3 resultados para Wear-Ever Aluminum Roaster.
em Iowa Publications Online (IPO) - State Library, State of Iowa (Iowa), United States
Resumo:
This report presents the results of surveys to determine studded tire usage in Iowa. Also reported are the results of measurements of transverse pavement profiles at selected locations where the pavement is subjected to a high volume of traffic. The surveys were made in January of each of the years 1969 through 1978 and in each of 27 areas into which the state was divided. Estimates of studded tire usage were also made at various locations on Interstate highways in Iowa. The lowest percentage of studded tires was observed in the initial count during the winter of 1968-69. Two years later the percentage had increased to the maximum (22.6%) and then began a gradual decline. The latest count in January of 1978 indicated 8.5% of the cars had studded tires. The decline in the use of studded tires is attributed to the efforts of the Iowa DOT and others to obtain a ban on studded tires and a continual increase in the use of radial tires with claims of improved traction. The wear measurements were recorded by camera. It was found that studded tires have worn ruts in Iowa pavements as deep as 5/16 inch. The ruts lead to water on the pavement and this causes hydroplaning, as well as splash and spray. The conclusion of the study was that studded tires should be banned in Iowa.
Resumo:
This report addresses the field testing and analysis of those results to establish the behavior of the original Clive Road Bridge that carried highway traffic over Interstate 80 (I-80) in the northwest region of Des Moines, Iowa. The bridge was load tested in 1959, shortly after its construction and in 1993, just prior to its demolition. This report presents some of the results from both field tests, finite element predictions of the behavior of aluminum bridge girders, and load distribution studies.
Resumo:
In 1957, the Iowa State Highway Commission, with financial assistance from the aluminum industry, constructed a 220-ft (67-m) long, four-span continuous, aluminum girder bridge to carry traffic on Clive Road (86th Street) over Interstate 80 near Des Moines, Iowa. The bridge had four, welded I-shape girders that were fabricated in pairs with welded diaphragms between an exterior and an interior girder. The interior diaphragms between the girder pairs were bolted to girder brackets. A composite, reinforced concrete deck served as the roadway surface. The bridge, which had performed successfully for about 35 years of service, was removed in the fall of 1993 to make way for an interchange at the same location. Prior to the bridge demolition, load tests were conducted to monitor girder and diaphragm bending strains and deflections in the northern end span. Fatigue testing of the aluminum girders that were removed from the end spans were conducted by applying constant-amplitude, cyclic loads. These tests established the fatigue strength of an existing, welded, flange-splice detail and added, welded, flange-cover plates and horizontal web plate attachment details. This part, Part 2, of the final report focuses on the fatigue tests of the aluminum girder sections that were removed from the bridge and on the analysis of the experimental data to establish the fatigue strength of full-size specimens. Seventeen fatigue fractures that were classified as Category E weld details developed in the seven girder test specimens. Linear regression analyses of the fatigue test results established both nominal and experimental stress-range versus load cycle relationships (SN curves) for the fatigue strength of fillet-welded connections. The nominal strength SN curve obtained by this research essentially matched the SN curve for Category E aluminum weldments given in the AASHTO LRFD specifications. All of the Category E fatigue fractures that developed in the girder test specimens satisfied the allowable SN relationship specified by the fatigue provisions of the Aluminum Association. The lower-bound strength line that was set at two standard deviations below the least squares regression line through the fatigue fracture data points related well with the Aluminum Association SN curve. The results from the experimental tests of this research have provided additional information regarding behavioral characteristics of full-size, aluminum members and have confirmed that aluminum has the strength properties needed for highway bridge girders.