Resumo:
Blends of natural rubber (NR) with styrene-butadiene rubber (SBR), polybutadiene rubber (BR), ethylene-propylene terpolymer (EPDM) and acrylonitrile-butadiene rubber (NBR) were vulcanised using an efficient vulcanisation (EV) system and a semi-EV system. Compatible blends show a definite pattern of curing whereas the incompatible blends show no such pattern.
Resumo:
Blends of 50/50 natural rubber (NR) and styrene-butadiene rubber (SBR) are vulcanized using several conventional and semi-EV systems. The cure characteristics and vulcanizate properties are compared. The quantity and quality of crosslinks in each case are deciphered by chemical probes to correlate them with the vulcanizate properties.
Resumo:
A carbon black filled 50/50 Natural Rubber (NR)/Polybutadiene Rubber (BR) blend is vulcanized using several conventional systems designed by varying the amounts of sulphur and accelerator . The cure characteristics and the vulcanizate properties are compared. The quality and quantity of crosslinks in each case are deciphered by chemical probes to correlate them with the vulcanizate properties.
Resumo:
Blends of styrene butadiene rubber (SBR) with maleic anhydride grafted whole tire reclaim (MA-g-WTR) have been prepared and the cure and mechanical properties have been studied with respect to the reclaim content. The grafting was carried out in the presence of dicumylperoxide (DCP) in a Brabender Plasticorder at 150'C. The presence of anhydride group on the WTR was confirmed by infrared spectrometry (IR) study. The properties were compared with those of the blends containing unmodified WTR. Though the cure time was marginally higher, the mechanical properties of the blends containing grafted WTR were better than that of the unmodified blends.
Resumo:
Blends of nitrile rubber and reclaimed rubber containing different levels of a coupling agent, Si 69 (bis(3- triethoxysilyl propyl)(tetrasulphide) were prepared and the cure characteristic's and mechanical properties were studied. Optimum loading of Si-69 was found to be a function of blend ratio. 3 phi- of Si 69 in a 70:30. Blend was found to be the optimum combination with respect to the mechanical properties. The rate and state of cure were also affected bv the conp/ing agent. Tensile strength, tear strength and abrasion resistance were improved in the presence of coupling agent. While the state of cure improved, the cure rate and scorch time decreased with increasing silane content. Ageing studies showed that the blends containing the coupling agent were inferior to the unmodified blends.
Resumo:
Chloroprene rubber was blended with whole tire reclaimed rubber (WTR) in presence of different levels of a coupling agent Si69 [bis- (3-(triethoxysilyl)propy1)tetrasuIfide] and the cure characteristics and mechanical properties were studied. The rate and state of cure were also affected by the coupling agent. While the cure time was increased, the cure rate and scorch time were decreased with increasing silane content. Tensile strength, tear strength, and abrasion resistance were improved in the presence of coupling agent. Compression set and resilience were adversely affected in presence of silane-coupling agent.Aging studies showed that the blends containing the coupling agent were inferior to the unmodified blends.
Resumo:
Cure characteristics and mechanical properties of short nylon fiber reinforced acrylonitrile butadiene rubber-reclaimed rubber composites were studied. Minimum torque, (maximum-minimum) torque and cure rate increased with fiber concentration. Scorch time and cure time decreased by the addition of fibers. Properties like tensile strength, tear strength, elongation at break, abrasion loss and heat build up were studied in both orientations of fibers. Tensile and tear properties were enhanced by the addition of fibers and were higher in the longitudinal direction. Heat build up increased with fiber concentration and were higher in the longitudinal direction. Abrasion resistance was improved in presence of short fibers and was higher in the longitudinal direction. Resilience increased on the introduction of fibers. Compression set was higher for blends.
Resumo:
The cure characteristics and mechanical properties of short nylon fiber- styrene /whole tyre reclaim (SBR/WTR) composites with and without an interfacial bonding agent based on 4,4 diphenyl methane diisocyanate and polyethylene glycol (MDI/PEG) have been studied. An 80:40 blend of SBR/ WTR reinforced with 20 phr of short nylon fiber has been selected and the MDI/ PEG ratio has been changed from 0.67:1 to 2:1. The minimum and maximum torques increased with isocyanate concentration. The scorch time and cure time showed an initial reduction. The cure rate showed an initial improvement. Tensile strength, tear strength and abrasion resistance increased with MDI/PEG ratio, these values were higher in longitudinal direction. Resilience and compression set increased with isocyanate concentration.
Resumo:
Cure characteristics of short polyester fiber-polyurethane composites with respect to different bonding agents (MD resins) based on 4, 4' diphenylmethanediisocyanate (MDI) and various diols like propyleneglycol (PG), polypropyleneglycol (PPG) and glycerol (GL) were studied. Tmax. - Tmin. of composites having MD resin were found to be higher than the composite without MD resin. Minimum torque and Tmax. - Tmin., scorch time and optimum cure time were increased with the increase of MDI equivalence. Optimum ratio of MDI / -of in the resin was found to be within the range of 1-1.5. It was observed from the cure characteristics that for getting better adhesion between short polyester fiber and the polyurethane matrix the best choice of MD resin was one based on MDI and 1:1 equivalent mixture of polypropyleneglycol and glycerol.
Resumo:
Ultra fine nickel ferrite have been synthesized by the sol-gel method. By heat treating different portions of the prepared powder separately at different temperatures, nano-sized particles of nickel ferrite with varying particle sizes were obtained. These powders were characterised by the X-ray diffraction and then incorporated in the nitrile rubber matrix according to a specific recipe for various loadings. The cure characteristics and the mechanical properties of these rubber ferrite composites (RFCs) were evaluated. The effect of loading and the grain size of the filler on the cure characteristics and tensile properties were also evaluated. It is found that the grain size and porosity of the filler plays a vital role in determining the mechanical properties of the RFCs
Resumo:
Composite magnetic materials have the unique advantage of property modification for tailoring devices for various applications. Rubber ferrite composites (RFCs) prepared by incorporating ferrites in rubber matrixes have the advantage of easy mouldability and flexibility. RFCs containing various loadings of nickel zinc ferrite (NZF) (Ni1 xZnxFe2O4) in a natural rubber matrix have been prepared. The cure characteristics and the mechanical properties of these composites were evaluated. The effect of loading on the cure characteristics and tensile properties were also evaluated. It is found that the loading dependence on the cure time and mechanical properties exhibit an identical pattern.
Resumo:
Zinc butyl xanthate [Zn(bxt)2] was prepared in the laboratory . The effect of this xanthate with zinc diethyl dithiocarbamate (ZDC) on the vulcanization of natural rubber ( NR), polybutadiene rubber (BR), and NR/BR blend has been studied at different temperatures. The amounts of Zn (bxt)2 and ZDC in the compounds were optimized by varying the amount of ZDC from 0 . 75 to 1.5 phr and Zn (bxt)2 from 0 . 75 to 1 .5 phr. The cure characteristics were also studied . HAF filled NR, BR, and NR / BR blend compounds were cured at different temperatures from 60 to 150 C. The sheets were molded and properties such as tensile strength, tear strength, crosslink density and elongation at break, compression set, abrasion resistance, etc. were evaluated. The results show that the mechanical properties of 80NR/20BR blends are closer to that of NR vulcanizates, properties of 60NR/40BR blends are closer to BR vulcanizates, while the 70NR/30BR blends show an intermediate property.
Resumo:
Blends of chlorobutyl rubber (CIIR) with two grades of ethylene-propylene diene monomer rubber (EPDM) were prepared and the effect of blend ratio on the cure characteristics, hot air ageing resistance, steam ageing resistance, and mechanical properties were evaluated. The blend of CIIR with EPDM grade 301 T showed additive behavior and the blend with the other grade of EPDM (NDR 4640) showed synergistic behavior.
Resumo:
Amine Terminated Liquid Natural Rubber (ATNR) was used as a plasticiser in filled NR and NBR compounds replacing oil/DOP. The scorch time and cure time were found to be lowered when ATNR was used as the plasticiser. ATNR was found to improve the mechanical properties like tensile strength, tear strength and modulus of the vulcanizates . The ageing resistance of the vulcanizates containing ATNR was superior compared to the vulcanizates containing oil/DOP.
Resumo:
A carbon black filled 50/50 natural rubber (NR)/styrene-butadiene rubber (SBR) blend is vulcanized using several conventional curing systems designed by varying the amounts of sulphur and accelerator. The cure characteristics and the properties of the vulcanizates are compared. The quantity and quality of crosslinks in each case are evaluated by chemical probes to correlate them with the properties.