62 resultados para Laser deposition

em Doria (National Library of Finland DSpace Services) - National Library of Finland, Finland


Relevância:

100.00% 100.00%

Publicador:

Resumo:

Due to font problem on the tilte field the titlte of the thesis is corrected here. The title of the thesis is: Superconducting properties and their enhancement in ReBa2Cu3O7-delta (RE = Y and Gd) films prepared by pulsed laser deposition

Relevância:

60.00% 60.00%

Publicador:

Resumo:

In this work, a colossal magnetoresistive (CMR) Pr1−xCaxMnO3 (PCMO) man- ganite thin films and polycrystalline samples were studied with the main focus on the properties of the insulator to metal Mott phase transition. The polycrystalline PCMO samples were fabricated with the solid state reaction method. The polycrystalline sam- ples were further processed into the epitaxial thin films with the pulsed laser deposition method (PLD). The structural and magnetic properties of the samples were systemat- ically investigated and the thin films samples were further investigated with magneto- transport measurement where the thin films response to illumination was also studied. After the successful synthesis of polycrystalline PCMO samples with varying x = between 0.0 - 0.5, the magnetic characterization of the samples showed rich magnetic properties having the signatures of the magnetic phase coexistence of antiferromag- netic (AFM) and ferromagnetic (FM) ordering and cluster glass behaviour. With the increased doping concentration from x = 0.3 to 0.5, the AFM charge-order (CO) phase started to form up being strongest on the sample x = 0.5. This AFM CO phase could be melted with the high external magnetic field at temperatures below Neel’s tempera- ture TN inducing an irreversible first order metamagnetic AFM to FM phase transition. The strength of the AFM CO phase decreased with decreasing Ca concentration and increasing temperature. The polycrystalline PCMO samples with Ca concentrations of 0.3 - 0.5, showing metamagnetic behaviour, were selected for the fabrication of the thin film samples. The films were grown using two different in situ oxygen treatment temperatures at 500 ◦C and 700 ◦C in the PLD system. The films with x = 0.4 and 0.5 showed weaker AFM CO phase with greatly reduced melting fields when compared to polycrystalline samples. Also, the robustness of the AFM CO phase was further decreased in thin films with the lower oxygen treatment temperature of 500 ◦C. The magneto-transport measurements made on the thin films showed that the melting of AFM CO phase was connected to CMR effect where the increasing magnetic field induced an insulator to metal phase transition, which reduces the resistivity of the film around nine orders of magnitude. The use of illumination during the magneto-transport measurements showed a vari- ety of intriguing phenomena including magnetophotoresistance. The illumination had a huge effect to the insulator to metal transition (IMT) reducing the transition magnetic field significantly. Moreover, by magnetically biasing the thin films with the constant external magnetic field, the IMT could be induced by switching on the illumination.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The purpose of this study is to find out how laser based Directed Energy Deposition processes can benefit from different types of monitoring. DED is a type of additive manufacturing process, where parts are manufactured in layers by using metallic powder or metallic wire. DED processes can be used to manufacture parts that are not possible to manufacture with conventional manufacturing processes, when adding new geometries to existing parts or when wanting to minimize the scrap material that would result from machining the part. The aim of this study is to find out why laser based DED-processes are monitored, how they are monitored and what devices are used for monitoring. This study has been done in the form of a literature review. During the manufacturing process, the DED-process is highly sensitive to different disturbances such as fluctuations in laser absorption, powder feed rate, temperature, humidity or the reflectivity of the melt pool. These fluctuations can cause fluctuations in the size of the melt pool or its temperature. The variations in the size of the melt pool have an effect on the thickness of individual layers, which have a direct impact on the final surface quality and dimensional accuracy of the parts. By collecting data from these fluctuations and adjusting the laser power in real-time, the size of the melt pool and its temperature can be kept within a specified range that leads to significant improvements in the manufacturing quality. The main areas of monitoring can be divided into the monitoring of the powder feed rate, the temperature of the melt pool, the height of the melt pool and the geometry of the melt pool. Monitoring the powder feed rate is important when depositing different material compositions. Monitoring the temperature of the melt pool can give information about the microstructure and mechanical properties of the part. Monitoring the height and the geometry of the melt pool is an important factor in achieving the desired dimensional accuracy of the part. By combining multiple different monitoring devices, the amount of fluctuations that can be controlled will be increased. In addition, by combining additive manufacturing with machining, the benefits of both processes could be utilized.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Selostus: Kasvien raskasmetallien otto ilmasta ja saastuneesta maasta

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Perinteisten kaarihitsausmenetelmien suhteellisen suuri lämmöntuonti aiheuttaa huomattavia muodonmuutoksia laivan rungon valmistusprosessin alkuvaiheessa. Muodonmuutosten seurauksena rakenteiden mitta- ja muototarkkuus heikkenee, mikä lisää oikaisu- ja sovitustyötä myöhemmissä työvaiheissa. Hitsausmuodonmuutoksia voidaan vähentää siirtymällä käyttämään laser-MAG-hybridihitsausta, jossa lämmöntuonti on merkittävästi pienempi kuin kaarihitsauksessa. Näin kyetään oleellisesti leikkaamaan oikaisu- ja sovitustyöstä syntyviä kustannuksia. Tämän diplomityön tavoitteena oli kehittää tuotantovalmiiksi kuitulaser- ja MAG-hitsauksen yhdistelmäprosessi Aker Yards Oy:n Turun telakalla loppuvuoden 2006 aikana. Hitsauslaitteiston asennus oli valmistunut kesäkuussa 2006, minkä jälkeen aloitettiin luokituslaitoksen hyväksymän koeohjelman hitsaukset. Käyttöönotto suunnitelmaan sisältyvä koehitsausohjelma oli laadittu Det Norske Veritaksen julkaisemaa ohjetta (Guidelines no. 19) mukaillen. Ensimmäiseksi määritettiin hitsauskokeiden avulla prosessille laadun ja tehokkuuden suhteen optimaalinen railogeometria. Seuraavaksi optimoitiin prosessin hitsausparametrit 6 mm:n aineenpaksuudelle hyödyntäen Taguchi-koesuunnittelumenetelmää. Tämän jälkeen optimiparametreilla hitsattiin koekappale väsytyskokeisiin, jotka suoritettiin Teknillisen korkeakoulun laivalaboratoriossa. Väsytyskoetulokset täyttivät luokituslaitoksen vaatimukset. Myös hitsauksen menetelmäkoe suoritettiin hyväksytetysti. Viimeinen koeohjelman mukainen hitsauskoesarja tehtiin prosessiparametrien sallittujen vaihtelurajojen määrittämiseksi. Diplomityön tavoite täyttyi joulukuussa 2006, jolloin 'laivan kansipaneeli hitsattiin ensimmäistä kertaa uudella hitsausprosessilla. Hitsauksen laatu korreloi hyvin menetelmäkokeen tulosten kanssa ¿ hitsit olivat tasalaatuisia ja ne täyttivät B-luokan vaatimukset.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The purpose of this thesis is to reveal how the laser cutting parameters influence lasercutting of particleboard, HDF and MDF. The literature review introduces the basic principle of CO2 laser, CO2 laser equipment and its usage in cutting of wood-based materials. The experimental part focuses on the discussion and analysis ofthe test data and attempts to draw conclusions on the influence of various parameters, including laser power, focal length of the lens and cutting gas, on the cutting speed and kerf quality. The tested materials include various thicknesses of particleboard, HDF and MDF samples. A TRUMPF TLF2700 HQ laser equipment was used for the experiments. To obtain valid data, the test samples must be completely cut through without any bonding of wood fibre. The maximum cutting speed is linear dependent on the laser power in thecondition that the other parameters are constant. For each thickness of a specific material type, there is a minimum laser power for cutting. Normally, the topand bottom kerf widths increase with the enhancement of laser power. There may be a critical laser power which can generate the minimum cross-sectional kerf width. Lens of larger focal length may achieve higher cutting speed. As the focal length becomes larger, the top kerf width tends to increase while the bottom andcross-sectional kerf widths to the opposite. Of all cutting gases, oxygen can help achieve higher cutting speed. The gas pressure of nitrogen does not seem to have strong influence on the cutting result. Generally, 2 bar air is more preferable for higher cutting speed. For particleboard and MDF samples of larger thickness than 12 mm, 2 bar argon can be used to reach remarkably higher cutting speed than the 5 bar. Generally, the 190.5 mm lens can produce smallest total kerf width. The kerf sides of thicker samples are darker than the thinner ones. The sample darkness tends to be lower as laser power increased. 63.5 mm lens seemed tocause more darkness than other lens. 5 bar cutting gases can produce less dark side kerfs than 2 bar ones. Oxygen normally causes darker kerfs than other gases. No distinct differences were found between nitrogen and argon.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

High reflectivity and high thermal conductivity, high vapour pressure of alloyingelements as well as low liquid surface tension and low ionisation potential, make laser welding of aluminium and its alloys a demanding task.Problems that occur during welding are mainly process instabilities of the keyhole and the melt pool, increased plasma formation above the melt pool and loss of alloying elements. These problems lead to unwanted metallurgical defects like hot cracks and porosity in the weld bead andother problems concerning the shape and appearance of the weld bead. In order to minimise the defects and improve the weld quality, the process and beam parameters need to be carefully adjusted along with a consideration concerning the use of filler wire for the welding process. In this work the welding of 3,0 mm thick grade 5083 aluminium alloy plates using a 3,0 kW Nd:YAG laser with grade 5183 filler wire addition is investigated. The plates were welded as butt joints with air gap sizes 0,5 mm, 0,7mm and 1,0 mm. The analysis of the weld beads obtained from the weldedsamples showed that the least imperfections were produced with 0,7 mm air gaps at moderate welding speeds. The analysis also covered the calculation of the melting efficiency and the study of the shape of the weld bead. The melting efficiency was on average around 20 % for the melting process of the welded plates. The weld beads showed the characteristic V-shape of a laser weld and retained this shape during the whole series of experiments.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

High reflectivity to laser light, alloying element evaporation during high power laser welding makes aluminium alloys highly susceptibility to weld defects such as porosity, cracking and undercutting. The dynamic behaviour of the keyhole, due to fluctuating plasma above the keyhole and the vaporization ofthe alloying elements with in the keyhole, is the key problem to be solved for the improvement of the weld quality and stabilization of the keyhole dynamics isperhaps the single most important development that can broaden the application of laser welding of aluminium alloys. In laser welding, the shielding gas is commonly used to stabilize the welding process, to improve the welded joint features and to protect the welded seam from oxidation. The chemicalcomposition of the shielding gas is a key factor in achieving the final qualityof the welded joints. Wide range of shielding gases varying from the pure gasesto complex mixtures based on helium, argon, nitrogen and carbon dioxide are commercially available. These gas mixtures should be considered in terms of their suitability during laser welding of aluminium alloys to produce quality welds. The main objective of the present work is to study the effect of the shielding gascomposition during laser welding of aluminium alloys. Aluminium alloy A15754 was welded using 3kW Nd-YAG laser (continuous wave mode). The alloy samples were butt welded with different shielding gases (pure and mixture of gases) so that high quality welds with high joint efficiencies could be produced. It was observed that the chemical composition of the gases influenced the final weld quality and properties. In general, the mixture gases, in correct proportions, enabled better utilisation of the properties of the mixing gases, stabilized the welding process and produced better weld quality compared to the pure shielding gases.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The thin disk and fiber lasers are new solid-state laser technologies that offer a combinationof high beam quality and a wavelength that is easily absorbed by metal surfacesand are expected to challenge the CO2 and Nd:YAG lasers in cutting of metals ofthick sections (thickness greater than 2mm). This thesis studied the potential of the disk and fiber lasers for cutting applications and the benefits of their better beam quality. The literature review covered the principles of the disk laser, high power fiber laser, CO2 laser and Nd:YAG laser as well as the principle of laser cutting. The cutting experiments were made with thedisk, fiber and CO2 lasers using nitrogen as an assist gas. The test material was austenitic stainless steel of sheet thickness 1.3mm, 2.3mm, 4.3mm and 6.2mm for the disk and fiber laser cutting experiments and sheet thickness of 1.3mm, 1.85mm, 4.4mm and 6.4mm for the CO2 laser cutting experiments. The experiments focused on the maximum cutting speeds with appropriate cut quality. Kerf width, cutedge perpendicularity and surface roughness were the cut characteristics used to analyze the cut quality. Attempts were made to draw conclusions on the influence of high beam quality on the cutting speed and cut quality. The cutting speeds were enormous for the disk and fiber laser cutting experiments with the 1.3mm and 2.3mm sheet thickness and the cut quality was good. The disk and fiber laser cutting speeds were lower at 4.3mm and 6.2mm sheet thickness but there was still a considerable percentage increase in cutting speeds compared to the CO2 laser cutting speeds at similar sheet thickness. However, the cut quality for 6.2mm thickness was not very good for the disk and fiber laser cutting experiments but could probably be improved by proper selection of cutting parameters.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Tässä työssä raportoidaan hybridihitsauksesta otettujen suurnopeuskuvasarjojen automaattisen analyysijärjestelmän kehittäminen.Järjestelmän tarkoitus oli tuottaa tietoa, joka avustaisi analysoijaa arvioimaan kuvatun hitsausprosessin laatua. Tutkimus keskittyi valokaaren taajuuden säännöllisyyden ja lisäainepisaroiden lentosuuntien mittaamiseen. Valokaaria havaittiin kuvasarjoista sumean c-means-klusterointimenetelmän avullaja perättäisten valokaarien välistä aikaväliä käytettiin valokaaren taajuuden säännöllisyyden mittarina. Pisaroita paikannettiin menetelmällä, jossa yhdistyi pääkomponenttianalyysi ja tukivektoriluokitin. Kalman-suodinta käytettiin tuottamaan arvioita pisaroiden lentosuunnista ja nopeuksista. Lentosuunnanmääritysmenetelmä luokitteli pisarat niiden arvioitujen lentosuuntien perusteella. Järjestelmän kehittämiseen käytettävissä olleet kuvasarjat poikkesivat merkittävästi toisistaan kuvanlaadun ja pisaroiden ulkomuodon osalta, johtuen eroista kuvaus- ja hitsausprosesseissa. Analyysijärjestelmä kehitettiin toimimaan pienellä osajoukolla kuvasarjoja, joissa oli tietynlainen kuvaus- ja hitsausprosessi ja joiden kuvanlaatu ja pisaroiden ulkomuoto olivat samankaltaisia, mutta järjestelmää testattiin myös osajoukon ulkopuolisilla kuvasarjoilla. Testitulokset osoittivat, että lentosuunnanmääritystarkkuus oli kohtuullisen suuri osajoukonsisällä ja pieni muissa kuvasarjoissa. Valokaaren taajuuden säännöllisyyden määritys oli tarkka useammassa kuvasarjassa.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fiber laser for materials processing have undergone a rapid development in the pastseveral years. As fiber laser provides a combination of high beam quality and awavelength that is easily absorbed by metal surfaces, the named future laser isexpected to challenge the CO2 and Nd:YAG lasers in the area of metal cutting. This thesis studied the performance of fiber laser cutting mild steel. In the literature review part, it introduced the laser cutting principle and the principle of fiber laser including the newest development of fiber laser cuttingtechnology. Because the fiber laser cutting mild steel is a very young technology, a preliminary test was made in order to investigate effect of the cutting parameters on cut quality. Then the formal fiber laser cutting experiment was madeby using 3 mm thickness S355 steel with oxygen as assistant gas. The experimentwas focused on the cut quality with maximum cutting speed and minimum oxygen gas pressure. And the cut quality is mainly decided by the kerf width, perpendicularity tolerance, surface roughness and striation patterns. After analysis the cutting result, several conclusions were made. Although the best result got in the experiment is not perfect as predicted, the whole result of the test can be accepted. Compared with CO2 laser, a higher cutting speed was achieved by fiber laser with very low oxygen gas pressure. A further improvement about the cutting quality might be possible by proper selection of process parameters. And in order to investigate the cutting performance more clearly, a future study about cutting different thickness mild steel and different shape was recommended.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This research has been focused at the development of a tuned systematic design methodology, which gives the best performance in a computer aided environment and utilises a cross-technological approach, specially tested with and for laser processed microwave mechanics. A tuned design process scheme is also presented. Because of the currently large production volumes of microwave and radio frequency mechanics even slight improvements of design methodologies or manufacturing technologies would give reasonable possibilities for cost reduction. The typical number of required iteration cycles could be reduced to one fifth of normal. The research area dealing with the methodologies is divided firstly into a function-oriented, a performance-oriented or a manufacturability-oriented product design. Alternatively various approaches can be developed for a customer-oriented, a quality-oriented, a cost-oriented or an organisation-oriented design. However, the real need for improvements is between these two extremes. This means that the effective methodology for the designers should not be too limited (like in the performance-oriented design) or too general (like in the organisation-oriented design), but it should, include the context of the design environment. This is the area where the current research is focused. To test the developed tuned design methodology for laser processing (TDMLP) and the tuned optimising algorithm for laser processing (TOLP), seven different industrial product applications for microwave mechanics have been designed, CAD-modelled and manufactured by using laser in small production series. To verify that the performance of these products meets the required level and to ensure the objectiveness ofthe results extensive laboratory tests were used for all designed prototypes. As an example a Ku-band horn antenna can be laser processed from steel in 2 minutes at the same time obtaining a comparable electrical performance of classical aluminium units or the residual resistance of a laser joint in steel could be limited to 72 milliohmia.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Raaka-aineen hiukkaskoko on lääkekehityksessä keskeinen materiaaliparametri. Lääkeaineen partikkelikoko vaikuttaa moneen lääketuotteen tärkeään ominaisuuteen, esimerkiksi lääkkeen biologiseen hyväksikäytettävyyteen. Tässä diplomityössä keskityttiin jauhemaisten lääkeaineiden hiukkaskoon määrittämiseen laserdiffraktiomenetelmällä. Menetelmä perustuu siihen, että partikkeleista sironneen valon intensiteetin sirontakulmajakauma on riippuvainen partikkelien kokojakaumasta. Työn kirjallisuusosassa esiteltiin laserdiffraktiomenetelmän teoriaa. PIDS (Polarization Intensity Differential Scattering) tekniikka, jota voidaan käyttää laserdiffraktion yhteydessä, on myös kuvattu kirjallisuusosassa. Muihin menetelmiin perustuvista analyysimenetelmistä tutustuttiin mikroskopiaan sekä aerodynaamisen lentoajan määrittämiseen perustuvaan menetelmään. Kirjallisuusosassa esiteltiin myös partikkelikoon yleisimpiä esitystapoja. Työn kokeellisen osan tarkoituksena oli kehittää ja validoida laserdiffraktioon perustuva partikkelikoon määritysmenetelmä tietylle lääkeaineelle. Menetelmäkehitys tehtiin käyttäen Beckman Coulter LS 13 320 laserdiffraktoria. Laite mahdollistaa PIDS-tekniikan käytön laserdiffraktiotekniikan ohella. Menetelmäkehitys aloitettiin arvioimalla, että kyseinen lääkeaine soveltuu parhaiten määritettäväksi nesteeseen dispergoituna. Liukoisuuden perusteella väliaineeksi valittiin tällä lääkeaineella kyllästetty vesiliuos. Dispergointiaineen sekä ultraäänihauteen käyttö havaittiin tarpeelliseksi dispergoidessa kyseistä lääkeainetta kylläiseen vesiliuokseen. Lopuksi sekoitusnopeus näytteensyöttöyksikössä säädettiin sopivaksi. Validointivaiheessa kehitetyn menetelmän todettiin soveltuvan hyvin kyseiselle lääkeaineelle ja tulosten todettiin olevan oikeellisia sekä toistettavia. Menetelmä ei myöskään ollut herkkä pienille häiriöille.