Ammonia can be used as a pH controller in chloride-based metal recovery processes. In chloride conditions, ammonia reacts to ammonium chloride which can be regenerated back to ammonia with lime. Although the regeneration process itself has been known for a long time, the concentrations, non-reacting species, conditions, and even goals are different when comparing the ammonia regeneration process in different industries. The main objective of this thesis was to study the phenomena, equipment, and challenges in ammonia regeneration in the nickel process and to make a preliminary process design. The study concentrated on the regeneration and recovery units. The thesis was made by process simulation and laboratory tests using the current processes as initial information. The results were combined from all of the information obtained during the studies to provide a total process solution, which can be used as a basis when designing an ammonia regeneration process to be used in industry. In particular, it was possible to determine ammonia recovery with a stripping column and the achievement of the desired ammonia water product within the scope of this thesis. The required mass flows and process conditions were also determined. The possible challenges and solutions or further studies to overcome them were provided as well to ease the prediction and design of the ammonia regeneration process in the future. On the basis of the results of this thesis, the ammonia regeneration process can be developed further and implemented in the nickel chloride leaching process.