1 resultado para LACCASE

em Doria (National Library of Finland DSpace Services) - National Library of Finland, Finland


Relevância:

10.00% 10.00%

Publicador:

Resumo:

Hemicelluloses are potential raw material for several items produced in future wood-based biorefineries. One possible method for recovering hemicelluloses from wood extracts is ultrafiltration (UF). However, low filtration capacities and severe fouling restrict the use of tight UF membranes in the treatment of wood extracts. The lack of suitable commercial membranes creates a need for pretreatment which would decrease fouling and increase the filtration capacity. This thesis focuses on the evaluation of the possibility to improve the filtration capacity and decrease fouling with the pretreatment of wood extracts. Methods which remove harmful compounds and methods which degrade them are studied, as well as combinations of the methods. The tested pretreatments have an influence on both the concentration of different compounds and the molecular mass distribution of the compounds in the extract. This study revealed that in addition to which kind of compounds were removed, also the change in molecular size distribution affected the filtration capacity significantly. It was shown that the most harmful compounds for the filtration capacity of the hydrophobic 5 kDa membrane were the ones capable of permeating the membrane and fouling also the inner membrane structure. Naturally, the size of the most harmful compounds depends on the used UF membrane and is thus case-specific. However, in the choice of the pretreatment method, the focus should be on the removal of harmful compound sizes rather than merely on the total amount of removed foulants. The results proved that filtration capacity can be increased with both adsorptive and oxidative pretreatments even by hundreds of per cents. For instance, the use of XAD7 and XAD16 adsorbents increased the average flux in the UF of a birch extract from nearly zero to 107 kg/(m2h) and 175 kg/(m2h), respectively. In the treatment of a spruce extract, oxidation by pulsed corona discharge (PCD) increased the flux in UF from 46 kg/(m2h) to 158 kg/(m2h). Moreover, when a birch extract batch was treated with laccase enzyme, the flux in UF increased from 15 kg/(m2h) to 36 kg/(m2h). However, fouling was decreased only by adsorptive pretreatment while oxidative methods had a negligible or even negative impact on it. This demonstrates that filtration capacity and fouling are affected by different compounds and mechanisms. The results of this thesis show that filtration capacity can be improved and fouling decreased through appropriate pretreatment. However, the choice of the best possible pretreatment is case-specific and depends on the wood extract and the membrane used. Finding the best option requires information on the extract content and membrane characteristics as well as on the filtration performance of the membrane in the prevailing conditions and a multivariate approach. On the basis of this study, it can be roughly concluded that adsorptive pretreatment improves the filtration capacity and decreases fouling rather reliably, but it may lead to significant hemicellulose losses. Oxidation reduces the loss of valuable hemicelluloses and could improve the filtration capacity, but fouling challenges may remain. Combining oxidation with adsorptive pretreatment was not a solution for avoiding hemicellulose losses in the tested cases.