18 resultados para Transverse Shear
em Iowa Publications Online (IPO) - State Library, State of Iowa (Iowa), United States
Resumo:
The members of the Iowa Concrete Paving Association, the National Concrete Pavement Technology Center Research Committee, and the Iowa Highway Research Board commissioned a study to examine alternative ways of developing transverse joints in portland cement concrete pavements. The present study investigated six separate variations of vertical metal strips placed above and below the dowels in conventional baskets. In addition, the study investigated existing patented assemblies and a new assembly developed in Spain and used in Australia. The metal assemblies were placed in a new pavement and allowed to stay in place for 30 days before the Iowa Department of Transportation staff terminated the test by directing the contractor to saw and seal the joints. This report describes the design, construction, testing, and conclusions of the project.
Resumo:
Load transfer across transverse joints has always been a factor contributing to the useful life of concrete pavements. For many years, round steel dowels have been the conventional load transfer mechanism. Many problems have been associated with the round steel dowels. The most detrimental effect of the steel dowel is corrosion. Repeated loading over time also damages joints. When a dowel is repeatedly loaded over a long period of time, the high bearing stresses found at the top and bottom edge of a bar erode the surrounding concrete. This oblonging creates multiple problems in the joint. Over the past decade, Iowa State University has performed extensive research on new dowel shapes and materials to mitigate the effects of oblonging and corrosion. This report evaluates the bearing stress performance of six different dowel bar types subjected to two different shear load laboratory test methods. The first load test is the AASHTO T253 method. The second procedure is an experimental cantilevered dowel test. The major objective was to investigate and improve the current AASHTO T253 test method for determining the modulus of dowel support, k0. The modified AASHTO test procedure was examined alongside an experimental cantilever dowel test. The modified AASHTO specimens were also subjected to a small-scale fatigue test in order to simulate long-term dowel behavior with respect to concrete joint damage. Loss on ignition tests were also performed on the GFRP dowel specimens to determine the resin content percentage. The study concluded that all of the tested dowel bar shapes and materials were adequate with respect to performance under shear loading. The modified AASHTO method yielded more desirable results than the ones obtained from the cantilever test. The investigators determined that the experimental cantilever test was not a satisfactory test method to replace or verify the AASHTO T253 method.
Resumo:
In July 2006, construction began on an accelerated bridge project in Boone County, Iowa that was composed of precast substructure elements and an innovative, precast deck panel system. The superstructure system consisted of full-depth deck panels that were prestressed in the transverse direction, and after installation on the prestressed concrete girders, post-tensioned in the longitudinal direction. Prior to construction, laboratory tests were completed on the precast abutment and pier cap elements. The substructure testing was to determine the punching shear strength of the elements. Post-tensioning testing and verification of the precast deck system was performed in the field. The forces in the tendons provided by the contractor were verified and losses due to the post-tensioning operation were measured. The stress (strain) distribution in the deck panels due to the post-tensioning was also measured and analyzed. The entire construction process for this bridge system was documented. Representatives from the Boone County Engineers Office, the prime contractor, precast fabricator, and researchers from Iowa State University provided feedback and suggestions for improving the constructability of this design.
Resumo:
Experiments with early entry light sawing of Portland cement concrete (PCC) contraction joints began in Iowa in 1989. Since that time, changes in early sawing equipment have occurred as well as changes in specifications for sawing. The option to use early sawing for transverse contraction joints was specified in 1992. A problem happening occasionally with early sawing was the break out of some of the concrete around the end of the joint as the saw blade approached the edge of the slab. To prevent this, it was proposed that the sawing would terminate approximately 1/2" to 3/4" before the edge of the slab, creating a "short joint". This procedure would also leave a concrete "dam" to prevent the run-out and waste of the hot liquid joint sealant onto the shoulder. It would also eliminate the need for the labor and material for applying a duct tape dam at the open ends of each sawed joint to stop hot liquid sealant run-out Agreements were made with the contractor to apply the "short joint" technique for 1 day of paving. The evaluation and results are compared with an adjoining control section. The research found no negative aspects from sawing the "short joint". Three specific findings were noted. They are the following: 1) No joint end "blow-out" spalls of concrete occurred. 2) The need for the duct tape dam to stop liquid sealant overflow was eliminated. 3) Joint end corner spalls appear to be caused mainly by construction shouldering operations equipment. The "short joint" sawing technique can be routinely applied to early entry sawed transverse contraction joints with expectations of only positive results.
Resumo:
The use of non-metallic load transfer and reinforcement devices for concrete highway pavements is a possible alternative to avoid corrosion problems related to the current practice of steel materials. Laboratory and field testing of highway pavement dowel bars, made of both steel and fiber composite materials, and fiber composite tie rods were carried out in this research investigation. Fatigue, static, and dynamic testing was performed on full-scale concrete pavement slabs which were supported by a simulated subgrade and which included a single transverse joint. The bahavior of the full-scale specimens with both steel and fiber composite dowels placed in the test joints was monitored during several million load cycles which simulated truck traffic at a transverse joint. Static bond tests were conducted on fiber composite tie rods to determine the required embedment length. These tests took the form of bending tests which included curvature and shear in the embedment zone and pullout tests which subjected the test specimen to axial tension only. Fiber composite dowel bars were placed at two transverse joints during construction of a new concrete highway pavement in order to evaluate their performance under actual field conditions. Fiber composite tie rods were also placed in the longitudinal joint between the two fiber composite doweled transverse joints.
Resumo:
The Iowa Department of Transportation (DOT) is continually improving the pavement management program and striving to reduce maintenance needs. Through a 1979 pavement management study, the Iowa DOT became a participant in a five state Federal Highway Administration (FHWA) study of "Transverse Cracking of Asphalt Pavements". There were numerous conclusions and recommendations but no agreement as to the major factors contributing to transverse cracking or methods of preventing or reducing the occurrence of transverse cracking. The project did focus attention on the problem and generated ideas for research. This project is one of two state funded research projects that were a direct result of the FHWA project. Iowa DOT personnel had been monitoring temperature susceptibility of asphalt cements by the Norman McLeod Modified Penetration Index. Even though there are many variables from one asphalt mix to another, the trend seemed to indicate that the frequency of transverse cracking was highly dependent on the temperature susceptibility. Research project HR-217 "Reducing the Adverse Effects of Transverse Cracking" was initiated to verify the concept. A final report has been published after a four-year evaluation. The crack frequency with the high temperature susceptible asphalt cement was substantially greater than for the low temperature susceptible asphalt cement. An increased asphalt cement content in the asphalt treated base also reduced the crack frequency. This research on prevention of transverse cracking with fabric supports the following conclusions: 1. Engineering fabric does not prevent transverse cracking of asphalt cement concrete. 2. Engineering fabric may retard the occurrence of transverse cracking. 3. Engineering fabric does not contribute significantly to the structural capability of an asphalt concrete pavement.
Resumo:
This research was initiated to identify methods of reducing the occurrence of transverse cracking. Eight (four repetitive) research sections were established to study three variations in the asphalt concrete pavement. The first variation was the comparison of low- and high-temperature-susceptible asphalt cement (AC) from two different sources. The second variable was to saw and seal transverse joints at spacings varying from 40 to 100 ft. The third variable was to increase the AC content in the asphalt treated base by 1 percent. The research sections were constructed with relatively few problems. Crack and joint surveys have been conducted on all research sections at intervals of less than 1 year since construction. No cracking was identified after the first winter season. The sawed joints also remained sealed through the first winter. At an age of approximately 1 1/2 years there was substantial cracking of the high-temperature-susceptible AC sections and substantial failure of the sealant material in the sawed joints. After almost 4 years, the asphalt pavement constructed with the high-temperature-susceptible AC produced a crack interval of 35 ft, the low-temperature-susceptible AC yielded an interval of 170 ft, and the low-temperature-susceptible AC with an increased AC content yielded an interval of 528 ft. The Pen-Vis number is an effective measure of temperature susceptibility of asphalt cements. The frequency of transverse cracking is affected by the temperature susceptibility of the AC. An increased AC content also reduces the frequency of transverse cracking.
Resumo:
The need for upgrading a large number of understrength bridges in the United States has been well documented in the literature. This manual presents two methods for strengthening continuous-span composite bridges: post-tensioning of the positive moment regions of the bridge stringers and the addition of superimposed trusses at the piers. The use of these two systems is an efficient method of reducing flexural overstresses in undercapacity bridges. Before strengthening a given bridge however, other deficiencies (inadequate shear connection, fatigue problems, extensive corrosion) should be addressed. Since continuous-span composite bridges are indeterminant structures, there is longitudinal and transverse distribution of the strengthening axial forces and moments. This manual basically provides the engineer with a procedure for determining the distribution of strengthening forces and moments throughout the bridge. As a result of the longitudinal and transverse force distribution, the design methodology presented in this manual for continuous-span composite bridges is extremely complex. To simplify the procedure, a spreadsheet has been developed for use by practicing engineers. This design aid greatly simplifies the design of a strengthening system for a given bridge in that it eliminates numerous tedious hand calculations, computes the required force and moment fractions, and performs the necessary iterations for determining the required strengthening forces. The force and moment distribution fraction formulas developed in this manual are primarily for the Iowa DOT V12 and V14 three-span four-stringer bridges. These formulas may be used on other bridges if they are within the limits stated in this manual. Use of the distribution fraction formulas for bridges not within the stated limits is not recommended.
Resumo:
There are many miles of portland cement concrete pavement in Iowa that due to normal wear, and in some cases accelerated wear from studded tires, the surface has become polished resulting in less than desirable friction values. Retexturing the surface may be an economical way to re-establish desirable friction values. Retexturing by grinding with diamond blades and transverse grooving with diamond blades are two methods of rehabilitating p.c.c. surfaces. MU Inc. of Lebanan, Tennessee proposed to provide without charge to the Iowa Department of Transportation, one 1500 ft x 12 ft section each of three methods of texturing. They are longitudinal grinding, transverse grooving and longitudinal grinding followed by transverse grooving. A section of 1500 feet is needed to properly evaluate a texturing method. It was decided by Iowa DOT personnel that due to possible differential friction it would be undesirable to texture only one lane. The decision was made to do test sections of 1500 ft x 24 ft with the cost of the additional texturing paid by the Iowa DOT. Iowa also has areas where the p.c.c. pavement has faulted at the joints and cracks which results in poor riding quality. Methods of correcting the faulting are to underseal the pavement where needed and/or grinding the surface to eliminate the faulted areas. It was decided to include in this research project a section for profiling by grinding.
Resumo:
The objective of this research project was to identify a method of reducing the adverse effect of transverse cracking and to improve the performance of asphalt pavement. The research involved three variations from the contractor's planned operation. Briefly, they were: (1) use of another asphalt cement; (2) saw and seal transverse joints; and (3) increased asphalt cement content. The following conclusions were reached: (1) an improved sealant or sealing procedure is needed if transverse joints are to be used in asphalt pavements; (2) the penetration-viscosity number (PVN) is an effective measure of the temperature susceptibility of asphalt cements; (3) the use of a high temperature susceptible asphalt cement produced severe transverse cracking; (4) the use of asphalt cements with low temperature susceptibility will reduce the frequency of transverse cracking; and (5) an increased asphalt cement content in the asphalt treated base will reduce the frequency of transverse cracking.
Resumo:
Triaxial compression tests of two crushed limestones of differing highway service records indicate a fundamental difference in their shear strength -- void ratio relationship. Analyses were based on stress parameters at minimum sample volume, i.e., before there was significant sample dilation due to shear. The better service record sample compacted to higher density, and had a high effective angle of internal friction and zero effective cohesion. The other sample compacted to lower density and had a lower friction angle, but gained significant stability from effective cohesion. Repeated loading-unloading cycles reduced the cohesion, apparently due to modification of the sample structure. Extrapolations of the results to zero void ratio agree with sliding friction data reported on calcite, or with triaxial parameters reported on carbonate rocks.
Resumo:
The objective of this research was to evaluate the performance of portland cement concrete pavement contraction joints utilizing a variety of sealants and joint preparations and to identify an effective sealant system. The variables evaluated were: (1) sealant material; (2) joint preparation; (3) size of saw cut (sealant reservoir); and (4) the use of backing material. This progress report contains project results to date.
Resumo:
To conserve natural resources and energy, the amount of recycled asphalt pavement has been steadily increasing in the construction of asphalt pavements. The objective of this study is to develop quality standards for inclusion of high RAP content. To determine if the higher percentage of RAP materials can be used on Iowa’s state highways, three test sections with target amounts of RAP materials of 30%, 35% and 40% by weight were constructed on Highway 6 in Iowa City. To meet Superpave mix design requirements for mixtures with high RAP contents, it was necessary to fractionate the RAP materials. Three test sections with actual RAP materials of 30.0%, 35.5% and 39.2% by weight were constructed and the average field densities from the cores were measured as 95.3%, 94.0%, and 94.3%, respectively. Field mixtures were compacted in the laboratory to evaluate moisture sensitivity using a Hamburg Wheel Tracking Device. After 20,000 passes, rut depths were less than 3mm for mixtures obtained from three test sections. The binder was extracted from the field mixtures from each test section and tested to identify the effects of RAP materials on the performance grade of the virgin binder. Based on Dynamic Shear Rheometer and Bending Beam Rheometer tests, the virgin binders (PG 64-28) from test sections with 30.0%, 35.5% and 39.2% RAP materials were stiffened to PG 76-22, PG 76-16, and PG 82-16, respectively. The Semi-Circular Bending (SCB) test was performed on laboratory compacted field mixtures with RAP amounts of 30.0%, 35.5% and 39.2% at two different temperatures of -18 and -30 °C. As the test temperature decreased, the fracture energy decreased and the stiffness increased. As the RAP amount increased, the stiffness increased and the fracture energy decreased. Finally, a condition survey of the test sections was conducted to evaluate their short-term pavement performance and the reflective transverse cracking did not increase as RAP amount was increased from 30.0% to 39.2%.
Resumo:
Iowa's first portland cement concrete pavement was constructed in 1904 in the City of LeMars. A portion of that pavement served traffic until 1974 at which time it was resurfaced. The first rural Iowa pee pavement (16' wide, 6" to 7" thick) was constructed under the direction of the Iowa State Highway Commission in 1913. Some of Iowa's early pavements had transverse joints at 25-foot spacings. At that time, joint spacings across the nation ranged from 24 to 100 ft. There have been many changes in joint design over the years with some pavements being constructed without transverse joints. Joint spacing on Iowa primary pavements has generally remained around 20 feet with this spacing having been adopted as an Iowa standard in 1954. Until 1978 it was common to specify a 40-foot joint spacing on secondary pavements. The performance of the pavements with joint spacings greater than 20 feet, and in some cases no contraction joints, generated a 1955 research project on joint spacing. This project was 16 miles long containing sections without contraction joints and sections with joints sawed at intervals of 20, 50 and 80 feet. Approximately half of the sawed joints were left unsealed. The results of this research supported the 20-foot spacing, but were inconclusive regarding the benefits of sealing. One of the desired characteristics of joint sealing material is that it should act as a moisture barrier and prevent the intrusion of surface water. It was generally accepted from past experience that the hot poured type joint seals did not provide this effective moisture barrier.
Resumo:
Concern about premature joint sealant failures occurring in portland cement concrete (PCC) pavements gave impetus to initiating this research project. Eight sealants, including three silicone sealants, were evaluated and tested in the lab as well as incorporated in approximately 700 joints in the field and evaluated over a six-year period. The preliminary data show that among the silicone sealants, Dow Corning 888 rated the highest. However, this was rated third overall behind the W. R. Meadows cold-applied Sof Seal and Crafco #231 hot pour sealants. The W. R. Meadows and Crafco sealants cost approximately 30 percent and 50 percent less to furnish and place than the Dow Corning product. All joint sealants will continue to be evaluated.