped Polymer Optical Fibre Preforms
Resumo:
The direction dependant wavelength selective transmission mechanism in poly (methyl methacrylate)(PMMA) rods doped with C 540 dye and C 540:Rh.B dye mixture as a combination has been investigated. When a polished slice of pure C 540 doped polymer rod was used side by side with a C540:Rh B doped rod with acceptor concentration [A] = 7x10-4 m/l , we could notice more than 100% change in the transmitted intensity along opposite directions at the C 540, Rh B emission and the excitation wavelengths . A blue high bright LED emitting at a peak wavelength 465nm was used as the excitation source.
Direction Dependent Transmission Characteristics of Dye Mixture Doped Polymer Optical Fibre Preforms
Resumo:
The direction dependant wavelength selective transmission mechanism in poly (methyl methacrylate)(PMMA) rods doped with C 540 dye and C 540:Rh.B dye mixture as a combination has been investigated. When a polished slice of pure C 540 doped polymer rod was used side by side with a C540:Rh B doped rod with acceptor concentration [A] = 7x10-4 m/l , we could notice more than 100% change in the transmitted intensity along opposite directions at the C 540, Rh B emission and the excitation wavelengths . A blue high bright LED emitting at a peak wavelength 465nm was used as the excitation source.