19 resultados para Metallic iron
em Doria (National Library of Finland DSpace Services) - National Library of Finland, Finland
Resumo:
In this thesis, cleaning of ceramic filter media was studied. Mechanisms of fouling and dissolution of iron compounds, as well as methods for cleaning ceramic membranes fouled by iron deposits were studied in the literature part. Cleaning agents and different methods were closer examined in the experimental part of the thesis. Pyrite is found in the geologic strata. It is oxidized to form ferrous ions Fe(II) and ferric ions Fe(III). Fe(III) is further oxidized in the hydrolysis to form ferric hydroxide. Hematite and goethite, for instance, are naturally occurring iron oxidesand hydroxides. In contact with filter media, they can cause severe fouling, which common cleaning techniques competent enough to remove. Mechanisms for the dissolution of iron oxides include the ligand-promoted pathway and the proton-promoted pathway. The dissolution can also be reductive or non-reductive. The most efficient mechanism is the ligand-promoted reductive mechanism that comprises two stages: the induction period and the autocatalytic dissolution.Reducing agents(such as hydroquinone and hydroxylamine hydrochloride), chelating agents (such as EDTA) and organic acids are used for the removal of iron compounds. Oxalic acid is the most effective known cleaning agent for iron deposits. Since formulations are often more effective than organic acids, reducing agents or chelating agents alone, the citrate¿bicarbonate¿dithionite system among others is well studied in the literature. The cleaning is also enhanced with ultrasound and backpulsing.In the experimental part, oxalic acid and nitric acid were studied alone andin combinations. Also citric acid and ascorbic acid among other chemicals were tested. Soaking experiments, experiments with ultrasound and experiments for alternative methods to apply the cleaning solution on the filter samples were carried out. Permeability and ISO Brightness measurements were performed to examine the influence of the cleaning methods on the samples. Inductively coupled plasma optical emission spectroscopy (ICP-OES) analysis of the solutions was carried out to determine the dissolved metals.
Resumo:
Työssä tutkittiin metalli- ja anioniepäpuhtauksien myötäuuttautumista sinkin mukana di(2-etyyliheksyyli)fosforihappoalla (D2EHPA). Laboratoriokokeissa selvitettiin pH:n vaikutusta metalliepäpuhtauksien uuttautumiseen pH-alueella -O, l... 3 sekä pesujen vaikutusta sinkillä ladatun orgaanisen faasin metallipitoisuuksiin. Kokeita tehtiin sekä synteettisillä että autenttisilla prosessiliuoksilla. Anionikokeissa tutkittiin raudan ja sinkin vaikutusta kloridin ja fluoridin uuttautumiseen. Synteettisillä liuoksilla tehdyissä kokeissa tutkittiin kadmiumin, koboltin, nikkelin, kuparin sekä antimonin uuttautumista sinkkisulfaattiliuoksesta. Kokeissa havaittiin D2EHPA:n uuttavan sinkkiä selvästi em. metalleja paremmin. Sinkki uuttautui sulfaattiliuoksesta lähes täydellisesti tasapaino-pH:n ollessa yli 2,3. Sinkin jälkeen muista metalleista uuttautui eniten kadmium ja järjestyksessä sitten kupari, koboltti ja nikkeli. Epäpuhtausmetallien myötäuuttautumista lisääntyi uuton tasapaino-pH:n kasvaessa ja väheni sinkkilatauksen kasvaessa. Kahdella peräkkäisellä pesuaskeleella, joissa ensimmäinen pesuliuos sisälsi 5 g/L rikkihappoa ja toinen sekä 15 g/L rikkihappoa että 5 g/L sinkkiä saatiin kaikkien epäpuhtausmetallien pitoisuudet jäämään alle 3 mg/L. Antimonin uuttokokeissa huomattiin antimonin uuttautuvan täydellisesti D2EHPA:lla pH:sta riippumatta pH-alueella0...3. Prosessiliuoksilla tehdyissä kokeissa todettiin D2EHPA:n pystyvän tehokkaasti erottamaan sinkin magnesiumista ßzn,Mg ˜107 ja kadmiumista ßzn,cd ˜106. Havaittiin myös, että mitä suurempi sinkki- ja rautalataus orgaanisessa faasissa on sitä vähemmän magnesiumia ja kadmiumia uuttautuu. Ensimmäisessä pesussa saatiin sekä kadmiumin että magnesiumin pitoisuudet putoamaan keskimäärin 0,1 mg/L eli 30 alkuperäisestä pitoisuudesta. Toisella pesuaskeleella ei enää ollut vaikutusta kadmiumin ja magnesiumin pitoisuuksiin orgaanisessa faasissa. Kokeissa havaittiin myös, että D2EHPA:n latausasteen ylittäessä 0,7 alkaa sinkki-D2EHPA-kompleksit polymeroitua ja faasit eivät enää selkeytyneet helposti. Anionikokeissa huomattiin, ettei D2EHPA uuttanut kloridi tai fluoridi sinkin tai raudan mukana. D2EHPA:n havaittiin myös itsessään sisältävän hieman kloridia.
Resumo:
Työssä on tutkittu epäpuhtauksien vaikutusta kastelulannoitesuolojen monokaliumfosfaatin, kaliumnitraatin ja ureafosfaatin kiteytyksessä. Kirjallisuusosassa on käsitelty kastelulannoiteprosessit ja epäpuhtauksien vaikutus kastelulannoitteiden valmistuksessa. Kiteytys ja kiteenkasvu on esitetty perusyhtälöin, joissa on otettu epäpuhtauksien vaikutus huomioon. Tarkemmin on perehdytty monokaliumfosfaatin kiteytykseen ja kolmenarvoisten kationeiden, Al3+, Fe3+ ja Cr3+, vaikutukseen kiteiden kasvuun. Kolmenarvoiset metalli-ionit adsorboituvat kiteen pintaan haitaten kiteenkasvua, mikä vaikuttaa erityisesti kiteen prismapinnan kasvuun. Lisäksi on esitelty muita kiteenkasvuun vaikuttavia olosuhteita. Lopuksi on käsitelty kompleksinmuodostajia metalli-ionien haitallisten vaikutusten ehkäisijöinä. Kokeellisessa osassa suoritettiin liukoisuuskokeita monokaliumfosfaatin liukoisuuden selvittämiseksi eri pH-olosuhteissa. Suoritetuissa yksikidekokeissa tutkittiin pH:n ja kolmenarvoisten kationeiden; Al3+, Fe3+ ja Cr3+, vaikutus monokaliumfosfaattikiteen pituus- ja leveyskasvuun ja kidemuotoon eri ylikylläisyyksillä. Lisäksi tutkittiin voidaanko lämpötilaa ja pH muuttamalla tai pyrofosfaattia lisäämällä poistaa raudan kasvua inhiboima vaikutus. Kiteytyslämpötilaa nostamalla voidaan poistaa raudan haitallinen vaikutus kiteen kasvuun.
Resumo:
Direct leaching is an alternative to conventional roast-leach-electrowin (RLE) zinc production method. The basic reaction of direct leach method is the oxidation of sphalerite concentrate in acidic liquid by ferric iron. The reaction mechanism and kinetics, mass transfer and current modifications of zinc concentrate direct leaching process are considered. Particular attention is paid to the oxidation-reduction cycle of iron and its role in direct leaching of zinc concentrate, since it can be one of the limiting factors of the leaching process under certain conditions. The oxidation-reduction cycle of iron was experimentally studied with goal of gaining new knowledge for developing the direct leaching of zinc concentrate. In order to obtain this aim, ferrous iron oxidation experiments were carried out. Affect of such parameters as temperature, pressure, sulfuric acid concentration, ferrous iron and copper concentrations was studied. Based on the experimental results, mathematical model of the ferrous iron oxidation rate was developed. According to results obtained during the study, the reaction rate orders for ferrous iron concentration, oxygen concentration and copper concentration are 0.777, 0.652 and 0.0951 respectively. Values predicted by model were in good concordance with the experimental results. The reliability of estimated parameters was evaluated by MCMC analysis which showed good parameters reliability.
Resumo:
By alloying metals with other materials, one can modify the metal’s characteristics or compose an alloy which has certain desired characteristics that no pure metal has. The field is vast and complex, and phenomena that govern the behaviour of alloys are numerous. Theories cannot penetrate such complexity, and the scope of experiments is also limited. This is why the relatively new field of ab initio computational methods has much to give to this field. With these methods, one can extend the understanding given by theories, predict how some systems might behave, and be able to obtain information that is not there to see in physical experiments. This thesis pursues to contribute to the collective knowledge of this field in the light of two cases. The first part examines the oxidation of Ag/Cu, namely, the adsorption dynamics and oxygen induced segregation of the surface. Our results demonstrate that the presence of Ag on the Cu(100) surface layer strongly inhibits dissociative adsorption. Our results also confirmed that surface reconstruction does happen, as experiments predicted. Our studies indicate that 0.25 ML of oxygen is enough for Ag to diffuse towards the bulk, under the copper oxide layer. The other part elucidates the complex interplay of various energy and entropy contributions to the phase stability of paramagnetic duplex steel alloys. We were able to produce a phase stability map from first principles, and it agrees with experiments rather well. Our results also show that entropy contributions play a very important role on defining the phase stability. This is, to the author’s knowledge, the first ab initio study upon this subject.
Resumo:
Magnetic nanoparticles are very important in modern industry. These particles are used in many different spheres of life. Nanoparticles have unusual physical and chemical properties connected both with quantum dimensional effects and with the increased role of the surface atoms. Most clearly the difference between the properties of bulk materials and nanoparticles can be seen in the magnetic properties of these materials. The most typical magnetic properties of nanomaterials are superparamagnetism with the size of the cluster from 1 to 10 nm; single-domain magnetic state of nanoclusters and nanostructures up to 20 nm; magnetization processes connected with magnetic cluster ordering and with its forms and sizes; quantum magnetic tunneling effects when magnetization changes by jumps and giant magnetoresistance effects. For research of the magnetic properties of iron-containing nanostructures, it is convenient to apply Mӧssbauer spectroscopy. In this work a number of nano-sized samples of iron oxides were examined by Mössbauer spectroscopy. The Mössbauer spectra of nanoparticles with various sizes were obtained. Mössbauer spectra of iron oxide nanoparticles were compared with the spectra of bulk samples. It was shown how the spectra of iron oxide nanoparticles change depending on the particle sizes.
Resumo:
This thesis is part of the Arctic Materials Technologies Development –project, which aims to research and develop manufacturing techniques, especially welding, for Arctic areas. The main target of this paper is to clarify what kind of European metallic materials are used, or can be used, in Arctic. These materials include mainly carbon steels but also stainless steels and aluminium and its alloys. Standardized materials, their properties and also some recent developments are being introduced. Based on this thesis it can be said that carbon steels (shipbuilding and pipeline steels) have been developed based on needs of industry and steels exist, which can be used in Arctic areas. Still, these steels cannot be fully benefited, because rules and standards are under development. Also understanding of fracture behavior of new ultra high strength steels is not yet good enough, which means that research methods (destructive and non-destructive methods) need to be developed too. The most of new nickel-free austenitic and austenitic-ferritic stainless steels can be used in cold environment. Ferritic and martensitic stainless steels are being developed for better weldability and these steels are mainly developed in nuclear industry. Aluminium alloys are well suitable for subzero environment and these days high strength aluminium alloys are available also as thick sheets. Nanotechnology makes it possible to manufacture steels, stainless steels and aluminium alloys with even higher strength. Joining techniques needs to be developed and examined properly to achieve economical and safe way to join these modern alloys.
Resumo:
The quasiclassical approach was applied to the investigation of the vortex properties in the ironbased superconductors. The special attention was paid to manifestation of the nonlocal effects of the vortex core structure. The main results are as follows: (i) The effects of the pairing symmetries (s+ and s₊₊) on the cutoff parameter of field distribution, ξh, in stoichiometric (like LiFeAs) and nonstoichiometric (like doped BaFe₂As₂) iron pnictides have been investigated using Eilenberger quasiclassical equations. Magnetic field, temperature and impurity scattering dependences of ξh have been calculated. Two opposite behavior have been discovered. The ξh /ξc2 ratio is less in s+ symmetry when intraband impurity scattering (Γ₀) is much larger than one and much larger than interband impurity scattering (Γπ), i.e. in nonstoichiometric iron pnictides. Opposite, the value ξh /ξc2 is higher in s+ case and the field dependent curve is shifted upward from the "clean" case (Γ₀ = Γπ = 0) for stoichiometric iron pnictides (Γ₀ = Γπ ≪ 1). (ii) Eilenberger approach to the cutoff parameter, ξh, of the field distribution in the mixed state of high
Resumo:
The dewatering of iron ore concentrates requires large capacity in addition to producing a cake with low moisture content. Such large processes are commonly energy intensive and means to lower the specific energy consumption are needed. Ceramic capillary action disc filters incorporate a novel filter medium enabling the harnessing of capillary action, which results in decreased energy consumption in comparison to traditional filtration technologies. As another benefit, the filter medium is mechanically and chemically more durable than, for example, filter cloths and can, thus, withstand harsh operating conditions and possible regeneration better than other types of filter media. In iron ore dewatering, the regeneration of the filter medium is done through a combination of several techniques: (1) backwashing, (2) ultrasonic cleaning, and (3) acid regeneration. Although it is commonly acknowledged that the filter medium is affected by slurry particles and extraneous compounds, published research, especially in the field of dewatering of mineral concentrates, is scarce. Whereas the regenerative effect of backwashing and ultrasound are more or less mechanical, regeneration with acids is based on chemistry. The chemistry behind the acid regeneration is, naturally, dissolution. The dissolution of iron oxide particles has been extensively studied over several decades but those studies may not necessarily be directly applicable in the regeneration of the filter medium which has undergone interactions with the slurry components. The aim of this thesis was to investigate if free particle dissolution indeed correlates with the regeneration of the filter medium. For this purpose, both free particle dissolution and dissolution of surface adhered particles were studied. The focus was on acidic dissolution of iron oxide particles and on the study of the ceramic filter medium used in the dewatering of iron ore concentrates. The free particle dissolution experiments show that the solubility of synthetic fine grained iron oxide particles in oxalic acid could be explained through linear models accounting for the effects of temperature and acid concentration, whereas the dissolution of a natural magnetite is not so easily explained by such models. In addition, the kinetic experiments performed both support and contradict the work of previous authors: the suitable kinetic model here supports previous research suggesting solid state reduction to be the reaction mechanism of hematite dissolution but the formation of a stable iron oxalate is not supported by the results of this research. Several other dissolution mechanisms have also been suggested for iron oxide dissolution in oxalic acid, indicating that the details of oxalate promoted reductive dissolution are not yet agreed and, in this respect, this research offers added value to the community. The results of the regeneration experiments with the ceramic filter media show that oxalic acid is highly effective in removing iron oxide particles from the surface of the filter medium. The dissolution of those particles did not, however, exhibit the expected behaviour, i.e. complete dissolution. The results of this thesis show that although the regeneration of the ceramic filter medium with acids incorporates the dissolution of slurry particles from the surface of the filter medium, the regeneration cannot be assessed purely based upon free particle dissolution. A steady state, dependent on temperature and on the acid concentration, was observed in the dissolution of particles from the surface even though the limit of solubility of free iron oxide particles had not been reached. Both the regeneration capacity and efficiency, with regards to the removal of iron oxide particles, was found to be temperature dependent, but was not affected by the acid concentration. This observation further suggests that the removal of the surface adhered particles does not follow the dissolution of free particles, which do exhibit a dependency on the acid concentration. In addition, changes in the permeability and in the pore structure of the filter medium were still observed after the bulk concentration of dissolved iron had reached a steady state. Consequently, the regeneration of the filter medium continued after the dissolution of particles from the surface had ceased. This observation suggests that internal changes take place at the final stages of regeneration. The regeneration process could, in theory, be divided into two, possibly overlapping, stages: (1) dissolution of surface-adhered particles, and (2) dissolution of extraneous compounds from within the pore structure. In addition to the fundamental knowledge generated during this thesis, tools to assess the effects of parameters on the regeneration of the ceramic filter medium are needed. It has become clear that the same tools used to estimate the dissolution of free particles cannot be used to estimate the regeneration of a filter medium unless only a robust characterisation of the order of regeneration efficiency is needed.
Resumo:
Iron ore treatment processes are usually continuous and high tonnage and filtration equipment has to meet these requirements. In magnetite (Fe3O4) treatment process continuous rotary disc filters are often used for filtration. Carbon dioxide (CO2) treatment is a fairly novel and un-known filtration enhancing process. The interest to use CO2 is quite high because CO2 is a greenhouse gas that is abundant, readily available and capture and use of CO2 would be environmentally beneficial. The focus of this thesis was to investigate if CO2 could be used to enhance the filtration of magnetite with ceramic disc filter. Previous studies have suggested that CO2 could be used to enhance the filtration properties of different iron ores thus increasing the filtration capacity. In the literature part, the basic theory of filtration and the particle properties affecting filtration were discussed. The basic steps of a typical ore treatment process were presented. The reasons why CO2 might enhance the filtration properties of different ores were investigated. A literature survey of earlier studies of CO2 addition as a filter aid was presented and the basic chemical properties and reactions of CO2 were also discussed. The experimental part was done at the LUT Laboratory of Separation Technology using different magnetite samples from the industry. The filtration experiments indicated that CO2 had a positive influence on the filtration properties of magnetite slurry. Zeta potential of untreated and CO2 treated magnetite was measured and CO2 treated magnetite had lower zeta potential values than the untreated magnetite. The filtration capacity was increased while the cake moisture levels were only slightly increased.
Resumo:
Oxidized starch is a key component in the paper industry, where it is used as both surfacing sizer and filler. Large quantities are annually used for this purpose; however, the methods for the oxidation are not environmentally friendly. In our research, we have studied the possibility to replace the harmful oxidation agents, such as hypochlorite or iodates and transition metal catalysts, with a more environmentally friendly oxidant, hydrogen peroxide (H2O2), and a special metal complex catalyst (FePcS), of which only a small amount is needed. The work comprised batch and semi-batch studies by H2O2, ultrasound studies of starch particles, determination of low-molecular by-products and determination of the decomposition kinetics of H2O2 in the presence of starch and the catalyst. This resulted in a waste-free oxidation method, which only produces water and oxygen as side products. The starch oxidation was studied in both semi-batch and batch modes in respective to the oxidant (H2O2) addition. The semi-batch mode proved to yield a sufficient degree of substitution (COOH groups) for industrial purposes. Treatment of starch granules by ultrasound was found to improve the reactivity of starch. The kinetic results were found out to have a rather complex pattern – several oxidation phases were observed, apparently due to the fact that the oxidation reaction in the beginning only took place on the surface, whereas after a prolonged reaction time, partial degradation of the solid starch granules allowed further reaction in the interior parts. Batch-mode experiments enabled a more detailed study of the mechanisms of starch in the presence of H2O2 and the catalyst, but yielded less oxidized starch due to rapid decomposition of H2O2 due to its high concentrations. The effect of the solid-liquid (S/L) ratio in the reaction system was studied in batch experiments. These studies revealed that the presence of the catalyst and the starch enhance the H2O2 decomposition.
Resumo:
The iron ore pelletizing process consumes high amounts of energy, including nonrenewable sources, such as natural gas. Due to fossil fuels scarcity and increasing concerns regarding sustainability and global warming, at least partial substitution by renewable energy seems inevitable. Gasification projects are being successfully developed in Northern Europe, and large-scale circulating fluidized bed biomass gasifiers have been commissioned in e.g. Finland. As Brazil has abundant biomass resources, biomass gasification is a promising technology in the near future. Biomasses can be converted into product gas through gasification. This work compares different technologies, e.g. air, oxygen and steam gasification, focusing on the use of the product gas in the indurating machine. The use of biosynthetic natural gas is also evaluated. Main parameters utilized to assess the suitability of product gas were adiabatic flame temperature and volumetric flow rate. It was found that low energy content product gas could be utilized in the traveling grate, but it would require burner’s to be changed. On the other hand, bio-SGN could be utilized without any adaptions. Economical assessment showed that all gasification plants are feasible for sizes greater than 60 MW. Bio-SNG production is still more expensive than natural gas in any case.
Resumo:
The superconducting gap is a basic character of a superconductor. While the cuprates and conventional phonon-mediated superconductors are characterized by distinct d- and s-wave pairing symmetries with nodal and nodeless gap distributions respectively, the superconducting gap distributions in iron-based superconductors are rather diversified. While nodeless gap distributions have been directly observed in Ba1–xKxFe2As2, BaFe2–xCoxAs2, LiFeAs, KxFe2–ySe2, and FeTe1–xSex, the signatures of a nodal superconducting gap have been reported in LaOFeP, LiFeP, FeSe, KFe2As2, BaFe2–xRuxAs2, and BaFe2(As1–xPx)2. Due to the multiplicity of the Fermi surface in these compounds s± and d pairing states can be both nodeless and nodal. A nontrivial orbital structure of the order parameter, in particular the presence of the gap nodes, leads to effects in which the disorder is much richer in dx2–y2-wave superconductors than in conventional materials. In contrast to the s-wave case, the Anderson theorem does not work, and nonmagnetic impurities exhibit a strong pair-breaking influence. In addition, a finite concentration of disorder produces a nonzero density of quasiparticle states at zero energy, which results in a considerable modification of the thermodynamic and transport properties at low temperatures. The influence of order parameter symmetry on the vortex core structure in iron-based pnictide and chalcogenide superconductors has been investigated in the framework of quasiclassical Eilenberger equations. The main results of the thesis are as follows. The vortex core characteristics, such as, cutoff parameter, ξh, and core size, ξ2, determined as the distance at which density of the vortex supercurrent reaches its maximum, are calculated in wide temperature, impurity scattering rate, and magnetic field ranges. The cutoff parameter, ξh(B; T; Г), determines the form factor of the flux-line lattice, which can be obtained in _SR, NMR, and SANS experiments. A comparison among the applied pairing symmetries is done. In contrast to s-wave systems, in dx2–y2-wave superconductors, ξh/ξc2 always increases with the scattering rate Г. Field dependence of the cutoff parameter affects strongly on the second moment of the magnetic field distributions, resulting in a significant difference with nonlocal London theory. It is found that normalized ξ2/ξc2(B/Bc2) dependence is increasing with pair-breaking impurity scattering (interband scattering for s±-wave and intraband impurity scattering for d-wave superconductors). Here, ξc2 is the Ginzburg-Landau coherence length determined from the upper critical field Bc2 = Φ0/2πξ2 c2, where Φ0 is a flux quantum. Two types of ξ2/ξc2 magnetic field dependences are obtained for s± superconductors. It has a minimum at low temperatures and small impurity scattering transforming in monotonously decreasing function at strong scattering and high temperatures. The second kind of this dependence has been also found for d-wave superconductors at intermediate and high temperatures. In contrast, impurity scattering results in decreasing of ξ2/ξc2(B/Bc2) dependence in s++ superconductors. A reasonable agreement between calculated ξh/ξc2 values and those obtained experimentally in nonstoichiometric BaFe2–xCoxAs2 (μSR) and stoichiometric LiFeAs (SANS) was found. The values of ξh/ξc2 are much less than one in case of the first compound and much more than one for the other compound. This is explained by different influence of two factors: the value of impurity scattering rate and pairing symmetry.
Resumo:
The iron and steelmaking industry is among the major contributors to the anthropogenic emissions of carbon dioxide in the world. The rising levels of CO2 in the atmosphere and the global concern about the greenhouse effect and climate change have brought about considerable investigations on how to reduce the energy intensity and CO2 emissions of this industrial sector. In this thesis the problem is tackled by mathematical modeling and optimization using three different approaches. The possibility to use biomass in the integrated steel plant, particularly as an auxiliary reductant in the blast furnace, is investigated. By pre-processing the biomass its heating value and carbon content can be increased at the same time as the oxygen content is decreased. As the compression strength of the preprocessed biomass is lower than that of coke, it is not suitable for replacing a major part of the coke in the blast furnace burden. Therefore the biomass is assumed to be injected at the tuyere level of the blast furnace. Carbon capture and storage is, nowadays, mostly associated with power plants but it can also be used to reduce the CO2 emissions of an integrated steel plant. In the case of a blast furnace, the effect of CCS can be further increased by recycling the carbon dioxide stripped top gas back into the process. However, this affects the economy of the integrated steel plant, as the amount of top gases available, e.g., for power and heat production is decreased. High quality raw materials are a prerequisite for smooth blast furnace operation. High quality coal is especially needed to produce coke with sufficient properties to ensure proper gas permeability and smooth burden descent. Lower quality coals as well as natural gas, which some countries have in great volumes, can be utilized with various direct and smelting reduction processes. The DRI produced with a direct reduction process can be utilized as a feed material for blast furnace, basic oxygen furnace or electric arc furnace. The liquid hot metal from a smelting reduction process can in turn be used in basic oxygen furnace or electric arc furnace. The unit sizes and investment costs of an alternative ironmaking process are also lower than those of a blast furnace. In this study, the economy of an integrated steel plant is investigated by simulation and optimization. The studied system consists of linearly described unit processes from coke plant to steel making units, with a more detailed thermodynamical model of the blast furnace. The results from the blast furnace operation with biomass injection revealed the importance of proper pre-processing of the raw biomass as the composition of the biomass as well as the heating value and the yield are all affected by the pyrolysis temperature. As for recycling of CO2 stripped blast furnace top gas, substantial reductions in the emission rates are achieved if the stripped CO2 can be stored. However, the optimal recycling degree together with other operation conditions is heavily dependent on the cost structure of CO2 emissions and stripping/storage. The economical feasibility related to the use of DRI in the blast furnace depends on the price ratio between the DRI pellets and the BF pellets. The high amount of energy needed in the rotary hearth furnace to reduce the iron ore leads to increased CO2 emissions.
Resumo:
Systemic iron overload (IO) is considered a principal determinant in the clinical outcome of different forms of IO and in allogeneic hematopoietic stem cell transplantation (alloSCT). However, indirect markers for iron do not provide exact quantification of iron burden, and the evidence of iron-induced adverse effects in hematological diseases has not been established. Hepatic iron concentration (HIC) has been found to represent systemic IO, which can be quantified safely with magnetic resonance imaging (MRI), based on enhanced transverse relaxation. The iron measurement methods by MRI are evolving. The aims of this study were to implement and optimise the methodology of non-invasive iron measurement with MRI to assess the degree and the role of IO in the patients. An MRI-based HIC method (M-HIC) and a transverse relaxation rate (R2*) from M-HIC images were validated. Thereafter, a transverse relaxation rate (R2) from spin-echo imaging was calibrated for IO assessment. Two analysis methods, visual grading and rSI, for a rapid IO grading from in-phase and out-of-phase images were introduced. Additionally, clinical iron indicators were evaluated. The degree of hepatic and cardiac iron in our study patients and IO as a prognostic factor in patients undergoing alloSCT were explored. In vivo and in vitro validations indicated that M-HIC and R2* are both accurate in the quantification of liver iron. R2 was a reliable method for HIC quantification and covered a wider HIC range than M-HIC and R2*. The grading of IO was able to be performed rapidly with the visual grading and rSI methods. Transfusion load was more accurate than plasma ferritin in predicting transfusional IO. In patients with hematological disorders, the prevalence of hepatic IO was frequent, opposite to cardiac IO. Patients with myelodysplastic syndrome were found to be the most susceptible to IO. Pre-transplant IO predicted severe infections during the early post-transplant period, in contrast to the reduced risk of graft-versus-host disease. Iron-induced, poor transplantation results are most likely to be mediated by severe infections.