13 resultados para the amylose content
em Iowa Publications Online (IPO) - State Library, State of Iowa (Iowa), United States
Resumo:
The Iowa State Highway Commission Laboratory is called upon to determine the cement content of hardened concrete when field problems relating to batch weights are encountered. The standard test for determining the cement content is ASTM C-85. An investigation of this method by the New Jersey State Highway Department involving duplicate samples and four cooperating laboratories produced very erratic results, however, the results obtained by this method have not been directly compared to known cement contents of concrete made with various cements and various aggregates used in Iowa.
Resumo:
The relation between the properties and the water content of an undisturbed loess were investigated to provide insight into the mechanical behavior of the natural soil. Hand-carved samples from a single deposit, at their natural water contents, and at water contents modified in the laboratory to provide a range from 870 to 3270, were subjected to unconsolidated-undrained triaxial compression tests, consolidation tests, and initial negative pore water pressure tests. In addition, the clay-size fraction was separated from the remainder of the loess for a separate series of tests to establish its properties. The natural water content of the deposit in the field was measured at regular intervals for one year to provide an example of the range in properties that would be encountered. at this site. The test results are presented and their interpretation leads to conclusions regarding the volumetric relations that exist as the water content varies. The significance of the water content in relation to the properties of the natural soil is explored and the concept of a critical water content for loess is introduced.
Resumo:
This research investigated the effects of changing the cementitious content required at a given water-to-cement ratio (w/c) on workability, strength, and durability of a concrete mixture. An experimental program was conducted in which 64 concrete mixtures with w/c ranging between 0.35 and 0.50, cementitious content ranging from 400 to 700 per cubic yard (pcy), and containing four different supplementary cementitious material (SCM) combinations were tested. The fine-aggregate to total-aggregate ratio was fixed at 0.42 and the void content of combined aggregates was held constant for all the mixtures. Fresh (i.e., slump, unit weight, air content, and setting time) and hardened properties (i.e., compressive strength, chloride penetrability, and air permeability) were determined. The hypothesis behind this study is that when other parameters are kept constant, concrete properties such as strength, chloride penetration, and air permeability will not be improved significantly by increasing the cement after a minimum cement content is used. The study found that about 1.5 times more paste is required than voids between the aggregates to obtain a minimum workability. Below this value, water-reducing admixtures are of no benefit. Increasing paste thereafter increased workability. In addition, for a given w/c, increasing cementitious content does not significantly improve compressive strength once the critical minimum has been provided. The critical value is about twice the voids content of the aggregate system. Finally, for a given w/c, increasing paste content increases chloride penetrability and air permeability.
Resumo:
This research investigated the effects of changing the cementitious content required at a given water-to-cement ratio (w/c) on workability, strength, and durability of a concrete mixture. An experimental program was conducted in which 64 concrete mixtures with w/c ranging between 0.35 and 0.50, cementitious content ranging from 400 to 700 per cubic yard (pcy), and containing four different supplementary cementitious material (SCM) combinations were tested. The fine-aggregate to total-aggregate ratio was fixed at 0.42 and the void content of combined aggregates was held constant for all the mixtures. Fresh (i.e., slump, unit weight, air content, and setting time) and hardened properties (i.e., compressive strength, chloride penetrability, and air permeability) were determined. The hypothesis behind this study is that when other parameters are kept constant, concrete properties such as strength, chloride penetration, and air permeability will not be improved significantly by increasing the cement after a minimum cement content is used. The study found that about 1.5 times more paste is required than voids between the aggregates to obtain a minimum workability. Below this value, water-reducing admixtures are of no benefit. Increasing paste thereafter increased workability. In addition, for a given w/c, increasing cementitious content does not significantly improve compressive strength once the critical minimum has been provided. The critical value is about twice the voids content of the aggregate system. Finally, for a given w/c, increasing paste content increases chloride penetrability and air permeability.
Resumo:
This research was initiated to identify methods of reducing the occurrence of transverse cracking. Eight (four repetitive) research sections were established to study three variations in the asphalt concrete pavement. The first variation was the comparison of low- and high-temperature-susceptible asphalt cement (AC) from two different sources. The second variable was to saw and seal transverse joints at spacings varying from 40 to 100 ft. The third variable was to increase the AC content in the asphalt treated base by 1 percent. The research sections were constructed with relatively few problems. Crack and joint surveys have been conducted on all research sections at intervals of less than 1 year since construction. No cracking was identified after the first winter season. The sawed joints also remained sealed through the first winter. At an age of approximately 1 1/2 years there was substantial cracking of the high-temperature-susceptible AC sections and substantial failure of the sealant material in the sawed joints. After almost 4 years, the asphalt pavement constructed with the high-temperature-susceptible AC produced a crack interval of 35 ft, the low-temperature-susceptible AC yielded an interval of 170 ft, and the low-temperature-susceptible AC with an increased AC content yielded an interval of 528 ft. The Pen-Vis number is an effective measure of temperature susceptibility of asphalt cements. The frequency of transverse cracking is affected by the temperature susceptibility of the AC. An increased AC content also reduces the frequency of transverse cracking.
Resumo:
The major objective of this research project was to investigate how Iowa fly ashes influenced the chemical durability of portland cement based materials. Chemical durability has become an area of uncertainty because of the winter application of deicer salts (rock salts) that contain a significant amount of sulfate impurities. The sulfate durability testing program consisted of monitoring portland cement-fly ash paste, mortar and concrete test specimens that had been subjected to aqueous solutions containing various concentrations of salts (both sulfate and chloride). The paste and mortar specimens were monitored for length as a function of time. The concrete test specimens were monitored for length, relative dynamic modulus and mass as a function of time. The alkali-aggregate reactivity testing program consisted of monitoring the expansion of ASTM C311 mortar bar specimens that contained three different aggregates (Pyrex glass, Oreapolis and standard Ottawa sand). The results of the sulfate durability study indicated that the paste and concrete test specimens tended to exhibit surface spalling but only very slow expansive tendencies. This suggested that the permeability of the test specimens was controlling the rate of deterioration. Concrete specimens are still being monitored because the majority of the test specimens have expanded less than 0.05%; hence, this makes it difficult to estimate the service life of the concrete test specimens or to quantify the performance of the different fly ashes that were used in the study. The results of the mortar bar studies indicated that the chemical composition of the various fly ashes did have an influence on their sulfate resistance. Typically, Clinton and Louisa fly ashes performed the best, followed by the Ottumwa, Neal 4 and then Council Bluffs fly ashes. Council Bluffs fly ash was the only fly ash that consistently reduced the sulfate resistance of the many different mortar specimens that were investigated during this study. None of the trends that were observed in the mortar bar studies have yet become evident in the concrete phase of this project. The results of the alkali-aggregate study indicated that the Oreapolis aggregate is not very sensitive to alkali attack. Two of the fly ashes, Council Bluffs and Ottumwa, tended to increase the expansion of mortar bar specimens that contained the Oreapolis aggregate. However, it was not clear if the additional expansion was due to the alkali content of the fly ash, the periclase content of the fly ash or the cristobalite content of the fly ash, since all three of these factors have been found to influence the test results.
Resumo:
The Troxler 3241-B Asphalt Content Gauge is intended for rapidly determining the bitumen content of bituminous paving mixtures. A 300 Millicurie Americuium 241: Beryllium source emitts neutrons which are affected by the hydrogen in the mix. The affected neutrons are detected by Helium 3 detectors, counted and computed into a percentage bitumen of the asphalt mix. The current methods of determining the bitumen content of bituminous paving mixtures requires the use of potentially hazardous chemicals and several hours of testing time. When extracted aggregates are not needed, determination of the bitumen content of a paving mixture by the nuclear method may be easier, quicker and potentially safer. The objective of the project is to study the accuracy of the Troxler 3241-B Nuclear Asphalt Content Gauge in measuring the asphalt cement (AC) content of asphalt concrete mixtures produced with different asphalt cements and different aggregates.
Resumo:
Due to the hazardous nature of chemical asphalt extraction agents, nuclear gauges have become an increasingly popular method of determining the asphalt content of a bituminous mix. This report details the results of comparisons made between intended, tank stick, extracted, and nuclear asphalt content determinations. A total of 315 sets of comparisons were made on samples that represented 110 individual mix designs and 99 paving projects. All samples were taken from 1987 construction projects. In addition to the comparisons made, seventeen asphalt cement samples were recovered for determination of penetration and viscosity. Results were compared to similar tests performed on the asphalt assurance samples in an attempt to determine the amount of asphalt hardening that can be expected due to the hot mix process. Conclusions of the report are: 1. Compared to the reflux extraction procedure, nuclear asphalt content gauges determine asphalt content of bituminous mixes with much greater accuracy and comparable precision. 2. As a means for determining asphalt content, the nuclear procedure should be used as an alternate to chemical extractions whenever possible. 3. Based on penetration and viscosity results, softer grade asphalts undergo a greater degree 'of hardening due to hot mix processing than do harder grades, and asphalt viscosity changes caused by the mixing process are subject to much more variability than are changes in penetration. 4. Based on changes in penetration and viscosity, the Thin Film Oven Test provides a reasonable means of estimating how much asphalt hardening can be anticipated due to exposure to the hot mix processing environment.
Resumo:
The Lane-Wells Road Logger was utilized primarily to determine the feasibility of employing such a device for moisture and density control in Iowa highway construction. A secondary objective was the use of the Road Logger to obtain information concerning moisture content and density during and after construction. Correlation studies with conventional test results required a small portion of the lease period. Practically all phases of construction and most materials utilized in base and surface courses were surveyed. Results of this study were good, in general, with the Road Logger indicating dry density slightly higher and the moisture content slightly lower than conventional results in most instances. Economic feasibility seemed to pose the greatest problem for the acceptance of the Road Logger as a standard compaction control device. It would appear from the findings of this study that probably only large projects, or several smaller contracts tested simultaneously, could justify the expense of the Logger. A total of about 128 miles were surveyed with the Logger during the lease period. Approximately 16 days of downtime due to minor breakdowns were recorded. Inclement weather forcing construction delays resulted in several idle days in which the Logger's full capabilities were not realized.
Resumo:
Based on results of an evaluation performed during the winter of 1985-86, six Troxler 3241-B Asphalt Content Gauges were purchased for District use in monitoring project asphalt contents. Use of these gauges will help reduce the need for chemical based extractions. Effective use of the gauges depends on the accurate preparation and transfer of project mix calibrations from the Central Lab to the Districts. The objective of this project was to evaluate the precision and accuracy of a gauge in determining asphalt contents and to develop a mix calibration transfer procedure for implementation during the 1987 construction. The first part of the study was accomplished by preparing mix calibrations in the Central Lab gauge and taking multiple measurements of a sample with known asphalt content. The second part was accomplished by preparing transfer pans, obtaining count data on the pans using each gauge, and transferring calibrations from one gauge to another through the use of calibration transfer equations. The transferred calibrations were tested by measuring samples with a known asphalt content. The study established that the Troxler 3241-B Asphalt Content Gauge yields results of acceptable accuracy and precision as evidenced by a standard deviation of 0.04% asphalt content on multiple measurements of the same sample. The calibration transfer procedure proved feasible and resulted in the calibration transfer portion of Materials I.M. 335 - Method of Test For Determining the Asphalt Content of Bituminous Mixtures by the Nuclear Method.
Resumo:
Plastic air content is typically tested by the pressure method, ASTM C138. Loss of air content through the paver has been shown to exceed 2 percent at times. Research has shown that early deterioration of pavements in Iowa may be directly or indirectly related to low or inadequate air content. Hardened air content is typically checked using the linear traverse method, ASTM C457. The linear traverse method is very time consuming and could not be used on a production scale. A quick and effective method of testing in place air content is needed. Research has shown a high degree of correlation with the high-pressure method of determining air content of hardened concrete versus plastic air content in laboratory conditions. This research indicated that air contents are more variable when comparing core results to plastic air content, although the overall average for the air content was comparable. Perhaps, the location of the plastic air content test, obtained from construction records, versus location of the cores was not as accurate as needed.
Resumo:
The main objective of this study is to determine the effectiveness of the Electrochemical Chloride Extraction (ECE) technique on a bridge deck with very high concentrations of chloride. This ECE technique was used during the summer of 2003 to reverse the effects of corrosion, which had occurred in the reinforcing steel embedded in the pedestrian bridge deck over Highway 6, along Iowa Avenue, in Iowa City, Iowa, USA. First, the half cell potential was measured to determine the existing corrosion level in the field. The half-cell potential values were in the indecisive range of corrosion (between -200 mV and -350 mV). The ECE technique was then applied to remove the chloride from the bridge deck. The chloride content in the deck was significantly reduced from 25 lb/cy to 4.96 lb/cy in 8 weeks. Concrete cores obtained from the deck were measured for their compressive strengths and there was no reduction in strength due to the ECE technique. Laboratory tests were also performed to demonstrate the effectiveness of the ECE process. In order to simulate the corrosion in the bridge deck, two reinforced slabs and 12 reinforced beams were prepared. First, the half-cell potentials were measured from the test specimens and they all ranged below -200 mV. Upon introduction of 3% salt solution, the potential reached up to -500 mV. This potential was maintained while a salt solution was being added for six months. The ECE technique was then applied to the test specimens in order to remove the chloride from them. Half-cell potential was measured to determine if the ECE technique can effectively reduce the level of corrosion.
Resumo:
The main objective of this research is to examine the effects that different methods of RAP stockpile fractionation would have on the volumetric mix design properties for high-RAP content surface mixes, with the goal of meeting all specified criteria for standard HMA mix designs. To determine the distribution of fine aggregates and binder in RAP stockpile, RAP materials were divided by each sieve size. The composition of RAP materials retained on each sieve was analyzed to determine the optimum fractionation method. Fractionation methods were designed to separate the stockpile at a specified sieve size to control the amount of fine RAP materials which contain higher amounts of fine aggregates and dust contents. These fine RAP materials were used in reduced proportions or completely eliminated, thereby decreasing the amount of fine aggregate materials introduced to the mix. Mix designs were performed using RAP materials from four different stockpiles and the two fractionated methods were used with high-RAP contents up to 50% by virgin binder replacement. By using a fractionation method, a mix with up to 50% RAP was successfully designed while meeting all Superpave criteria and asphalt film thickness requirement by controlling the dust content from RAP stockpiles.